978 resultados para Materials testing laboratories


Relevância:

80.00% 80.00%

Publicador:

Resumo:

The aim of this study was to investigate the effects of mineral trioxide aggregate (MTA), Sealapex, and a combination of Sealapex and MTA (Sealapex Plus) on the reaction of subcutaneous connective tissue of rats, and on cell viability and cytokine production in mouse fibroblasts. The tissue reaction was carried out with dentin tubes containing the materials implanted in the dorsal connective tissue of rats. The histological analysis was performed after 7 and 30 days. Millipore culture plate inserts with polyethylene tubes filled with materials were placed into 24-well cell culture plates with mouse fibroblasts to evaluate the cell viability by MTT assay. ELISA assays were also performed after 24 h of exposure of the mouse fibroblasts to set material disks. Histopathologic examination showed Von Kossa-positive granules that were birefringent to polarized light for all the studied materials at the tube openings. No material inhibited the cell viability in the in vitro test. It was detected IL-6 production in all root-end filling materials. MTA and Sealapex Plus induced a slight raise of mean levels of IL-1β. The results suggest that Sealapex Plus is biocompatible and stimulates the mineralization of the tissue.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Purpose: To evaluate the shear bond strength and bond durability between a dual-cured resin cement (RC) and a high alumina ceramic (In-Ceram Alumina), subjected to two surface treatments. Materials and Methods: Forty disc-shaped specimens (sp) (4-mm diameter, 5-mm thick) were fabricated from In-Ceram Alumina and divided into two groups (n = 20) in accordance with surface treatment: (1) sandblasting by aluminum oxide particles (50 μm Al 2O 3) (SB) and (2) silica coating (30 μm SiO x) using the CoJet system (SC). After the 40 sp were bonded to the dual-cured RC, they were stored in distilled water at 37°C for 24 hours. After this period, the sp from each group were divided into two conditions of storage (n = 10): (a) 24 h-shear bond test 24 hours after cementation; (b) Aging-thermocycling (TC) (12,000 times, 5 to 55°C) and water storage (150 days). The shear test was performed in a universal test machine (1 mm/min). Results: ANOVA and Tukey (5%) tests noted no statistically significant difference in the bond strength values between the two surface treatments (p= 0.7897). The bond strengths (MPa) for both surface treatments reduced significantly after aging (SB-24: 8.2 ± 4.6; SB-Aging: 3.7 ± 2.5; SC-24: 8.6 ± 2.2; SC-Aging: 3.5 ± 3.1). Conclusion: Surface conditioning using airborne particle abrasion with either 50 μm alumina or 30 μm silica particles exhibited similar bond strength values and decreased after long-term TC and water storage for both methods. © 2011 by The American College of Prosthodontists.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The purpose of this in vitro study was to evaluate the effect of neodymium:yttrium-aluminum-garnet (Nd:YAG) laser irradiation on intracanal dentin surface by SEM analysis and its interference in the apical seal of filled canals. After endodontic treatment procedures, 34 maxillary human incisors were randomly assigned to 2 groups. In the negative control group (n=17), no additional treatment was performed and teeth were filled with vertically condensed gutta-percha; in the laser-treated group (n=17), the root canals were irradiated with Nd:YAG laser (1.5 W, 100 mJ, 15 Hz) before filling as described for the control group. Two specimens of each group were prepared for SEM analysis to evaluate the presence and extent of morphological changes and removal of debris; the other specimens were immersed in 0.5% methylene blue dye (pH 7.2) for 24 h for evaluation of the linear dye leakage at the apical third. SEM analysis of the laser-treated group showed dentin fusion and resolidification without smear layer or debris. The Student's t-test showed that the laser-treated group had significantly less leakage in apical third than the control group. Within the limitations of this study, it may be concluded that the morphological changes on the apical intraradicular dentin surface caused by Nd:YAG laser resulted in less linear dye apical leakage.