Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
This study evaluated the influence of light-curing units (LCUs) on Knoop microhardness (KHN) of different composite resins formulations. Four LCUs, one Quartz-Tungsten-Halogen (QTH) for 20 s, one Argon-Ion-Laser (AL) for 10 s, one Plasma-Arc-Curing (PAC) for 9 s, and one Light-Emitting-Diode (LED) for 20 s, and three composite resins, nanofill and easy cure (Filtek (TM) Supreme), microhybrid and medium cure (Herculite XRV), and microfill and difficult cure (Heliomolar) were used. Discs (4 x 2 mm(2)) of each composite resin were divided in 12 Groups and KHN was measured at the top (T) and bottom (B) surfaces. Data were analyzed using two-way ANOVA and Tukey's test (p < 0.05). Top presented significantly higher KHN than bottom surface for all composite resins and LCUs tested. Statistical significant differences were observed among the LCUs. At the bottom surface QTH and LED presented higher KHN than PAC and LA. However, at the top surface PAC and LA presented similar results than QTH for nanofill and microhybrid composite resins. Different LCUs play an important effect on Knoop microhardness and the composite resin formulations were significant factor on the photosensitivity.
Resumo:
The purpose of this study was to evaluate the influence of different light sources for in-office bleaching on surface microhardness of human enamel. One hundred and five blocks of third molars were distributed among seven groups. The facial enamel surface of each block was polished and baseline Knoop microhardness of enamel was assessed with a load of 25 g for 5 s. Subsequently, the enamel was treated with 35% hydrogen peroxide bleaching agent and photo-activated with halogen light (group A) during 38 s, LED (group B) during 360 s, and high intensity diode laser (group C) during 4 s. The groups D (38 s), E (360 s), and F (4 s) were treated with the bleaching agent without photo-activated. The control (group G) was only kept in saliva without any treatment. Microhardness was reassessed after 1 day of the bleaching treatment, and after 7 and 21 days storage in artificial saliva. The mean percentage and standard deviation of microhardness in Knoop Hardness Number were: A 97.8 +/- 13.1 KHN; B 95.5 +/- 12.7 KHN; C 84.2 +/- 13.6 KHN; D 128.6 +/- 20.5 KHN; E 133.9 +/- 14.2 KHN; F 123.9 +/- 14.2 KHN; G 129.8 +/- 18.8 KHN. Statistical analysis (p < 0.05; Tukey test) showed that microhardness percentage values were significantly lower in the groups irradiated with light when compared with the non-irradiated groups. Furthermore, the non-irradiated groups showed that saliva was able to enhance the microhardness during the measurement times. The enamel microhardness was decreased when light sources were used during the bleaching process and the artificial saliva was able to increase microhardness when no light was used.
Resumo:
The aim of this study was to determine the effect of two light-curing units (QTH and LED) on microleakage of Class II composite resin restorations with dentin cavosurface margins. Twenty extracted mandibular first premolars, free of caries and fractures were prepared two vertical slot cavities in the occluso-mesial and -destal surfaces (2 mm buccal-lingually, 2 mm proximal-axially and cervical limit in enamel) and divided into 4 equal groups (n = 8): GI and GII: packable posterior composite light-activated with LED and QTH, respectively; GIII and GIV: micro-hybrid composite resin light-activated with LED and QTH, respectively. The composite resins were applied following the manufacturer's instructions. After 24 h of water storage specimens were subjected to thermocycling for a total of 500 cycles at 5 and 55A degrees C and the teeth were then sealed with impermeable material. Teeth were immersed in 0.5% Basic fuchsin during 24 h at room temperature, and zero to three levels of penetration score were attributed. The Mann-Whitney and Kruskal-Wallis tests showed significant statistically similar (P > 0.05) from GI to GII and GIII to GIV, which the GII (2.750) had the highest mean scores and the GIII and GIV (0.875) had lowest mean scores. The use of different light-curing units has no influence on marginal integrity of Class II composite resin restorations and the proprieties of composite resins are important to reduce the microleakage.
Resumo:
The germination of seeds of Psidium guajava L. (Myrtaceae) is controlled by phytochrome. Guava seeds can germinate with at least one hour per day of irradiation of high red:far-red ratio light preceeded or followed by shade light, indicating that phytochrome B controls germination in these conditions. Under alternating temperatures, in a range of at least 5degreesC, seeds will germinate in darkness, suggesting that in gaps of the canopy, when seeds are covered by a thin layer of soil they will germinate once the alternating temperatures are experienced. Under these conditions phytochrome A is responsible for the control of guava seed germination.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Purpose: To evaluate the effect of cement shade, light-curing unit, and water storage on tensile bond strength (a) of a feldspathic ceramic resin bonded to dentin.Materials and Methods: The dentin surface of 40 molars was exposed and etched with 37% phosphoric acid, then an adhesive system was applied. Forty blocks of feldspathic ceramic (Vita VM7) were produced. The ceramic surface was etched with 10% hydrofluoric acid for 60 s, followed by the application of a silane agent and a dual-curing resin cement (Variolink II). Ceramic blocks were cemented to the treated dentin using either A3 or transparent (Tr) shade cement that was activated using either halogen or LED light for 40 s. All blocks were stored in 37 degrees C distilled water for 24 h before cutting to obtain non-trimmed bar-shaped specimens (adhesive area = 1 mm(2) +/- 0.1) for the microtensile bond strength test. The specimens were randomly grouped according to the storage time: no storage or stored for 150 days in 37 degrees C distilled water. Eight experimental groups were obtained (n = 30). The specimens were submitted to the tensile bond strength test using a universal testing machine at a crosshead speed of 1 mm/min. The data were statistically analyzed using ANOVA and Tukey's post-hoc tests (alpha = 0.05).Results: The mean bond strength values were significantly lower for the corresponding water stored groups, except for the specimens using A3 resin cement activated by halogen light. There was no significance difference in mean bond strength values among all groups after water storage.Conclusion: Water storage had a detrimental effect under most experimental conditions. For both cement shades investigated (Tr and A3) under the same storage condition, the light-curing units (QTH and LED) did not affect the mean microtensile bond strengths of resin-cemented ceramic to dentin.
Morphological and physiological responses of Cedrela Fissilis Vellozo (Meliaceae) seedlings to light
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)