921 resultados para ANATASE TIO2(101)


Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this work, crystalline titanium dioxide (TiO2) nanoparticles with variable average crystallite sizes (e.g., 8 nm) and surface areas (e.g., 192 m² g-1) were synthesized in pure anatase phase using H2O2 to reduce the hydrolysis rate of the titanium ions. An isopropanol (IP) solution was employed as the reaction medium. The TiO2 nanoparticles were characterized by powder X-ray diffraction analysis (XRD), Raman spectroscopy and transmission electron microscopy (TEM). By changing the synthesis parameters it was possible to control nanoparticle size and avoid the coalescence process. A dependence of the Raman wavenumber on the nanocrystal sizes was determined, which is quite useful for a quick check of the size of TiO2 nanocrystals.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Pós-graduação em Química - IQ

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Among the many methods developed for the synthesis of titanium dioxide, cathodic electrosynthesis has not received much attention because the resulting amorphous oxy-hydroxide matrix demands a further thermal annealing step to be transformed into crystalline titania. However, the possibility of filling deep recessed templates by the control of the solidliquid interface makes it a potentially suitable technique for the fabrication of porous scaffolds for photovoltaics and photocatalysis. Furthermore, a careful control of the crystallization process enables the growth of larger grains with lower density of grain boundaries, which act as electron traps that slow down electronic transport and promote charge recombination. In this report, well crystallized titania deposits were obtained by thermal annealing of amorphous deposits fabricated by cathodically assisted electrosynthesis on indium-tin oxide (ITO)substrates. The combined use of Raman spectroscopy and X-ray diffraction showed that the crystallization process is more intricate than previously assumed. It is shown that the amorphous matrix evolves into a rutile-free mixture of brookite and anatase at temperatures as low as 200 degrees C that persists up to 800 degrees C, when pure anatase dominates. The amount of brookite in the brookiteanatase mixture reaches a maximum at 400 degrees C. This very simple method for obtaining a brookiteanatase mixture and the ability to tune their proportions by thermal annealing is a promising alternative whose potential for solar cells and photocatalysis deserves a careful evaluation. Copyright (C) 2011 John Wiley & Sons, Ltd.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

[EN] This article describes a photocatalytic nanostructured anatase coating deposited by cold gas spray (CGS) supported on titanium sub-oxide (TiO22x) coatings obtained by atmospheric plasma spray (APS) onto stainless steel cylinders. The photocatalytic coating was homogeneous and preserved the composition and nanostructure of the starting powder. The inner titanium sub-oxide coating favored the deposition of anatase particles in the solid state. Agglomerated nano-TiO2 particles fragmented when impacting onto the hard surface of the APS TiO22x bond coat. The rough surface provided by APS provided an ideal scenario for entrapping the nanostructured particles, which may be adhered onto the bond coat due to chemical bonding; a possible bonding mechanism is described. Photocatalytic experiments showed that CGS nano-TiO2 coating was active for photodegrading phenol and formic acid under aqueous conditions. The results were similar to the performance obtained by competitor technologies and materials such as dip-coating P25 photocatalysts. Disparity in the final performance of the photoactive materials may have been caused by differences in grain size and the crystalline composition of titanium dioxide.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Analysis of lithology, grain-size composition, clay minerals, and geochemistry of Upper Pleistocene bottom sediments from the submarine Shirshov Ridge (Bering Sea) showed that the Yukon-Tanana terrane of the Central Alaska was main source area of the sediments. Sedimentary material was transported by the Yukon River through Beringia up to the shelf break, where they were entrained by a strong north-west sea current. Lithological data revealed several pulses of ice-rafted debris deposition roughly synchronous with Heinrich events and periods of weaker bottom current intensity. Based on geochemical results we distinguished intervals of an increase in paleoproductivity and extension of the oxygen minimum zone. Our results suggest that there were three stages of deposition driven by glacioeustatic sea-level fluctuations and glacial cycles in Alaska.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Comprehensive investigations revealed that modern deposits in the northern Caspian Sea involve terrigenous sands and aleurites with admixture of detritus and intact bivalve shells, including coquina. Generally, these deposits overlay dark grayish viscous clays. Similar geological situation occurs in the Volga River delta; however, local deposits are much poorer in biogenic constituents. Illite prevails among clay minerals. In coarse aleurite fraction (0.100-0.050 mm) heavy transparent minerals are represented mostly by epidotes, while light minerals - mostly by quartz and feldspars. Sedimentary material in the Volga River delta is far from completely differentiated into fractions due to abundant terrigenous inflows. Comparatively better grading of sediments from the northern Caspian Sea is due to additional factors such as bottom currents and storms. When passing from the Volga River delta to the northern Caspian Sea, sediments are enriched in rare earth elements (except Eu), Ca, Au, Ni, Se, Ag, As, and Sr, but depleted in Na, Rb, Cs, K, Ba, Fe, Cr, Co, Sc, Br, Zr, ??, U, and Th. Concentrations of Zn remain almost unchanged. Sedimentation rates and types of recent deposits in the northern Caspian Sea are governed mainly by abundant runoff of the Volga River.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