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Objectives: The present study used strain gauge analysis to perform an in vitro evaluation of the effect of axial loading on 3 elements of implant-supported partial fixed prostheses, varying the type of prosthetic cylinder and the loading points. Material and methods: Three internal hexagon implants were linearly embedded in a polyurethane block. Microunit abutments were connected to the implants applying a torque of 20 Ncm, and prefabricated Co-Cr cylinders and plastic prosthetic cylinders were screwed onto the abutments, which received standard patterns cast in Co-Cr alloy (n = 5). Four strain gauges (SG) were bonded onto the surface of the block tangentially to the implants, SG 01 mesially to implant 1, SG 02 and SG 03 mesially and distally to implant 2, respectively, and SG 04 distally to implant 3. Each metallic structure was screwed onto the abutments with a 10 Ncm torque and an axial load of 30 kg was applied at five predetermined points (A, B, C, D, E). The data obtained from the strain gauge analyses were analyzed statistically by RM ANOVA and Tukey's test, with a level of significance of p<0.05. Results: There was a significant difference for the loading point (p=0.0001), with point B generating the smallest microdeformation (239.49 με) and point D the highest (442.77 με). No significant difference was found for the cylinder type (p=0.748). Conclusions: It was concluded that the type of cylinder did not affect in the magnitude of microdeformation, but the axial loading location influenced this magnitude.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Purpose: Staining of prosthodontic materials may result in patient dissatisfaction and additional expense for replacement. This study aimed to determine the color stability of two heat-cured denture base acrylic (Lucitone 550, Vipi Cril) and one nylon denture base resin (Transflex) after immersion in beverages. Materials and Methods: Forty disks of each resin (20.0-mm diameter, 3.0-mm thick) were prepared and stored in distilled water for 24 hours at 37°C. During that time (T 0), the color of all specimens was spectrophotometrically measured. Each specimen was immersed in coffee, cola, red wine, and distilled water as a means of control. After 15-day (T 1) and 30-day (T 2) periods of immersion, the color of the specimens was measured again. The CIE (Commission Internationale de L' Eclairage) L*a*b* system was used to determine mean ΔE (color changes) values for each material and compared statistically with two-way ANOVA and Bonferroni intervals at 0.95. Results: In ΔET 0T 1 and ΔET 0T 2 the most severe staining was apparent with red wine (p < 0.001), followed by coffee (p < 0.01), when compared to the specimens stored in distilled water. Transflex also showed significant color change after immersion in cola (p < 0.01). In ΔET 1T 2 only red wine promoted significant staining of all resins (p < 0.0001). Conclusion: Chromatic changes were exhibited by specimens immersed in red wine, followed by coffee. For Transflex, cola also promoted color changes. The values of color changes converted to National Bureau of Standard units showed them to be perceivable to the human eye. © 2011 by the American College of Prosthodontists.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The objective of this study was to evaluate the use of a two-step total etch and rinse adhesive, the correlation between the hyybrid layer thickness (HL) and bond strength (BS), and between resin tag length (RT) and bond strength in the same teeth, and also to evaluate the fracture patterns of the tested specimens. Ten human molars were used for the restorative procedure and then sectioned in two halves (mesio-distally). The materials used were Adper Single Bond 2, 3M ESPE, Ultra etch gel, Ultradent and Filtek Z250, 3M ESPE. One half were utilized to measure the HL thickness and RT length through light microscopy analysis (400x), and the other half was subject to a microtensile test to measure the BS. The fractured surfaces were analyzed by scanning electron microscopy and fracture patterns classified. The Pearson correlation test was applied (p = 0.05). The results of the analyses of each specimen then were correlated: mean HL thickness = 4.39 (0.48) microm, mean length of RT = 9.94 (1.69) microm, mean BS = 23.98 (10.24) MPa. A statistically significant correlation between HL thickness and bond strength was found (r = 0.93). The two step etch and rinse adhesive system, showed a strong correlation between HL thickness and bond strength. The most common fractures were adhesive, followed by cohesive in resin.