The development of high performance ceramics and ceramic composites often relies on assumptions about their behaviour during loading and at failure. A crucial influence on the mechanical properties of these materials is the degree of sub-critical cracking, which post mortem investigations cannot adequately reveal. Hence a clear picture of the dynamic micromechanisms of cracking is required if applications of fracture and damage mechanics to theoretical models is to be meaningful.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

CaCu3Ti(4-x)Nb(x)O(12) (x = 0, 0.01, 0.08, 0.2) ceramics were fabricated by a conventional solid-state reaction method. The ceramics showed the body-centered cubic structure without any foreign phases and the grain size decreases with Nb doping. Two Debye-type relaxations were observed for the Nb-doped samples at low frequency and high frequency, respectively. The complex electric modulus analysis revealed that the surface layer, grains and grain boundaries contributed to the dielectric constant. The low-frequency dielectric constant relative to the surface layer decreased to a minimum and then increased with the dc bias voltage at 100 Hz, which were well explained in terms of a model containing two metal oxide semiconductors in series, confirming the surface layer in the ceramics. The shift voltage V-B corresponding to the minimal capacitance increased with increase of the composition x. (C) 2009 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

SPIE; COS; Wuhan Municipal Government

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Porous silicon nitride/silicon oxynitride composite ceramics were fabricated by silica sol infiltration of aqueous gelcasting prefabricated Si3N4 green compact. Silica was introduced by infiltration to increase the green density of specimens, so suitable properties with low shrinkage of ceramics were achieved during sintering at low temperature. Si2N2O was formed through reaction between Si3N4 and silica sol at a temperature above 1550 degrees C. Si3N4/Si2N2O composite ceramics with a low linear shrinkage of 1.3-5.7%, a superior strength of 95-180 MPa and a moderate dielectric constant of 4.0-5.0 (at 21-39 GHz) were obtained by varying infiltration cycle and sintering temperature. (C) 2010 Published by Elsevier B.V.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A critical Biot number, which determines both the sensitivity of spherical ceramics to quenching and the durations of the temperature-wave propagation and the thermal stresses in the ceramics subjected to thermal shock, is theoretically obtained. The results prove that once the Biot number of a ceramic sphere is greater than the critical number, its thermal shock failure will be such a rapid process that the failure only occurs in the initial regime of heat conduction, whereas the thermal shock failure of the ceramic sphere is uncertain in the course of heat conduction. The presented results provide a guide to the selection of the ceramics applied in the thermostructural engineering with thermal shock.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We propose here a new method to make ceramics insensitive to thermal shock up to their melting temperature. In this method the surface of ceramics was biomimetically roughened into nanofinned surface that creates a thin air layer enveloping the surface of the ceramics during quenching. This air layer increases the heat transfer resistance of the surface of the ceramics by about 10 000 times so that the strong thermal gradient and stresses produced by the steep temperature difference in thermal shock did not occur both on the actual surface and in the interior of the ceramics. This method effectively extends the applications of existing ceramics in the extreme thermal environments.