937 resultados para metallic biomaterial
Resumo:
The nanoindentation technique was employed to examine the strain rate sensitivity, m, and its dependence on the structural state of a Zr-based bulk metallic glass (BMG). The free volume content in the BMG was varied by examining samples in the as-cast (AC), shot-peened (SP), and structurally relaxed (SR) states. Hardness values measured at different loading rates and over a temperature range of 300-423 K as well as the strain-rate jump tests conducted in the quasi-static regime at room temperature, show that m is always negative. All the load-displacement (P-h) curves in this temperature regime exhibit serrated load-displacement responses, indicating that the shear band mediated inhomogeneous plastic flow governs deformation. Such localization of flow and associated softening is the raison d'etre for the negative m. Significant levels of pile-up around the indents were also noted. The order in the average values of hardness, pile-up heights, and the displacement bursts on the P-h curves was always such that SR > AC > SP, which is also the order of increasing free volume content. These observations were utilized to discuss the reasons for the negative strain rate sensitivity, and its dependence on the structural state of metallic glasses. It is suggested that the positive values of m reported in the literature for them are possibly experimental artefacts that arise due to large pile ups around the indents which lead to erroneous estimation in hardness values. (C) 2014 Elsevier B.V. All rights reserved.
Resumo:
Here, we demonstrate an uninterrupted galvanic replacement reaction (GRR) for the synthesis of metallic (Ag, Cu and Sn) and bimetallic (Cu M, M=Ag, Au, Pt and Pd) sponges/dendrites by sacrificing the low reduction potential metals (Mg in our case) in acidic medium. The acidic medium prevents the oxide formation on Mg surface and facilitates the uninterrupted reaction. The morphology of dendritic/spongy structures is controlled by the volume of acid used for this reaction. The growth mechanism of the spongy/dendritic microstructures is explained by diffusion-limited aggregate model (DLA), which is also largely affected by the volume of acid. The significance of this method is that the yield can be easily predicted, which is a major challenge for the commercialization of the products. Furthermore, the synthesis is complete in 1-2 minutes at room temperature. We show that the sponges/dendrites efficiently act as catalysts to reduce 4-nitrophenol (4-NP) to 4-aminophenol (4-AP) using NaBH4-a widely studied conversion process.
Resumo:
Significant progress in understanding the mechanical behavior of metallic glasses (MGs) was made over the past decade, particularly on mechanisms of plastic deformation. However, recent research thrust has been on exploring the mechanics and physics of fracture. MGs can be very brittle with K-Ic values similar to silicate glasses and ceramics or very tough with K-Ic akin to high toughness crystalline metals. Even the tough MGs can become brittle with structural relaxation following annealing at temperatures close to glass transition temperature (T-g). Detailed experimental studies coupled with complementary numerical simulations of the recent past have provided insights on the micromechanisms of failure as well as nature of crack tip fields, and established the governing fracture criteria for ductile and brittle glasses. In this paper, the above advances are reviewed and outstanding issues in the context of fracture of amorphous alloys that need to be resolved are identified.
Resumo:
The mode I fracture toughness, K-Ic, of ductile bulk metallic glasses (BMGs) exhibits a high degree of specimen-to-specimen variability. By conducting fracture experiments in modes I and II, we demonstrate that the observed high variability in mode I, vis-a-vis mode II, is a result of highly variable propensity for the conversion of shear bands into cracks in mode I whereas in mode II, crack growth direction is fixed. Thus, the measured variability in K-Ic is intrinsic to the nature of BMGs. (C) 2015 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
ESD behavior of metallic carbon nanotubes (CNTs) is explored. Unique TLP I-V characteristics and failure mechanism of carbon shells are discussed. ESD failure in CNTs is attributed to shell burning. It was found that CNT interconnect changes resistance in steps of fundamental quantum resistance (h/2e(2)) after individual shell burning.
