Resumo:
In general, among the corrosion inhibitors surfactants are the most commonly used compounds, because they are significantly effective by forming protective films on anodic and cathodic areas. In this study, microemulsions containing he biodegradable saponified coconut oil as surfactant (SME-OCS) was used as green corrosion inhibitors. With this purpose, methanolic extracts of Ixora coccinea Linn (IC) and a polar fraction rich in alkaloids (FA) obtained from Croton cajucara Benth solubilized in the SME-OCS system were examined in the presence of AISI 1020 carbon steel, in saline solution (NaCl 3,5 %). The efficiency of corrosion inhibition of IC and FA were evaluated in the following microemulsions: SME-OCS-IC and SME-OCS-FA. The microemulsion system SME-OCS in the presence and absence of IC and FA was assessed by measurements of weight loss and the electrochemical method of polarization resistance, with variation in the concentration of IC and FA (50 - 400 ppm), showing significant results of corrosion inhibition (83,6 % SME-OCS; 92,2 % SME-OCS-FA; and 95,3 % SME-OCS-IC)
Resumo:
In the search for products that act as corrosion inhibitors and do not cause environmental, impact the use of plant extracts as corrosion inhibitors is becoming a promising alternative. In this work the efficiency of polar extracts (ethanol extracts) obtained from the plants Anacardium occidentale Linn (AO) and Phyllantus amarus Schum. & Thonn (PA) as corrosion inhibitors were evaluated in different concentrations. For that AO and PA extracts were solubilized in the microemulsion systems (SME) containing saponified coconut oil as surfactant (SME -OCS and SME-OCS-1) in saline (NaCl 3,5 %) solution, which was also used as electrolyte. Both SME-OCS and SME-OCS-1 were characterized by surface tension and viscosity methods showing a Newtonian fluid behavior. The SME-OCS and SME-OCS-1 systems satisfactorily solubilized the polar extracts AO and PA with measurements carried out by ultraviolet spectroscopy. The measurements of corrosion inhibition efficiencies were performed by the electrochemical linear polarization resistance (LPR) technique as well as weight loss, on the surface of AISI 1020 carbon steel. The maximum corrosion inhibition efficiencies were determined by extrapolation of Tafel plots, showing the following values: 95,6 % for the system SME-OCS-AO, 98,9 % for the system SME-OCS-AO-1 and 93,4 % for the system SME-OCS-PA
Resumo:
Artigo licenciado sob uma Licença Creative Commons: https://creativecommons.org/licenses/by-nc/4.0/deed.pt
Resumo:
The main problem on the exploration activity on petroleum industry is the formation water resulted on the fields producing. The aggravating of this problem is correlated with the advancing technologies used on the petroleum extractions and on its secondary approach objecting the reobtainment of this oil. Among the main contaminants of the water formation are corrosives gases such as: O2, CO2 and H2S, some solids in suspension and dissolved salts. Concerning to those gases the CO2 is the one that produce significant damage for carbon steel on corrosion process of the petroleum and gas industries. Corrosion inhibitors for carbon steel in formation water is one of the most used agents in control of those damages. In this context, the poor investigations of carbon steel corrosion proceeding from solids in suspension is an opened field for studies. On this work the inhibitor effect of the commercial CORRTREAT 703 was evaluated on some specific solids in suspension at saline medium containing 10.000 ppm of de-aerated chloride using CO2 until non oxygen atmosphere been present. For that, quartz, calcium carbonate, magnetite and iron sulphide were subjected to this investigation as the selected solids. The effect of this inhibitor on corrosion process correlated with those specific solids, was measured using electrochemical (resistance of linear polarization and galvanic pair) and gravimetrical techniques. During all the experimental work important parameters were monitored such as: pH, dissolved oxygen, temperature, instantaneous corrosion rate and galvanic current. According to the obtained results it was proved that the suspension solids calcium carbonate and iron sulphide decrease the corrosion process in higher pH medium. Meanwhile the quartz and magnetite been hardness increase corrosion by broking of the passive layer for erosion. In the other hand, the tested inhibitor in concentration of 50 ppm, showed to be effective (91%) in this corrosion process
Resumo:
