974 resultados para POLY(ARYL ETHER KETONE)
Resumo:
Two kinds of macrocyclic arylene ketone oligomers have been synthesized in high yield from phthaloyl dichloride and various bridge-linking electron-rich aromatic hydrocarbons via the modified Friedel-Crafts acylation reaction. The presence of a Lewis base in this reaction is demonstrated to be advantageous for forming macrocycle oligomers. These resultant oligomers can undergo melt ring-opening polymerization to give polymers with high T. and excellent thermal stability.
Resumo:
Sulfonated poly(p-phenylene)s (SPPs) containing sulfonic acid groups in their side chains had been directly synthesized by Ni(0) catalytic coupling of sodium 3-(2,5-dichlorobenzoyl)benzenesulfonate and 2,5-dichlorobenzophenone. The synthesized copolymers possessed high molecular weights revealed by their high viscosity, and the formation of tough and flexible membranes by casting from DMAc solution. The copolymers exhibited excellent oxidative stability and mechanical properties due to their fully aromatic structure extending through the backbone and pendent groups. Transmission electron microscopic (TEM) analysis revealed that these side-chain type SPP membranes have a microphase-separated structure composed of hydrophilic side-chain domains and hydrophobic polyphenylene main chain domains. The proton conductivities of copolymer membranes increased with the increase of IEC and temperature, reaching values above 3.4 x 10(-1) S/cm at 120 degrees C, which are almost 2-3 times higher than that of Nafion 117 at the same measurement conditions. Consequently, these materials proved to be promising as proton exchange membranes.
Resumo:
The effect of PMR-polyimide(POI) as the interfacial agent on the interface characteristics, morphology features and crystallization of poly (ether sulfone) /poly (phenylene sulfide) (PES/PPS) and poly(ether ether ketone)/poly (ether sulfone) (PEEK/PES) partly miscible blends were investigated by means of the scanning electron microscopy, WAXD and XPS surface analysis. It is found that the interfacial adhesion was enhanced remarkably, the size of the dispersed phase particles was reduced significantly and the miscibility was improved by the addition of POI. During melt blending cross-link and/or grafting reaction of POI with PES, PEEK and PPS homopolymers was detected, however the reaction activity of POI with PPS was much higher than that of PES and PEEK. It was also found that POI was an effective nucleation agent of the crystallization of PPS.
Resumo:
Miscibility and crystallization behavior of solution-blended poly(ether ether ketone)/polyimide (PEEK/PI) blends were investigated by using DSC, optical microscopy and SAXS methods. Two kinds of PIs, YS-30 and PEI-E, which consist of the same diamine but different dianhydrides, were used in this work. The experimental results show that blends of PEEK/YS-30 are miscible over the entire composition range, as all the blends of different compositions exhibit a single glass transition temperature. The crystallization of PEEK was hindered by YS-30 in PEEK/YS-30 blends, of which the dominant morphology is interlamellar. On the other hand, blends of PEEK/PEI-E are immiscible, and the effect of PEI-E on the crystallization behavior of PEEK is weak. The crystallinity of PEEK in the isothermally crystallized PEEK/YS-30 blend specimens decreases with the increase in PI content. But the crystallinity of PEEK in the annealed samples almost keeps unchanged and reaches its maximum value, which is more than 50%. The spherulitic texture of the blends depends on both the blend composition and the molecular structure of the PIs used. The more PI added, the more imperfect the crystalline structure of PEEK. (C) 1998 John Wiley & Sons, Inc.
Resumo:
Some novel macrocylic(arylene ether ketone)oligomers were synthesized in high yields by a nucleophilic aromatic substitution reaction of 4,4'-dinitrobenzophenone with bisphenols in the presence of anhydrous potassium carbonate under pseudo-high-dilution conditions. Detailed structural characterization of these oligomers by matrix-assisted laser desorption/ionization-time of flight-mass spectrometry (MALDI-TOF-MS), H-1 NMR and FT-IR confirmed their cyclic nature and the compositions of the oligomeric mixtures was indicated by GPC analysis. Ring-opening polymerization of cyclic oligomers 3a to a high molecular weight polymer with M-w of 52.3 and M-n of 17.2 k was achieved by heating at 280 degrees C for 40 min in the presence of a nucleophilic initiator.
