822 resultados para Composite cement slurries
Resumo:
STUDY DESIGN: The biomechanics of vertebral bodies augmented with real distributions of cement were investigated using nonlinear finite element (FE) analysis. OBJECTIVES: To compare stiffness, strength, and stress transfer of augmented versus nonaugmented osteoporotic vertebral bodies under compressive loading. Specifically, to examine how cement distribution, volume, and compliance affect these biomechanical variables. SUMMARY OF BACKGROUND DATA: Previous FE studies suggested that vertebroplasty might alter vertebral stress transfer, leading to adjacent vertebral failure. However, no FE study so far accounted for real cement distributions and bone damage accumulation. METHODS: Twelve vertebral bodies scanned with high-resolution pQCT and tested in compression were augmented with various volumes of cements and scanned again. Nonaugmented and augmented pQCT datasets were converted to FE models, with bone properties modeled with an elastic, plastic and damage constitutive law that was previously calibrated for the nonaugmented models. The cement-bone composite was modeled with a rule of mixture. The nonaugmented and augmented FE models were subjected to compression and their stiffness, strength, and stress map calculated for different cement compliances. RESULTS: Cement distribution dominated the stiffening and strengthening effects of augmentation. Models with cement connecting either the superior or inferior endplate (S/I fillings) were only up to 2 times stiffer than the nonaugmented models with minimal strengthening, whereas those with cement connecting both endplates (S + I fillings) were 1 to 8 times stiffer and 1 to 12 times stronger. Stress increases above and below the cement, which was higher for the S + I cases and was significantly reduced by increasing cement compliance. CONCLUSION: The developed FE approach, which accounts for real cement distributions and bone damage accumulation, provides a refined insight into the mechanics of augmented vertebral bodies. In particular, augmentation with compliant cement bridging both endplates would reduce stress transfer while providing sufficient strengthening.
Resumo:
PURPOSE To determine the best-performing combination of three core buildup materials and three bonding materials based on their bond strength to ceramic blocks in vitro. MATERIALS AND METHODS The materials used for core buildup were a composite (Tetric EvoCeram), a compomer (Compoglass F), and a glass-ionomer cement (Ketac Fil Plus), and for bonding, a three-step etch-and-rinse adhesive (Syntac), a two-step etch-and-rinse adhesive (ExciTE), and a single-step system (RelyX Unicem). Bond strength to ceramic blocks was determined by shear bond strength testing. Fracture behavior was evaluated by scanning electron microscopy. RESULTS The highest adhesive values between buildup and ceramic were obtained using the materials Compoglass F and Syntac, followed by Compoglass F and ExciTE. Among the two other core buildups, Tetric EvoCeram performed better than Ketac Fil Plus, which was independent of the bonding materials. Adhesive fractures were characteristically observed with Syntac and ExciTE, and cohesive fractures were characteristically observed with RelyX Unicem. CONCLUSION These data show that compomers bonded with a multistep adhesive system achieved statistically significantly higher shear bond strength than composites and glass-ionomer cements. Within the limitations inherent to this in vitro study, the use of compomers for core buildup can be recommended.
Resumo:
GRC is a cementitious composite material made up of a cement mortar matrix and chopped glass fibers. Due to its outstanding mechanical properties, GRC has been widely used to produce cladding panels and some civil engineering elements. Impact failure of cladding panels made of GRC may occur during production if some tool falls onto the panel, due to stone or other objects impacting at low velocities or caused by debris projected after a blast. Impact failure of a front panel of a building may have not only an important economic value but also human lives may be at risk if broken pieces of the panel fall from the building to the pavement. Therefore, knowing GRC impact strength is necessary to prevent economic costs and putting human lives at risk. One-stage light gas gun is an impact test machine capable of testing different materials subjected to impact loads. An experimental program was carried out, testing GRC samples of five different formulations, commonly used in building industry. Steel spheres were shot at different velocities on square GRC samples. The residual velocity of the projectiles was obtained both using a high speed camera with multiframe exposure and measuring the projectile’s penetration depth in molding clay blocks. Tests were performed on young and artificially aged GRC samples to compare GRC’s behavior when subjected to high strain rates. Numerical simulations using a hydrocode were made to analyze which parameters are most important during an impact event. GRC impact strength was obtained from test results. Also, GRC’s embrittlement, caused by GRC aging, has no influence on GRC impact behavior due to the small size of the projectile. Also, glass fibers used in GRC production only maintain GRC panels’ integrity but have no influence on GRC’s impact strength. Numerical models have reproduced accurately impact tests.
