930 resultados para grazing-incidence small angle X-ray scattering
Resumo:
Structural studies of poly(aryl ether ether ketone ketone) (PEEKK) using small-angle X-ray scattering and one-dimensional electron density correlation function methods revealed that its aggregated state structure was significantly influenced by the annealing temperature. The long period L, the average thickness of the lamellae d, the electron density difference between the crystalline and amorphous regions eta(c) - eta(a), and the invariant Q increased with increasing annealing temperature, but it was opposite to the case of the specific inner surfaces O-s. A transition zone existed between the traditional "two phases" with a dimension about 0.5 nm for semicrystalline PEEKK. (C) 1998 John Wiley & Sons, Inc. J Appl Polym Sci 69: 1829-1835, 1998.
Resumo:
The positive temperature coefficient (PTC) and negative temperature coefficient (NTC) effect of carbon black (CB) filled low density polyethylene (LDPE) composites was studied using electrical resistivity spectra, DSC, tensile mechanical analysis (TMA) and small-angle X-ray scattering (SAXS) techniques. The three LDPEs used have a similar crystallinity and different melting index (MI). The experimental results indicate that the CB has no significant effect on the crystallinity and the long spacing of crystalline domains of LDPE. Based upon the TMA and dynamic elastic modulus spectra, it can be concluded that the PTC effect is related to the thermal expansion of the polymer matrix, and the NTC effect is caused by a decrease of the elastic modulus of the polymer at high temperatures. The NTC effect can be reduced by enhancing either the elastic modulus or the interaction between carbon black and matrix. (C) 1997 Elsevier Science Ltd.
Resumo:
The interface thickness in two-component interpenetrating polymer networks (IPN) system based on polyacrylate and epoxy were determined using small-angle X-ray scattering (SAXS) in terms of the theory proposed by Ruland. The thickness was found to be nonexistent for the samples at various compositions and synthesized at variable conditions-temperature and initiator concentration. By viewing the system as a two-phase system with a sharp boundary, the roughness of the interface was described by fractal dimension, D, which slightly varies with composition and synthesis condition. Length scales in which surface fractals are proved to be correct exist for each sample and range from 0.02 to 0.4 Angstrom(-1). The interface in the present IPN system was treated as fractal, which reasonably explained the differences between Pored's law and experimental data, and gained an insight into the interaction between different segments on the interface. (C) 1997 Elsevier Science Ltd.
Resumo:
In this paper microcrystalline structures of polyamide-1010 (PA1010) mixed with neodymium oxide (Nd2O3) were studied by Wide Angle X-ray Diffraction (WAXD) and Small Angle X-ray Scattering (SAXS). Crystallization behavior was investigated by DSC. The transition and relaxation of macromolecules in the crystalline phase were explored by Differential Scanning Calorimetry (DSC). It was revealed that neodymium oxide plays an important role in PA1010 crystallization as a heterogeneous nucleating agent. It can improve the crystallization rate, reduce crystallite size and introduce crystal imperfections. The microcrystalline structure was imposed by the addition of Nd2O3 However, the heterogeneous nucleation effect obviously does not exert its influence on the transition and relaxation of macromolecules in the crystalline phase.
Resumo:
Blends of high-density polyethylene (HDPE) with novel linear low-density polyethylene (LLDPE) samples in the whole range of compositions were investigated by means of differential scanning calorimetry (DSC), small-angle X-ray scattering (SAXS) and wide-angle X-ray diffraction (WAXD). The LLDPEs are ethylene/octene-1 copolymers prepared with a single-site catalyst, with a narrower distribution of branches compared to Ziegler-Natta type polymers. It was found that cocrystallization or separate crystallization in the blends profoundly depends on the content of branches in the LLDPE, while the critical branch content of the novel LLDPE for separate crystallization is much lower than that of commercial LLDPE (prepared with Ziegler-Natta catalysts). This implies that the miscibility of linear and branched polyethylene is also affected by the distribution of branches. The marked expansion of the unit cell in cocrystals, which are formed by HDPE with the novel LLDPE, indicates that the branches are included in the crystal lattice during the cocrystallization process. The result is very helpful to understand the phenomenon that the unit cell dimensions of commercial branched polyethylene are larger than those of linear polyethylene.
