261 resultados para Eutectic
Resumo:
A high toughness wear resistant coating is produced by laser clad Fe-Cr-W-Ni-C alloys. The microstructural and compositional features of the laser-solidified microstructures and phase evolutions occurring during high temperature tempering at 963 K were investigated by using analytical electron microscopy with energy dispersive X-ray analysis. The clad coating possesses the hypereutectic microstructure consisted of M7C3 + (Y + M7C3) Du ring high temperature aging, the precipitation of M23C6 and M2C in austenite and in situ transformation of dendritic M7C3 to M23C6 and eutectic M7C3 to M6C occurred. The laser clad coating reveals an evident secondary hardening and superior impact wear resistance.
Resumo:
Glass transition and crystallization process of bulk Nd60Al10Fe20Co10 metallic glass were investigated by means of dynamic mechanical thermal analysis (DMTA), differential scanning calorimetry (DSC), X-ray diffraction (XRD) and scanning electronic microscopy (SEM). It is shown that the glass transition and onset crystallization temperature determined by DMTA at a heating rate of 0.167 K/s are 480 and 588 K respectively. The crystallization process of the metallic glass is concluded as follows: amorphous alpha-->alpha' + metastable FeNdAl novel phase -->alpha' + primary delta phase-->primary delta phase + eutectic delta phase Nd3Al phase + Nd3Co phase. The appearance of hard magnetism in this alloy is ascribed to the presence of amorphous phase with highly relaxed structure. The hard magnetism disappeared after the eutectic crystallization of amorphous phase.
Resumo:
Minor yttrium addition can improve the glass-forming ability of Cu-Zr-Al ternary alloys via suppression of the growth of eutectic clusters. Yttrium addition also makes the room temperature ductility of the alloys decrease, and both the compressive strength and elastic strain limits increase slightly.
Resumo:
Lattice-resolved, video-rate environmental transmission electron microscopy shows the formation of a liquid Au-Ge layer on sub-30-nm Au catalyst crystals and the transition of this two-phase Au-Ge/Au coexistence to a completely liquid Au-Ge droplet during isothermal digermane exposure at temperatures far below the bulk Au-Ge eutectic temperature. Upon Ge crystal nucleation and subsequent Ge nanowire growth, the catalyst either recrystallizes or remains liquid, apparently stabilized by the Ge supersaturation. We argue that there is a large energy barrier to nucleate diamond-cubic Ge, but not to nucleate the Au-Ge liquid. As a result, the system follows the more kinetically accessible path, forming a liquid even at 240 degrees C, although there is no liquid along the most thermodynamically favorable path below 360 degrees C.
Resumo:
采用玻璃包覆的方法获得具有较大过冷度的亚共晶、共晶以及过共晶Ag-Ge合金熔体,并通过高能离子束轰击Cu箔产生Cu原子团簇溅射到过冷合金熔体中来触发非均质形核过程.凝固后合金显微组织的分析结果表明:在深过冷合金熔体中引入Cu原子团簇,它对亚共晶、共晶以及过共晶Ag-Ge合金的显微组织演变有着不同的影响效果,分析了显微组织的演变规律与形成机制. The Ag-Ge alloy melts with deeply undercooled hypoeutectic, eutectic and hypereutectic were obtained via glass fluxing technique. The nucleation of the deeply undercooled alloy melts were triggered by atoms cluster sputtering on the surface of the melts. The atoms clusters were generated by an ion beam bombarding on the Cu foil fixed above the alloy melts. The resultant microstructure reveals that the induced atom clusters exert great influence on the microstructural evolution of the highly undercooled eutectic and hypereutectic Ag-Ge alloys, but no obvious influence on the highly undercooled hypoeutectic alloy. The microstructural evolution and formation mechanism were analyzed and discussed.
Resumo:
The feasibility of the fabrication of coatings for elevated-temperature structural applications by laser cladding MoSi2 powder on steel was investigated. A dense and crack-free fine coating, well-bonded with the substrate has been obtained by this technique. This coating consists of FeMoSi, Fe2Si and a small amount of Mo5Si3 due to dilution of the substrate in the coating. The microstruelure of the coating is characterized of typical fine dendrites. The dendrites are composed of FeMoSi primary phase, and the interdendritic areas are two eutectic phases of FeMoSi and Fe2Si. The hardness of the coating reaches 845 Hv(0.5), 3.7 times larger than that of the steel substrate (180Hv(0.5)).