Resumo:
La presente tesis doctoral aborda el estudio de un nuevo material mineral, compuesto principalmente por una matriz de yeso (proveniente de un conglomerante industrial basado en sulfato de calcio multifase) y partículas de aerogel de sílice hidrófugo mesoporoso, compatibilizadas mediante un surfactante polimérico, debido a su alto carácter hidrófugo. La investigación se centra en conocer los factores que influyen en las propiedades mecánicas y conductividad térmica del material compuesto generado. Este estudio pretende contribuir al conocimiento sobre el desarrollo de nuevos morteros de elevado aislamiento térmico que puedan ser utilizados en la rehabilitación energética de edificios de viviendas existentes, debido a que estos representan gran parte del consumo energético del parque de viviendas de España, aunque también a nivel internacional. De los materiales utilizados para desarrollar los morteros estudiados, el yeso, además de ser un material muy abundante, especialmente en España, requiere una menor cantidad de energía para la fabricación de un conglomerante (debido a una menor temperatura de fabricación), en comparación con el cemento o la cal, por lo que presenta una menor huella de carbono que estos últimos. Por otro lado, el aerogel de sílice hidrófugo mesoporoso es, de acuerdo con la documentación disponible, el material que posee actualmente la mayor capacidad de aislamiento térmico en el mercado. El desarrollo de nuevos morteros minerales con una capacidad de aislamiento térmico mayor que los materiales aislantes utilizados tradicionalmente, tiene una aplicación relevante en los casos de rehabilitación energética de edificios históricos y patrimoniales, en los que se requiere la aplicación del aislamiento por el interior de la fachada, ya que este tipo de soluciones tienen el inconveniente de reducir el espacio habitable de las áreas involucradas, especialmente en zonas climáticas en las que el aislamiento térmico puede suponer un espesor considerable, por lo que es ideal utilizar materiales de altas prestaciones de aislamiento térmico capaces de aportar el mismo nivel de aislamiento (o incluso mayor), pero en un espesor considerablemente menor. La investigación se desarrolla en tres etapas: bibliográfica, experimental y de simulación. La primera etapa, parte del estudio de la bibliografía existente, relacionada con materiales aislantes, incluyendo soluciones basadas, tanto en morteros aislantes, como en paneles de aislamiento térmico. La segunda, de carácter experimental, se centra en estudiar la influencia de la microestrucrura y macroestructura, del nuevo material mineral, en las propiedades físicas elementales, mecánicas y conductividad térmica del compuesto. La tercera etapa, mediante una simulación del consumo energético, consiste en cuantificar teóricamente el potencial ahorro energético que puede aportar este material en un caso de rehabilitación energética en particular. La investigación experimental se centró principalmente en conocer los factores principales que influyen en las propiedades mecánicas y conductividad térmica de los materiales compuestos minerales desarrollados en esta tesis. Para ello, se llevó a cabo una caracterización de los materiales de estudio, así como el desarrollo de distintas muestras de ensayo, de tal forma que se pudo estudiar, tanto la hidratación del yeso en los compuestos, como su posterior microestructura y macroestructura, aspectos fundamentales para el entendimiento de las propiedades mecánicas y conductividad térmica del compuesto aislante. De este modo, se pudieron conocer y cuantificar, los factores que influyen en las propiedades estudiadas, aportando una base de conocimiento y entendimiento de este tipo de compuestos minerales con aerogel de sílice hidrófugo, no existiendo estudios publicados hasta el momento de finalización de esta tesis, con la aproximación al material propuesta en este estudio, ni con yeso (basado en sulfato de calcio multifase), ni con otro tipo de conglomerantes. Particularmente, se determinó la influencia que tiene la incorporación de partículas de aerogel de sílice hidrófugo, en grandes proporciones en volumen, en un compuesto mineral basado en distintas fases de sulfato de calcio. No obstante, para llevar a cabo las mezclas, fue necesario utilizar un surfactante para compatibilizar este tipo de partículas, con el conglomerante basado en agua. El uso de este tipo de aditivos tiene una influencia, no solo en el aerogel, sino en las propiedades del compuesto en general, dependiendo de su concentración, por lo que se establecieron dos porcentajes de adición: la primera, determinada a partir de la cantidad mínima necesaria para compatibilizar