988 resultados para Nickel alloys.


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The reaction of the title complexes (FIG. 1) with N-bromosuccinimide or bromine in chloroform yields isomeric bromo complexes on substitution of the γ-CH carbon proton by bromine. The brominated products have been characterised by ir, pmr, electronic absorption spectra, conductivity and magnetic susceptibility measurements. The linkage isomerisation of the brominated products in chloroform has been shown to depend on the diamine residue.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

I-isonitroso-imine ligand complexes of nickel(II), namely, bis(isonitrosomethylacetoacetate-imino)Ni(II), Ni(IMI)(IMI); bis(isonitrosobenzoylacetoneimino)Ni(II), Ni(IBI)(IBI) and bis(isonitrosoacetoacetanilideimino)Ni(II), Ni(IANI)(IANI), have been prepared and characterized. On the basis of their spectroscopic and magnetic properties, these complexes are suggested to have a square-planar stereochemistry around the metal ion with both nitrogen (ligand denoted without prime) and oxygen (ligand denoted with prime) coordinated isonitroso groups. The i.r. and NMR spectra of these and other similar complexes are discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The goal of this thesis was to examine the ecophysiological responses of Scots pine (Pinus sylvestris L.), with an emphasis on the oxidative enzyme peroxidase and plant phenolics to environmental stresses like elevated levels of nickel (Ni) and copper (Cu), and herbivory. The effects of Ni and Cu were studied in a gradient survey at a sulphur dioxide contaminated site in the Kola Peninsula, and with experiments in which seedlings were exposed to Ni mist or to Ni and Cu amended into the soil. In addition, experimental Ni exposure was combined with disturbance of the natural lichen cover of the forest ground layer. Pine sawfly attack was simulated in the early season defoliation experiment, in which mature Scots pine were defoliated (100 %) during two successive years in a dry, nutrient-poor Scots pine stand. In addition, the effect of previous defoliation on the growth of sawfly (Diprion pini L.) larvae was studied. Apoplastic peroxidase activity was elevated in the needles of pine in a Ni- , Cu- and SO2- polluted environment, which indicated an increased oxidative stress. Increased foliar peroxidase activity due to Ni contamination was shown in the experiment, in which Ni was added as mist. No such response was found in peroxidase acitivity of the roots exposed to elevated Ni and/or Cu in the soil. Elevated Ni in the soil increased the concentration of foliar condensed tannins, which are able to bind heavy metals in the cells. Addition of low levels of Ni in the soil appeared to benefit pine seedlings, which was seen as promoted shoot growth and better condition of the roots. Wet Ni deposition of 2000 mg m-2 reduced growth and survival of pine seedlings, whereas deposition levels 200 mg m-2 or 20 mg m-2 caused no effects in a 2-y lasting experiment. The lichen mat on the forest floor did not act as an effective buffer against the adverse impacts of heavy metals on pine seedlings. However, some evidence was found indicating that soil microbes profited from the lichen mat. Artificial defoliation increased peroxidase activity in the Scots pine needles. In addition, defoliation decreased nitrogen, diamine putrescine and glucose concentrations in the needles and increased the concentrations of several phenolic compounds, starch and sucrose. Previous artificial defoliation led to poor growth of sawfly larvae reared on the pines, suggesting delayed induced resistance in Scots pine. However, there was no consistent relationship between inducibility (proportional increase in a compound following defoliation) and adverse effects on the growth of pine sawfly larvae. The observed inducible responses in needle phenolics due to previous defoliation thus appear to represent non-specific responses against sawflies.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

