996 resultados para Solani Ag-8
Resumo:
Bi-2212 tapes are prepared by a combination of dip-coating and partial melt processing. We investigate the effect of re-melting of those tapes by partial melting followed by slow cooling on the structure and superconducting properties. Microstructural studies of re-melted samples show that they have the same overall composition as partially melted tapes. However, the fractional volumes of the secondary phases differ and the amounts and distribution of the secondary phases have a significant effect on the critical current. Critical current of Bi-2212/Ag tapes strongly depends on the maximum processing temperature. Initial J(c)'s of the tapes, which are partially melted, then slowly solidified at optimum conditions and finally post-annealed in an inert atmosphere, are up to 10.4 x 10(3) A/cm(2). It is found that the maximum processing temperature at initial partial melting has an influence on the optimum re-heat treatment conditions for the tapes. Re-melted tapes processed at optimum conditions recover superconducting properties after post-annealing in an inert atmosphere: the J(c) values of the tapes are about 80-110% of initial J(c)'s of those tapes.
Resumo:
Different types of HTS joints of Bi-2212/Ag tapes and laminates, which are fabricated by dip-coating and partial-melt processes, have been investigated. All joints are prepared using green single and laminated tapes and according to the scheme: coating-joining-processing. The heat treated tapes have critical current (Ic) between 7 and 27 A, depending on tape thickness and the number of Bi-2212 ceramic layers in laminated tapes. It is found that the current transport properties of joints depend on the type of laminate, joint configuration and joint treatment, Ic losses in joints of Bi-2212 tapes and laminates are attributed to defects in their structure, such as pores, secondary phases and misalignment of Bi-2212 grains near the Ag edges. By optimizing joint configuration, current transmission up to 100% is achieved for both single tapes and laminated tapes.
Resumo:
Superconducting Bi-2212 tapes and laminates are fabricated by a combination of dip-coating and partial melt processing. The heat treated tapes have critical current densities (Jc) up to 11 kAcm -2. We investigate the degradation of critical current (Ic) during bending experiments for both single tapes and tapes with laminate structure. Although degradation of Ic is observed in both forms, the characteristics of the degradation differ. It is determined that laminated tapes perform better than single tapes when critical current is measured against bending radius, and laminated tapes tolerate a higher strain for a given reduction in critical current. It is found that increasing the number of Bi-2212 layers increases the total Ic of the laminated tape, but degradation of critical current is more pronounced during bending because of the increased total thickness of the laminate structure. It is also found that addition of silver to the Bi-2212 layers reduces critical current degradation during bending for both tapes and laminates.
Resumo:
Superconducting thick films of Bi2Sr2CaCu2Oy (Bi-2212) on single-crystalline (100) MgO substrates have been prepared using a doctor-blade technique and a partial-melt process. It is found that the phase composition and the amount of Ag addition to the paste affect the structure and superconducting properties of the partially melted thick films. The optimum heat treatment schedule for obtaining high Jc has been determined for each paste. The heat treatment ensures attainment of high purity for the crystalline Bi-2212 phase and high orientation of Bi-2212 crystals, in which the c-axis is perpendicular to the substrate. The highest Tc, obtained by resistivity measurement, is 92.2 K. The best value for Jct (transport) of these thick films, measured at 77 K in self-field, is 8 × 10 3 Acm -2.
Resumo:
The assembly of retroviruses such as HIV-1 is driven by oligomerization of their major structural protein, Gag. Gag is a multidomain polyprotein including three conserved folded domains: MA (matrix), CA (capsid) and NC (nucleocapsid)(1). Assembly of an infectious virion proceeds in two stages(2). In the first stage, Gag oligomerization into a hexameric protein lattice leads to the formation of an incomplete, roughly spherical protein shell that buds through the plasma membrane of the infected cell to release an enveloped immature virus particle. In the second stage, cleavage of Gag by the viral protease leads to rearrangement of the particle interior, converting the non-infectious immature virus particle into a mature infectious virion. The immature Gag shell acts as the pivotal intermediate in assembly and is a potential target for anti-retroviral drugs both in inhibiting virus assembly and in disrupting virus maturation(3). However, detailed structural information on the immature Gag shell has not previously been available. For this reason it is unclear what protein conformations and interfaces mediate the interactions between domains and therefore the assembly of retrovirus particles, and what structural transitions are associated with retrovirus maturation. Here we solve the structure of the immature retroviral Gag shell from Mason-Pfizer monkey virus by combining cryo-electron microscopy and tomography. The 8-angstrom resolution structure permits the derivation of a pseudo-atomic model of CA in the immature retrovirus, which defines the protein interfaces mediating retrovirus assembly. We show that transition of an immature retrovirus into its mature infectious form involves marked rotations and translations of CA domains, that the roles of the amino-terminal and carboxy-terminal domains of CA in assembling the immature and mature hexameric lattices are exchanged, and that the CA interactions that stabilize the immature and mature viruses are almost completely distinct.
