888 resultados para Silica incorporation


Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper presents the instrumentation and control architecture for a laboratory based two-stage 4-bed silica gel + water adsorption system. The system consists of primarily two fluids: refrigerant (water vapour) and heat transfer fluid (water) flowing through various components. Heat input to the system is simulated using multiple heaters and ambient air is used as the heat sink. The laboratory setup incorporates a real time National Instruments (NI) controller to control several digital and analog valves, heaters, pumps and fans along with simultaneous data acquisition from various flow, pressure and temperature sensors. The paper also presents in detail the various automated and manual tasks required for successful operation of the system. Finally the system pressure and temperature dynamics are reported and its performance evaluated for various cycle times. (C) 2015 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Cost effective and low temperature synthesis methods namely solution combustion and hydrothermal methods were used to prepare chromium incorporated nanocrystalline zinc ferrites. The effect of incorporation of low concentration Cr3+ ions on the structural, morphological, magnetic and transport properties of the zinc ferrite compounds were investigated. The crystalline nature and size variation with chromium content were valid from powder x-ray diffraction. Particles size and crystallite size variation were valid from scanning electron microscopy and transmission electron microscopy respectively. With the increase in chromium incorporation, the crystallite and particles sizes were decreased. Fourier transform infrared spectroscopy (FTIR) studies confirmed the presence of strong metal-oxygen bonds. The elastic properties of the materials in both the methods were estimated by FTIR studies. Magnetic properties namely saturation magentization, remanent magnetization and coercivity values were decreased with increase in Cr3+ ions concentration. The dielectric properties of the samples decreased with increase in the Cr3+ ions. The dielectric constant was observed to be of the order of 10(6) at low frequency and almost 1 at higher frequency range. The activation energy estimated using Arrhenius plots was of the order of 0.182 eV and 0.368 eV respectively for the compounds prepared by solution combustion and hydrothermal methods. The emission spectra of the samples excited at 344 nm were reported using photoluminescence (PL) spectroscopy. Further, the approximate energy band gap(E-g) was estimated from PL studies. The E-g of the materials were lie in the range of 2.11-1.98 eV. (C) 2015 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An innovative technique to obtain high-surface-area mesostructured carbon (2545m(2)g(-1)) with significant microporosity uses Teflon as the silica template removal agent. This method not only shortens synthesis time by combining silica removal and carbonization in a single step, but also assists in ultrafast removal of the template (in 10min) with complete elimination of toxic HF usage. The obtained carbon material (JNC-1) displays excellent CO2 capture ability (ca. 26.2wt% at 0 degrees C under 0.88bar CO2 pressure), which is twice that of CMK-3 obtained by the HF etching method (13.0wt%). JNC-1 demonstrated higher H-2 adsorption capacity (2.8wt%) compared to CMK-3 (1.2wt%) at -196 degrees C under 1.0bar H-2 pressure. The bimodal pore architecture of JNC-1 led to superior supercapacitor performance, with a specific capacitance of 292Fg(-1) and 182Fg(-1) at a drain rate of 1Ag(-1) and 50Ag(-1), respectively, in 1m H2SO4 compared to CMK-3 and activated carbon.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This article presents a theoretical analysis of heat and mass transfer in a silica gel + water adsorption process using scaling principles. A two-dimensional columnar packed adsorber domain is chosen for the study, with side and bottom walls cooled and vapour inlet from the top. The adsorption process is initiated from the cold walls with a temperature jump of 15 K, whereas the water vapour supply is maintained at a constant inlet pressure of 1 kPa. The first part of the study is dedicated to deriving relevant scales for the adsorption process by an order of magnitude analysis of energy, continuity and momentum equations. In the latter part, the derived scales are compared with the outcome of numerical studies performed for various domain widths and aspect ratio of bed. A good correlation between scaling and simulation results is observed, thereby validating the scaling approach. (C) 2015 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An innovative technique to obtain high-surface-area mesostructured carbon (2545m(2)g(-1)) with significant microporosity uses Teflon as the silica template removal agent. This method not only shortens synthesis time by combining silica removal and carbonization in a single step, but also assists in ultrafast removal of the template (in 10min) with complete elimination of toxic HF usage. The obtained carbon material (JNC-1) displays excellent CO2 capture ability (ca. 26.2wt% at 0 degrees C under 0.88bar CO2 pressure), which is twice that of CMK-3 obtained by the HF etching method (13.0wt%). JNC-1 demonstrated higher H-2 adsorption capacity (2.8wt%) compared to CMK-3 (1.2wt%) at -196 degrees C under 1.0bar H-2 pressure. The bimodal pore architecture of JNC-1 led to superior supercapacitor performance, with a specific capacitance of 292Fg(-1) and 182Fg(-1) at a drain rate of 1Ag(-1) and 50Ag(-1), respectively, in 1m H2SO4 compared to CMK-3 and activated carbon.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, mechanical properties of silica-filled epoxy resin are tested. The tests show that at elevated temperatures, the material’s properties (e.g. yield stress, flow stress, etc.) vary immonotonically with filler volume fraction. Nanoindentation test results suggest that an interface region, stronger than the matrix, is formed in the materials. The formation of the interface has positive effects on the yield strengths of materials. The addition of particles in the matrix produces a large disturbance in stress distribution, leading to stress concentration in the matrix. The stress concentration has negative effects on the yield strengths of materials. The calculation demonstrates that the maximum stress in samples varies immonotonically with particulate concentration. So, the immonotonic variation of mechanical behavior of materials may be rooted in the contradictory effects of the interface region and the stress concentration caused by particulate addition.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The slurry erosion-corrosion behaviour of aluminium in aqueous silica slurries containing 0.5 M NaCl, acetic acid and 0.1 M Na2CO3 at open circuit has been investigated using a modified slurry erosion rig. The erosion rates of aluminium in the NaCl and acetic acid slurries were much higher than those in an aqueous slurry without electrolyte additives even though the pure corrosion component was very small. Eroded specimens were examined by scanning electron and optical microscopy. In pure aqueous slurry erosion, the basic mechanism leading to mass loss was the ductile fracture of flakes formed on the eroded surface. In corrosive slurries, however, the mass loss was enhanced by cracking of the flakes induced by stress and corrosion. © 1995.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Structural changes induced by the incorporation of nitrogen into ta-C : H films have been studied by Electron Energy Loss Spectroscopy, X-Ray Photoelectron Spectroscopy, Fourier Transformed Infrared Spectroscopy and Ultraviolet-Visible Spectroscopy. ta-C:H films have been synthesised using a low pressure Electron Cyclotron Wave Resonance (ECWR) source which provides a plasma beam with a high degree of ionisation and dissociation. Nitrogen was incorporated by adding N2 to the C2H2 plasma used for the deposition of ta-C : H films. The N/C atomic ratio in the films rises rapidly until the N2/C2H2 gas ratio reaches three, and then increases more gradually, while the deposition rate decreases steeply. Chemical sputtering of the forming films and the formation of molecular nitrogen within the films limit the maximum nitrogen content to about N/C = 0.6. For low nitrogen content the films retain their diamond-like properties, however as N/C atomic ratio increases, a polymeric-like material is formed, with >C=N- structures and terminating C=N and NH groups that decrease the connectivity of the network.