This thesis has as objective presents a methodology to evaluate the behavior of the corrosion inhibitors sodium nitrite, sodium dichromate and sodium molybdate, as well as your mixture, the corrosion process for the built-in steel in the reinforced concrete, through different techniques electrochemical, as well as the mechanical properties of that concrete non conventional. The addition of the inhibitors was studied in the concrete in the proportions from 0.5 to 3.5 % regarding the cement mass, isolated or in the mixture, with concrete mixture proportions of 1.0:1.5:2.5 (cement, fine aggregate and coarse aggregate), superplasticizers 2.0 % and 0.40 water/cement ratio. In the modified concrete resistance rehearsals they were accomplished to the compression, consistence and the absorption of water, while to analyze the built-in steel in the concrete the rehearsals of polarization curves they were made. They were also execute, rehearsals of corrosion potential and polarization resistance with intention of diagnose the beginning of the corrosion of the armors inserted in body-of-proof submitted to an accelerated exhibition in immersion cycle and drying to the air. It was concluded, that among the studied inhibitors sodium nitrite , in the proportion of 2.0 % in relation to the mass of the cement, presented the best capacity of protection of the steel through all the studied techniques and that the methodology and the monitoring techniques used in this work, they were shown appropriate to evaluate the behavior and the efficiency of the inhibitors
Resumo:
With the increasing of demand for natural gas and the consequent growth of the pipeline networks, besides the importance of transport and transfer of oil products by pipeline, and when it comes to product quality and integrity of the pipeline there is an important role regarding to the monitoring internal corrosion of the pipe. This study aims to assess corrosion in three pipeline that operate with different products, using gravimetric techniques and electrical resistance. Chemical analysis of residues originated in the pipeline helps to identify the mechanism corrosive process. The internal monitoring of the corrosion in the pipelines was carried out between 2009 and 2010 using coupon weight loss and electrical resistance probe. Physico-chemical techniques of diffraction and fluorescence X-rays were used to characterize the products of corrosion of the pipelines. The corrosion rate by weight loss was analyzed for every pipeline, only those ones that has revealed corrosive attack were analyzed located corrosion rate. The corrosion potential was classified as low to pipeline gas and ranged from low to severe for oil pipelines and the pipeline derivatives. Corrosion products were identified as iron carbonate, iron oxide and iron sulfide
Resumo:
Removable partial dentures (RPD) demand specific hygienic cleaning and the combination of brushing with immersion in chemical solutions has been the most recommended method for control of biofilm. However, the effect of the cleansers on metallic components has not been widely investigated. This study evaluated the effect of different cleansers on the surface of RPD. Five disc specimens (12 mm x 3 mm metallic disc centered in a 38 x 18 x 4 mm mould filled with resin) were obtained for each experimental situation: 6 solutions [Periogard (PE), Cepacol (CE), Corega Tabs (CT), Medical Interporous (MI), Polident (PO), 0.05% sodium hypochlorite (NaOCl), and distilled water (DW) control] and 2 Co-Cr alloys [DeguDent (DD) and VeraPDI (VPDI)] were used for each experimental situation. A 180-day immersion was simulated and the measurements of roughness (Ra, µm) of metal and resin were analyzed using 2-way ANOVA and Tukey’s test. The surface changes and tarnishes were examined with a scanning electronic microscopy (SEM). In addition, energy dispersive x-ray spectrometry (EDS) analysis was carried out at representative areas. Visually, NaOCl and MI specimens presented surface tarnishes. The roughness of materials was not affected by the solutions (p>0.05). SEM images showed that NaOCl and MI provided surface changes. EDS analysis revealed the presence of oxygen for specimens in contact with both MI and NaOCl solutions, which might suggest that the two solutions promoted the oxidation of the surfaces, thus leading to spot corrosion. Within the limitations of this study, it may be concluded that the NaOCl and MI may not be suitable for cleaning of RPD.
Resumo:
Foi estudado o comportamento eletroquímico a 37°C do aço inoxidável ISO 5832-9, em meios de NaCl 0,9 %, de Ringer Lactato e meio mínimo de Eagle (MEM), por voltametria linear e análises da superfície por microscopia eletrônica de varredura (MEV) e por espectroscopia por dispersão de energia (EDS). Foram feitos ensaios mecânicos e testes de toxicidade. O aço ISO 5832-9 se encontra passivado no potencial de corrosão e não apresenta corrosão por pite nos três meios estudados em toda faixa de potencial investigada, desde o potencial de corrosão até 50 mV acima do potencial de transpassivação. Em meio de MEM, no entanto, as análises por MEV e EDS mostraram que o referido aço, nesse valor mais elevado de potencial, apresentou um comportamento diferente, com perda das inclusões de óxido de manganês. Os potenciais de corrosão, Ecorr (potencial de circuito aberto estacionário) bem como os valores de densidade de corrente de passivação, variaram na seguinte ordem: Ecorr, RL < Ecorr, NaCl < Ecorr, MEM. e jMEM << jRL ≅ jNaCl. No ensaio de citotoxicidade, o aço foi caracterizado como não-tóxico.