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The purpose of this study was to evaluate the correlation between the hybrid layer thickness/resin tag length and the microtensile bond strength of conventional two-step adhesive system, when applied to healthy dentinal tissue. After performing the restorative adhesive procedures and tooth extractions, ten specimens were sectioned in the mesiodistal direction. One section was used for microscopic analysis of the resin tag lengths and the hybrid layer thickness, while the other was used for the microtensile bond strength test (0.5 mm/min). The fractured surface was classified according to the fracture pattern, under a stereoscopic microscope at 40x magnification. Data obtained were submitted to analysis using one-way ANOVA and Pearson's Correlation test (alpha=0.05). The means corresponding to the hybrid layer thickness, resin tag lengths and the microtensile test were 2.68 microm, 6.43 microm and 16.23 MPa, respectively. There was no correlation between the means of the values obtained for the microtensile test, and those presented by the hybrid layer (r2=0.40, p>0.05) and resin tags (r2=0.21, p>0.05). The microtensile bond strength of the conventional two-step adhesive system Adper Single Bond 2 did not depend on the thickness of the hybrid layer and length of resin tags.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coloring in drinks decreases the color stability of composite restorations, reducing their longevity. The purpose of this in vitro study was to evaluate the effect of immersion media on color stability of seven different composite resins (Solidex - Shofu, Resilab-Wilcos, Signum - Heraeus, Epricord - Tokuyama, Adoro - Ivoclar Vivadent, Admira - Voco and Sinfony - 3MESPE). Seven resin-based composite specimens were prepared using a cylindrical teflon mold 2 mm thick and 10 mm in diameter Fifteen specimens of each resin were light-cured according to manufacturers' instructions and randomized into 3 groups (n= 5) according to immersion media: coffee, cola beverage and water A digital spectrophotometer Easy Shade (VITA) was used to evaluate the color changes at baseline and 7 days after immersion in each solution. Specimens were stored in the different staining media for 24 h/day during one week. The color differences were analyzed by two-way ANOVA and Tukey 's test (p< 0.05). Color change was observed after one week of immersion and there were statistical differences in staining, composite and interaction factors. The least staining was observed in Admira (deltaE= 3.934+/-0.814) and Resilab (deltaE= 3.993+/-0.735), followed by Adoro (deltaE= 4.044+/-1.001), Epri-cord (deltaE= 4.049+/-1.234), Signum (deltaE= 4.260+/-1.785), Solidex (deltaE=5,122+/-0.534) and Sinfony (deltaE=5.126+/-0.838). All of the composites tested except Adoro were susceptible to staining by substances present in coffee and cola, when stored in beverage for seven days. The lowest deltaE means were obtained with Admira.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

This research work develops new methods to produce biodegradable starch-based trays for the purpose of replacing expanded polystyrene in the food packaging market. The starch based biopolymers present several drawbacks like poor mechanical properties and very high density. In order to overcome these drawbacks two research lines have been set up: blending thermoplastic starch with biobased reinforcements from agricultural wastes like barley straw and grape wastes, and testing the foamability of these materials with a Microwave-foaming method.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The aim of this study was to evaluate the effect of specific parameters of low-level laser therapy (LLLT) on biofilms formed by Streptococcus mutans, Candida albicans or an association of both species. Single and dual-species biofilms - SSB and DSB - were exposed to laser doses of 5, 10 or 20 J/cm 2 from a near infrared InGaAsP diode laser prototype (LASERTable; 780 ± 3 nm, 0.04 W). After irradiation, the analysis of biobilm viability (MTT assay), biofilm growth (cfu/mL) and cell morphology (SEM) showed that LLLT reduced cell viability as well as the growth of biofilms. The response of S. mutans (SSB) to irradiation was similar for all laser doses and the biofilm growth was dose dependent. However, when associated with C. albicans (DSB), S. mutans was resistant to LLLT. For C. albicans, the association with S. mutans (DSB) caused a significant decrease in biofilm growth in a dose-dependent fashion. The morphology of the microorganisms in the SSB was not altered by LLLT, while the association of microbial species (DSB) promoted a reduction in the formation of C. albicans hyphae. LLLT had an inhibitory effect on the microorganisms, and this capacity can be altered according to the interactions between different microbial species.