Resumo:
The microphase transition in a styrene-butadiene-styrene triblock copolymer was studied by rheometric mechanical spectroscopy. A high-temperature-melt rheological transition from the highly elastic, nonlinear viscous behavior typical of a multiphase structure to linear viscous behavior with insignificant elasticity typical of a single-phase structure was observed. The transition temperature is determined according to the discontinuity of the rheological properties across the transition region, which agrees well with the results obtained from the small angle X-ray scattering data and the expectation of the random phase approximation theory. Maybe for the first time, microphase dissolution was investigated theologically. The storage modulus (G') and the loss modulus (G '') increase with time during the process. An entanglement fluctuation model based on the segmental density fluctuations is presented to explain the rheological behavior in this dissolution process. (C) 1997 John Wiley & Sons.
Resumo:
The change in the microphase separation transition (MST) temperature of a styrene-butadiene-styrene (SBS) triblock copolymer induced by the addition of polystyrene (PS) was investigated by small-angle X-ray scattering. It was found that the transition temperature was determined from the molecular weight (M(H)) Of the added PS in relation to that of the corresponding blocks (M(A)) in the copolymer. The MST temperature decreased with added PS if M(H)/M(A) < 1/4, while it increased with added PS when M(H)/M(A) > 1/4 Analysis of the theoretical expression based on the random phase approximation showed exactly the same tendency of change in the transition temperatures as that observed experimentally. The interaction parameter, chi(SB), obtained by nonlinear fitting of the scattering profiles of SBS/PS blends in the disordered state, was found to be a function of temperature and composition. Composition fluctuations were found to exist in SBS/PS blends, increasing with increasing addition of PS but diminishing with increasing molecular weight of the added PS.
Resumo:
Phase behavior of blends of poly(vinyl methyl ether) (PVME) with four styrene-butadienestyrene (SBS) triblock copolymers, being of various molecular weights, architecture, and compositions, was investigated by small-angle light scattering. Small-angle X-ray scattering investigation was accomplished for one blend. Low critical solution temperature (LCST) and a unique phase behavior, resembling upper critical solution temperature (UCST), were observed. It was found that the architecture of the copolymer greatly influenced the phase behavior of the blends. Random phase approximation theory was used to calculate the spinodal phase transition curves of the ABA/C and BAB/C systems; LCST and resembling UCST phase behavior were observed as the parameters of the system changed. Qualitatively, the experimental and the theoretical results are consistent with each other. (C) 1996 John Wiley & Sons, Inc.
Resumo:
The miscibility and crystallization behaviour of the blends of poly(ether ether ketone) (PEEK) with two thermoplastic polyimides (PI), PEI-E and YS-30, prepared by solution blending were studied by the use of small-angle X-ray scattering (SAXS), differential scanning calorimetry (d.s.c.) and polarizing microscopy techniques. The results obtained show that PEEK/YS-30 is miscible, while PEEK/PEI-E is partially miscible only in the composition range with PEI-E content up to 20 wt%. The crystallization behaviour of PEEK in PEEK/PI blends depends on the crystallization condition of the blend sample as well as the chemical structure and the content of the PI added. Our SAXS results indicate that the segregation of PI molecular chains during crystallization of PEEK chains in the blends is interfibrillar for PEEK/PEI-E blends, but interlamellar for PEEK/YS-30 blends. The compatibility and the crystallization behaviour are discussed in terms of charge transfer interaction between PI and PI molecules and between PI and PEEK molecules.
Resumo:
Structures of poly(ether ether ketone ketone)-poly(ether biphenyl ether ketone ketone) copolymers were studied by using small angle X-ray scattering and the one-dimensional electron density correlation function method. The results revealed that structures of the aggregated state of the copolymers depend closely on the biphenyl content (n(b)). When n(b) = 0.35, invariant Q, long period L, average thickness of crystal lamellae (d) over bar, electron density difference eta(c) - eta(a) and degree of crystallinity W-c,W-x assume minimum values.
