974 resultados para Copper Aluminum Silver Alloys


Relevância:

30.00% 30.00%

Publicador:

Resumo:

The use of high-strength aluminium alloys as material for injection molding tools to produce small and medium batches of plastic products as well as prototyping molds is becoming of increasing demand by the tooling industry. These alloys are replacing the traditional use of steel in the cases above because they offer many advantages such as very high thermal conductivity associated with good corrosion and wear resistance presenting good machinability in milling and electrical discharge machining operations. Unfortunately there is little technological knowledge on the Electrical Discharge Machining (EDM) of high-strength aluminium alloys, especially about the AMP 8000 alloy. The duty factor, which means the ratio between pulse duration and pulse cycle time exerts an important role on the performance of EDM. This work has carried out an experimental study on the variation of the duty factor in order to analyze its influence on material removal rate and volumetric relative wear under roughing conditions of EDM process. The results showed that high values of duty factor are possible to be applied without bringing instability into the EDM process and with improvement of material removal rate and volumetric relative wear.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nanoporous materials with large surface area and well-ordered pore structure have been synthesized. Thiol groups were grafted on the materials' surface to make heavy metal ion pre-concentration media. The adsorption properties ofthe materials were explored. Mercury, gold and silver can be strongly adsorbed by these materials, even in the presence of alkaline earth metal ion. Though the materials can adsorb other heavy metal ions such as lead and copper, they show differential adsorption ability when several ions are present in solution. The adsorption sequence is: mercury> == silver> copper » lead and cadmium. In the second part of this work, the memory effects of mercury, gold, silver and boron were investigated. The addition of 2% L-cysteine and 1% thiourea eliminates the problems of the three metal ions completely. The wash-out time for mercury dropped from more than 20 minutes to 18 seconds, and the wash-out time for gold decreased from more than 30 minutes to 49 seconds. The memory effect of boron can be reduced by the use of mannitol.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Ce mémoire prend la forme d’une réflexion critique sur le modèle proposé par Hosler afin d’expliquer les taux quantifiés d’étain et d’arsénique dans des objets de statut métalliques Mésoaméricains provenant principalement de l’Occident mésoaméricain et couvrant les deux phases de développement de la métallurgie mésoaméricaine. Ces objets font partie de la collection du Museo Regional de Guadalajara. Plus particulièrement, ce mémoire s’intéresse aux grelots mésoaméricains puisqu’ils représentent un élément important de la métallurgie préhispanique en Mésoamérique. Cette réflexion critique soulève plusieurs considérations techniques, méthodologiques, étymologiques, iconographiques, ethnohistoriques et logiques du modèle de Hosler relativement à la couleur des alliages constituant les grelots mésoaméricains. Les paramètres sur lesquels Hosler base son modèle sont questionnables à plusieurs niveaux. Ainsi, le fait que les niveaux d’arsenic ou d’étain observés dans les alliages cupriques de biens utilitaires sont généralement inférieurs à ceux quantifiés dans les alliages cupriques usités pour la fabrication de biens de statut de la Période 2 pourrait s’expliquer par le fait qu’il s’agit de deux méthodes de fabrication distinctes ayant des contraintes techniques différentes ou que ces artéfacts ont des paramètres et des fonctions distinctes. Les limites de l’association soleil-or, lune-argent y sont également exposées et un chapitre est consacré à la sonorité.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Laser-induced plasma generated from a silver target under partial vacuum conditions using the fundamental output of nanosecond duration from a pulsed Nd:yttrium aluminum garnet laser is studied using a Langmuir probe. The time of flight measurements show a clear twin peak distribution in the temporal profile of electron emission. The first peak has almost the same duration as the laser pulse while the second lasts for several microseconds. The prompt electrons are energetic enough ('60 eV) to ionize the ambient gas molecules or atoms. The use of prompt electron pulses as sources for electron impact excitation is demonstrated by taking nitrogen, carbon dioxide, and argon as ambient gases.