Resumo:
An alternative technique for the fabrication of disposable electrochemical microcells containing working, reference and auxiliary electrodes on a single device is reported. The procedure is based on thermal-transfer of toner masks onto CD-R (recordable compact discs) gold surfaces to define the layout of the electrodes (contour). In a subsequent step, the layout is manually painted with a permanent marker pen. The unprotected gold surface is conveniently etched (chemical corrosion) and the ink is then easily removed with ethanol, generating gold surfaces without contamination. The final and reproducible area of the electrodes is defined by heat transference of a second toner mask. Silver epoxy is deposited on one of the gold bands which is the satisfactorily used as reference electrode. These microcells were electrochemically characterized by cyclic, linear, and square wave voltammetry, and several electroactive species were used as model systems. The area reproducibility of the electrodes for different microcells was studied and a relative standard deviation better than 1,0% (n = 10) was obtained. Disposable electrochemical microcells were successfully used in analysis of liquid samples with volumes lower than 200 µL and good stability and reproducibility (RSD less than 2.0%) were achieved. These microcells were also evaluated for quantification of paracetamol and dipyrone in pharmaceutical formulations.
Resumo:
As infra-estruturas de rede de radiocomunicações são o suporte físico para a instalação do equipamento de rádio para a emissão de ondas electromagnéticas que permitem as telecomunicações móveis, sendo um património valioso tanto a nível de bem como de garantia de serviço. Como qualquer infra-estrutura é imprescindível a sua manutenção de forma a garantir o prolongamento da vida do bem e a segurança dos seus utilizadores. Na degradação de um poste ou torre estão envolvidos vários factores nomeadamente relacionados com as características do material, construção, ambientais e utilização. Pretende o presente relatório descrever os principais aspectos relacionados com implementação do processo de avaliação do estado estrutural dos postes ou torres, através da observação, inspecção e ensaios e, ainda descrever a metodologia implementada para a conservação estrutural, prevenção dos riscos na sua utilização e manutenção. Todo o processo implementado teve em consideração a segurança de pessoas e bens prevista na lei bem com a garantia dos trabalhos executados na fase de execução e a longo prazo, com ferramentas específicas de controlo e fiscalização.
Resumo:
A carbonatação e as suas consequências sobre o betão são do conhecimento do meio científico e técnico, e tem sido analisada há já algumas décadas. A perda do ambiente favorável criado pelo betão em torno das armaduras, provocada pela reacção do dióxido de carbono existente no ar com o hidróxido de cálcio do betão, é o início de um processo que conduz à degradação das estruturas de betão armado. Esta dissertação está estruturada em duas partes fundamentais. Na primeira parte ilustra-se o estado da arte ao desenvolver os temas, directa e indirectamente relacionados com o fenómeno da carbonatação e sua influência sobre as armaduras. Pretendeu-se envolver o conhecimento adquirido, nos temas que vão desde o fabrico do cimento até à sua hidratação, correlacionando as suas características e propriedades. Na segunda parte é analisado o caso de estudo relativo à cidade de Lisboa, pelo esforço de obter algum conhecimento, no que respeita ao fenómeno da carbonatação nas edificações e do respectivo impacto passados mais de 50 anos. Em face do actual estado da arte da edificação e da reabilitação no país, e concretamente na cidade Lisboa, considera-se com sentido de oportunidade o tema desenvolvido. É deste modo possibilitado o conhecimento efectivo da amplitude do fenómeno da carbonatação em alguns edifícios, bem como o estado de degradação da sua estrutura.
