987 resultados para fracture failure
Resumo:
The effects of temperature on the fast fracture behavior of aluminum nitride with 5 wt% Y(2)O(3) ceramic were investigated. Four-point flexural strength and fracture toughness were measured in air at several temperatures (30-1,300 A degrees C). The flexural strength gradually decreased with the increase of temperature up to 1,000 A degrees C due to the change in the fracture mode from transgranular to intergranular, and then became almost constant up to 1,300 A degrees C. Two main flaw types as fracture origin were identified: small surface flaw and large pores. The volume fraction of the large pores was only 0.01%; however, they limited the strength on about 50% of the specimens. The fracture toughness decreased slightly up to 800 A degrees C controlled by the elastic modulus change, and then decreased significantly at 1,000 A degrees C due to the decrease in the grain-boundary toughness. Above 1,000 A degrees C, the fracture toughness increased significantly, and at 1,300 A degrees C, its value was close to that measured at room temperature.
Resumo:
Coaracy Nunes was the first hydroelectric power plant in the Amazon region, being located in Araguari River, Amapa State, Brazil. The plant operates since 1976, presenting now a nominal capacity of 78 MW. The shear pins, which are installed in the turbine hydraulic arms to control the wicket gate and regulate the water flow into the turbine blades, suffered several breakdowns since 2004. These shear pins are made of an ASTM 410 stainless steel and were designed to break by a shear overload of 120 kN. Fractographic investigation of the pins, however, revealed two types of fracture topographies: a region of stable crack propagation area, with non-pronounced striation and secondary cracks; and a region of unstable propagation, featuring elongated dimples. These results indicated that the stable crack propagation occurred by fatigue (bidirectional bending), which was nucleated at machining marks under high nominal load. Finite element analysis was carried out using two loading conditions (pure shear and a combination of shear and bending) and the results indicated that the presence of a bending stress strongly increased the stress concentration factor (85% rise in the shear stress and 130% rise in the Von Mises stress). Misalignment during shear pins assembly associated with vibration might have promoted the premature failure of the shear by bending fatigue. (C) 2008 Elsevier Ltd. All rights reserved.
Resumo:
The premature failure of a horizontal heat-exchanger, which occurred after service exposure at 580 degrees C for 50,000 h, revealed the occurrence of extensive through-thickness cracking in approximately 40% of the tube/stationary tube-sheet welds. Additionally, the internal surface of the welded joint featured intensive secondary intergranular cracking (up to 250 mu m deep), preferential formation of a 150 mu m thick layer of (Fe, Cr)(3)O-4 and internal intergranular oxidation (40 mu m deep). The welded region also showed intense carbon pick-up and, as consequence, severe precipitation of intergranular M7C3 and M23C6 carbides. The fracture surface was composed of two distinct regions: a ""planar"" region of 250 mu m, formed due to the stable crack growth along by the intergranular oxidation; and a slant region with radial marks, formed by the fast crack growth along the network of intergranular carbides. The association of intergranular oxidation pre-cracks with microstructural embrittlement promoted the premature failure, which took place by an overload mechanism, probably due to the jamming of the floating tube-sheet during the maintenance halt (cooling operation). (C) 2007 Elsevier Ltd. All rights reserved.
Resumo:
This work investigates the effects of photodegradation on the environmental stress cracking resistance of polycarbonate (PC). Injection molded samples were exposed to the ultraviolet (UV) light for various times in the laboratory prior to solvent contact. The bars were then stressed with two different loads in a tensile testing machine under the presence of ethanol. During this period, the stress relaxation was monitored and, after unloading, the ultimate properties were evaluated. Complementary tests were done by size exclusion chromatography, UV-visible spectroscopy, scanning electron microscopy, and light microscopy. The results indicated that ethanol causes significant modification in PC, with extensive surface crazing as well as reduction in mechanical properties. The previous degraded samples showed a higher level of stress relaxation and a greater loss in tensile strength in comparison with the undegraded ones. The synergist action of photodegradation and stress cracking in PC may be a consequence of the chemical changes caused by oxidation.