Resumo:
A simple microstructural rationale for successful anodization of metallic films into ordered oxide nanostructures has been identified. It applies to three of the most commonly studied systems, Zr, Ti and Al films and can be extended to other such oxides. A dense Zone T or II microstructure, in sputtered films, is the most critical ingredient. While T-substrate > 0.3T(melting) Ching is the simplest route, pressure and plasma heating can also be exploited. Such microstructures are also associated with a unique growth stress signature. (C) 2015 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
One of the desired properties for any new biomaterial composition is its long-term stability in a suitable animal model and such property cannot be appropriately assessed by performing short-term implantation studies. While hydroxyapatite (HA) or bioglass coated metallic biomaterials are being investigated for in vivo biocompatibility properties, such study is not extensively being pursued for bulk glass ceramics. In view of their inherent brittle nature, the implant stability as well as impact of long-term release of metallic ions on bone regeneration have been a major concern. In this perspective, the present article reports the results of the in vivo implantation experiments carried out using 100% strontium (Sr)-substituted glass ceramics with the nominal composition of 4.5 SiO2-3Al(2)O(3)-1.5P(2)O(5)-3SrO-2SrF(2) for 26 weeks in cylindrical bone defects in rabbit model. The combination of histological and micro-computed tomography analysis provided a qualitative and quantitative understanding of the bone regeneration around the glass ceramic implants in comparison to the highly bioactive HA bioglass implants (control). The sequential polychrome labeling of bone during in vivo osseointegration using three fluorochromes followed by fluorescence microscopy observation confirmed homogeneous bone formation around the test implants. The results of the present study unequivocally confirm the long-term implant stability as well as osteoconductive property of 100% Sr-substituted glass ceramics, which is comparable to that of a known bioactive implant, that is, HA-based bioglass. (c) 2014 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 103B: 1168-1179, 2015.
Resumo:
Thin films of conducting palladium selenide phases (Pd17Se15 and Pd7Se4) are prepared using a single source molecular precursor by thermolysis. Varying the mole ratios of palladium and selenium precursors results in palladium organo-selenolate complexes which on thermolysis at different temperatures yield Pd17Se15 and Pd7Se4 phases that are very stable and adherent to the substrate. The organo-selenolate complexes are characterized using small angle XRD, Se-77 NMR and thermogravimetric analysis (TGA). The palladium selenide films are characterized by various techniques such as XRD, XPS, TEM and SEM. Electrical conductivities of the films are determined using the four probe method. The strong adherence of the films to glass substrates coupled with high corrosion resistant behavior towards strong acid and alkaline environments render them to be very effective as electrocatalysts. The catalytic activity towards the I-3(-)/I- redox couple, which is an important reaction in the regeneration of the dye in a dye-sensitized solar cell, is studied. Between the two phases, the Pd17Se15 film shows superior activity as the counter electrode for dye sensitized solar cells with a photocurrent conversion efficiency of 7.45%.
Resumo:
The dependence of shear yield strain, the activation energy and volume of shear transformation zone on the glass transition temperature was investigated through the analysis of statistical distributions of the first pop-in events during spherical indentation of four different thin film metallic glasses. Only the Cu-Zr metallic glass exhibits a bimodal distribution of the first pop-in loads, whereas W-Ru-B, Zr-Cu-Ni-Al and La-Co-Al metallic glasses show an unimodal distribution. Results show that shear yield strain and activation energy of shear transformation zone decrease whereas the volume of shear transformation zone increases with increasing homologous temperature, indicating that it is the activation energy rather than the volume of shear transformation zone that controls shear yield strain. (C) 2015 Elsevier B.V. All rights reserved.
Resumo:
Recent experiments have shown that nano-sized metallic glass (MG) specimens subjected to tensile loading exhibit increased ductility and work hardening. Failure occurs by necking as opposed to shear banding which is seen in bulk samples. Also, the necking is generally observed at shallow notches present on the specimen surface. In this work, continuum finite element analysis of tensile loading of nano-sized notched MG specimens is conducted using a thermodynamically consistent non-local plasticity model to clearly understand the deformation behavior from a mechanics perspective. It is found that plastic zone size in front of the notch attains a saturation level at the stage when a dominant shear band forms extending across the specimen. This size scales with an intrinsic material length associated with the interaction stress between flow defects. A transition in deformation behavior from quasi-brittle to ductile becomes possible when this critical plastic zone size is larger than the uncracked ligament length. These observations corroborate with atomistic simulations and experimental results. (C) 2015 Elsevier Ltd. All rights reserved.
