949 resultados para LIQUID-CRYSTALLINE PHASES
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Glasses with compositions (1-x)ZrF4-xLnF(3), 0.2 less than or equal to x less than or equal to 0.4 and Ln = La or La, Eu have been synthesized and investigated using differential scanning calorimetry, X-ray diffraction, Raman scattering and Eu3+ optical spectroscopy. Single-phase polycrystalline lanthanum fluorozirconates with Zr/Ln ratio equal to 1, 2 and 3 have been investigated using the same techniques for comparison. The crystalline phases LnZrF(7), LnZr(2)F(11), LT-LnZr(3)F(15) (orthorhombic) and HT-LnZr(3)F(15) (trigonal) have been characterized in the recrystallized glasses and in samples spontaneously crystallized from the melt. Another phase has also been observed but remains undefined, the Raman scattering spectra of the vitreous samples are related to the vibration modes of [ZrF6] isolated octahedra, and of [ZrF7] and [ZrF8] structural units with bridging fluorine ions. The Eu3+ fluorescence data are related to a predominant local environment of the lanthanide ions in the glasses similar to that of the lanthanide in LnZrF(7).
Resumo:
Optically clear dispersions of dioctadecyldimethylammonium bromide and chloride (DODAX, X = Br-, Cl-) in water can be obtained by simply mixing the amphiphiles at low concentrations (I mM) and at a temperature safely above the gel to liquid crystalline phase transition temperature (T-m approximate to 45-48 degrees C) of DODAX in water. Under these conditions, dynamic light scattering shows that, at room temperature, the dispersions contain two well-defined populations of large vesicles with average hydrodynamic radii (RH) of 80 and 337 nm for DODAB and of 69 and 247 nm for DODAC. Cryo-transmission electron microscopy (cryo-TEM) micrographs show that DODAX vesicles are unilamellar and polydisperse with apparent radius up to 800 nm. The vesicles are stable for at least I month according to the ageing time-dependence of the turbidity and molar absorption coefficient. (c) 2006 Elsevier B.V.. All rights reserved.
Resumo:
A new approach for SrBi2Nb2O9 (SBN) thin films synthesis using aqueous solution was successfully experienced. The deposition solution was prepared from Sr-Bi-Nb mixed-citrate solution, requiring no special atmosphere and using common reagents. Films were deposited by dip coating onto Pt/Ti/SiO2/Si(100) substrates and hear treated at temperatures ranging from 300 to 700 degrees C. The process of formation and crystallization of SrBi2Nb2O9 thin films, prepared by the aqueous solution method have been studied with particular emphasis on the microstructure of crystallized films. Crystalline phases formation were followed by grazing incident X-ray diffraction (GIXRD), microstructure characterization was evaluated by scanning electron microscopy (SEM) and surface roughness were observed using atomic for ce microscopy (AFM). To reach the desired thickness, substrates were dipped in the deposition solution twice, forming double-layered films. The thickness of each layer ranged from 80 to 100 nm. (C) 1999 Elsevier B.V. Limited. All rights reserved.
Resumo:
Superconductor films of the BSCCO system have been grown by dip coating technique with good success. The chemical method allows us to grow high temperature superconductor thin films to get better control of stoichiometry, large areas and is cheaper than other methods. There is a great technological interest in growth oriented superconductor films due anisotropic characteristics of superconductor materials of high critical temperature, specifically the cuprates, as we know that the orientation may increase the electrical transport properties. Based on this, the polymeric precursor method has been used to obtain thin films of the BSCCO system. In this work we have applied that method together with the deposition technique known as dip coating to obtain Bi-based superconductor thin films, specifically, Bi1.6Pb0.4Sr2.0C2.0Cu3.0Ox+8, also known as 2223 phase with a critical temperature around 110 K. The films with multilayers have been grown on crystalline substrates of LaAlO3 and orientated (100) after being heat treated around 790 degrees C - 820 degrees C in lapse time of 1 hour in a controlled atmosphere. XRD measurements have shown the presence of a crystalline phase 2212 with a critical temperature around 85 K with (001) orientation, as well as a small fraction of 2223 phase. SEM has shown a low uniformity and some cracks that maybe related to the applied heat treatment. WDS has also been used to study the films composition. Different heat treatments have been used with the aim to increase the percentage of 2223 phase. Measurements of resistivity confirmed the presence of at least two crystalline phases, 2212 and 2223, with T-c around 85 K and 110 K, respectively.
Resumo:
Cellulose-phosphate composite membranes have been prepared from bacterial cellulose membranes ( BC) and sodium polyphosphate solution. The structure and thermal behavior of the new composites were evaluated by X-ray diffraction (XRD), P-31-nuclear magnetic resonance (NMR), scanning electron microscopy (SEM), differential scanning calorimetry (DSC), thermogravimetry (TG) and thermomechanical analysis (TMA). From XRD analyses the I alpha and I beta cellulose crystalline phases were identified together with crystalline sodium phosphate that covers the cellulose microfibrils as revealed by SEM. P-31 NMR spectra show peaks assigned to Q(0) and Q(1) phosphate structures to be compared to the Q(2) units that characterize the precursor polyphosphate. Glass transition temperature, T-g, obtained from TMA curves and thermal stability obtained from TG and DSC measurements, were observed to be dependent on the phosphate content.
