866 resultados para Magnetic carbon composites


Relevância:

40.00% 40.00%

Publicador:

Resumo:

Composites of recycled carbon fiber (CF) with up to 30 wt % loading with polyethylene (PE) were prepared via melt compounding. The morphology of the composites and the degree of dispersion of the CF in the PE matrix was examined using scanning electron microscopy, and revealed the CF to be highly dispersed at all loadings and strong interfacial adhesion to exist between the CF and PE. Raman and FTIR spectroscopy were used to characterize the surface chemistry and potential bonding sites of recycled CF. Both the Young's modulus and ultimate tensile stress increased with increasing CF loading, but the percentage stress at break was unchanged up to 5 wt % loading, then decreased with further successive addition of CF. The effect of CF on the elastic modulus of PE was examined using the Halpin-Tsai and modified Cox models, the former giving a better fit with the values determined experimentally. The electrical conductivity of the PE matrix was enhanced by about 11 orders of magnitude on addition of recycled CF with a percolation threshold of 7 and 15 wt % for 500-mu m and 3-mm thick samples. (c) 2007 Wiley Periodicals, Inc.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Pre-consolidated carbon fibre-reinforced polyphenylene sulphide (CF/PPS) laminates were
thermoformed into V-shaped parts via designed out of autoclave thermoforming experiments.
The different processing conditions tested in the experiment have resulted in final
part angles whose differences ranged from 2.087 to 3.431 from the original mould angle.
The test results show that processing conditions influenced finished part dimensions as the
final sample angles were found to decrease relative to the tooling dimensions, as mould
temperature increases. Higher mould temperature conditions produce thinner parts due
to the thermal expansion of mould tools. The mould temperature of 170C, which can
produce parts with high degree of crystallinity as well as small size of crystal, has been
established as the optimal thermoforming condition for CF/PPS composites.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Despite the increased applications of the composite materials in aerospace due to their exceptional physical and mechanical properties, the machining of composites remains a challenge. Fibre reinforced laminated composites are prone to different damages during machining process such as delamination, fibre pull-out, microcracks, thermal damages. Optimization of the drilling process parameters can reduces the probability of these damages. In the current research, a 3D finite element (FE) model is developed of the process of drilling in the carbon fibre reinforced composite (CFC). The FE model is used to investigate the effects of cutting speed and feed rate on thrust force, torque and delamination in the drilling of carbon fiber reinforced laminated composite. A mesoscale FE model taking into account of the different oriented plies and interfaces has been proposed to predict different damage modes in the plies and delamination. For validation purposes, experimental drilling tests have been performed and compared to the results of the finite element analysis. Using Matlab a digital image analysis code has been developed to assess the delamination factor produced in CFC as a result of drilling. © Springer Science+Business Media B.V. 2011.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Drilling is a major process in the manufacturing of holes required for the assemblies of composite laminates in aerospace industry. Simulation of drilling process is an effective method in optimizing the drill geometry and process parameters in order to improve hole quality and to reduce the drill wear. In this research we have developed three-dimensional (3D) FE model for drilling CFRP. A 3D progressive intra-laminar failure model based on the Hashin's theory is considered. Also an inter-laminar delamination model which includes the onset and growth of delamination by using cohesive contact zone is developed. The developed model with inclusion of the improved delamination model and real drill geometry is used to make comparison between the step drill of different stage ratio and twist drill. Thrust force, torque and work piece stress distributions are estimated to decrease by the use of step drill with high stage ratio. The model indicates that delamination and other workpiece defects could be controlled by selection of suitable step drill geometry. Hence the 3D model could be used as a design tool for drill geometry for minimization of delamination in CFRP drilling. © 2013 Elsevier Ltd.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This study aims to investigate drilling process in carbon-fiber reinforced plastic (CFRP) composites with multilayer TiAlN/TiN PVD-coated tungsten carbide drill. The effect of process parameters have been investigated in drilling of Hexcel M21-T700GC. Thrust force and torque were measured online throughout the drilling experiments. Delamination were observed using optical microscope and analyzed via a developed algorithm based on digital image processing technique. Surface roughness of each hole was measured using a surface profilometer. In addition, the progression of tool wear in various surfaces of drill was observed using tool microscope and measured using image software. Our results indicate that the thrust force and torque increased with the increasing cutting speed and feed rate. Delamination and average surface roughness that rose with the increase in feed rate, however, decreased with the increasing cutting speed. The average surface roughness tended to increase with the increase in feed rate and decrease with the increasing cutting speed in drilling of carbon-fiber reinforced plastic (CFRP). Feed rate was found as the predominant factor on the drilling outputs. Abrasive wear was observed on both flank and relief surfaces, which created edge wear on cutting edges. No sign of chipping or plastic deformation has been observed on the surfaces of drills. © 2012 The Author(s).