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The metastable phase diagram of the BCC-based ordering equilibria in the Fe-Al-Mo system has been calculated via a truncated cluster expansion, through the combination of Full-Potential-Linear augmented Plane Wave (FP-LAPW) electronic structure calculations and of Cluster Variation Method (CVM) thermodynamic calculations in the irregular tetrahedron approximation. Four isothermal sections at 1750 K, 2000 K, 2250 K and 2500 K are calculated and correlated with recently published experimental data on the system. The results confirm that the critical temperature for the order-disorder equilibrium between Fe(3)Al-D0(3) and FeAl-B2 is increased by Mo additions, while the critical temperature for the FeAl-B2/A2 equilibrium is kept approximately invariant with increasing Mo contents. The stabilization of the Al-rich A2 phase in equilibrium with overstoichiometric B2-(Fe,Mo)Al is also consistent with the attribution of the A2 structure to the tau(2) phase, stable at high temperatures in overstoichiometric B2-FeAl. (C) 2009 Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The coordination chemistry of the ligand N-thiazol-2-yl-toluenesulfonamidate towards the copper(II) ion has been investigated using an electrochemical synthesis method. The X-ray structure of this complex was elucidated and is discussed. The compound crystallised in the monoclinic crystal system, P2(1)/c space group with a = 17.3888(9), b = 16.3003(9), c = 18.3679(9) angstrom and beta = 114.3640(10)degrees. Four bidentate sulfathiazolato anions bridge two metal centers in a paddle-wheel fashion, with the nitrogen atoms as donors to give a dimeric species with a Cu center dot center dot center dot Cu distance of 2.7859(5) angstrom.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Carbon dioxide electroreduction on copper electrode was studied by surface enhanced Raman scattering (SERS) in K(2)SO(4) aqueous solutions with different pH values. CO(2) was bubbled into the solution at 0 V vs. Ag/AgCl, i.e., on an oxidized copper surface. In acidic solutions (pH around 2.5), at -0.2 V, bands indicative of the presence of ethylene on the electrode surface were detected. Although ethylene is knowledgably a product of CO(2) electroreduction on copper, it was not experimentally identified on the electrode`s surface at such a low cathodic potential in prior works. In solutions with pH around 2.5, CO bands were not observed, suggesting that hydrocarbons could be formed by a pathway that does not occur via adsorbed CO. In solutions with higher pHs, a complex spectral pattern, between 800 and 1700 cm(-1), was observed at approximately -0.4 V. The observed spectrum closely resembles those reported in the literature for adsorption of monocarboxylic acids with small chains. The spectral features indicate the presence of a structure containing a double C=C bond. a carboxyl group, and C-H bonds on the electrode`s surface. SERS spectra obtained in CO-saturated solution are also presented. However, in this case, no SERS bands were observed in the region between 800 and 1700 cm(-1) at low cathodic potentials. (c) 2009 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The nature of the protective film formed by benzotriazole (BTAH) on the surface of the 90/10 CuNi alloy in deaerated 0.5 mol L-1 H2SO4 solution containing Fe(III) ions as oxidant was investigated by weight-loss, calorimetric measurements, and by surface-enhanced Raman spectroscopy (SERS). The SERS measurements show that the protective film is composed by the [Cu(I)BTA](n), polymeric complex and that the BTAH molecules are also adsorbed on the electrode surface. A modification of the BET isotherm for adsorption of gases ill solids is proposed to describe the experimental results obtained from weight-loss experiments that suggest an adsorption in multilayers. Electrochemical studies of copper and nickel in 0.5 mol L-1 H2SO4 in presence and absence of BTAH have also been made as an aid to interpret the results. The calculated adsorption free energy of the cuprous benzotriazolate on the surface of the alloy is in accordance with the value for pure copper. (C) 2007 Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The thermal behavior of the Cu-10 mass%Al and Cu-10 mass% Al-4 mass%Ag alloys was studied using classical differential thermal analysis (DTA), optical microscopy (OM) and X-ray diffractometry (XRD). The DTA curves were obtained for annealed and quenched samples. The results indicated that the presence of silver introduces new thermal events, associated to the formation of a silver-rich phase, to the shift of the equilibrium concentration to higher A1 contents and to the decomposition of the silver-rich phase in the same temperature range of the beta(1) phase decomposition.