Resumo:
The thermotropic phase behavior of cationic liposomes in mixtures of two of the most investigated liposome-forming double-chain lipids, dioctadecyldimethylammonium bromide (DODAB) and didodecyldimethylammonium bromide (DDAB), was investigated by differential scanning calorimetry (DSC), turbidity, and Nile Red fluorescence. The dispersions were investigated at 1.0 mM total surfactant concentration and varying DODAB and DDAB concentrations. The gel to liquid-crystalline phase transition temperatures (T-m) of neat DDAB and DODAB in aqueous dispersions are around 16 and 43 degrees C, respectively, and we aim to investigate the T-m behavior for mixtures of these cationic lipids. Overall, DDAB reduces the T-m of DODAB, the transition temperature depending on the DDAB content, but the T-m of DDAB is roughly independent of the DODAB concentration. Both DSC and fluorescence measurements show that, within the mixture, at room temperature (ca. 22 degrees C), the DDAB-rich liposomes are in the liquid-crystalline state, whereas the DODAB-rich liposomes are in the gel state. DSC results point to a higher affinity of DDAB for DODAB liposomes than the reverse, resulting in two populations of mixed DDAB/DODAB liposomes with distinctive phase behavior. Fluorescence measurements also show that the presence of a small amount of DODAB in DDAB-rich liposomes causes a pronounced effect in Nile Red emission, due to the increase in liposome size, as inferred from turbidity results.
Resumo:
In this paper we report a study of the physicochemical, dielectric and piezoelectric properties of anionic collagen and collagen-hydroxyapatite (HA) composites, considering the development of new biomaterials which have potential applications in support for cellular growth and in systems for bone regeneration. The piezoelectric strain tensor element d(14), the elastic constant s(55) and the dielectric permittivity 8(11), were measured for the anionic collagen and collagen-HA films. The thermal analysis shows that the denaturation endotherm is at 59.47 degreesC for the collagen sample. The collagen-HA composite film shows two transitions, at 48.9 and 80.65 degreesC. The X-ray diffraction pattern of the collagen film shows a broad band characteristic of an amorphous material. The main peaks associated to the crystalline HA is present in the sample of collagen-HA. In the collagen-HA composite, one can also notice the presence of other peaks with low intensities which is an indication of the formation of other crystalline phases of apatite. The scanning electron photomicrograph of anionic collagen membranes shows very thin bundles of collagen. The scanning electron photomicrography of collagen-HA film also show deposits of hydroxyapatite on the collagen fibers forming larger bundles and suggesting that a collagenous structure of reconstituted collagen fibers could act as nucleators for the formation of apatite crystal similar to those of bone. The piezoelectric strain tensor element d(14) was measured for the anionic collagen, with a value of 0.062 pC N-1, which is in good agreement compared with values reported in the literature obtained with other techniques. For the collagen-HA composite membranes, a slight decrease of the value of the piezoelectricity (0.041 pC N-1) was observed. The anionic collagen membranes present the highest density, dielectric permittivity and lowest frequency constant f.L. (C) 2001 Elsevier B.V. B.V. All rights reserved.
Resumo:
Glass structure and fluorine motion dynamics are investigated in lead-cadmium fluorgermanate glasses by means of differential scanning calorimetry, Raman scattering, x-ray absorption (EXAFS), electrical conductivity (EC), and F-19 nuclear magnetic resonance (NMR) techniques. Glasses with composition 60PbGeO(3)-xPbF(2)-yCdF(2) (in mol %), with x+y=40 and x=10, 20, 30, 40, are studied. Addition of metal fluorides to the base PbGeO3 glass leads to a decrease of the glass transition temperature (T-g) and to an enhancement of the ionic conductivity properties. Raman and EXAFS data analysis suggest that metagermanate chains form the basic structural feature of these glasses. The NMR study leads to the conclusion that the F-F distances are similar to those found in pure crystalline phases. Experimental results suggest the existence of a heterogeneous glass structure at the molecular scale, which can be described by fluorine rich regions permeating the metagermanate chains. The temperature dependence of the NMR line shapes and relaxation times exhibits the qualitative and quantitative features associated with the high fluorine mobility in these systems. (C) 2004 American Institute of Physics.