Resumo:
Miscibility, crystallization, and mechanical properties of blends of thermosetting polyimide PMR-15 and phenolphthalein poly(ether ketone) (PEK-C) were examined. With the exception of the 90/10 blend, which has two glass transition peaks, all the blends with PMR-15 less than 90 wt % are miscible in the amorphous state according to DMA results. Addition of PEK-C hindered significantly the crystallization of PMR-15, indicating that there must exist some kind of interaction between molecular chains of PMR-15 and those of PEK-C. The semi-IPN system of PMR-15/PEK-C blends exhibits good toughness. Two distinct microphases, interweaving at the phase boundaries, were found in the PMR-15/PEK-C 60/40 blend. The toughness effect of the blends is discussed in terms of the interface adhesion between the two distinct phases and the domain sizes of the phases. The relation between miscibility and toughness of the blends was investigated. (C) 1996 John Wiley & Sons, Inc.
Resumo:
(1)H NMR spectroscopy is used to investigate a series of microporous activated carbons derived from a poly(ether ether ketone) (PEEK) precursor with varying amounts of burnoff (BO). In particular, properties relevant to hydrogen storage are evaluated such as pore structure, average pore size, uptake, and binding energy. High-pressure NMR with in situ H(2) loading is employed with H(2) pressure ranging from 100 Pa to 10 MPa. An N(2)-cooled cryostat allows for NMR isotherm measurements at both room temperature ( approximately 290 K) and 100 K. Two distinct (1)H NMR peaks appear in the spectra which represent the gaseous H(2) in intergranular pores and the H(2) residing in micropores. The chemical shift of the micropore peak is observed to evolve with changing pressure, the magnitude of this effect being correlated to the amount of BO and therefore the structure. This is attributed to the different pressure dependence of the amount of adsorbed and non-adsorbed molecules within micropores, which experience significantly different chemical shifts due to the strong distance dependence of the ring current effect. In pores with a critical diameter of 1.2 nm or less, no pressure dependence is observed because they are not wide enough to host non-adsorbed molecules; this is the case for samples with less than 35% BO. The largest estimated pore size that can contribute to the micropore peak is estimated to be around 2.4 nm. The total H(2) uptake associated with pores of this size or smaller is evaluated via a calibration of the isotherms, with the highest amount being observed at 59% BO. Two binding energies are present in the micropores, with the lower, more dominant one being on the order of 5 kJ mol(-1) and the higher one ranging from 7 to 9 kJ mol(-1).
Resumo:
Analysis of X-ray powder data for the melt-crystallisable aromatic poly(thioether thioether ketone) [-S-Ar-S-Ar-CO-Ar](n), ('PTTK', Ar= 1,4-phenylene), reveals that it adopts a crystal structure very different from that established for its ether-analogue PEEK. Molecular modelling and diffraction-simulation studies of PTTK show that the structure of this polymer is analogous to that of melt-crystallised poly(thioetherketone) [-SAr-CO-Ar](n) in which the carbonyl linkages in symmetry-related chains are aligned anti-parallel to one another. and that these bridging units are crystallographically interchangeable. The final model for the crystal structure of PTTK is thus disordered, in the monoclinic space group 121a (two chains per unit cell), with cell dimensions a = 7.83, b = 6.06, c = 10.35 angstrom, beta = 93.47 degrees. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
The family of semi-crystalline, aromatic, high-temperature thermoplastics known as poly(ether-ketone)s are insoluble in conventional organic solvents, but undergo completely general and quantitatively reversible reactions with alkanedithiols in strong acid media, to give soluble poly(dithioacetal)s, which are readily characterisable by GPC and light scattering techniques.
Resumo:
Spontaneous ring-opening polymerization of macrocyclic aromatic thioether ketones [-1,4-SC6H4CO-C6H4-](n) (n = 3 and 4), in which the thioether linkages are para to the ketone, occurs during rapid, transient heating to 480degreesC, to afford a soluble, semi-crystalline poly(thioether ketone) of high molar mass (eta(inh) > 1.0 dL . g(-1)). Corresponding macrocyclic ether ketone, and a macrocyclic thioether ether ketone in which the thioether linkage is para to the ether rather than to the ketone, show no evidence of polymerization under analogous conditions.