Resumo:
Metal and semiconductor nanowires (NWs) have been widely employed as the building blocks of the nanoelectromechanical systems, which usually acted a resonant beam. Recent researches reported that nanowires are often polycrystalline, which contains grain boundaries (GBs) that transect the whole nanowire into a bamboo like structure. Based on the larger-scale molecular dynamics (MD) simulations, a comprehensive investigation of the influence from grain boundaries on the vibrational properties of doubly clamped Ag NWs is conducted. It is found that, the presence of grain boundary will result in significant energy dissipation during the resonance of polycrystalline NWs, which leads a great deterioration to the quality factor. Further investigation reveals that the energy dissipation is originated from the plastic deformation of polycrystalline NWs in the form of the nucleation of partial dislocations or the generation of micro stacking faults around the GBs and the micro stacking faults is found to keep almost intact during the whole vibration process. Moreover, it is observed that the closer of the grain boundary getting to the regions with the highest strain state, the more energy dissipation will be resulted from the plastic deformation. In addition, either the increase of the number of grain boundaries or the decrease of the distance between the grain boundary and the highest strain state region is observed to induce a lower first resonance frequency. This work sheds lights on the better understanding of the mechanical properties of polycrystalline NWs, which benefits the increasing utilities of NWs in diverse nano-electronic devices.
Resumo:
Background: Extracorporeal circulation (ECC), the diversion of blood flow through a circuit located outside of the body, has been one of the major advances in modern medicine. Cardio-pulmonary bypass (CPB), renal dialysis, apheresis and extracorporeal membrane oxygenation (ECMO) are all different forms of ECC. Despite its major benefits, when blood comes into contact with foreign material, both the coagulation and inflammation cascades are activated simultaneously. Short periods of exposure to ECC e.g. CPB (�2 h duration), are known to be associated with haemolysis, coagulopathies, bleeding and inflammation which demand blood product support. Therefore, it is not unexpected that these complications would be exaggerated with prolonged periods of ECC such as in ECMO (days to weeks duration). The variability and complexities of the underlying pathologies of patients requiring ECC makes it difficult to study the cause and effect of these complications. To overcome this problem we developed an ovine (sheep) model of ECC. Method: Healthy female sheep (1–3 y.o.) weighing 40–50 kg were fasted overnight, anaesthetised, intubated and ventilated [1]. Half the group received smoke induced acute lung injury (S-ALI group) (n = 8) and the other half did not (healthy group) (n = 8). Sheep were subsequently cannulated (Medtronic Inc, Minneapolis, MN, USA) and veno-venous ECMO commenced using PLS ECMO circuit and Quadrox D oxygenator (Maquet Cardiopulmonary AG, Hechinger Straße, Germany). There was continuous physiological monitoring and blood was collected at specified time intervals for full blood counts, platelet function analysis (by Multiplate®), routine coagulation and assessment of clot formation and lysis (by ROTEM®). Preliminary results Full blood counts and routine coagulation results from normal healthy sheep were comparable to those of normal human adults. Within 15 min of initiating of ECMO, PT, PTT and EXTEM clot formation time increased, whilst EXTEM maximum clot firmness decreased in both cohorts. Discussion & Conclusions: Preliminary results of sheep from both 2 h ECMO cohorts showed that the anatomy, haematology and coagulation parameters of an adult sheep are comparable to that a human adult. Experiments are currently underway with healthy (n = 8) and S-ALI (n = 8) sheep on ECMO for 24 h. In addition to characterising how ECMO alters haematology and coagulation parameters, we hope that it will also define which blood components will be most effective to correct bleeding or clotting complications during ECMO support.
