956 resultados para Elastomer composites
Resumo:
One of the different issues limiting the wider application of monolithic hydroxyapatite (HA) as an ideal bone replacement material is the lack of reasonably good electrical transport properties. The comprehensive electrical property characterization to evaluate the efficacy of processing parameters in achieving the desired combination of electroactive properties is considered as an important aspect in the development of HA-based bioactive material. In this perspective, the present work reports the temperature (RT-200 degrees C) and frequency (100 Hz-1 MHz) dependent dielectric properties and AC conductivity for a range of HA-CaTiO3 (HA-CT) composites, densified using both conventional pressureless sintering in air as well as spark plasma sintering in vacuum. Importantly, the AC conductivity of spark plasma sintered ceramics similar to upto 10(-5) (Omega cm)(-1)] are found to be considerably higher than the corresponding pressureless sintered ceramics similar to upto 10(-8) (Omega cm)(-1)]. Overall, the results indicate the processing route dependent functional properties of HA-CaTiO3 composites as well as related advantages of spark plasma sintering route. (C) 2013 Elsevier Ltd. All rights reserved.
Resumo:
Damaged articulating joints can be repaired or replaced with synthetic biomaterials, which can release wear debris due to articulation, leading to the osteolysis. In a recent work, it has been shown that it is possible to achieve a better combination of flexural strength/fracture toughness as well as in vitro bioactivity and cytocompatibility properties in spark plasma sintered hydroxyapatite-titanium (HA-Ti) composites. Although hydroxyapatite and titanium are well documented for their good biocompatibility, nanosized hydroxyapatite (HA) and titanium (Ti) particles can cause severe toxicity to cells. In order to address this issue, fretting wear study of HA-Ti composites under dry and wet (1x SBF, supplemented with 5 g l(-1) bovine serum albumin (BSA)) condition was performed to assess the wear resistance as well as wear debris formation, in vitro. The experimental results reveal one order of magnitude lower wear rate for HA-10 wt% Ti (7.5 x 10(-5) mm(3) N-1 m(-1)) composite than monolithic HA (3.9 x 10(-4) mm(3) N-1 m(-1)) in simulated body fluid. The difference in the tribological properties has been analyzed in the light of phase assemblages and mechanical properties. Overall, the results suggest the potential use of HA-Ti composites over existing HA-based biocomposites in orthopedic as well as dental applications.
Resumo:
Electromagnetic field interactions with the composites made up of polyaniline (PANI) and single wall carbon nanotube (SWCNT) are simulated using the discrete dipole approximation. Recent observations on polymer nano-composites explain the interface interactions between the PANI host and the carbon nanostructures. These types of composite have potential applications in organic solar cell, gas sensor, bio-sensor and electro-chromic devices. Various nanostructures of PANI is possible in the form of nanowires, nanodisks, nanofibers and nanotubes have been reported. In the present study, we considered two types of composite, one is the PANI wrapped CNT and the other is CNT immersed in PANI nanotube. We use Modified Thole's parameters for calculating frequency dependent atomic polarizability of composites. Absorption spectra of the composites are studied by illuminating a wide range of electromagnetic energy spectrum. From the absorption spectra, we observe plasmon excitation in near-infrared region similar to that in SWCNTs reported recently. The interactions between the PANI and CNT in the composite, resulting electromagnetic absorptions are simulated.
Resumo:
We investigate the evolution of polymer structure and its influence on uniaxial anisotropic stress under time-varying uniaxial strain, and the role of external control variables such as temperature, strain rate, chain length, and density, using molecular dynamics simulation. At temperatures higher than glass transition, stress anisotropy in the system is reduced even though the bond stretch is greater at higher temperatures. There is a significant increase in the stress level with increasing density. At higher densities, the uncoiling of the chains is suppressed and the major contribution to the deformation is by internal deformation of the chains. At faster rates of loading stress anisotropy increases. The deformation mechanism is mostly due to bond stretch and bond bending rather than overall shape and size. Stress levels increase with longer chain length. There is a critical value of the functionality of the cross-linkers beyond which the uniaxial stress developed increases caused primarily by bond stretching due to increased constraint on the motion of the monomers. Stacking of the chains in the system also plays a dominant role in the behaviour in terms of excluded volume interactions. Low density, high temperature, low values of functionality of cross-linkers, and short chain length facilitate chain uncoiling and chain slipping in cross-linked polymers.
Resumo:
In developing materials with better tribological properties, it is always conceived that the addition of softer phase would result in better frictional behavior. In order to address this issue, we report here the results of fretting wear study on Cu-10 wt% TiB2 and Cu-10 wt% TiB2-10 wt% Pb composites, sintered using spark plasma sintering (SPS) technique. It was found out that the addition of softer phase i.e. 10 wt % Pb to Cu-10 wt% TiB2 composites has not resulted in the lowering of the coefficient of friction (COF). The combination of steady state COF (0.6) and wear rate (10(-3) mm(3)/N-m) was measured and such properties are even better than that obtained with TiB2 coatings reported in the literature. For Cu-10 wt% TiB2 sintered at different temperature, a lower wear resistance with increase in hardness is being measured. An attempt has been made to correlate the observed wear behavior with the surface and subsurface deformation. The formation of a wear-resistant delaminated tribolayer consisting of TiB2 particles and ultrafine oxide debris (Cu, Fe, Ti)(x)O-y was the reason assigned for the observed low wear rate of these composites. (C) 2013 Elsevier B.V. All rights reserved.