Resumo:
Semi-crystalline poly(ether ketone)s are important high-temperature engineering thermoplastics, but are difficult to characterize at the molecular level because of their insolubility in conventional organic solvents. Here we report that polymers of this type, including PEEK, react cleanly at high temperatures with low-volatility aralkyl amines to afford stable, noncrystalline poly(ether-imine)s, which are readily soluble in solvents such as chloroform, THF and DMF and so characterizable by conventional size-exclusion chromatography.
Resumo:
Present work proposed to map and features the wear mechanisms of structural polymers of engineering derived of the sliding contact with a metallic cylindrical spindle submitted to eccentricity due to fluctuations in it is mass and geometric centers. For this it was projected and makes an experimental apparatus from balancing machine where the cylindrical counterbody was supported in two bearings and the polymeric coupon was situated in a holder with freedom of displacement along counterbody. Thus, the experimental tests were standardized using two position of the two bearings (Fixed or Free) and seven different positions along the counterbody, that permit print different conditions to the stiffness from system. Others parameters as applied normal load, sliding velocity and distance were fixed. In this investigation it was used as coupon two structural polymers of wide quotidian use, PTFE (polytetrafluroethylene) and PEEK (poly-ether-ether-ketone) and the AISI 4140 alloy steel as counterbody. Polymeric materials were characterized by thermal analysis (thermogravimetric, differential scanning calorimetry and dynamic-mechanical), hardness and rays-X diffractometry. While the metallic material was submitted at hardness, mechanical resistance tests and metallographic analysis. During the tribological tests were recorded the heating response with thermometers, yonder overall velocity vibration (VGV) and the acceleration using accelerometers. After tests the wear surface of the coupons were analyzed using a Scanning Electronic Microscopy (SEM) to morphological analysis and spectroscopy EDS to microanalysis. Moreover the roughness of the counterbody was characterized before and after the tribological tests. It was observed that the tribological response of the polymers were different in function of their distinct molecular structure. It were identified the predominant wear mechanisms in each polymer. The VGV of the PTFE was smaller than PEEK, in the condition of minimum stiffness, in function of the higher loss coefficient of that polymer. Wear rate of the PTFE was more of a magnitude order higher than PEEK. With the results was possible developed a correlation between the wear rate and parameter (E/ρ)1/2 (Young modulus, E, density, ρ), proportional at longitudinal elastic wave velocity in the material.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Pyroelectric sensors work as a thermal transducer converting the non-quantified thermal flux into the output measurable quantity of electrical charge, voltage or current. Ferroelectric ceramics and ferroelectric polymers have been extensively used as thermal detectors. More recently the research in the field of pyroelectricity has been concentrated on discovering materials with higher figures of merit (FOM), which means better sensing materials. Composite materials obtained with ferroelectric ceramics embedded in polymer host have received great attention because of their formability, mechanical resistance and the possibility to change their dielectric property varying the volume fraction of ceramic particles. In this work composite films made of modified lead titanate (PZ34) and poly(ether-ether-ketone) (PEEK) were characterized and used as sensing element to measure X-ray intensity in the ortovoltage range (120 - 300 kVp). The sensor response varies from 2.70 V to 0.80 V in the energy fluency range of 6.30 to 37.20 W/m(2). Furthermore the absorbed energy was analyzed as a function of the ionizing energy. The results indicate that the PZ34/PEEK composite with 60/40 vol.% can be useful to monitor X-ray radiation therapy.
Resumo:
Composites made of Calcium-modified lead titanate (PTCa) and poly (ether-etherketone) (PEEK) high performance polymer matrix were prepared in the film form using a hot press. The ceramic volume fraction reaches up to 60 percent providing a composite with 0-3 and 1-3 mixed connectivities due to the high ceramic content and the resulting materials could be considered PEEK-bonded PTCa particulate composite. The composites were characterized using piezoelectric spectroscopy and ultrasonic immersion techniques. Values up to 38.5 pC/N were obtained for the longitudinal d33 piezoelectric coefficient. The composite was surface-mounted on a carbon fiber plate-like specimen and the ability of the PTCa/PEEK composite to detect acoustic emission (AE) is reported. © 2006 IEEE.