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The structure and properties of melt mixed high-density polyethylene/multi-walled carbon nanotube (HDPE/MWCNT) composites processed by compression molding and blown film extrusion were investigated to assess the influence of processing route on properties. The addition of MWCNTs leads to a more elastic response during deformations that result in a more uniform thick-ness distribution in the blown films. Blown film composites exhibit better mechanical properties due to the enhanced orientation and disentanglement of MWCNTs. At a blow up ratio (BUR) of 3 the breaking strength and elongation in the machine direction of the film with 4 wt % MWCNTs are 239% and 1054% higher than those of compression molded (CM) samples. Resistivity of the composite films increases significantly with increasing BURs due to the destruction of conductive pathways. These pathways can be recovered partially using an appropriate annealing process. At 8 wt % MWCNTs, there is a sufficient density of nanotubes to maintain a robust network even at high BURs.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Melt-mixed high density polyethylene (HDPE)/multi-walled carbon nanotube (MWCNT) nanocomposites with 1–10 wt% MWCNTs were prepared by twin screw extrusion and compression moulded into sheet form. The compression moulded nanocomposites exhibit a 112% increase in modulus at a MWCNT loading of 4 wt%, and a low electrical percolation threshold of 1.9 wt%. Subsequently, uniaxial, sequential (seq-) biaxial and simultaneous (sim-) biaxial stretching of the virgin HDPE and nanocomposite sheets was conducted at different strain rates and stretching temperatures to investigate the processability of HDPE with the addition of nanotubes and the influence of deformation on the structure and final properties of nanocomposites. The results show that the processability of HDPE is improved under all the uniaxial and biaxial deformation conditions due to a strengthened strain hardening behaviour with the addition of MWCNTs. Extensional deformation is observed to disentangle nanotube agglomerates and the disentanglement degree is shown to depend on the stretching mode, strain rate and stretching temperatures applied. The disentanglement effectiveness is: uniaxial stretching < sim-biaxial stretching < seq-biaxial stretching, under the same deformation parameters. In sim-biaxial stretching, reducing the strain rate and stretching temperature can lead to more nanotube agglomerate breakup. Enhanced nanotube agglomerate disentanglement exhibits a positive effect on the mechanical properties and a negative effect on the electrical properties of the deformed nanocomposites. The ultimate stress of the composite containing 4 wt% MWCNTs increased by ∼492% after seq-biaxial stretching, while the resistivity increased by ∼1012 Ω cm.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

High density polyethylene (HDPE)/multi-walled carbon nanotube (MWCNT) nanocomposites were prepared by melt mixing using twin-screw extrusion. The extruded pellets were compression moulded at 200°C for 5min followed by cooling at different cooling rates (20°C/min and 300°C/min respectively) to produce sheets for characterization. Scanning electron microscopy (SEM) shows that the MWCNTs are uniformly dispersed in the HDPE. At 4 wt% addition of MWCNTs composite modulus increased by over 110% compared with the unfilled HDPE (regardless of the cooling rate). The yield strength of both unfilled and filled HDPE decreased after rapid cooling by about 10% due to a lower crystallinity and imperfect crystallites. The electrical percolation threshold of composites, irrespective of the cooling rate, is between a MWCNT concentration of 1∼2 wt%. Interestingly, the electrical resistivity of the rapidly cooled composite with 2 wt% MWCNTs is lower than that of the slowly cooled composites with the same MWCNT loading. This may be due to the lower crystallinity and smaller crystallites facilitating the formation of conductive pathways. This result may have significant implications for both process control and the tailoring of electrical conductivity in the manufacture of conductive HDPE/MWCNT nanocomposites.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Thesis (Ph.D.)--University of Washington, 2013

