Epoxy-terminated polystyrene has been synthesized by radical polymerization using alpha-(t-butylperoxymethyl) styrene (TPMS) as the chain transfer agent. The chain transfer constants were found to be 0.66 and 0.80 at 60 and 70 degrees C, respectively. The presence of epoxy end groups was confirmed by functional group modification of epoxide to aldehyde by treatment with BF3.Et(2)O. Thermal stability of TPMS was followed by differential scanning calorimetry and iodimetry. Thermal decomposition of TPMS in toluene follows first order kinetics with an activation energy of 23 kcal/mol. (C) 1996 John Wiley & Sons, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The present review articulates the syntheses and properties of industrially important disulfide and tetrasulfide polymers. The diselenide and ditelluride polymers have also been reviewed, for the first time, so that a comprehensive view on the polymers containing group VIA elements can be obtained. The latter two polymers are gaining considerable current attention due to their semi-conducting properties. The emphasis has been made to sift through the developments in the last ten years or so to get the latest flavour in these rapidly developing polymers. We have also attempted to bring to the fore several contradicting results, like, for example, the crystallinity of ditelluride polymers, to clear the mist in such reports. We hope that this review will help those working in the field to assess the progress achieved in this area and that it may also provide useful orientation for those who wish to become involved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Cure kinetics for the formation of copolyurethane networks of various compositions based on hydroxy-terminated polybutadiene(HTPB), poly(12-hydroxy stearic acid-co-TMP) ester polyol(PEP), and different isocyanates has been studied through viscosity build up during the cure reaction. The viscosity (N)-time (t) plots conform to the equation N = ae(bt), where a and b are empirical constants, dependent on the composition and the nature of the polyols and the isocyanates. The rate constants (b) for viscosity build up, evaluated from the slopes of dN/dt versus N plots at different temperatures, were found to vary significantly from 0.0073 to 0.25 min(-1); and the activation energies for gelation were found to be in the range 20 to 40 kJ mol(-1). The results have been interpreted in terms of the dependence of the rate constants on structural characteristics of the prepolymers. (C) 1997 John Wiley & Sons, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The triphenylphosphine deoxygenation of the polyperoxides, poly(styrene peroxide), poly(methyl methacrylate peroxide), and poly(alpha-methylstyrene peroxide) proceed via the phosphorane intermediates, which in the presence of moisture hydrolyze to give the respective diols. At higher temperatures and under dry conditions the phosphorane decomposes into epoxide and triphenylphosphine oxide. The reaction has been studied by H-1-, C-13-, and P-31-NMR spectroscopy. The results obtained are consistent with a concerted insertion of the biphile, triphenylphosphine, into the peroxy bond and this reaction pathway seems to be new as far as the chemistry of polyperoxides is concerned. Though the aim of this investigation was to test the selective deoxygenation of polyperoxide by triphenylphosphine as a method of preparing polyethers, it turned out to be a fruitful method of synthesis of stereospecific diols. (C) 1997 John Wiley & Sons, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The thermal degradation of poly(methyl methacrylate) (PMMA) in the presence of polysulfide polymers, namely, poly( styrene disulfide) (PSD) and poly(styrene tetrasulfide) (PST) was studied using thermogravimetry (TG) and direct pyrolysis-mass spectrometric (DP-MS) analysis. Both PSD and PST were found to stabilizethe PMMA degradation, which was explained by both radical recombination and a chain-transfer mechanism. (C) 1997 John Wiley & Sons, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A new class of epoxy resins having N-N bonds in their structure has been synthesized by reacting N,N'-aliphatic dicarboxyl bis(hydrazones) (the aldehyde/ketone derivatives of malonic, adipic, and sebacic dihydrazides) with epichlorohydrin. The reactivity of the[GRAPHICS] protons as a function of the substituent group and the number of methylene spacer groups present in the hydrazone has been examined. The resins obtained have been characterized by elemental and epoxy equivalent analyses and IR and NMR spectra. All these resins are found to have adequate viscosity and cure easily with amine curatives at elevated temperatures. Relevant properties for their use as binders in propellant formulations, such as thermal stability, heat of combustion, density, temperature dependence of viscosity, and mechanical strength of the composites, have been