931 resultados para Crystal phase
Resumo:
Detailed molecular simulations are carried out to investigate the effect of temperature on orientational order in cubane molecular crystal. We report a transition from an orientationally ordered to an orientationally disordered plastic crystalline phase in the temperature range 425-450 K. This is similar to the experimentally reported transition at 395 K. The nature of this transition is first order and is associated with a 4.8% increase in unit Cell volume that is comparable to the experimentally reported unit cell volume change of 5.4% (Phys. Rev. Lett. 1997, 78, 4938). An orientational order parameter, eta(T), has been defined in terms of average angle of libration of a molecular 3-fold axis and the orientational melting has been characterized by using eta(T). The orientational melting is associated with an anomaly in specific heat at constant pressure (C-p) and compressibility (kappa). The enthalpy of transition and entropy of transition associated with this orientational melting are 20.8 J mol(-1) and 0.046 J mol(-1) K-1, respectively. The structure of crystalline as well as plastic crystalline phases is characterized by using various radial distribution functions and orientational distribution functions. The coefficient of thermal expansion of the plastic crystalline phase is more than twice that of the crystalline phase.
Resumo:
Crystal growth, electrical and magnetic properties are reported for mixed valence manganite Pr1-xPbxMnO3 (x = 0.2, 0.23, and 0.3). The crystals with x = 0.2 and 0.23 are ferromagnetic and insulating, whereas that with x = 0.3 is ferromagnetic below 200 K and shows an insulator-metal transition at 235 K. This composition shows a magnetoresistance of 90% in a field of 5 T. In the paramagnetic region, the temperature dependence of magnetic susceptibility of the crystals follows a Curie-Weiss behavior. The thermal evolution of magnetization in the ferromagnetic phase varies as T-3/2, in accordance with Bloch's law. The spin-stiffness constant D obtained from the Bloch constant is found to increase linearly with x. The magnetization does not reach complete saturation upto a field of 5 T. A possible contribution of the Pr spins to the total magnetic moment is discussed.
Resumo:
A solid solution of the type Ba5x/2Bi(1-x)5/3Nb5O15 has been identified in the BaO-Bi2O3-Nb2O5 system for the first time. The limits of the solid solution are within the range 0.52 <= x <= 0.80. The compositions x = 0.52, 0.60, 0.72, 0.77, 0.78, and 0.80 were synthesized by the solid-state technique from the starting materials in stoichiometric quantities. The powder X-ray patterns of all the phases in the domain indicate a structural similarity to tetragonal tungsten bronzes (TTBs). The compositions below x = 0.52 and those above x = 0.80 exhibit barium niobate and bismuth niobate impurities, respectively. Single crystals of the composition x = 0.77 were obtained by the melt cooling technique. The crystal structure of Ba3.85/2Bi1.15/3Nb5O15 (x = 0.77) was solved in the tetragonal space group P4bm (No. 100) with a = 12.4938 (14) angstrom, c = 3.9519 (2) A, V = 616.87 (10) angstrom(3), and Z = 2 and was refined to an R index of 0.034. Dielectric measurements on all the phases indicate a typical relaxor behavior with a broad phase transition at T-m approximate to 300 K.
Resumo:
The compound Bi3W2O10.5 was synthesized by the solid-state technique from Bi2O3 and WO3 in stoichiometric quantities. Single crystals were grown by the melt-cooling technique and the crystal structure was solved in the tetragonal 141in space group with a = 3.839 (1) A, c = 16-3S2 (5) A, V = 241.4 (1) angstrom(3), Z = 4 and was refined to an R index of 0.0672. The structure represents a modification of the Aurivillius phase and consists of [Bi2O2](2+) units separated by WO8 polyhedra. a.c. impedance studies indicate oxide ion conductivity of 2.91 10(-5) cm(-1) at 600 degrees C.
Resumo:
A detailed single-crystal EPR study of phase IV of lithium potassium sulphate below -138 degrees C has been carried out using NH3+, which substitutes for K+, as the paramagnetic probe. The spin-Hamiltonian parameters have been evaluated at -140 degrees C and yield an isotropic g=2.0034; (AH)XX=(AH)YY=25.3 G and (AH)ZZ=23.8 G; (AN)XX=8.1 G, (AN)YY=21.2 G and (AN)ZZ=25.9 G. In this phase there are 12 magnetically inequivalent K+ sites and their occurrence is ascribed to the loss of a c glide.
Resumo:
An optical investigation of the high-temperature structural phase transition in gel-grown single crystals of CslO4 is reported. This crystal undergoes a phase transition from the room-temperature orthorhombic phase of symmetry Pnma to a tetragonal phase at 150°C. The birefringence Δn = |na-nb| falls abruptly at Tc, indicating the first-order nature of the phase transition. Microscopic examination has revealed the existence of ferroelastic domains in the crystal. The domain structure and its dependence on temperature was studied in detail. The experimental results suggest that this crystal can be assigned to the ferroelastic Aizu species 4/mmmFmmm (p).
Resumo:
The present x-ray study has been undertook in order to correlate the phase transition in sodium metavanadate NaVO3 crystal with its structural aspects. The thermal expansion behaviour of NaVO3 was studied from room temperature up to 500 C, well beyond the transition temperature.
Resumo:
Ultraviolet radiation has been generated by tangentially phase-matched sum-frequency mixing in biaxial L-arginine phosphate (LAP) crystal for the first time using Nd:YAG output at 1064 nm and Rh 6G dye laser output at 560 nm as the two input sources. Characterization has also been made of such a cheap, biaxial crystal for its possible use in devices for tangentially phase-matched short wavelength generation. If the crystal is of proper cut, thickness and quality so that its maximum capability can be exploited it can replace the potassium dihydrogen phosphate (KDP) group of crystals for various applications.
