944 resultados para OPTICAL CRYSTAL


Relevância:

30.00% 30.00%

Publicador:

Resumo:

Growth-induced defects in Yb:FAP crystals grown by the Czochralski method have been investigated by optical microscopy, chemical etching, scanning electron microscopy (SEM) and energy-dispersive spectroscopy (EDS). Anisotropic etching features have been observed on two FAP crystal planes: (0001) and (1010). The shape of etch pits on the (0001) plane is hexagonal, while the etch pits on the (1010) plane have a variety of irregular shapes. It is also found that the density of etch pit varies along the boule. Based on the experimental observations, the formation mechanisnis of growth defects are discussed, and methods for reducing the growth-induced defect concentration is proposed. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

ZnO thin films were grown on single-crystal gamma-LiAlO2 (LAO) and sapphire (0001) substrate by pulsed laser deposition (PLD). The structural, optical and electrical properties of ZnO films were investigated. The results show that LAO is more suitable for fabricating ZnO films than sapphire substrate and the highest-quality ZnO film was attained on LAO at the substrate temperature of 550 degrees C. However, when the substrate temperature rises to 700 degrees C, lithium would diffuse from the substrate (LAO) into ZnO film which makes ZnO film on LAO becomes polycrystalline without preferred orientation, the stress in ZnO film increases dominantly and the resistivity of the film decreases exponentially. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

High-quality neodymium doped GGG laser crystals have been grown by Czochralski (Cz) method. Results of Nd:GGG thin chip laser operating at 1.064 μm pumped by Ti:sapphire laser operating at 808 nm were reported. The slop efficiency was as high as 20%.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

gamma-LiAlO2 (LAO) single crystal has been grown by the Czochralski method. However, its quality was deteriorated due to lithium volatilization during the crystal growth. The full width at half maximum value drops from 116.9 to 44.2 arc sec after the LAO slice was treated by vapor transport equilibration at 1000, 1100, and 1200 degrees C/48 h in sequence. The treated slice shows higher optical transmission than the as-grown one in the measured wavelength range of 190-1900 nm, meanwhile, its absorption edge exhibits a blueshift. According to Raman spectra, the treated slice has homogeneous quality at different depths from surface to 0.01 mm. The expansion coefficient of the treated slice for a axis drops from 17.2398x10(-6)/degrees C to 16.5240x10(-6)/degrees C, and that for c axis drops from 10.7664x10(-6)/degrees C to 10.0786x10(-6)/degrees C.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The Yb (10%):GGG and Yb (30%): GGG crystals have been grown by the Czochralski method. The chemical compositions are: Yb1.07Gd1.74Ga5.19O12 and Yb0.33Gd1.47Ga5.2O12. The absorption and emission spectra of Yb:GGG crystal at room temperature have been measured. The spectroscopic parameters of Yb:GGG and Yb:YAG have been compared. Optical absorption spectra of Yb:GGG show 4f-4f transitions related to Gd3+ ion around 300 nm, and also an onset of charge transfer (CT) transitions from oxygen ligands to Gd3+ or Yb3+ cations below 240nm. The CT absorption of Yb3+ is largely overlapped by that of Gd3+ ions. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

By using an Ar+ ion laser, a tunable Rh 6G dye laser(Linewidth : 0.5 cm(-1)) and a Coherent 899-21 dye laser as light sources and using a monochromator and a phase-locking amplifier, the optical properties of Eu3+ : Y2SiO5 crystal were detected. Persistent spectral hole burning (PSHB) were also observed in (5)Do-(7)Fo transition in the crystal at the temperature of 16 K. For 15 mW dye laser (Wavelength : 579.62 nm) burning the crystal for 0.1 s a spectral hole with about 80 MHz hole width were detected and the hole can been keep for longer than 10 h.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Absorption and emission spectral properties of GdVO4 single crystal doped with Ho3+ ions were investigated at room temperature. Polarized absorption cross section is calculated in the range of 400-2200nm. Results were analyzed and parameters were calculated based on Judd-Ofelt theory, the emission spectrum shows that the emission intensity around the wavelength of 546 nm associated with transition S-5(2) -> I-5(8) is much stronger than other bands in the observed range and potentially enable the green light output around this emission band in this crystal. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Transparent polycrystalline Nd:YAG ceramics were fabricated by solid-state reactive sintering a mixture of commercial Al2O3,Y2O3, and Nd2O3 powders. The powders were mixed in ethanol and doped with 0.5 wt% tetraethoxysilane, dried, and pressed. Pressed samples were sintered at 1750 degrees C in vacuum. Transparent fully dense samples with average grain sizes of 10 mu m were obtained. The 1 at.% Nd:YAG ceramic was used to research passively Q-switched laser output with a Cr4+:YAG crystal as a saturable absorber. An average output power of 94 mW with a pulse width of 50 ns was obtained when the incident pump power was 750 mW. The slope efficiency was 13%. The pulse energy is 5 mu J, and the peak power is about 100 W.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