Resumo:
In the present investigation, the corrosive behaviour of Al 6061-TiN particulate composites prepared by liquid metallurgy has been studied in chloride medium using electroanalytical techniques such as Tafel, cyclic polarization and electrochemical impedance spectroscopy (EIS). Surface morphology of the sample electrodes was examined using scanning electron micrography and energy dispersive X-ray methods. X-ray diffraction technique was used to confirm inclusion of TiN particulates in the matrix alloy and identify the alloying elements and intermetallic compounds in the Al 6061 composites. Polarization studies indicate an increase in the corrosion resistance in composites compared to the matrix alloy. EIS study reveals that the polarization resistance (R (p)) increases with increase in TiN content in composites, thus confirming improved corrosion resistance in composites. The observed decrease in corrosion rate in the case of composites is due to decoupling between TiN particles and Al 6061 alloy. It is understood that after the initiation of corrosion, interfacial corrosion products may have decoupled the conducting ceramic TiN from Al 6061 matrix alloy thus eliminating the galvanic effect between them.
Resumo:
Magneto-electric composites comprising Na0.5Bi0.5TiO3 (NBT) and MnFe2O4 (MFO) were fabricated using their fine powders obtained via sol-gel method. X-ray diffraction and scanning electron microscopy results confirmed the single-phase formation of NBT and MFO and the composite nature when these were mixed and sintered at appropriate temperatures. The dielectric constant (epsilon(r)) and dielectric loss (D) decreased with increase in frequency (40-110 MHz). Room temperature magnetization measurements established these composites to be soft magnetic. Further, the nature of these composites were established to be magneto-electric at 300 K. The highest ME response of 0.19 % was observed in 30NBT-70MFO composite. The ME coefficient (alpha) was 240 mV/cm Oe for the same composition. The present study demonstrated the effectiveness of NBT/MFO as a lead-free multiferroic composite and provides an alternative for environment-friendly ME device applications.
Resumo:
In view of the fact that bone healing can be enhanced due to external electric field application, it is important to assess the influence of the implant conductivity on the bone regeneration in vivo. To address this issue, this study reports the in vivo biocompatibility property of multistage spark plasma sintered hydroxyapatite (HA)-80 wt % calcium titanate (CaTiO3) composites and monolithic HA, which have widely different conductivity property (14 orders of magnitude difference). The ability of bone regeneration was assessed by implantation in cylindrical femoral bone defects of rabbit animal model for varying time period of 1, 4, and 12 weeks. The overall assessment of the histology results suggests that the progressive healing of bone defects around HA-80 wt % CaTiO3 is associated with a better efficacy with respect to (w.r.t) early stage neobone formation, which is histomorphometrically around 140% higher than monolithic HA. Overall, this study demonstrates that the in vivo biocompatibility property of HA-80 wt % CaTiO3 with respect to local effects after 12 weeks of implantation is not compromised both qualitatively and quantitatively, and a comparison with control implant (HA) points toward the critical role of electrical conductivity on better early stage bone regeneration. (c) 2013 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 102A: 842-851, 2014.
Resumo:
Glasses and glass-nanocrystal (anatase TiO2) composites in BaO-TiO2-B2O3 system were fabricated by conventional melt-quenching technique and controlled heat treatment respectively. Poisson's ratio and Young's moduli were predicted through Makishima-Mackenzie theoretical equation for the as-quenched glasses by taking the four and three coordinated borons into account. Mechanical properties of the glasses and glass-nanocrystal composites were investigated in detail through nanoindentation and microindentation studies. Predicted Young's moduli of glasses were found to be in reasonable agreement with nanoindentation Measurements. Hardness and Young's modulus were enhanced with increasing volume fraction of nanocrystallites of TiO2 in glass matrix whereas fracture toughness was found susceptible to the surface features. The results were correlated to the structural units and nanocrystals present in the glasses. (C) 2013 Elsevier B.V. All rights reserved.
Resumo:
Delamination is one of the most commonly occurring defects in laminated composite structures. Under operating fatigue loads on the laminate this delamination could grow and totally delaminate certain number of layers from the base laminate. This will result in loss of both compressive residual strength and buckling margins available. In this paper, geometrically non-linear analysis and evaluation of Strain Energy Release Rates using MVCCI technique is presented. The problems of multiple delamination, effect of temperature exposure and delamination from pin loaded holes are addressed. Numerical results are presented to draw certain inferences of importance to design of high technology composite structures such as aircraft wing.
Resumo:
Bacterial infection remains an important risk factor after orthopedic surgery. The present paper reports the synthesis of hydroxyapatite-silver (HA-Ag) and carbon nanotube-silver (CNT-Ag) composites via spark plasma sintering (SPS) route. The retention of the initial phases after SPS was confirmed by phase analysis using X-ray diffraction and Raman spectroscopy. Energy dispersive spectrum analysis showed that Ag was distributed uniformly in the CNT/HA matrix. The breakage of CNTs into spheroid particles at higher temperatures (1700 degrees C) is attributed to the Rayleigh instability criterion. Mechanical properties (hardness and elastic modulus) of the samples were evaluated using nanoindentation testing. Ag reinforcement resulted in the enhancement of hardness (by similar to 15%) and elastic modulus (similar to 5%) of HA samples, whereas Ag reinforcement in CNT, Ag addition does not have much effect on hardness (0.3 GPa) and elastic modulus (5 GPa). The antibacterial tests performed using Escherichia coli and Staphylococcus epidermidis showed significant decrease (by similar to 65-86%) in the number of adhered bacteria in HA/CNT composites reinforced with 5% Ag nanoparticles. Thus, Ag-reinforced HA/CNT can serve as potential antibacterial biocomposites.