Resumo:
Room-temperature Raman spectra of LiRbSO4 were studied as a function of pressure up to 170 kbar for two different orientations of the crystal. Four pressure-induced phase transitions at about 2, 17, 32 and 57 kbar were observed. The transitions at 17 and 57 kbar have slow kinetics, taking about 4 h for their completion. These phase transitions are associated with the orientations of the SO4 ions in the unit cell.
Resumo:
Monophasic CaNaBi2Nb3O12 powders were synthesized via the conventional solid-state reaction route. Rietveld refinement of the X-ray powder diffraction (XRD) data and selected area electron diffraction (SAED) studies confirmed the phase to be a three-layer Aurivillius oxide associated with an orthorhombic B2cb space group. The dielectric properties of the ceramics have been studied in the 300-800 K temperature range at various frequencies (1 kHz to 1 MHz). A dielectric anomaly was observed at 676 K for all the frequencies corresponding to the ferroelectric to paraelectric phase transition as it was also corroborated by the high temperature X-ray diffraction studies. The incidence of the polarization-electric field (P vs. E) hysteresis loop demonstrated CaNaBi2Nb3O12 to be ferroelectric.
Resumo:
We report a large decrease in tetragonal to cubic phase transformation temperature when grain size of bulk CuFe2O4 is reduced by mechanical ball milling. The change in phase transformation temperature was inferred from in situ high temperature conductivity and x-ray diffraction measurements. The decrease in conductivity with grain size suggests that ball milling has not induced any oxygen vacancy while the role of cation distribution in the observed decrease in phase transformation temperature is ruled out from in-field Fe-57 Mossbauer and extended x-ray absorption fine structure measurements. The reduction in the phase transformation temperature is attributed to the stability of structures with higher crystal symmetry at lower grain sizes due to negative pressure effect. (C) 2011 American Institute of Physics. doi: 10.1063/1.3493244]
Resumo:
Pure Y2O3 and Y2O3---ZrO2 solid solutions have been prepared by melt atomization and by pyrolysis of nitrate solutions. Extended solubility is readily achieved in both techniques for the entire composition range investigated: melts with 0–30% ZrO2 and precursors with 0–50% ZrO2. However, solidification of under cooled droplets yields almost exclusively single phase powders with the structure of cubic yttria (D53). In contrast, the pyrolysis route leads to a sequence of metastable microstructures beginning with a nanocrystalline disordered fluorite-based (C1) solid solution. Further heating leads to the evolution of much larger (micron size) flake crystals with a {001} texture, concurrent with partial ordering of the oxygen ions to the sites occupied in the D53 structure. The driving force for ordering and the rate of grain growth decrease with increasing ZrO2 addition. Abrupt heating to high temperatures or electron irradiation can induce ordering without substantial grain growth. There is no significant reduction in porosity during the recrystallization, which with the other observations suggests that grain growth is driven by the free energy available for the ordering transformation from fluorite to the yttria structure. This route offers opportunities for single crystal thin film development at relatively low processing temperatures.
Resumo:
Pure Y2O3 and Y2O3-ZrO2 solid solutions have been prepared by melt atomization and by pyrolysis of nitrate solutions. Extended solubility is readily achieved in both techniques for the entire composition range investigated: melts with 0-30% ZrO2 and precursors with 0-50% ZrO2. However, solidification of under cooled droplets yields almost exclusively single phase powders with the structure of cubic yttria (D5(3)). In contrast, the pyrolysis route leads to a sequence of metastable microstructures beginning with a nanocrystalline disordered fluorite-based (C1) solid solution. Further heating leads to the evolution of much larger (micron size) flake crystals with a {001} texture, concurrent with partial ordering of the oxygen ions to the sites occupied in the D5(3) structure. The driving force for ordering and the rate of grain growth decrease with increasing ZrO2 addition. Abrupt heating to high temperatures or electron irradiation can induce ordering without substantial grain growth. There is no significant reduction in porosity during the recrystallization, which with the other observations suggests that grain growth is driven by the free energy available for the ordering transformation from fluorite to the yttria structure. This route offers opportunities for single crystal thin film development at relatively low processing temperatures.
Resumo:
In this paper we report the mechanical alloying behaviour of elemental aluminium with diamond cubic elements Ge and Si. A metastable crystalline phase with rhombohedral crystal structure forms in Al-70 Ge-30 and Al-60 Ge-40 alloy compositions. The phase always coexists with elemental constituents and decomposes over a broad temperature range. No such metastable phase could be observed in the Al-Si system. We also report X-ray diffractometry and differential scanning calorimetry results suggestive of amorphization. Finally a comparison was made of the present result with that obtained in rapid solidification.
Resumo:
We prove that CdS nanocrystals can be thermodynamically stabilized in both wurtzite and zinc-blende crystallographic phases at will, just by the proper choice of the capping ligand. As a striking demonstration of this, the largest CdS nanocrystals (similar to 15 nm diameter) ever formed with the zinc-blende structure have been synthesized at a high reaction temperature of 310 degrees C, in contrast to previous reports suggesting the formation of zinc-blende CdS only in the small size limit (< 4.5 nm) or at a lower reaction temperature (<= 240 degrees C). Theoretical analysis establishes that the binding energy of trioctylphosphine molecules on the (001) surface of zinc-blende CdS is significantly larger than that for any of the wurtzite planes. Consequently, trioctylphosphine as a capping agent stabilizes the zinc-blende phase via influencing the surface energy that plays an important role in the overall energetics of a nanocrystal. Besides achieving giant zinc-blende CdS nanocrystals, this new understanding allows us to prepare CdSe and CdSe/CdS core/shell nanocrystals in the zinc-blende structure.