TiO2 nanoparticles with tailored morphology have been synthesized under exceptionally soft conditions. The strategy is based on the use of a non-aqueous alcoholic reaction medium in which water traces, coming either from the air (atmospheric water) or from an ethanol–water azeotropic mixture (ethanol 96%), are incorporated in order to accelerate hydrolysis of the Ti–precursor. Moreover, organic surfactants have been used as capping agents so as to tailor crystal growth in certain preferential directions. Combinations of oleic acid and oleylamine, which lead to the formation of another surfactant, dioleamide, are employed instead of fluorine-based compounds, thus increasing the sustainability of the process. As a result, TiO2 nanostructured hierarchical microspheres and individual nanoparticles with exposed high-energy facets can be obtained at atmospheric pressure and temperatures as low as 78 °C.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nanostructured TiO2 photocatalysts with small crystalline sizes have been synthesized by sol-gel using the amphiphilic triblock copolymer Pluronic P123 as template. A new synthesis route, based on the treatment of TiO2 xerogels with acid-ethanol mixtures in two different steps, synthesis and extraction-crystallization, has been investigated, analyzing two acids, hydrochloric and hydriodic acid. As reference, samples have also been prepared by extraction-crystallization in ethanol, being these TiO2 materials amorphous and presenting higher porosities. The prepared materials present different degrees of crystallinity depending on the experimental conditions used. In general, these materials exhibit high surface areas, with an important contribution of microporosity and mesoporosity, and with very small size anatase crystals, ranging from 5 to 7 nm. The activity of the obtained photocatalysts has been assessed in the oxidation of propene in gas phase at low concentration (100 ppmv) under a UVA lamp with 365 nm wavelength. In the conditions studied, these photocatalysts show different activities in the oxidation of propene which do not depend on their surface areas, but on their crystallinity and band gap energies, being sample prepared with HCl both during synthesis and in extraction-crystallizations steps, the most active one, with superior performance than Evonik P25.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In the present study, nanocrystalline titanium dioxide (TiO2) was prepared by sol–gel method at low temperature from titanium tetraisopropoxide (TTIP) and characterized by different techniques (gas adsorption, XRD, TEM and FTIR). Variables of the synthesis, such as the hydrolyzing agent (acetic acid or isopropanol) and calcination temperatures (300–800 °C), were analyzed to get uniform size TiO2 nanoparticles. The effect that these two variables have on the structure of the resultant TiO2 nanoparticles and on their photocatalytic activity is investigated. The photocatalytic activities of TiO2 nanoparticles were evaluated for propene oxidation at low concentration (100 ppmv) under two different kinds of UV light (UV-A ∼ 365 nm and UV-C ∼ 257.7 nm) and compared with Degussa TiO2 P-25, used as reference sample. The results show that both hydrolyzing agents allow to prepare TiO2 nanoparticles and that the hydrolyzing agent influences the crystalline structure and its change with the thermal treatments. Interestingly, the prepared TiO2 nanoparticles possess anatase phase with small crystalline size, high surface area and higher photocatalytic activity for propene oxidation than commercial TiO2 (Degussa P-25) under UV-light. Curiously, these prepared TiO2 nanoparticles are more active with the 365 nm source than with the 257.7 nm UV-light, which is a remarkable advantage from an application point of view. Additionally, the obtained results are particularly good when acetic acid is the hydrolyzing agent at both wavelengths used, possibly due to the high crystallinity, low anatase phase size and high surface oxygen groups’ content in the nanoparticles prepared with it, in comparison to those prepared using isopropanol.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The hybrid structure of Fe2O3 nanoparticles/TiO2 nanofibers (NFs), combines the merits of large surface areas of TiO2 NFs and absorption in ultraviolet light–visible light range. This structure can be used for many applications such as photoelectrochemical water splitting and photo-catalysis. Here, a sol-flame method is used for depositing Fe2O3 on TiO2 NFs that were prepared by hydrothermal on Ti sheets. The obtained materials were characterized by XRD, SEM, UV/Vis diffuse reflectance, Raman, and XPS. The results revealed the formation of rutile and anatase crystalline phases together with Fe2O3. This process moves the absorption threshold of TiO2 NFs support into visible spectrum range and enhances the photocurrent in comparison to bare TiO2 NFs, although no hole scavenger was used. The impedance measurement at low and high frequencies revealed an increase in series resistance and a decrease in resistance of charge transfer with sol-flame treatment time. A mechanism for explaining the charge transfer in these TiO2 NFs decorated with Fe2O3 nanoparticles was proposed.