Resumo:
In order to improve the wear resistance of the gamma-TiAl intermetallic alloy, microstructure, room- and high-temperature (600 degrees C) wear behaviors of laser clad gamma/Cr7C3/TiC composite coatings with different constitution of NiCr-Cr3C2 precursor-mixed powders have been investigated by optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), energy-dispersive spectrometer (EDS), block-on-ring (room-temperature) and pin-on-disk (high-temperature) wear tests. The responding wear mechanisms are discussed in detail. Results show that microstructures of the laser clad composite coatings have non-equilibrium solidified microstructures consisting of primary hard Cr7C3 and TiC carbides and the inter-primary gamma/Cr7C3 eutectic matrix, about three to five times higher average microhardness compared with the TiAl alloy substrate. Higher wear resistance than the original TiAl alloy is achieved in the clad composite coatings under dry sliding wear conditions, which is closely related to the formation of non-equilibrium solidified reinforced Cr7C3 and TiC carbides and the positive contribution of the relatively ductile and tough gamma/Cr7C3 eutectics matrix and their stability under high-temperature exposure.
Resumo:
Glass transition and thermal stability of bulk Nd60Al10Fe20Co10 metallic glass were investigated by means of dynamic mechanical thermal analysis (DMTA), differential scanning calorimetry (DSC), X-ray diffraction (XRD) and scanning electronic microscopy (SEM). The glass transition temperature, not revealed by DSC, is alternatively determined by DMTA via storage modulus E' and loss modulus E" measurement to be 498 K at a heating rate of 0.167 K s (-1). The calculated reduced glass transition temperature (T-g/T-m) is 0.63. The large value of T-g/T-m of this alloy is consistent with its good glass-forming ability. The crystallization process of the metallic glass is concluded as follows: amorphous --> amorphous + metastable FeNdAl phase --> amorphous + primary delta-FeNdAl phase --> primary delta-phase + eutectic delta-phase + Nd3Al + Nd3Co. The appearance of hard magnetism in this alloy is ascribed to the presence of amorphous phase with highly relaxed structure. The hard magnetism disappeared after the eutectic crystallization of the amorphous phase. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
The microstructural and compositional features of the laser-solidified microstructures and phase evolutions occurring during high temperature tempering were investigated by using analytical electron microscopy with energy dispersive X-ray analysis. The cladded alloy, a powder mixture of Fe, Cr, W, Ni and C with a weight ratio of 10:5:1:1:1, was processed with a 3 kW continuous wave CO2 laser. The cladded coating possessed the hypoeutectic microstructure of the primary dendritic gamma-austenite and interdendritic eutectic consisting of (gamma+M7C3). The gamma-austenite is a nonequilibrium phase with extended solid solution of alloying elements. And, a great deal of fine structures, i.e., a high density of dislocations, twins, and stacking faults existed in austenite phase. During high temperature aging, the precipitation of M23C6, MC and M2C in austenite and in situ transformation of M7C3(+gamma) --> M23C6 and M7C3+gamma --> M6C occurred. The laser clad coating revealed an evident secondary hardening and superior impact wear resistance.
Resumo:
The rapidly solidified microstructural and compositional features, the precipitation and transformation of carbides during tempering, and the impact wear resistance of an iron-based alloy coating prepared by laser cladding are investigated. The clad coating alloy, a powder mixture of Fe, Cr, W, Ni, and C with a weight ratio of 10:5:1.1.1, is processed using a continuous wave CO, laser. Microstructural studies demonstrate that the coating possesses the hypoeutectic microstructure comprising the primary dendritic gamma-austenite and interdendritic eutectic consisting of gamma-austenite and M7C3 carbides. gamma-Austenite is a non-equilibrium phase with an extended solid solution of alloying elements. During high temperature tempering at 963 K for 1 h, the precipitation of M23C6, MC and M2C carbides in austenite and in situ carbide transformation of M7C3 to M23C6 and M7C3 to M6C respectively are observed. In addition, the microstructure of the laser-clad coating reveals an evident secondary hardening and a superior impact wear resistance.
Resumo:
Isotopic fractionation due to sputtering has been investigated via a collector type experiment in which targets of known isotopic composition have been bombarded with several keV Ar+ and Xe+ ions with fluences down to 3.0x1014 ions/cm2 , believed to be the lowest fluences for which such detailed measurements have ever been made. The isotopes were sputtered onto carbon collectors and analyzed with Secondary Ion Mass Spectroscopy (SIMS.) There is clear indication of preferential effects several times that predicted by the dominant analytical theory. Results also show a fairly strong angular variation in the fractionation. The maximum effect is usually seen in the near normal direction, measured from the target surface, falling continuously, by a few percent in some cases, to a minimum in the oblique direction. Measurements have been made using Mo isotopes: 100Mo and 92Mo and a liquid metal system of In:Ga eutectic. The light isotope of Mo is found to suffer a 53 ± 5‰ (note: 1.0‰ ≡ 0.1%) enrichment in the sputtered flux in the near normal direction, compared to the steady state near normal sputtered composition, under 5.0 keV Xe+ bombardment of 3.0 x 1014 ions/cm2. In the liquid metal study only the angular dependence of the fractionation could be measured due to the lack of a well defined reference and the nature of the liquid surface, which is able to 'repair' itself during the course of a bombardment. The results show that 113In is preferentially sputtered over 115In in the near normal direction by about 8.7 ± 2.7‰ compared to the oblique direction. 69Ga, on the other hand, is sputtered preferentially over 71Ga in the oblique direction by about 13 ± 4.4‰ with respect to the near normal direction.