evaluated. (C) 1997 John Wiley & Sons, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A new class of biodegradable copolyesters was synthesized by the catalyst-free melt condensation of sorbitol with citric acid, tartaric acid, and sebacic acid. The resulting polymers were designated as poly(sorbitol citric sebacate) p(SCS)] and poly(sorbitol tartaric sebacate) p(STS)]. The synthesized polymers were characterized by Fourier transform infrared spectroscopy, H-1-NMR spectroscopy, and differential scanning calorimetry analysis. Porous spongelike scaffolds were prepared with a salt-leaching technique and characterized with scanning electron microscopy. Tensile testing of the p(SCS) and p(STS) polymers showed that they exhibited a wide range of mechanical properties. The Young's modulus and tensile strengths of the polymers ranged from 1.06 +/- 0.12 to 462.65 +/- 34.21 MPa and from 0.45 +/- 0.04 to 20.32 +/- 2.54 MPa, respectively. In vitro degradation studies were performed on disc-shaped polymer samples. The half-life of the polymers ranged from 0.54 to 38.52 days. The percentage hydration of the polymers was in the range 9.36 +/- 1.26 to 78.25 +/- 1.91, with sol contents of 2-14%. At any given polymer composition, the Young's modulus and tensile strength of p(SCS) was higher than that of p(STS), whereas the degradation rates of p(SCS) was lower than that of p(STS). This was attributed to the structural difference between the citric and tartaric monomers and to the degree of crosslinking. (C) 2011 Wiley Periodicals, Inc. J Appl Polym Sci 121: 2861-2869, 2011

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Polymer degradation in solution has several advantages over melt pyrolysis, The degradation of low-density polyethylene (LDPE) occurs at much lower temperatures in solution (280-360degreesC) than in conventional melt pyrolysis (400-450degreesC). The thermal degradation kinetics of LDPE in solution was investigated in this work. LDPE was dissolved in liquid paraffin and degraded for 3 h at various temperatures (280-360degreesC). Samples were taken at specific times and analyzed with high-pressure liquid chromatography/gel permeation chromatography for the molecular weight distribution (MWD), The time evolution of the MWD was modeled with continuous distribution kinetics. Data indicated that LDPE followed random-chain-scission degradation. The rapid initial drop in molecular weight, observed up to 45 min, was attributed to the presence of weak links in the polymer. The rate coefficients for the breakage of weak and strong links were determined, and the corresponding average activation energies were calculated to be 88 and 24 kJ/mol, respectively. (C) 2002 John Wiley Sons, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This article describes the results of the preparation and characterization of self-doped conducting copolymers of aniline and toluidine with m-aminobenzene sulfonic acid. The copolymers have an intrinsic acid group that is capable of doping polyaniline. Spectroscopic, morphological, and electrical conductivity studies have provided insight into the structural and electronic properties of the copolymers. The differences in the properties of polyaniline and polytoluidine due to the sulfonic acid ring substituent on the phenyl ring are discussed. The scanning electron micrographs of the copolymers reveal regions of sharp-edged, needle-shaped structures, whereas the X-ray diffraction patterns show that the copolymers are relatively more crystalline in nature. (C) 2002 Wiley Periodicals, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A polyphosphate ester was synthesized by interfacial polycondensation of bisphenol-A and phenylphosphorodichloridate. Accelerated hydrolytic degradation studies were conducted under alkaline conditions. The effect of concentration of alkali and temperature were monitored. The rate of degradation reached a maximum value at 6 molar sodium hydroxide solution and then reduced. The activation energy for hydrolytic degradation was found to be 45 kcal/mol. Diffusion of alkali into the polymer pellet was studied at various concentrations of alkali and at various temperatures. The rate of diffusion also attained a maximum at 6M NaOH and the activation energy for diffusion process was found to be 12 kcal/mol. (C) 2002 John Wiley Sons, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The kinetics of thermal degradation of poly(vinyl chloride) (PVC) in solution was investigated at various temperatures (210-250degreesC). The degradation rate coefficients were determined from the time evolution of the molecular weight distribution (MWD). The energy of activation, determined from the temperature dependence of the rate coefficient, was 26.6 kcal/mol. The degradation of PVC was also studied in the presence of a catalyst (HZSM-5 zeolite). The results indicated that increase of the degradation rate of PVC is first order with the HZSM-5 concentration up to 50 g/L and zero order at higher concentrations. The thermal degradation kinetics of PVC in the presence of 50 g/L of the catalyst was studied at various temperatures. The temperature dependency of the rate coefficient was used to calculate the activation energy (21.5 kcal/mol). This is consistent with the observation that the presence of a catalyst generally decreases the activation energy and promotes degradation. (C) 2002 John Wiley Sons, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