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Introduction: The aim of this study was to evaluate the pH, calcium ion release, setting time, and solubility of white mineral trioxide aggregate (WMTA) and white Portland cement (WPC) combined with the following radiopacifying agents: bismuth oxide (BO), calcium tungstate (CT), and zirconium oxide (ZO). Methods: Fifty acrylic teeth with root-end filling material were immersed in ultrapure water for measurement of pH and calcium release (atomic absorption spectrophotometry) at 3, 24, 72, and 168 hours. For evaluation of setting time, each material was analyzed according to the American Society for Testing and Materials guidelines 266/08. The solubility test was performed according to American National Standards Institute/American Dental Association specification no. 57/2000. Solubility, setting time, and pH values were compared by using analysis of variance and Tukey test, and the values of calcium release were compared by the Kruskal-Wallis and Miller tests. The significance level was set at 5%. Results: The pH and calcium release were higher at 3 and 24 hours. WPC was the material with the higher values for both properties. WMTA had the greatest solubility among all materials (P <.05). All radiopacifiers increased the setting time of WPC, and WMTA had the shortest setting time among all materials (P < .05). Conclusions: All materials released calcium ions. Except for WPC/CT at 168 hours, all materials promoted an alkaline pH. On the basis of the obtained results, ZO and CT can be considered as potential radiopacifying agents to be used in combination with Portland cement. Copyright © 2012 American Association of Endodontists.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The objective of this study was to evaluate the influence of different primers on the microtensile bond strength (μT BS) between a feldspathic ceramic and two composites. Forty blocks (6.0 × 6.0 × 5.0 mm 3) were prepared from Vita Mark II . After polishing, they were randomly divided into 10 groups according to the surface treatment: Group 1, hydrofluoric acid 10% (HF) + silane; Group 2, CoJet + silane; Group 3, HF + Metal/Zirconia Primer; Group 4, HF + Clearfil Primer; Group 5, HF + Alloy Primer; Group 6, HF + V-Primer; Group 7, Metal/Zirconia Primer; Group 8, Clearfil Primer; Group 9, Alloy Primer; Group 10, V-Primer. After each surface treatment, an adhesive was applied and one of two composite resins was incrementally built up. The sticks obtained from each block (bonded area: 1.0 mm2 ± 0.2 mm) were stored in distilled water at 37°C for 30 days and submitted to thermocycling (7,000 cycles; 5°C/55°C ± 1°C). The μT BS test was carried out using a universal testing machine (1.0 mm/min). Data were analyzed using ANOVA and a Tukey test (α = 0.05). The surface treatments significantly affected the results (P < 0.05); no difference was observed between the composites (P > 0.05). The bond strength means (MPa) were as follows: Group 1a = 29.6; Group 1b = 33.7; Group 2a = 28.9; Group 2b = 27.1; Group 3a = 13.8; Group 3b = 14.9; Group 4a = 18.6; Group 4b = 19.4; Group 5a = 15.3; Group 5b = 16.5; Group 6a = 11; Group 6b = 18; Groups 7a to 10b = 0. While the use of primers alone was not sufficient for adequate bond strengths to feldspathic ceramic, HF etching followed by any silane delivered higher bond strength.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The aim of the present study was to evaluate the effect of disinfection and accelerated ageing on the dimensional stability and detail reproduction of a facial silicone with different types of nanoparticle. A total of 60 specimens were fabricated with Silastic MDX 4-4210 silicone and they were divided into three groups: colourless and pigmented with nanoparticles (make-up powder and ceramic powder). Half of the specimens of each group were disinfected with Efferdent tablets and half with neutral soap for 60 days. Afterwards, all specimens were subjected to accelerated ageing. Both dimensional stability and detail reproduction tests were performed after specimen fabrication (initial period), after chemical disinfection, and after accelerated ageing periods (252, 504 and 1008 hours). The dimensional stability test was conducted using AutoCAD software, while detail reproduction was analysed using a stereoscope magnifying glass. Dimensional stability values were statistically evaluated by analysis of variance (ANOVA) followed by Tukey's test (p < 0.01). Detail reproduction results were compared using a score. Chemical disinfection and also accelerated ageing affected the dimensional stability of the facial silicone with statistically significant results. The silicone's detail reproduction was not affected by these two factors regardless of nanoparticle type, disinfection and accelerated ageing. © 2012 Informa UK, Ltd.