Effect of hydrophobic oxide, containing =Si-CH=CH2 groups, on the radiation crosslinking of low density polyethylene (LDPE) has been studied. It was found that mechanical stability of irradiated LDPE containing improved SiO2 is higher than that of samples containing unimproved SiO2.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Ultrahigh molecular weight polyethylene (UHMWPE) has been irradiated (0-40 Mrad) with a Co-60 source at room temperature under vacuum. The crystallinity has been investigated by differential scanning calorimetry (DSC) and small-angle X-ray scattering (SAXS). The mechanical properties have been determined at room temperature. A significant increase of heat of fusion can be seen at low irradiation doses, which is attributed to crystallization, caused by chain scission during the process of irradiation. It is also observed that the thickness of the lamellae changes with irradiation dose. The Young's modulus has been improved significantly after irradiation at low doses. (C) 1993 John Wiley & Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The melt flow behaviour of LDPE/HDPE blends with various compositions have been determined by melt flow index (MFI) measurement. The effects of stabilizers, photo-sensitizers, multiple extrusions and short-term photooxidation have been studied. The results show that there is no marked thermal stability difference between homopolymers and blends without multiple extrusions, no matter whether stabilizers or photo-sensitizers are added. Multiple extrusions or photo-sensitizers reduce their thermal stability, shown by the decrease in MFI. The decrease in MFI of photooxidized samples does not imply serious structural change and shows that the active species formed during photooxidation induce a crosslinking reaction in the melt indexer. Multiple extrusions increase the number of active species formed in LDPE or blends and lead to an obvious decrease in MFI. It is suggested that LDPE and LDPE-rich blends after short-term photooxidation can be characterized by MFI measurement. In contrast, HDPE cannot be characterized by this method due to its linear structure.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

By using WAXD, DSC and gel fraction determination techniques, the mechanism of radiation crosslinking of polyethylene oxide (PEO) was explored, and the dependence of aggregated state on the chemical reaction and physical structure was also discussed. It was found that just like other semi-crystalline polymers, the state of aggregation of the specimen has a profound influence on the radiation effects on PEO. On the contrary, the crystalline structure of the specimen is severely affected with the increase in radiation dose and eventually amorphortized when subjected to an extremely high radiation dose.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The epitaxial crystallization of syndiotactic polypropylene (sPP) on uniaxially oriented polyethylene (PE) has been investigated by electron microscopy and electron diffraction. It is found that the sPP lamellae grow epitaxially on the PE substrate film with the preference in sPP for the b axis as the fast growth direction. Instead of 50-degrees as in the system of isotactic polypropylene with PE, the molecular chains of the sPP crystals are approximately +/- 37-degrees inclined to the chain direction of PE.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Epitaxial crystallization of high-density polyethylene (HDPE) on isotactic polypropylene (iPP) in solution-cast films has been investigated by electron microscopy. The specimen-tilt technique of electron microscopy has been used to study the structural relationship between HDPE and iPP crystals. HDPE exhibits different crystalline morphologies in the two basic types of iPP spherulite textures, cross-hatched and lathlike regions. In the former, the crystallographic c axis of HDPE lamellae is in the film plane, while in the latter, the c axis of HDPE crystallites is at an angle of about 50-degrees with the normal of the film. In both structural regions of iPP, however, the contact planes of epitaxial growth are (0 1 0) for iPP and (1 0 0) for HDPE.