The effect of seed addition on the microstructure and non-ohmic properties of the SnO2 + 1%CoO + 0.05%Nb2O5 ceramic-based system was analyzed. Two classes of seeds were prepared: 99% SnO2 + 1%CuO and 99% SnO2 + 1%CoO (mol%); both classes were added to the ceramic-based system in the amount of 1%, 5%, and 10%. The two systems containing 1% of seeds resulted in a larger grain size and a lower breakdown voltage. The addition of 1% copper seeds produces a breakdown voltage (V b) of ∼ 37 V and a leakage current (fic) of 29 μA. On the other hand, the addition of 1% cobalt seeds produced a breakdown voltage of 57 V and a leakage current of 70 μA. Both systems are of great technological interest for low voltage varistor applications, by means of appropriate strategies to reduce the leakage current. Using larger amounts of seeds was not effective since the values of breakdown voltage in both cases are close to a system without seeds. To our knowledge, there are no reports in the literature regarding the use of seeds in the SnO2 system for low voltage applications. A potential barrier model which illustrates the formation of oxygen species (O′2(ads), O′ads, and O″ads) at the expense of clusters near the interface between grains is proposed. © 2012 The American Ceramic Society.
Sintering of porous alumina obtained by biotemplate fibers for low thermal conductivity applications
Resumo:
In this research report, a sintering process of porous ceramic materials based on Al2O3 was employed using a method where a cation precursor solution is embedded in an organic fibrous cotton matrix. For porous green bodies, the precursor solution and cotton were annealed at temperatures in the range of 100-1600°C using scanning electron microscopy (SEM) and thermogravimetric (TG) analysis to obtain a porous body formation and disposal process containing organic fibers and precursor solution. In a structure consisting of open pores and interconnected nanometric grains, despite the low porosity of around 40% (calculated geometrically), nitrogen physisorption determined a specific surface area of 14m2/g, which shows much sintering of porous bodies. Energy dispersive X-ray (EDX) and X-ray diffraction (XRD) analytical methods revealed a predominant amount of α-Al2O3 in the sintered samples. Thermal properties of the sintered Al2O3 fibers were obtained by using the Laser Flash which resulted in the lower thermal conductivity obtained by α-Al2O3 and therefore improved its potential use as an insulating material. © 2012 Elsevier Ltd.
Resumo:
In the current article, we studied the effect of yttrium [Y3+] ions' substitution on the structure and electric behavior of barium zirconate titanate (BZT) ceramics with a general formula [Ba1-x Y 2x/3](Zr0.25Ti0.75)O3 (BYZT) with [x = 0, 0.025, 0.05] which were prepared by the solid-state reaction method. X-ray diffraction patterns indicate that these ceramics have a single phase with a perovskite-type cubic structure. Rietveld refinement data confirmed [BaO 12], [ZrO6], [TiO6], [YO6] clusters in the cubic lattice. The Y3+ ions' effects on the electric conductivity behavior of BZT ceramics as a function of temperature and frequency are described, which are based on impedance spectroscopy analyses. The complex impedance plots display a double semicircle which highlights the influences of grain and grain boundary on the ceramics. Impedance analyses showed that the resistance decreased with the increasing temperature and resulted in a negative temperature coefficient of the resistance property in all compositions. Modulus plots represent a non-Debye-type dielectric relaxation which is related to the grain and grain boundary as well as temperature-dependent electric relaxation phenomenon and an enhancement in the mobility barrier by Y3+ ions. Moreover, the electric conductivity increases with the replacement of Ba 2+ by Y3+ ions may be due to the rise in oxygen vacancies. © 2013 The Minerals, Metals & Materials Society and ASM International.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Pós-graduação em Ciência e Tecnologia de Materiais - FC
Resumo:
Pós-graduação em Reabilitação Oral - FOAR
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Pós-graduação em Ciências Odontológicas - FOAR
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Pós-graduação em Reabilitação Oral - FOAR
Resumo:
Pós-graduação em Reabilitação Oral - FOAR
Resumo:
Neste trabalho, estudou-se o comportamento térmico, a evolução das fases cristalinas com a temperatura e as propriedades físico-mecânicas da Lama Vermelha (LV) procedente da indústria de alumínio do Estado do Maranhão. O estudo foi realizado por Análise Termogravimétrica (TG) e Calorimetria Exploratória Diferencial (DSC), Dilatometria Ótica até 1350 ºC; enquanto a evolução das fases cristalinas com a temperatura foi realizada no intervalo entre 750 a 1150 ºC por Difração de Raios-X (DRX). As propriedades físico-mecânicas como Superfície Específica, Granulometria, Limite Plástico (LP), Limite de Liquidez (LL), Índice de Plasticidade (IP), Tensão de Ruptura a Flexão (TRF), Absorção de Água (AA), Retração Linear Após Queima (RL) e Porosidade Aparente (PA) foram determinadas nas mesmas temperaturas. As seguintes fases cristalinas foram detectadas: hematita, sodalita e anatásio entre 750-850 ºC; e hematita, nefelina e sodalita entre 950-1150 ºC. Os ensaios tecnológicos demonstraram que a LV pode ser aplicada para o processamento de materiais cerâmicos estruturais, pois apresenta pouca reatividade entre 870-950 ºC, com elevada AA, e baixas RL e TRF. Entre 950 e 1350 ºC, a LV sofreu uma retração que variou entre 5-50 %, com fusão total a 1350 ºC, devido à presença de fases minerais do tipo feldespatoides em sua composição.