Resumo:
Surface modifications have been applied in endosteal bone devices in order to improve the osseointegration through direct contact between neoformed bone and the implant without an intervening soft tissue layer. Surface characteristics of titanium implants have been modified by addictive methods, such as metallic titanium, titanium oxide and hydroxyapatite powder plasma spray, as well as by subtractive methods, such as acid etching, acid etching associated with sandblasting by either AlO2 or TiO2, and recently by laser ablation. Surface modification for dental and medical implants can be obtained by using laser irradiation technique where its parameters like repetition rate, pulse energy, scanning speed and fluency must be taken into accounting to the appropriate surface topography. Surfaces of commercially pure Ti (cpTi) were modified by laser Nd:YVO4 in nine different parameters configurations, all under normal atmosphere. The samples were characterized by SEM and XRD refined by Rietveld method. The crystalline phases alpha Ti, beta Ti, Ti6O, Ti3O and TiO were formed by the melting and fast cooling processes during irradiation. The resulting phases on the irradiated surface were correlated with the laser beam parameters: the aim of the present work was to control titanium oxides formations in order to improve implants osseointegration by using a laser irradiation technique which is of great importance to biomaterial devices due to being a clean and reproducible process. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Magnesium and zinc ferrites have been prepared by the polymeric precursor method. The organic material decomposition was studied by thermogravimetry (TG) and differential thermal analysis (DTA). The variation of crystalline phases and particle morphology with calcination temperature were investigated using X-ray diffraction (XRD) and scanning electronic microscopy (SEM), respectively. The colors of the ferrites were evaluated using colorimetry. Magnesium ferrite crystallizes above 800 degrees C, presenting a yellow-orange color with a reflectance peak at the 600-650 nm range, while zinc ferrite crystallizes at 600 degrees C, with a reflectance peak between 650-700 nm, corresponding to the red-brick color.
Resumo:
Results of differential scanning calometry (DSC), x-ray diffraction (XRD), and F-19 nuclear magnetic resonance (NMR) of InF3-based glasses, treated at different temperatures, ranging from glass transition temperature (T-g) to crystallization temperature (T-c), are reported. The main features of the experimental results are as follows. DSC analysis emphasizes several steps in the crystallization process. Heat treatment at temperatures above T-g enhances the nucleation of the first growing phases but has little influence on the following ones. XRD results show that several crystalline phases are formed, with solid state transitions when heated above 680 K, the F-19 NMR results show that the spin-lattice relaxation, for the glass samples heat treated above 638 K, is described by two time constants. For samples treated below this temperature a single time constant T-1 was observed. Measurements of the F-19 spin-lattice relaxation time (T-1), as a function of temperature,made possible the identification of the mobile fluoride ions. The activation energy, for the ionic motion, in samples treated at crystallization temperature was found to be 0.18 +/- 0.01 eV. (C) 1998 American Institute of Physics.
Resumo:
New glasses have been obtained in the system InF3-BaF2-ErPO4. Glass compositions with up to 30% mol Er3+ were shown to exist and characterized by thermal analysis, x-ray: diffraction, IR absorption and electronic spectroscopy. The systems with high Er3+ content were studied recording IR and visible emission spectral characteristics. A specially elaborated technique allowed the preparation of a high purity phosphate precursor ErPO4. X-ray identification of the crystalline phases appearing during thermal treatment have been carried out and parameters of a mixed fluoride Ba4In3-nErnF17 calculated.
Resumo:
The complex crystallization process of a Brazilian blast-furnace slag glass was investigated using differential scanning calorimetry (DSC), X-ray diffraction, optical microscopy, transmission electron microscopy (TEM), selected area diffraction (SAD), energy dispersive spectroscopy (EDS) and micro-Raman spectroscopy. Three crystalline phases (merwinite, melilite and larnite) were identified after heat treatment between Tg (742°C) and the DSC crystallization peak (T = 1000°C). Merwinite was identified as a metastable phase. A small amount (0.004 wt%) of metallic platinum was found in the glass composition. Particles of Pt3Fe, detected by EDS and SAD-TEM, were the starting points of crystallization acting, therefore, as heterogeneous nucleating sites. Only melilite and larnite precipitated in a glass sample heat-treated at 1000°C for 1 h. The flexural strength of this crystallized sample was less than that of the glass, probably due the allotropic phase transformation of larnite. © 2000 Published by Elsevier Science B.V. All rights reserved.
Resumo:
Dielectric ceramics have been widely investigated and used for microwave applications such as resonators and filters. The present study deals with the influence of sintering temperature on microwave dielectric properties of TiO2 ceramics with 10, 20, and 30 wt% ZrO2. Three compositions have been developed through mixing procedures and then tested for each sintering temperature: 1500 and 1400°C. X-ray diffraction and scanning electron microscopy are carried out aiming to explain the ceramic behavior of each sample. The dielectric constants of different ceramics for both temperatures varied from 85.4 to 62.6, while their quality factor due to dielectric losses varied from 3110 to 1630. The Q decrease is attributed to the non uniform grain growth and to the obtained crystalline phases. The best microwave parameters were obtained for the ceramics sintered at 1400°C, which can be applied in microwave circuits as dielectric resonators. © (2010) Trans Tech Publications.