795 resultados para lanthanum promotion
Resumo:
Lanthanum magnesium hexaluminate (LaMgAl11O19, LMA) is an attractive material for thermal barrier coatings (TBCs), and the failure of its coating was studied in this work by thermal cycling, X-ray diffraction, dilatometric measurement and thermal gravimetric-differential thermal analysis. The dilatometric measurement indicates that even though the bulk material of LMA has a higher sintering-resistance than the typical TBC material, i.e. yttria-stabilized zirconia (YSZ), the plasma sprayed coating of LMA has two serious contractions due to the re-crystallization of LMA and phase transitions of alumina.
Resumo:
La2Zr2O7 (LZ) is a promising thermal barrier coating material for the high-temperature applications, which could be significantly toughened by the BaTiO3 piezoelectric phase incorporated into the matrix. The composites of xBaTiO(3)/(l-x)LZ (x=5, 10, 15, 20 vol%, LZ-x-BaTiO3) were densified by means of high-pressure sintering (HPS) under a pressure of 4.5 GPa at 1450 degrees C for 10 min, by which a high relative density above 93% could be obtained.
Resumo:
Lanthanum, zirconate (La2Zr2O7, LZ) coatings were prepared under four different deposition conditions by electron beam-physical vapor deposition (EB-PVD). The composition, crystal structure, surface and cross-sectional morphology, cyclic oxidation behavior of these coatings were studied. Elemental analysis indicates that the coating composition has partially deviated from the stoichiometry of pyrochlore, and the existence of excess La2O3 is also observed. The deviation could be reduced by properly controlling the electron beam current or by changing the ingot composition.
Resumo:
Lanthanum magnesium hexaaluminate is a very important ceramic material for high temperature applications. In this paper lanthanum magnesium hexaaluminate has been synthesized directly by solid-state reaction. The forming mechanism was investigated by XRD. The SEM photographs show that the prepared powders are made of hexagonal plates. These powders can be well sintered at the high temperature (1600 degrees C) under the high pressure (4.5 GPa), and the relative density reaches 94.8%.
Resumo:
Lanthanum magnesium hexaalumminate (LMA) is an important candidate for thermal barrier coatings due to its thermal stability and low thermal conductivity. On the other hand, laser glazing method can potentially make thermal barrier coatings impermeable, resistant to corrosion on the surface and porous at bulk. LMA powder was synthesized at 1600 degrees C by solid-state reaction, pressed into tablet and laser glazed with a 5-kW continuous wave CO2 laser.
Effects of Y2O3 addition on the phase evolution and thermophysical properties of lanthanum zirconate
Resumo:
Lanthanum zirconate (La2Zr2O7, LZ) powders with the addition of various Y2O3 contents for potential thermal barrier coatings (TBCs) application were synthesized by solid-state reaction. The structure evolution, sintering-resistance and thermophysical properties of the synthesized powders and sintered ceramics were systematically studied. X-ray diffraction (XRD) results indicate that LZ containing 3-12 wt.% Y2O3 mainly keeps a pyrochlore-type structure, and two new phases of LaYO3 and Y0.18Zr0.82O1.91 are also detected. Raman spectra confirm that the higher the Y2O3 content, the easier is the formation of LaYO3.
Resumo:
Lanthanum-zirconium-cerium composite oxide (La-2(Zr0.7Ce0.3)(2)O-7, LZ7C3) as a candidate material for thermal barrier coatings (TBCs) was prepared by electron beam-physical vapor deposition (EB-PVD). The composition, crystal structure, thermophysical properties, surface and cross-sectional morphologies and cyclic oxidation behavior of the LZ7C3 coating were studied. The results indicated that LZ7C3 has a high phase stability between 298 K and 1573 K, and its linear thermal expansion coefficient (TEC) is similar to that of zirconia containing 8 wt% yttria (8YSZ). The thermal conductivity of LZ7C3 is 0.87 W m(-1) K-1 at 1273 K, which is almost 60% lower than that of 8YSZ. The deviation of coating composition from the ingot can be overcome by the addition of excess CeO2 and ZrO2 during ingot preparation or by adjusting the process parameters.
Resumo:
Die-cast Mg-4Al-4RE-0.4Mn (RE = Ce-rich mischmetal) and Mg-4Al-4La-0.4Mn magnesium alloys were prepared successfully and their microstructure, tensile and creep properties have been investigated. The results show that two binary Al-RE phases, Al11RE3 and Al2RE, are formed along grain boundaries in Mg-4Al-4RE-0.4Mn alloy, while the phase compositions of Mg-4Al-4La-0.4Mn alloy mainly consist of alpha-Mg phase and Al11La3 phase. And in Mg-4Al-4La-0.4Mn alloy the Al11La3 phase occupies a large grain boundary area and grows with complicated morphologies, which is characterized by scanning electron microscopy in detail. Changing the rare earth content of the alloy from Ce-rich mischmetal to lanthanum gives a further improvement in the tensile and creep properties, and the later could be attributed to the better thermal stability of Al11La3 phase in Mg-4Al-4La-0.4Mn alloy than that of Al11RE3 phase in Mg-4Al-4RE-0.4Mn alloy.
