Resumo:
C-13 and H-1 relaxation times were measured as a function of temperature in two magnetic fields for dilute solutions of phenolphthalein poly(ether sulfone) (PES-C) in deuterated chloroform. The spin-lattice relaxation times were interpreted in terms of segmental motion characterized by the sharp cutoff model of Jones and Stockmayer (J. S. model). The phenyl group rotation is treated as a stochastic diffusion by the J. S. model. The restricted butterfly motion of the phenyl group attached to the cardo ring in PES-C is mentioned but is not discussed in detail in this work. Correlation times for the segmental motion are in the picosecond range which indicates the high flexibility of PES-C chains. The correlation time for the phenyl group internal rotation is similar to that of the segmental motion. The temperature dependence of these motions is weak. The apparent activation energy of the motions considered is less than 10 kJ/mol. The simulating results for PES are also reasonable considering the differences in structure compared with PES-C. The correlation times and the apparent activation energy obtained using the J. S. model for the main chain motion of PES-C are the same as those obtained using the damped orientational diffusion model and the conformational jump model.
Resumo:
Block copolymers of poly(ethersulphone) (PES) oligomers with liquid crystalline polyester units were synthesized by the reaction of dihydroxy-terminated poly(ether sulphone) oligomers (number-average molecular weights: 704, 1,158 and 2570) and terephthaloyl bis(4-oxybenzoyl chloride), and their properties were investigated. The results indicated that the copolymer with PES segments of molecular weight of 704 possessed birefringent features when annealed at 360 degrees C, while the copolymer with PES segments of molecular weight of 2,570 became isotropic. Also, the block copolymers had a better chemical resistance and high-temperature stability than PES.
Resumo:
The morphology and dynamic mechanical properties of blends of poly(ether imide) (PEI) and nylon 66 over the full composition range have been investigated. Torque changes during mixing were also measured. Lower torque values than those calculated by the log-additivity rule were obtained, resulting from the slip at the interface due to low interaction between the components. The particle size of the dispersed phase and morphology of the blends were examined by scanning electron microscopy. The composition of each phase was calculated. The blends of PEI and nylon 66 showed phase-separated structures with small spherical domains of 0.3 similar to 0.7 mu m. The glass transition temperatures (T(g)s) of the blends were shifted inward, compared with those of the homopolymers, which implied that the blends were partially miscible over a range of compositions. T-g1, corresponding to PEI-rich phase, was less affected by composition than T-g2, corresponding to nylon 66-rich phase. This indicated that the fraction of PEI mixed into nylon 66-rich phase increased with decreasing PEI content and that nylon 66 was rarely mixed into the PEI-rich phase. The effect of composition on the secondary relaxations was examined. Both T-beta, corresponding to the motion of amide groups in nylon 66, and T-gamma, corresponding to that of ether groups in PEI, were shifted to higher temperature, probably because of the formation of intermolecular interactions between the components.
Resumo:
The fracture behavior of phenolphthalein polyether-ether ketone (PEK-C) affected by physical aging at 200 degrees C was studied by tensile experiments, scanning electron microscopy, and differential scanning calorimetry observations. The ductile-brittle fracture transition (DBT) caused by physical aging can be considered as a competition between fracture mechanisms of crazing and shear yielding. The aging time required for the DBT is found to be around 400 h, based on the morphological studies and tensile experiments. The shear yielding component of the mechanical deformation could erase the aging effect, thus a deaging phenomenon occurs. We found that the deaging phenomenon has an intrinsic relationship with the extent of aging in the specimen and as a result of the fracture behavior. (C) 1995 John Wiley and Sons, Inc.
