855 resultados para phenolic-epoxy blends
Resumo:
Blends of polychloroprene rubber and plasticized polyvinylchloride have been prepared in various compositions and their properties evaluated. The properties of the blends show that they can be used to replace polychloroprene in many applications
Resumo:
Ethylene-propylene-diene rubber (EPDM) and isobutylene-isoprene rubber (IIR) were compounded, precured to a low degree, and then were blended with natural rubber (NR). The compounding ingredients for NR were then added and the final curing was done. NR/ EPDM and NR/IIR blends, prepared using this method, were found to possess much improved mechanical properties as compared to their conventional counterparts. The optimum precuring crosslink density that has to be given to the EPDM and IIR phases has been determined.
Resumo:
Butyl (IIR) tube reclaim (RR) was mixed with carbon black filled natural rubber (NR) compounds at various percentages. The blend containing a low percentage of RR was found to show improved ageing resistance and improved processability with out much reduction in the mechanical properties.
Resumo:
Polymer-solvent interaction parameters for the blends of natural rubber (NR) with styrene-butadiene rubber (SBR) and polybutadiene rubber ( BR) are calculated using the Flory-Rehner equation by equating the network density of the vulcanizates in two solvents.
Resumo:
Blends of natural rubber (NR) with styrene-butadiene rubber (SBR), polybutadiene rubber (BR), ethylene-propylene terpolymer (EPDM) and acrylonitrile-butadiene rubber (NBR) were vulcanised using an efficient vulcanisation (EV) system and a semi-EV system. Compatible blends show a definite pattern of curing whereas the incompatible blends show no such pattern.
Resumo:
Compounding of styrene-butadiene copolymer/polybutadiene , natural rubber/ ethylene-propylene-diene terpolymer and natural rubber/butadiene-acrylonitrile copolymer blends was done in three different ways and their curing behaviour and the tensile properties of the es are compared.
Resumo:
ABSTRACT: The rheological and extrudate behaviour of natural rubber/latex reclaim blends were evaluated using a capillary viscometer . The study shows that the viscosity of natural rubber decreases marginally on the addition of latex reclaim while the variation of viscosity with shear rate is not affected. The temperature sensitivity of the blends is not affected significantly with the addition of latex reclaim . The extrudates of natural rubber/latex reclaim blends are smooth up to the addition of about 50 wt. percent latex reclaim in filled natural rubber compounds.
Resumo:
ABSTRACT: Phenol was chemically attached to low molecular weight chlorinated polyisobutylene and stearic acid respectively. These phenolic antioxidants were characterised by IR, 1H NMR and TGA. The efficiency and permanence of these bound antioxidants were compared with conventional antioxidants in natural rubber vulcanisates. The vulcanisates showed comparable ageing resistance in comparison to vulcanisates containing conventional antioxidants. The presence of liquid polymer bound phenol reduce the amount of plasticiser required for compounding.
Resumo:
Blends of styrene butadiene rubber (SBR) with maleic anhydride grafted whole tire reclaim (MA-g-WTR) have been prepared and the cure and mechanical properties have been studied with respect to the reclaim content. The grafting was carried out in the presence of dicumylperoxide (DCP) in a Brabender Plasticorder at 150'C. The presence of anhydride group on the WTR was confirmed by infrared spectrometry (IR) study. The properties were compared with those of the blends containing unmodified WTR. Though the cure time was marginally higher, the mechanical properties of the blends containing grafted WTR were better than that of the unmodified blends.
Resumo:
Blends of Acrylonitrile rubber with Maleic anhydride grafted Whole Tyre Reclaim WTR (MA-g-WTR) have been prepared and the cure and mechanical properties have been studied with respect to reclaim content. Control compounds containing unmodified WTR were also prepared for comparison. Grafting was confirmed by IR studies. Blends containing grafted WTR showed higher minimum torque and (max-min) torque. They also showed longer cure time, scorch time and lower cure rate. Grafting of the WTR with maleic anhydride also resulted in the improved tensile strength, abrasion resistance, compression set and resilience. However, the heat build up under dynamic loading was marginally higher for the blends containing grafted reclaimed rubber.
Resumo:
The rheological characteristics of short Nylon-6 fiber-reinforced Styrene Butadiene rubber (SBR) in the presence of epoxy resin-based bonding agent were studied with respect to the effect of shear rate, fiber concentration , and temperature on shear viscosity and die swell using a capillary rheonzeter. All the composites containing bonding agent showed a pseudoplastic nature, which decreased with increasing temperature. Shear viscosity was increased in the presence of fibers. The temperature sensitivity of the SBR matrices was reduced on introduction of fibers. The temperature sensitivity of the melts was found to be lower at higher shear rates. Die swell was reduced in the presence of fibers. Relative viscosity of the composites increased with shear rate. In the presence of epoxy resin bonding agent the temperature sensitivity of the mixes increased. Die swell was larger in the presence of bonding agent.
Resumo:
Cure characteristics and mechanical properties of short nylon fiber reinforced acrylonitrile butadiene rubber-reclaimed rubber composites were studied. Minimum torque, (maximum-minimum) torque and cure rate increased with fiber concentration. Scorch time and cure time decreased by the addition of fibers. Properties like tensile strength, tear strength, elongation at break, abrasion loss and heat build up were studied in both orientations of fibers. Tensile and tear properties were enhanced by the addition of fibers and were higher in the longitudinal direction. Heat build up increased with fiber concentration and were higher in the longitudinal direction. Abrasion resistance was improved in presence of short fibers and was higher in the longitudinal direction. Resilience increased on the introduction of fibers. Compression set was higher for blends.
Resumo:
Cure characteristics and mechanical properties of acrylonitrile butadiene rubber/reclaimed rubber blends were studied. Minimum torque, (ma)dmum -minimum) torque, scorch time, cure time and cure rate decreased in presence of reclaimed rul3ber. Tensile strength, elongation at break and compression set increased'with increase in reclaim content. Resilience and abrasion resistance decreased with reclaim loading. Heat build up was higher for the blends. The ageing resistance of the blends was inferior to that of the gum compound.
Resumo:
Cure characteristics and mechanical properties of styrene butadiene rubber reclaimed rubber blends were studied. The blends showed improved processability, as indicated by the minimum torque values. Cure characteristics like minimum torque, (maximum-minimum) torque, cure time and cure rate decreased in the presence of reclaimed rubber. Tensile strength, tear strength, elongation at break were higher for blends. Resilience decreased with reclaim content. Compression set and abrasion loss were higher in the blends.