An AB(2) monomer, 1-(2-hydroxyethoxy)-3,5-bis-(methoxymethyl)-2,4,6-trimethylbenzene, was synthesized from mesitol and melt-polycondensed in the presence of an acid catalyst via a transetherification process at 145-150 degreesC to yield a soluble, moderately high molecular weight hyperbranched polyether. The degree of branching in the polymer was calculated to be 0.78 by a comparison of its NMR spectrum with that of an appropriately designed model compound. The weight-average molecular weight of the hyperbranched polymer was determined to be 64,600 (weight-average molecular weight/number-average molecular weight = 5.2) by size exclusion chromatography (SEC) in CHCl3, with polystyrene standards. The origin of the broad molecular weight distribution, which could either be intrinsic to such hyperbranched structures or be due to structural heterogeneity, was further probed by the fractionation of the samples by SEC and by the subjection of each fraction to matrix-assisted laser desorption/ionization time-of-flight mass spectral analysis. The mass spectral analysis suggested the presence of two primary types of species: one corresponding to the simple branched structure and the other to macrocyclics. Interestingly, from the relative intensities of the two peaks, it was apparent that cyclization became favorable at higher conversions in the melt transetherification process. (C) 2002 Wiley Periodicals, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Solid, propellants are widely used in modern rockets and missiles. Although the history of solid rockets could be traced to the discovery of gunpowder over a thousand years ago, the technology could be perfected only by the later half of the 20(th) century. The failure of gunpowder rockets was largely due to the unknown consolidating technique of the powder composition. The emergence of large solid propellant motors had, to await the dawn of polymer. science and technology(S&T). Specific syntheses of functionally terminated polymers having cross-linking capability led to the emergence of casting technology of solid composite propellants. This review describes the various polymeric fuel/binder systems used or considered for use in solid,propellants. It includes a brief background, advantages, and shortcomings of the various systems, an account of the currently used binders and a critical survey of the advanced polymers envisaged for future usage. Special emphasis has been laid on recently synthesized polymers having N-N bonds in their structures, and-on the feasibility of developing smokeless propellants based on ammonium nitrate.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The most stable vinyl polyperoxide, namely, poly(indene peroxide) (PINDP), an alternating copolymer of indene and oxygen, was synthesized by the oxidative polymerization of indene. It was characterized by H-1-NMR and C-13-NMR, Fourier transform infrared, differential scanning calorimetry, direct pyrolysis mass spectrometry, and gas chromatography mass spectrometry studies. The overall activation energy for the degradation and the glass-transition temperature of PINDP were 47 kcal/mol and 327 K respectively, which were very high compared to those of other vinyl polyperoxides. (C) 2002 Wiley Periodicals, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Polypyrrole was synthesized by chemical oxidation of pyrrole in water containing various sulphonic acids like toluene sulphonic acid (TSA), sulphosalicylic acid (SSA), and camphor sulphonic acid (CSA), as well as a combination of each sulphonic acid with sodium dodecyl benzene sulphonate (NaDBS) to investigate the effect of doping on conductivity, yield, and processability of the conducting polymer. Free-standing blend films of polypyrrole and plasticized polyvinyl chloride (PVC) were obtained by casting an homogeneous suspension of the two polymers in tetrahydrofuran. The maximum conductivity of the blend film is similar to 0.3 S/cm, corresponding to a weight fraction of 0.16 w/w polypyrrole. The blend film is semiconducting in the range 300-10 K. A TG-DTA scan indicates the blend film to be amorphous with a stepwise decomposition process similar to pristine PVC. The choice of a dual dopant system during synthesis and the plasticised polymer during subsequent processing were keys to obtaining homogeneous high-quality films. (C) 2001 John Wiley & Sons, Inc.