[Ni(NCS)2(CHsN3S)2], Mr = 356.7, monoclinic, P21/c , a = 5-297 (1), b = 7.869 (1), c - 16-078 (2) A,/3 = 91.53 (1) °, V-= 669.9 A 3, Z= 2, Om = 1"76, Dx = 1"771 g cm -3, A(Mo Ka) = 0-71069 ]k, /.~ = 19"9 cm-l, F(000) = 364, T = 295 K, final R = 0.026 for 1576 significant [F > 10g(F)] reflections. The complex lies on a crystallographic centre of symmetry. The Ni atom is octahedrally coordinated by two thiocyanates (through N atoms) and by two thiosemicarbazide molecules (through hydrazinic N and S atoms). The crystal structure is stabilized by N--H...S hydrogen bonds. Early work on this structure [Garaj & Dunaj-Jurco (1968). Chem. Commun. p. 518] used photographic data and was refined to R = 0-13 for 512 reflections.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A microbeam testing geometry is designed to study the variation in fracture toughness across a compositionally graded NiAl coating on a superalloy substrate. A bi-material analytical model of fracture is used to evaluate toughness by deconvoluting load-displacement data generated in a three-point bending test. It is shown that the surface layers of a diffusion bond coat can be much more brittle than the interior despite the fact that elastic modulus and hardness do not display significant variations. Such a gradient in toughness allows stable crack propagation in a test that would normally lead to unstable fracture in a homogeneous, brittle material. As the crack approaches the interface, plasticity due to the presence of Ni3Al leads to gross bending and crack bifurcation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Silicon particles standing proud on aluminium-silicon alloy surfaces provide protection in tribology. Permanent sinking of such particles into the matrix under load can be deleterious. The mechanical response of the alloy to nano-indentation of single silicon particles embedded in the matrix is explored. A nominal critical pressure required to plastically deform the matrix to permanently embed the particle is determined experimentally. Within a framework suggested by two-dimensional models of plastic response to indentation, a probable correlation is established between the normal mean pressure required to cause permanent sinking of silicon particles and a factor which relates the relevant particle dimensions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Crack loading and crack extension in pseudoelastic binary NiTi shape memory alloy (SMA) miniature compact tension (CT) specimens with 50.7 at.% Ni (austenitic, pseudoelastic) was investigated using infrared (IR) thermography during in situ loading and unloading. IR thermographic measurements allow for the observation of heat effects associated with the stress-induced transformation of martensite from B2 to BIT during loading and the reverse transformation during unloading. The results are compared with optical images and discussed in terms of the crack growth mechanisms in pseudoelastic NiTi SMAs. Direct experimental evidence is presented which shows that crack growth occurs into a stress-induced martensitic microstructure, which immediately retransforms to austenite in the wake of the crack.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An anomalous variation in the experimental elastic modulus, E, of Ti-6Al-4V-xB (with x up to 0.55 wt.%) is reported. Volume fractions and moduli of the constituent phases were measured using microscopy and nanoindentation,respectively. These were used in simple micromechanical models to examine if the E values could be rationalized. Experimental E values higher than the upper bound estimates suggest complex interplay between microstructural modifications, induced by the addition of B, and properties.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The nanoindentation hardness of individual shear bands in a Zr-based metallic glass was investigated in order to obtain a better understanding of how shear band plasticity is influenced by non-crystalline defects. The results clearly showed that the shear band hardness in both as-cast and structurally relaxed samples is much lower than the respective hardness of undeformed region. Interestingly, inter-band matrix also exhibited lower hardness than undeformed region. The results are discussed in terms of the influence of structural state and the prevailing mechanism of plastic deformation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Four new 5-aminoisophthalates of cobalt and nickel have been prepared employing hydro/solvothermal methods: [Co2(C8H5NO4)2(C4H4N2)(H2O)2]·3H2O (I), [Ni2(C8H5NO4)2(C4H4N2)(H2O)2]·3H2O (II), [Co2(H2O)(μ3-OH)2(C8H5NO4)] (III), and [Ni2(H2O)(μ3-OH)2(C8H5NO4)] (IV). Compounds I and II are isostructural, having anion-deficient CdCl2 related layers bridged by a pyrazine ligand, giving rise to a bilayer arrangement. Compounds III and IV have one-dimensional M−O(H)−M chains connected by the 5-aminoisophthalate units forming a three-dimensional structure. The coordinated as well as the lattice water molecules of I and II could be removed and inserted by simple heating−cooling cycles under the atmospheric conditions. The removal of the coordinated water molecule is accompanied by changes in the coordination environment around the M2+ (M = Co, Ni) and color of the samples (purple to blue, Co; green to dark yellow, Ni). This change has been examined by a variety of techniques that include in situ single crystal to single crystal transformation studies and in situ IR and UV−vis spectroscopic studies. Magnetic studies indicate antiferromagnetic behavior in I and II, a field-induced magnetism in III, and a canted antiferromagnetic behavior in IV.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The β-phase aging response of Cu–Al–Ni single crystal shape memory alloys (SMAs) within the temperature range of 473–573 K has been investigated. Alloys in austenitic (Cu–14.1Al–4Ni wt.%, alloy A) and martensitic (Cu–13.4Al–4Ni wt.%, alloy M) conditions at room temperature were considered. Aged samples show presence of β1′ and γ1′ martensites in both the alloys and formation of γ2 precipitates in the alloy A. The differential scanning calorimetry (DSC) thermograms of the aged samples show increase in transformation temperatures as well as transformation hysteresis with aging. Dynamic mechanical analysis (DMA) was conducted on both the alloys to ascertain the role of precipitates and martensitic transition on tan δ, which characterizes the damping behaviour of the material. With aging, a steady decrease in tan δ value was observed in both the alloys, which was attributed to the decrease in the number of interfaces per unit area with increasing aging temperature. Moreover, in alloy A, as the volume fraction of precipitate increases with aging, the movement of martensitic interfaces is restricted causing a decreased tan δ.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

P-Nickel hydroxide comprises a long range periodic arrangement of atoms with a stacking sequence of AC AC AC-having an ideal composition Ni(OH)(2). Variation in the preparative conditions can lead to the changes in the stacking sequence (AC AC BA CB AC AC or AC AC AB AC AC) This type of variation in stacking sequence can result in the formation of stacking fault in nickel hydroxide. The stability of the stacking fault depends on the free energy content of the sample. Stacking faults in nickel hydroxide is essential for better electrochemical activity. Also there are reports correlating particle size to the better electrochemical activity. Here we present the effect of crystallite size on the stacking faulted nickel hydroxide samples. The electrochemical performance of stacking faulted nickel hydroxide with small crystallite size exchanges 0.8e/Ni, while the samples with larger crystallite size exchange 0.4e/Ni. Hence a right combination of crystallite size and stacking fault content has to be controlled for good electrochemical activity of nickel hydroxide. (C) 2008 Elsevier B.V. All rights reserved.