Resumo:
Thermal interface materials (TIMs) form a mechanical and thermal link between a heat source and a heat sink. Thus, they should have high thermal conductivity and high compliance to efficiently transfer heat and accommodate any differential strain between the heat source and the sink, respectively. This paper reports on the processing and the characterization of potential metallic TIM composite solders comprising of Cu, a high conductivity phase, uniformly embedded in In matrix, a highly compliant phase. We propose the fabrication of such a material by a two-step fabrication technique comprising of liquid phase sintering (LPS) followed by accumulative roll bonding (ARB). To demonstrate the efficacy of the employed two-step processing technique, an In-40 vol. % Cu composite solder was produced first using LPS with short sintering periods (30 or 60 s at 160 degrees C) followed by ARB up to five passes, each pass imposing a strain of 50%. Mechanical response and electrical and thermal conductivities of the fabricated samples were evaluated. It was observed that processing through ARB homogenizes the distribution of Cu in an In matrix, disintegrates the agglomerates of Cu powders, and also significantly increases thermal and electrical conductivities, almost attaining theoretically predicted values, without significantly increasing the flow stress. Furthermore, the processing technique also allows the insertion of desired foreign species, such as reduced graphene oxide, in In-Cu for further enhancing a target property, such as electrical conductivity.
Resumo:
Molecular dynamics simulations were employed to investigate the specimen thickness-dependent tensile behavior of a series of Cu(x)Z(100-x) (x = 20, 40, 50, 64 and 80 at%) metallic glass (MG) films, with a particular focus on the critical thickness, tc, below which non-localized plastic flow takes place. The simulation results reveal that while the transition occurs in all the alloys examined, t(c) is sensitive to the composition. We rationalize t(c) by postulating that the strain energy stored in the sample at the onset of plastic deformation has to be sufficient for the formation of shear bands. The composition-dependence of t(c) was found to correlate with the average activation energy of the atomic level plastic deformation events. (C) 2015 Elsevier Ltd. All rights reserved.
Resumo:
The structural evolution and property changes in Nd60Al10Fe20Co10 bulk metallic glass (BMG) upon crystallization are investigated by the ultrasonic method, x-ray diffraction, density measurement, and differential scanning calorimetry. The elastic constants and Debye temperature of the BMG are obtained as a function of annealing temperature. Anomalous changes in ultrasonic velocities, elastic constants, and density are observed between 600–750 K, corresponding to the formation of metastable phases as an intermediate product in the crystallization process. The changes in acoustic velocities, elastic constants, density, and Debye temperature of the BMG relative to its fully crystallized state are much smaller, compared with those of other known BMGs, the differences being attributed to the microstructural feature of the BMG.
Resumo:
The thermal stability of Nd60Fe20Co10Al10 bulk metallic glass (BMG) has been studied by differential scanning calorimetry (DSC), dynamic mechanical thermal analysis (DMTA), isochronal dilatation and compression tests. The results show that the glass transition of the BMG takes place quite gradually between about 460 and 650 K at a heating rate of 0.17 K/s. Several transformation processes are observed during continuous heating with the first crystallization process beginning at about 460 K, while massive crystallization takes place near the solidus temperature of the alloy. The positive heat of mixing between the two major constituents, Nd and Fe, and, consequently, a highly inhomogeneous composition of the attained amorphous phase are responsible for the anomalous thermal stability in this system. (C) 2002 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.
Resumo:
The room temperature creep behaviors of Ce-based bulk metallic glasses were examined by the use of nanoindentation. The creep rate and creep rate sensitivity of Ce-based BMGs were derived from indentation creep curves. The low creep rate sensitivity of Ce-based BMGs indicates that the room temperature creep is dominated by localized shear flow. The experimental creep curves can be described by a generalized Kelvin model. Furthermore, the creep retardation spectrum is calculated for the Ce-based metallic glasses. The results showed that creep retardation spectrum consists of two relatively separated peaks with the well defined characteristic relaxation times.