Resumo:
For the first time, we introduce and study some mathematical properties of the Kumaraswamy Weibull distribution that is a quite flexible model in analyzing positive data. It contains as special sub-models the exponentiated Weibull, exponentiated Rayleigh, exponentiated exponential, Weibull and also the new Kumaraswamy exponential distribution. We provide explicit expressions for the moments and moment generating function. We examine the asymptotic distributions of the extreme values. Explicit expressions are derived for the mean deviations, Bonferroni and Lorenz curves, reliability and Renyi entropy. The moments of the order statistics are calculated. We also discuss the estimation of the parameters by maximum likelihood. We obtain the expected information matrix. We provide applications involving two real data sets on failure times. Finally, some multivariate generalizations of the Kumaraswamy Weibull distribution are discussed. (C) 2010 The Franklin Institute. Published by Elsevier Ltd. All rights reserved.
Resumo:
Analytical expressions are derived for the time and magnitude of failure of an isothermal CSTR with substrate-inhibited kinetics, caused by slow catalyst deactivation under three types of parallel and series mechanisms. Reactors operating at high space velocity are found to be most susceptible to early failure and poisoning by product is more dangerous than by reactant. The magnitude of the jump across steady states depends solely on the Langmuir-Hinshelwood kinetic parameters and a detailed analysis of reactor behavior during the jump itself is given.
Resumo:
Background-Catecholamines hasten cardiac relaxation through beta-adrenergic receptors, presumably by phosphorylation of several proteins, but it is unknown which receptor subtypes are involved in human ventricle. We assessed the role of beta(1)- and beta(2)-adrenergic receptors in phosphorylating proteins implicated in ventricular relaxation. Methods and Results-Right ventricular trabeculae, obtained from freshly explanted hearts of patients with dilated cardiomyopathy (n=5) or ischemic cardiomyopathy (n=5), were paced at 60 bpm. After measurement of the contractile and relaxant effects of epinephrine (10 mu mol/L) or zinterol (10 mu mol/L), mediated through beta(2)-adrenergic receptors, and of norepinephrine (10 mu mol/L), mediated through beta(1)-adrenergic receptors, tissues were freeze clamped. We assessed phosphorylation of phospholamban, troponin I, and C-protein, as well as specific phosphorylation of phospholamban at serine 16 and threonine 17, Data did not differ between the 2 disease groups and were therefore pooled. Epinephrine, zinterol, and norepinephrine increased contractile force to approximately the same extent, hastened the onset of relaxation by 15+/-3%, 5+/-2%, and 20+/-3%, respectively, and reduced the time to half-relaxation by 26+/-3%, 21+/-3%, and 37+/-3%. These effects of epinephrine, zinterol, and norepinephrine were associated with phosphorylation (pmol phosphate/mg protein) of phospholamban 14+/-3, 12+/-4, and 12+/-3, troponin I 40+/-7, 33+/-7, and 31+/-6; and C-protein 7.2+/-1.9, 9.3 +/- 1.4, and 7.5 +/- 2.0. Phosphorylation of phospholamban occurred at both Ser16 and Thr17 residues through both beta(1)- and beta(2)-adrenergic receptors. Conclusions-Norepinephrine and epinephrine hasten human ventricular relaxation and promote phosphorylation of implicated proteins through both beta(1)- and beta(2)-adrenergic receptors, thereby potentially improving diastolic function.
Resumo:
Objective To assess how well B-type natriuretic peptide (BNP) predicts prognosis in patients with heart failure. Design Systematic review of studies assessing BNP for prognosis m patients with heart failure or asymptomatic patients. Data sources Electronic searches of Medline and Embase from January 1994 to March 2004 and reference lists of included studies. Study selection and data extraction We included all studies that estimated the relation between BNP measurement and the risk of death, cardiac death, sudden death, or cardiovascular event in patients with heart failure or asymptomatic patients, including initial values and changes in values in response to treatment. Multivariable models that included both BNP and left ventricular ejection fraction as predictors were used to compare the prognostic value of each variable. Two reviewers independently selected studies and extracted data. Data synthesis 19 studies used BNP to estimate the relative risk of death or cardiovascular events in heart failure patients and five studies in asymptomatic patients. In heart failure patients, each 100 pg/ml increase was associated with a 35% increase in the relative risk of death. BNP was used in 35 multivariable models of prognosis. In nine of the models, it was the only variable to reach significance-that is, other variables contained no prognostic information beyond that of BNP. Even allowing for the scale of the variables, it seems to be a strong indicator of risk. Conclusion Although systematic reviews of prognostic studies have inherent difficulties, including die possibility of publication bias, the results of the studies in this review show that BNP is a strong prognostic indicator for both asymptomatic patients mid for patients with heart failure at all stages of disease.