Resumo:
超分辨近场结构(super-RENS)技术通过在传统光盘结构中插入掩膜结构而实现近场超分辨,是目前最具实用化前景的超高密度光存储技术之一,其中掩膜层的近场光学特性是决定其光存储性能的关键。利用三维时域有限差分法(3D-FDTD)对合金掩膜的近场光强分布进行了数值仿真和分析,提出二元共晶合金薄膜在激光作用下形成的规则微结构可能是以其作为掩膜层的超分辨近场结构光盘产生较高信噪比(SNR)的原因。
Resumo:
A novel pair of the E- and Z-isomeric 1R,4R-2-(4-heptyloxyphenyl)-benzylidene-p-menthan-3-ones has been prepared and the influence of distinctions in their molecular geometry on macroscopic properties of liquid crystal systems with the induced supra-molecular helical structure has been studied. The significantly lower helical twisting power of the chiral Z-isomer in comparison with that of E- one has been confirmed in the case of induced cholesteric systems based on 4-pentyl-4-cyanobiphenyl. The phase behavior and ferroelectric characteristics have been investigated for smectic-C* compositions based on the eutectic mixture of the homological 4-hexyloxyphenyl-4'-hexyloxy- and 4-hexyloxyphenyl-4'-octyloxybenzoates containing the novel isomeric chiral dopants. The spontaneous polarisation of the opposite signs induced by the isomeric chiral components has been revealed for the compositions studied. Distinctions in phase states, absolute values of the spontaneous polarization, smectic tilt angle and rotation viscosity of the systems obtained are discussed.
Resumo:
Some 1R,4R-2-(4-phenylbenzylidene)-p-menthane-3-one derivatives containing the ether or ester linking group between benzene rings of the arylidene fragment have been studied as chiral dopants in ferroelectric liquid crystal systems based on the eutectic mixture (1:1) of two phenylbenzoate derivatives CmH2m+1OC6H4COOC6 H4OCnH2n+1 (n = 6; m = 8, 10). The ferroelectric properties of these compositions (spontaneous polarization, rotation viscosity, smectic tilt angle as well as quantitative characteristics of their concentration dependences) were compared with those for systems including chiral dopants containing no linking group. Ferroelectric parameters of the induced ferroelectric compositions studied have been shown to depend essentially on the presence of the linking group between benzene rings and its nature as well as on the number of the benzene rings in the rigid molecular core of the chiral dopants used. For all ferroelectric liquid crystal systems studied, the influence of the chiral dopants on the thermal stability of N*, SmA and SmC* mesophases has been quantified. The influence of the linking group nature in the dopant molecules on the characteristics of the systems studied is discussed taking into account results of the conformational analysis carried out by the semi-empirical AM1 and PM3 methods.
Resumo:
Taper-free and vertically oriented Ge nanowires were grown on Si (111) substrates by chemical vapor deposition with Au nanoparticle catalysts. To achieve vertical nanowire growth on the highly lattice mismatched Si substrate, a thin Ge buffer layer was first deposited, and to achieve taper-free nanowire growth, a two-temperature process was employed. The two-temperature process consisted of a brief initial base growth step at high temperature followed by prolonged growth at lower temperature. Taper-free and defect-free Ge nanowires grew successfully even at 270 °C, which is 90 °C lower than the bulk eutectic temperature. The yield of vertical and taper-free nanowires is over 90%, comparable to that of vertical but tapered nanowires grown by the conventional one-temperature process. This method is of practical importance and can be reliably used to develop novel nanowire-based devices on relatively cheap Si substrates. Additionally, we observed that the activation energy of Ge nanowire growth by the two-temperature process is dependent on Au nanoparticle size. The low activation energy (∼5 kcal/mol) for 30 and 50 nm diameter Au nanoparticles suggests that the decomposition of gaseous species on the catalytic Au surface is a rate-limiting step. A higher activation energy (∼14 kcal/mol) was determined for 100 nm diameter Au nanoparticles which suggests that larger Au nanoparticles are partially solidified and that growth kinetics become the rate-limiting step. © 2011 American Chemical Society.