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This article reports a study of the effects of synthesis parameters on the preparation and formation of mesoporous titania nanopowders by employing a two-step sol-gel method. These materials displayed crystalline domains characteristic of anatase. The first step of the process involved the hydrolysis of titanium isopropoxide in a basic aqueous solution mediated by neutral surfactant. The solid product obtained from step 1 was then treated in an acidified ethanol solution containing the same titanium precursor to thicken the pore walls. Low pH and higher loading of the Ti precursor in step 2 produced better mesoporosity and crystallinity of titanium dioxide polymorphs. The resultant powder exhibited a high surface area (73.8 m(2)/g) and large pore volume (0.17 cm(3)/g) with uniform mesopores. These materials are envisaged to be used as precursors for mesoporous titania films as a wide band gap semiconductor in dye-sensitized nanocrystalline TiO2 solar cells.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A porous, high surface area TiO2 with anatase or rutile crystalline domains is advantageous for high efficiency photonic devices. Here, we report a new route to the synthesis of mesoporous titania with full anatase crystalline domains. This route involves the preparation of anatase nanocrystalline seed suspensions as the titania precursor and a block copolymer surfactant, Pluronic P123 as the template for the hydrothermal self-assembly process. A large pore (7 - 8 nm) mesoporous titania with a high surface area of 106 - 150 m(2)/g after calcination at 400degreesC for 4 h in air is achieved. Increasing the hydrothermal temperature decreases the surface area and creates larger pores. Characteristics of the seed precursors as well as the resultant mesoporous titania powder were studied using XRD analysis, N-2-adsorption/desorption analysis, and TEM. We believe these materials will be especially useful for photoelectrochemical solar cell and photocatalysis applications.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nanocystalline TiO2 particles were successfully synthesized on porous hosts (SBA-15 and ZSM-15) via a sol-gel impregnation method. Resulting nanocomposites were characterized by XRD, TEM, BET surface analysis, Raman and UV-vis diffuse reflectance spectroscopy, and their photocatalytic activity for H2 production evaluated. XRD evidences the formation of anatase nanoparticles over both ZSM-5 and SBA-15 porous supports, with TEM highlighting a strong particle size dependence on titania precursor concentration. Photocatalytic activities of TiO2/ZSM-5 and TiO2/SBA-15 composites were significantly enhanced compared to pure TiO2, owing to the smaller TiO2 particle size and higher surface area of the former. TiO2 loadings over the porous supports and concomitant photocatalytic hydrogen production were optimized with respect to light absorption, available surface reaction sites and particle size. 10%TiO2/ZSM-5 and 20%TiO2/SBA-15 proved the most active photocatalysts, exhibiting extraordinary hydrogen evolution rates of 10,000 and 8800μmolgTiO2 -1 h-1 under full arc, associated with high external quantum efficiencies of 12.6% and 5.4% respectively under 365nm irradiation.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This study involved the synthesis of photocatalysts based on titanium dioxide (TiO2). The photocatalysts were synthesized by the sol-gel method using three different proportions of acetone (25%, 50% and 75% v/v) in water/acetone mixtures, in order to control the hydrolysis of the precursor of titanium (titanium tetraisopropoxide). Aiming to investigate the structural, morphological and electronic changes provoked by the use of the solvent mixtures, different methodologies were used to characterize the oxides, such as X-ray diffraction (XRD), RAMAN spectroscopy, UV-Vis diffuse reflectance spectroscopy, and measurements of specific surface area (BET). XRD combined to RAMAN analyses revealed that the products are two-phase highly crystalline oxides involving anatase as main phase and brookite. Besides, the refined XRD using the method of Rietveld demonstrated that the presence of acetone during the synthesis influenced in the composition of the crystalline phases, increasing the proportion of the brookite phase between 13 and 22%. The band gap energy of these oxides practically did not suffer changes as function of the synthesis conditions. As shown by the isotherm, these photocatalysts are mesoporous materials with mean diameter of pores of 7 nm and approximately 20% of porosity. The surface area of the oxides prepared by hydrolysis in presence of acetone was 12% higher compared to the bare oxide. After characterized, these oxides had their photocatalytic activities evaluated by photodegradation of the azo dyes Ponceau 4R (P4R), Tartrazine (TTZ) and Reactive Red 120 (RR120), and also by the ability to mediate the photocatalytic production of hydrogen. Using the most efficient photocatalyst, the mineralization achieved for the dyes P4R, RR120 and TTZ was of respectively 83%, 79% and 56% in 120 minutes of reaction, while the discoloration of P4R e RR120 reached 100% and 94% for TTZ. In addition, the same photocatalyst in the presence of 0.5% w/w of Platinum and suspended in a 5:1 v/v water/methanol mixture, produced 56 mmol of gaseous hydrogen in five hours of experiment, corresponding to a specific rate of hydrogen production of 139.5 mmol h-1 g-1.