Resumo:
Blends of a new phenolphthalein poly (ether sulfone) (PES-C) and a thermotropic liquid crystalline polymer (LCP) were prepared by melt-blending in a twin-screw extruder. Rheological properties, fracture toughness, K(IC), and morphology of the blends were
Resumo:
Blends of poly(hydroxyether of phenolphthalein) (PHP) with poly(ether sulphone) (PES) were prepared by casting from a common solvent; they were found to be miscible and show a single, composition-dependent glass transition temperature. All the PHP/PES blends exhibited lower critical solution temperature behaviour, i.e. phase separation occurred at elevated temperatures. A F.T.-i.r. study revealed that a hydrogen-bonding interaction occurs between these polymers but it is weaker than in pure PHP. The observed miscibility is hence proposed to be the result of specific interactions between the polymers.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Triblock copolymers are made of monomer segments, being the central part usually hydrophobic and the outer parts hydrophilic. By varying sizes, molecular weights and monomer types of the segments one obtains different final molecules, with different physico-chemical properties, which are directly related to the performance of the final product. Looking for new products to be used, among other possibilities, in biological applications, a new polymer (Figure 1) was synthesized by the Dow Chemical and studied by Size Exclusion Chromatography, Fourier Transformed Infrared Spectrometry, Small-angle X-ray Scattering (SAXS) and its cloud point was determined by measuring light transmittance. The studies showed low molecular polydispersivety, but different polarities in the macromolecules fractions. Due to the low solubility of Diol in water, a mixture of water/butyl diglycol was used as solvent. An extensive analysis by SAXS was performed for concentrations from 50 wt% to 80 wt% of Diol in solution. Small concentrations showed very low signal to noise ratio, making it impossible to be analysed. The scattering intensity including the form factor of polydisperse non-homogeneous spheres, and the structure factor of interacting hard spheres was fitted to the curves. As the polymer concentration is high, the fitting of form factors of direct and reverse micelles were compared. The results for direct micelles were better up to 80 wt%, whereas at 90 wt% and 95 wt% the curves were better fitted by reverse micelles. It might seem odd that direct micelles are present up to such high concentrations, but it might have been caused by the presence of butyl diglycol, which increases the solubility of Diol in water. The inner and outer radius of the micelles, electron density distribution, and interaction radius of the micelles were obtained. The polydispersivety increases with Diol concentration. Besides, the interaction radius increases with solvent concentration, even when reversed micelles are present. In the last case, accompanied by an increase of inner radius (water content), as there are fewer Diol molecules to involve the water nuclei, which become larger, further apart, and in less number.
Resumo:
The Charpy impact fracture behavior of notched specimens of phenolphthalein poly(ether ketone) (PEK-C) has been studied over a range of temperature using a JJ-20 Model instrumented impact tester. For PEK-C, there exist two temperature regions which distinguish the fracture mechanism, and the brittle fracture was preferentially governed by slip or shear bands at relatively high temperatures, but by crazes at low temperatures. The temperature dependence of the ductility index (DI) shows similar peaks to the tan delta loss. (C) 1995 John Wiley and Sons, Inc.
Resumo:
The miscibility and phase behavior of poly(4-vinylphenol) (PVPh) with poly(vinyl methyl ketone) (PVMK) was investigated by differential scanning calorimetry (DSC), Fourier transform infrared spectroscopy (FTIR) and scanning electron microscopy (SEM). It was shown that all blends of PVPh/PVMK are totally miscible. A DSC study showed the apparition of a single glass transition (T-g) over their entire composition range. When the amount of PVPh exceeds 50% in blends, the obtained T(g)s are found to be significantly higher than those observed for each individual component of the mixture, indicating that these blends are capable of forming interpolymer complexes. FTIR analysis revealed the existence of preferential specific interactions via hydrogen bonding between the hydroxyl and carbonyl groups, which intensified when the amount of PVPh was increased in blends. Furthermore, the quantitative FTIR study carried out for PVPh/PVMK blends was also performed for the vinylphenol (VPh) and vinyl methyl ketone (VMK) functional groups. These results were also established by scanning electron microscopy study (SEM).
Resumo:
Miscibility, crystallization, and mechanical properties of blends of thermosetting polyimide PMR-15 and phenolphthalein poly(ether ketone) (PEK-C) were examined. With the exception of the 90/10 blend, which has two glass transition peaks, all the blends with PMR-15 less than 90 wt % are miscible in the amorphous state according to DMA results. Addition of PEK-C hindered significantly the crystallization of PMR-15, indicating that there must exist some kind of interaction between molecular chains of PMR-15 and those of PEK-C. The semi-IPN system of PMR-15/PEK-C blends exhibits good toughness. Two distinct microphases, interweaving at the phase boundaries, were found in the PMR-15/PEK-C 60/40 blend. The toughness effect of the blends is discussed in terms of the interface adhesion between the two distinct phases and the domain sizes of the phases. The relation between miscibility and toughness of the blends was investigated. (C) 1996 John Wiley & Sons, Inc.