Relevância:

40.00% 40.00%

Publicador:

Resumo:

In the present study the preparation and characterisation of rubber ferrite composites containing nickel ferrite and gamma ferric oxide have been dealt with.Synthetic rubbers viz. ethylene propylene diene rubber and neoprene rubber were used for the incorporation of nickel ferrite and gamma ferric oxide for the synthesis of RFCs. Incorporation of ferrites were carried out according to a specific recipe for various loadings of the magnetic fillers. The ferrites used for the preparation of RFCs were synthesised using sol-gel method and structural characterisation was carried out. Experimental techniques like X-ray diffraction, Transmission electron microscopy and other analytical techniques were used for this. Precharaterised ferrites were then incorporated at different loading into rubber according to conventional mixing methods. The cure characteristics, mechanical, dielectric, magnetic and microwave properties of these composites were evaluated. The effect of carbon black on these properties of RFCs were carried out.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This thesis mainly deals with the preparation and studies on magnetic composites based on spinel ferrites prepared both chemically and mechanically. Rubber ferrite composites (RFC) are chosen because of their mouldability and flexibility and the ease with which the dielectric and magnetic properties can be manipulated to make them as useful devices. Natural rubber is chosen as the Matrix because of its local availability and possible value addition. Moreover, NR represents a typical unsaturated nonpolar matrix. The work can be thought of as two parts. Part l concentrates on the preparation and characterization of nanocomposites based on y-Fe203. Part 2 deals with the preparation and characterization of RFCs containing Nickel zinc ferrit In the present study magnetic nanocomposites have been prepared by ionexchange method and the preparation conditions have been optimized. The insitu incorporation of the magnetic component is carried out chemically. This method is selected as it is the easiest and simplest method for preparation of nanocomposite. Nanocomposite samples thus prepared were studied using VSM, Mossbauer spectroscopy, Iron content estimation, and ESR spectroscopy. For the preparation of RFCs, the filler material namely nickel zinc ferrite having the general formula Ni)_xZnxFez04, where x varies from 0 to 1 in steps of 0.2 have been prepared by the conventional ceramic techniques. The system of Nil_xZn"Fe204 is chosen because of their excellent high frequency characteristics. After characterization they are incorporated into the polymer matrix of natural rubber by mechanical method. The incorporation is done according to a specific recipe and for various Loadings of magnetic fillers and also for all compositions. The cure characteristics, magnetic properties and dielectric properties of these composites are evaluated. The ac electrical conductivity of both ceramic nickel zinc ferrites and rubber ferrite composites are also calculated using a simple relation. The results are correlated.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Polycrystalline single phasic mixed ferrites belonging to the series Ni1−xZnxFe2O4 for various values of x have been prepared by conventional ceramic techniques. Pre-characterized nickel zinc ferrites were then incorporated into a natural rubber matrix according to a specific recipe for various loadings. The processability and cure parameters were then determined. The magnetic properties of the ceramic filler as well as the ferrite loaded rubber ferrite composites (RFC) were evaluated and compared. A general equation for predicting the magnetic properties was also formulated. The validity of these equations were then checked and correlated with the experimental data. The coercivity of the RFCs almost resemble that of the ceramic component in the RFC. Percolation threshold is not reached for a maximum loading of 120 phr (parts per hundred rubber by weight) of the filler. These studies indicate that flexible magnets can be made with appropriate magnetic properties namely saturation magnetisation (Ms) and magnetic field strength (Hc) by a judicious choice of x and a corresponding loading. These studies also suggest that there is no possible interaction between the filler and the matrix at least at the macroscopic level. The formulated equation will aid in synthesizing RFCs with predetermined magnetic