For the first time, a high optical quality Yb3+-doped lutetium pyrosilicate laser crystal Lu2Si2O7 (LPS) was grown by the Czochralski (Cz) method. The segregation coefficient of ytterbium ion in Yb:LPS crystal detected by the inductively coupled plasma atomic emission spectrometer (TCP-AES) method is equal to 0.847. X-ray powder diffraction result confirms the C2/m phase monoclinic space group of the grown crystal and the peaks corresponding to different phases were indexed. The absorption and fluorescence spectra, as well as fluorescence decay lifetime of Yb3+ ion in LPS have been investigated. The absorption and fluorescence cross-sections of the transitions F-2(7/2) <-> F-2(5/2) of Yb3+ ion in LPS crystal have been determined. The advantages of the Yb:LPS crystal including high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections (1.33 x 10(-2) cm(2)) and particularly broad emission bandwidth (similar to 62 nm) indicated that the Yb:LPS crystal seemed to be a promising candidate used as compact, efficient thin chip lasers when LD is pumped at 940 and 980 nm due to its low-symmetry monoclinic structure and single crystallographic site. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Spectroscopic properties of Ce-doped yttrium orthoaluminate (Ce:YAlO3 or Ce:YAP) crystals grown by temperature gradient technique (TGT) were investigated, and the effects of the growth conditions on the properties were analyzed.. Methods of optical absorption (OA), photoluminescence (PL), photoluminescence decay (PLD), X-ray excited luminescence (XL) and cathodeluminescence (CL) were used in these investigations. The results showed that the absorption band peak at 202, 394 and 532 nm originated from F and F+ color center induced by the weak reducing growth atmosphere, green emission band near 500 ran derived from Ce3+ -Ce3+ pairs and band at 650 similar to 850 run from some unintentional impurity in crystals.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Passive Q-switching of a diode-pumped Yb:LYSO laser at 1060 nm with a Yb3+ ions-doped CaF2 crystal without the excited-state absorption (ESA) was demonstrated. An average output power of 174 mW with pulse duration of 5.6 mu s and repetition rate of 27 kHz have been obtained under the unoptimized conditions. And the Q-switching conversion efficiency was as high as 51.7%. (c) 2007 Optical Society of America.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

We report the measured group delay dispersion (GDD) of new crystals Yb:Gd2SiO5 (Yb:GSO), Yb:GdYSiO5 (Yb:GYSO) and Yb:LuYSiO5 (Yb:LYSO) over wavelengths from 1000nm to 1200nm, with a white-light interferometer. Those GDD data should be useful for the dispersion compensation for femtosecond pulse generation in the lasers with these new crystals as the gain media. (C) 2007 Optical Society of America

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this paper, single crystal of ytterbium (Yb) doped Ca-5(PO4)(3)F (FAP) has been grown along the c-axis by using the Czochralski method. The segregation coefficients of Yb3+ in the Yb:FAP crystal has been determined by ICP-AES method. The absorption spectrum, fluorescence spectrum and fluorescence lifetime of the Yb:FAP crystal has been also measured at room temperature. In the absorption spectra, there are two absorption bands at 904 and 982 nm, respectively, which are suitable for InGaAs diode laser pumping. The absorption cross-section (sigma(abs)) is 5.117 x 10(-20) cm(2) with an FWHM of 4 nm at 982 nm. The emission cross-section is (sigma(em)) 3.678 x 10(-20) cm(2) at 1042 nm. Favorable values of the absorption cross-section at about 982 nm are promising candidates for laser diode (LD) pumping. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this work, alpha-Al2O3:C, a highly sensitive thermoluminescence dosimetry crystal, was grown by the EFG method in which a graphite heating unit and shield acted as the carbon source during the growth process. The optical, luminescent properties and dosimetric characteristics of the crystal were investigated. The as-grown crystal shows a single glow peak at 536 K, which is associated with Cr3+ ions. After annealing in H-2 at 1673 K for 80 h, the crystal shows a single glow peak at 460 K and a blue emission band at 415 nm. The thermoluminescent response of the annealed crystal shows linear-sublinear-saturation characteristics in the dose range from 5 x 10(-6) to 100 Gy.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

g-LiAlO2 single crystal is a promising substrate for GaN heteroepitaxy. In this paper, we present the growth of large-sized LiAlO2 crystal by modified Czochralski method. The crystal quality was characterized by high-resolution X-ray diffraction and chemical etching. The results show that the as-grown crystal has perfect quality with the full width at half maximum (FWHM) of 17.7-22.6 arcsec and etch pits density of (0.3-2.2) x 10(4) cm(-2) throughout the crystal boule. The bottom of the crystal boule shows the best quality. The optical transmission spectra from UV to IR exhibits that the crystal is transparent from 0.2 to 5.5 mu m and becomes completely absorbing around 6.7 mu m wavelength. The optical absorption edge in near UV region is about 191 nm.