Resumo:
A presente dissertação expõe o trabalho desenvolvido ao longo do estágio de natureza profissional, integrado no curso de Mestrado de Engenharia Mecânica - Perfil de Manutenção e Produção. Sob uma orientação bem definida, a principal motivação deste trabalho consistiu na análise de eficácia dos métodos do projecto, construção e instalação dos gasodutos de gás natural em conformidade com os códigos e normas aplicáveis, de forma a verificar se a sua integridade pode ser eficazmente monitorizada pelas diversas técnicas de inspecção executadas. No presente documento é inicialmente abordado o impacto do gás natural nos tempos actuais, seguidamente é descrita a metodologia adjacente aos processos de construção em que se incluiu a análise de um aço para o fabrico de tubagens. Seguidamente é efectuada a descrição das etapas no terreno que constituem a construção de um gasoduto, designadamente a: Abertura de Pista, Alinhamento de Tubagem, Colocação do Tubo à Vala, Curvatura de Tubos, Atravessamentos, Soldadura, Controlo não Destrutivo, Revestimento, Ensaios diversos (Dieléctricos, Resistência Mecânica, Estanquidade), Cobertura da Vala, Protecção Catódica, Sinalização e Instrumentação (e.g.: SCADA). Posteriormente são descritas as técnicas de inspecção. Posteriormente são analisadas as técnicas de inspecção mais utilizadas em fase de exploração de um gasoduto, considerando a inspecção a sistemas de Protecção Catódica, a inspecção por PIGs e a inspecção por Ondas Guiadas. Sob uma lógica de constante evolução tecnológica torna-se imperativo adaptar os actuais processos de construção a sistemas onde a optimização ao nível dos materiais (aços) pode constituir uma mais valia para o projecto, pelo que é efectuada uma análise de abordagem futura para os gasodutos. A instalação de uma gasoduto obedece ao complexo cumprimento das diversas etapas, sendo a fiabilidade de cada actividade determinante para o sucesso das fases subsequentes. Foi dada uma especial atenção à Protecção Catódica, tendo-se demostrado que esta técnica é actualmente um dos meios mais eficazes para atenuar e prevenir a degradação por corrosão, pois este é o mecanismo de falha mais premente. A adopção de novos aços poderá traduzir-se numa redução de recursos materiais na construção e redução dos custos associados. Um gasoduto é uma infra-estrutura ainda em constante dinamismo. A evolução tecnológica ao nível dos materiais tem efeitos práticos no cálculo, construção e exploração reflectindo a optimização dos processos e a satisfação das necessidades energéticas, por via da inovação nos gasodutos de alta pressão.
Resumo:
Pretende-se com a realização deste trabalho apresentar um estudo sobre os materiais existentes no mercado para a execução de impermeabilizações e, em particular, sobre os de impermeabilização capilar do betão por meio de argamassas cimentícias pré-doseadas. Numa primeira abordagem, e como análise inicial, far-se-á uma apresentação resumida de alguns dos sistemas de impermeabilização mais usados actualmente e serão comparadas as suas caraterísticas. Em relação ao sistema de impermeabilização capilar do betão por meio de argamassas cimentícias pré-doseadas será apresentado o processo físico-quimico de actuação e explicado, em termos teóricos, como se processa a sua aplicação e funcionamento. Por fim, demonstrar-se-ão casos práticos de aplicação de um material, com as várias fases de actuação e intervenção necessárias, para diferentes tipos de patologias e situações.
Resumo:
A presente tese teve por base o estudo da conversão química da liga de alumínio 2024T3 de aplicação aeronáutica. O trabalho experimental foi desenvolvido na OGMA, Indústria Aeronáutica de Portugal S.A., durante o período de, aproximadamente 1 ano, que coincidiu com a realização de um estágio profissional nesta empresa por parte da mestranda. A referida empresa, tem como actividade a prestação de serviços de Manutenção, Revisão, Modernização, de Aeronaves, Motores e Componentes, Fabricação e Montagem de Estruturas. Integrada na OGMA, encontra-se a área de tratamentos electroquímicos, TE’S, na qual são realizados serviços de manutenção de material aeronáutico e de peças de fabricação. Estes serviços baseiam-se em processos de electrodeposição e conversão química. De modo a garantir um controlo de qualidade e correcto funcionamento dos diversos processos existe, inserido na área TE’S, um laboratório químico. O presente trabalho experimental, realizado na área TE’S, assenta no processo de conversão química, por imersão, de provetes da liga Al 2024-T3, referente a todos os contratos da OGMA. Estes contratos possuem especificações para aplicação do revestimento de conversão química, por imersão, em alumínio e suas ligas. Estas especificações incluem requisitos de qualidade, nos quais se encontra inserido o controlo periódico do processo. Deste modo, o processo é sujeito a um controlo periódico mensal que consiste na avaliação da qualidade dos tratamentos. A qualidade dos revestimentos obtidos, por conversão química, é assegurada através da avaliação dos resultados dos ensaios aos provetes. O estudo experimental desenvolvido focou-se nos ensaios de resistência à corrosão (nevoeiro salino) requeridos nos contratos. O intuito de realizar um estudo sobre o processo de conversão química por imersão de provetes da liga Al 2024 T3 e subsequente foco no ensaio de resistência à corrosão (nevoeiro salino), assenta no facto de ter-se vindo a observar, nos últimos anos, corrosão por pitting em vários lotes destes provetes, após serem sujeitos às sequências de processo de conversão química e antes de perfazerem a totalidade de 168 horas na câmara de nevoeiro salino, não superando este critério de qualidade do revestimento. Na perspectiva de colmatar a referida situação, procedeu-se à realização de ensaios de despiste nos provetes representativos da liga, com especial incidência na variação dos intervalos de tempo de imersão, pré-estabelecidos pelas especificações aplicáveis, e observação do seu comportamento quando sujeitos ao ensaio de nevoeiro salino.