Resumo:
Compatibility, morphology, crystalline structure and mechanical properties of the blends of a thermosetting polyimide with thermoplastic polyimides consisting of dianhydrides of different lengths have been studied by the use of dynamic mechanical analysis (DMA), differential scanning calorimetry (DSC), scanning electron microscopy (SEM) and small-angle X-ray scattering (SAXS) techniques. The results of our research show that the blends change from compatible to semi-compatible when the difference between the length of the dianhydrides of the two components increases. Addition of a thermoplastic polyimide inhibits the crystallization of the thermosetting component. However, this effect decreases with increasing length of the dianhydrides and the distribution of the molecules of the thermoplastic polyimide component changes from interlamellar to interfibrillar. Impact strength and morphology of the fractured surfaces indicate that among the semiinterpenetrating polymer networks (semi-IPN) obtained the toughening effect of the partially compatible one is the best. The results are discussed in terms of charge transfer interaction between imide group and p-phenylene group.
Resumo:
The influence of gamma-radiation on polyamide 1010 aggregate structures and crystal damage were examined by using wide angle X-ray diffraction (WAXD) and small angle X-ray scattering (SAXS) techniques. The results revealed that some structural parameters of the aggregated state, the density differences and the degree of crystallinity W-c,W-x, essentially decreased with increasing radiation dose, but the specific surface O-s increased. Crosslinking and scission of irradiated polyamide 1010 samples occurred mainly in amorphous and interphase regions, and crystal damage and amorphization induced by gamma-radiation spread from the interphase and extended into the crystal phase with increasing radiation dose. This result also indicated that the (010) reflection with the hydrogen bond was more susceptible to the action of radiation.
Resumo:
Ultrahigh molecular weight polyethylene (UHMWPE) has been irradiated (0-40 Mrad) with a Co-60 source at room temperature under vacuum. The crystallinity has been investigated by differential scanning calorimetry (DSC) and small-angle X-ray scattering (SAXS). The mechanical properties have been determined at room temperature. A significant increase of heat of fusion can be seen at low irradiation doses, which is attributed to crystallization, caused by chain scission during the process of irradiation. It is also observed that the thickness of the lamellae changes with irradiation dose. The Young's modulus has been improved significantly after irradiation at low doses. (C) 1993 John Wiley & Sons, Inc.
Resumo:
The structure and miscibility of polyimide PBPI-E/PTI-E blends were studied by wide- and small-angle X-ray scattering and dynamic mechanical analysis, where PBPI-E is a biphenyl-dianhydride-based polyimide, and PTI-E is a polyimide from 4,4'-thiodiphthalic anhydride and 4,4'-oxydianiline. The results obtained show that there exists a paracrystalline structure in the blends with high content of PBPI-E, but this does not affect the miscibility of the blends. The blends are miscible over the entire composition range, since only one T(g) was observed for each blend. Meanwhile, the segregation of PTI-E during crystallization of PBPI-E in the blends is interlamellar.
Resumo:
The structure of quenched isotactic polypropylene (iPP) films, including samples etched with fuming nitric acid (FNA), has been studied by infrared (IR) spectra, wide-angle x-ray diffraction (WAXD), small-angle x-ray scattering (SAXS), and differential scanning calorimetry (DSC) measurements. The changes of IR, SAXS, DSC, and WAXD results induced by annealing for etched samples have been compared with those for unetched ones. The IR absorbance spectrum of the quenched iPP etched by FNA did not change. In addition, the SAXS intensity did not increase when these samples were annealed, indicating that the total (IR) crystallinity (i.e., the content of chain segments in the helical conformations) of the etched samples does not increase. However, WAXD patterns of the samples changed in a manner similar to those of the unetched one, from the original two blurred diffraction peaks to the sharp crystal patterns of alpha-form iPP, suggesting that the mesomorphic (or liquid crystal-like) phase has reorganized to alpha-form crystals. It is concluded that the change of WAXD of quenched iPP films during annealing results mainly from transformation of order in the mesomorphic phase, rather than only from an increase of crystal size. In other words, mesomorphic-form iPP is not constituted by any known crystals (such as alpha or beta crystals) in small sizes; its WAXD pattern reflects truly the degree of order in the mesomorphic phase.