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The aim of this study was to evaluate the effect of conventional and whitening dentifrices on the weight loss, surface roughness, and early in situ biofilm formation on the surface of dental ceramics. Standardized feldspar ceramic specimens (Vita VM7 and Vita VM13) were submitted to the following experimental conditions: no brushing; brushing without a dentifrice; brushing with a conventional dentifrice; and brushing with a whitening dentifrice. A brushing machine was used to simulate brushing. The mass and surface roughness of all specimens from the test groups were evaluated prior to and after brushing. Ten participants used an oral device for eight hours to evaluate the biofilm formed in situ on the specimens. Scanning electron microscopy was used for qualitative and quantitative analysis of the biofilm. ANOVA and Tukey tests were used to analyze the results of weight loss, surface roughness, and presence of bacteria. A one-way Kruskal-Wallis test was used for bacterial colonization results. For both ceramics, brushing with a whitening dentifrice resulted in weight loss that was significantly greater when compared to brushing without a dentifrice or with a conventional dentifrice. Increased surface roughness was noticed on VM13 ceramic samples with both dentifrices, whereas only conventional dentifrice had a significant effect on the surface roughness of VM7 samples. For both VM7 and VM13, no difference was found between the experimental conditions with regard to the presence or number of bacteria. Cocci and short rods were the predominant microbial morphotypes. Granular or fibrillar acellular material partially covered the specimens. Brushing with a whitening dentifrice resulted in significant weight loss of ceramic restorations, while brushing with both conventional and whitening dentifrices can roughen ceramic surfaces. The increase in roughness was not clinically significant to contribute to increased biofilm formation.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Purpose: Bioactive glass and bioactive glass-ceramic cone implants were placed in the rabbit eviscerated socket to assess their biocompatibility. Methods: Fifty-one Norfolk albino rabbits underwent evisceration of the right eye followed by implantation of cones made from Bioglass® 45S5 (control group) and two types of bioactive glass-ceramic (Biosilicate®), a single- and a two-phase bioactive glass-ceramic implants into the scleral cavity. Postoperative reactions, animal behavior and socket conditions were monitored daily. Clinical exam, biochemical evaluations, and orbit computed tomographic scan were done at 7, 90, and 180 days post-procedure. After that, the animals were euthanized, and the orbital content was removed and prepared to light microscopy with morphometric evaluation and scanning electron microscopy examination. Statistical analysis was done by parametric and non-parametric analysis of variance, complemented by Dunn's and Tukey's tests (p<0.05). Results: All animals did not develop systemic toxicity throughout the experimental period and also did not have orbit infection, implant migration or extrusion. Morphological analysis demonstrated pseudocapsule around all implants. Bioglass® and single-phase Biosilicate® implants induced less inflammation and pseudocapsule formation than two-phase Biosilicate® cones. Seven days post-procedure, the inflammatory reaction was intense and gradually decreased throughout the experiment. Tissue reaction was least intense in animals receiving Bioglass® implants. Conclusions: We observe discrete differences among the studied materials, with best responses obtained with use of Bioglass® 45S5 and single-phase Biosilicate®. The authors agree these implants might be useful in the management of the anophthalmic socket. © 2012 Informa Healthcare USA, Inc.