Resumo:
In this paper, the formation of heteroepitaxial interfacial layers was investigated by molecular dynamics simulation of soft silver particles landing on the (001) surface of single-crystal copper. In our simulations, the clusters Ag13, Ag55, Ag147 and Ag688 were chosen as projectiles. A small cluster will rearrange into an f.c.c. structure when it is supported on the substrate, due to the large value of its surface/volume ratio. Contact epitaxy appeared in large clusters. The characteristic structure of an epitaxial layer in large silver cluster shows the 〈111〉 direction to be the preferential orientation of heteroepitaxial layers on the surface because of the lattice mismatch between the cluster and the substrate. This was confirmed by studying soft landing events in other systems (Au/Cu and Al/Ni).
Resumo:
Multiple sclerosis (MS) is a serious cause of neurological disability among young adults. The clinical course remains difficult to predict, and the pathogenesis of the disease is still modestly understood. Autoimmunity is thought to be a key aspect of the disease, with autoreactive T cells thought to mediate central nervous system (CNS) inflammation to some extent. Toll-like receptors are known to mediate cellular recognition of pathogens by way of patterns of molecular presentation. Toll-like receptor 3 is coded by the gene TLR3 and is recognized as an important factor in virus recognition and is known to be involved in the expression of neuroprotective mediators. We set out to investigate two variations within the TLR3 gene, an 8 bp insertion-deletion \[-/A](8) and a single base-pair variation C1236T, in subjects with MS and matched healthy controls to determine whether significant differences exist in these markers in an Australian population. We used capillary gel electrophoresis and TaqMan genotyping assay techniques to resolve genotypes for each marker, respectively. Our work found no significant difference between frequencies for TLR3 \[-/A](8) by genotype (chi(2)=1.03, p=0.60) or allele (chi(2)=1.09, p=0.30). Similarly, we found no evidence for the association of TLR3 C1236T by genotype (chi(2)=0.35, p=0.84) or allele frequency (chi(2)=0.31, p=0.58). This work reveals no evidence to suggest that these markers are associated with MS in the tested population. Although the role of TLR3 and the wider toll-like receptor family remain significant in neurological and CNS inflammatory disorders, our current work does not support a role for the two tested variants in this gene with regard to MS susceptibility.
Resumo:
Migraine is a common, genetically influenced neurovascular disorder. The dopamine transporter gene is a candidate for migraine association studies. This study tested a functionally linked variable number tandem repeat (VNTR) in intron 8 of the dopamine transporter gene (DATInt8) in 550 migraine cases (401 with aura, 149 without aura) and 550 non-migraine controls. Chi-squared analysis of the DATInt8 revealed that the allele and genotype frequency distributions for migraine cases (including subtype analysis) and controls were not different (P > 0.1). These findings offer no evidence for an association of the DATInt8 with migraine with and without aura and therefore do not implicate the dopamine transporter gene as a modifier of migraine risk.
Resumo:
Materials used in the engineering always contain imperfections or defects which significantly affect their performances. Based on the large-scale molecular dynamics simulation and the Euler–Bernoulli beam theory, the influence from different pre-existing surface defects on the bending properties of Ag nanowires (NWs) is studied in this paper. It is found that the nonlinear-elastic deformation, as well as the flexural rigidity of the NW is insensitive to different surface defects for the studied defects in this paper. On the contrary, an evident decrease of the yield strength is observed due to the existence of defects. In-depth inspection of the deformation process reveals that, at the onset of plastic deformation, dislocation embryos initiate from the locations of surface defects, and the plastic deformation is dominated by the nucleation and propagation of partial dislocations under the considered temperature. Particularly, the generation of stair-rod partial dislocations and Lomer–Cottrell lock are normally observed for both perfect and defected NWs. The generation of these structures has thwarted attempts of the NW to an early yielding, which leads to the phenomenon that more defects does not necessarily mean a lower critical force.