Resumo:
La2Zr2O7 (LZ) is a promising thermal barrier coating material for the high-temperature applications, which could be significantly toughened by the YAG nanopowder incorporated into the matrix. The composites of xYAG/(1-x)LZ (Y=10, 15, 20 vol. %, LZ-x-YAG) were densified by means of high-pressure sintering (HPS) under a pressure of 4.5 GPa at 1650 degrees C for 5 min, by which a high-relative density above 93% could be obtained. The morphologies of the fractured surfaces were investigated by the scanning electron microscope, and the fracture toughness and Vicker's-hardness of the composites were evaluated by the microindentation. The grain size of the LZ matrix drops significantly with the addition of YAG nanoparticles and the fracture type changes from the intergranular to a mixture type of the transgranular and intergranular in the nanocomposites. The LZ-20-YAG nanocomposite has a fracture toughness of 1.93 MPa m(1/2), which is obviously higher than that of the pure LZ (1.57 MPa m(1/2)), and the toughening mechanism is discussed in this paper.
Resumo:
La-2, Yb-2, and Lu-2 have been studied by use of the density-functional methods B3LYP, BLYP, B3PW91, BHLYP, BP86, B3P86, MPW1PW91, and PBE1PBE. In these density-functional methods, the exchange functional is from either Becke's three-parameter HF-DFT hybrid exchange functional (B3), pure DFT exchange functional of 1988 (B), a modification of the half-and-half HF/DFT hybrid method (BH), Perdew-Wang 1991 (PW91), or Barone's modified PW91 (MPW1), while the correlation functional is from either Lee, Yang, and Parr (LYP), Perdew-Wang 1991 (PW91), or Perdew 86 (P86). PBE1PBE is the generalized-gradient-approximation exchange-correlation functional of Perdew, Burke, and Ernzerhof. For La-2, the calculated bond distance is in reasonable agreement with the experiment, but the calculated vibrational frequency is underestimated significantly compared with the experiment. Only BP86 and B3P86 have the best performance in reproducing the experimental dissociation energy for La-2. For the van der Waals dimer Yb-2, three functionals, B3LYP, BLYP, and BHLYP have excellent performance in reproducing the spectroscopic constants compared with both the experiment and previous theoretical studies.
Resumo:
The extractions of the selected rare earths (Sc, Y, La and Gd) from hydrochloric acid solutions have been investigated using bis(2,4,4-trimethylpentyl)-mono thiophosphinic acid (Cyanex 302, HL) in heptane as an extractant. The results demonstrate that the extractions of rare earths occur via the following reaction: Sc(OH)(2+) + 2[(HL)(2)]((O)) double left right arrow [Sc(OH)L-2 (.) 2(HL)]((O)) + 2H(+) Y3+ + 3[(HL)(2)]((O)) double left right arrow [Y(HL2)(3)]((O)) + 3H(+) La(OH)(2)(+) + 3[(HL)(2)](O) double left right arrow [La(OH)(2)L (.) 5(HL)]((O)) + H+ Gd(OH)(2+) + 3[(HL)(2)]((O)) double left right arrow [Gd(OH)L-2 (.) 4(HL)]((O)) + 2H(+) The pH(1/2) values and equilibrium constants of the extracted complexes have been deduced by taking into account the aqueous phase complexation of the metal ion with hydroxyl ligands and plausible complexes extracted into the organic phase. According to the pH(1/2) values, it is possible to realize mutual separation among Sc(III), Y(III), La(III) and Gd(III) with Cyanex 302 by controlling aqueous acidity.
Resumo:
The phase stability of lanthanum cerium oxide (La2Ce2O7), which is stable up to 1400 degrees C, and the thermal expansion coefficient of La2Ce2O7 doped with Ta2O5 or WO3 were studied. The thermal expansion coefficient of La2Ce2O7 below 400 degrees C was increased by adding more CeO2 or doping with either Ta2O5 or WO3.
Resumo:
Bulk material and coatings of Lanthanum-Cerium Oxide (La2Ce2O7) with a fluorite structure were studied as a candidate material for thermal barrier coating (TBC). It has been showed that such material has the properties of low thermal conductivity about four times lower than YSZ, the difference in the thermal expansion coefficient between La2Ce2O7 and bond coat is smaller than that of YSZ in TBC systems, high phase stability between room temperature and 1673 K, about 300 K higher than that of the YSZ. The coating prepared by electron beam physical vapor deposition (EB-PVD) showed that it has good thermal cycling behavior, implying that Such material can be a promising thermal barrier coating material. The deviation of coating composition from ingot can be overcome by the addition of excess La2O3 during ingot preparation and/or by adjusting the process parameters.
Resumo:
The PVP/lanthanum nitrate/zirconium oxychloride (PVP-precursor) nanofiber was prepared by electrospinning technique. Lanthanum zirconate (La2Zr2O7, LZ) in the nanofiber is formed after calcination at 800 degrees C and the nanofiber with pyrochlore structure and a diameter of 100-500 nm can be obtained by calcination of the above precursor fiber at 1000 degrees C for 12 h. The surface of the fiber is rough but the continuous microstructure is still maintained after calcination. LZ fibers stack randomly, resulting in a structure with a low contact area between the fibers. This special structure makes the fiber to have a high resistance to sintering at elevated temperatures. The BET (Brunauer-Emmett-Teller) specific surface areas of the LZ fiber and powder calcined at different temperatures are shown in this paper, and the fiber was characterized by TG-DTA (thermal gravimetry-differential thermal analysis), XRD (X-ray diffraction), N-2 absorption-desorption porosimetry and SEM (scanning electron microscopy).