las mezclas (0,1% del agua de amasado), y la segunda, como límite superior, la concentración utilizada habitualmente a nivel industrial para estabilizar burbujas de aire en hormigones espumados (5%). El surfactante utilizado mostró la capacidad de modificar la superficie del aerogel, cambiando el comportamiento de las partículas frente al agua, permitiendo una invasión parcial de su estructura porosa, por parte del agua de amasado. Este comportamiento supone un aumento muy importante en la relación agua/yeso, afectando el hábito cristalino e influenciando negativamente las propiedades mecánicas de la matriz de yeso, presentando un efecto aún notable a mayor concentración de surfactante (5%). En cuanto a las propiedades finales alcanzadas, fue posible lograr un compuesto mineral ultraligero (200 kg/m3), con alrededor de un 60% de aerogel en volumen y de alta capacidad aislante (0,028 W/m•K), presentando una conductividad térmica notablemente menor que los morteros aislantes del mercado, e incluso también menor que la de los aislantes tradicionales basado en las lanas minerales o EPS; no obstante, con la limitante de presentar bajas propiedades mecánicas, condicionando su posible aplicación futura. Entre los factores principales relacionados con las propiedades mecánicas, se encontró que estas dependen exponencialmente del volumen de yeso en el compuesto; no obstante, factores de segundo orden, como el grado de hidratación, o una mejor distribución del conglomerante entre las partículas de aerogel, debido al aumento de la superficie específica del polvo mineral, pueden aumentar las propiedades mecánicas entre el doble y el triple, dependiendo del volumen de aerogel en cuestión. Además, se encontró que el aerogel, en conjunto con el surfactante, es capaz de introducir una gran cantidad de aire (0,70 m3 por cada m3 de aerogel), que unido al agua evaporada (no consumida por el conglomerante durante la hidratación), el volumen de aire total alcanza, generalmente, un 40%, independientemente de la cantidad de aerogel en la mezcla. De este modo, el aire introducido en la matriz desplaza las proporciones en volumen del aerogel y del yeso, disminuyendo, tanto las propiedades mecánicas, como la capacidad aislante de compuesto mineral. Por otro lado, la conductividad térmica mostró tener una dependencia directa de la contribución de las tres fases principales en el compuesto: yeso, aerogel y aire ocluido. De este modo, se pudo desarrollar un modelo matemático, adaptado de uno existente, capaz de calcular, con bastante precisión, la relación de los tres componentes mencionados, en la conductividad térmica de los compuestos, para el rango de volúmenes y materiales utilizados en esta tesis. Finalmente, la simulación del consumo energético realizada a una vivienda típica de España, de los años 1900 a 1959 (basada en muros de ladrillo macizo), para las zonas climáticas estudiadas (A, D y E), permitió observar el potencial ahorro energético que puede aportar este material, dependiendo de su espesor, como aislamiento interior de los muros de fachada. Particularmente, para la zona A, se determinó un espesor óptimo de 1 cm, mientras que para la zona D y E, 3,5 y 3,9 cm respectivamente. En este sentido, el nuevo material estudiado es capaz de disminuir, entre un 35% y un 80%, el espesor de la capa aislante, en comparación con paneles de lana de roca o los morteros minerales de mayor capacidad aislante del mercado español respectivamente. ABSTRACT The present doctoral thesis studies a new mineral-based composite material, composed by a gypsum matrix (based on an industrial multiphase gypsum binder) and mesoporous hydrophobic silica aerogel particles, compatibilized with a polymeric surfactant due to the high hydrophobic character of the insulating particles. This study pretends to contribute to the development of new composite insulating materials that could be used in energy renovation of existing dwellings, in order to reduce their high energy consumption, as they represent a great part of the total energy consumed in Spain, but also internationally. Between the materials used to develop de studied insulating mortars, gypsum, besides being an abundant material, especially in Spain, requires less energy for the manufacture of a mineral binder (due to lower manufacturing temperatures), compared to lime or cement, thus presenting lower carbon footprint. In other hand, the hydrophobic mesoporous silica aerogel, is, according to the existing references, the material with the highest know insulating capacity in the market. The development of new mineral mortars with higher thermal insulation capacity than traditional insulating materials, presents a relevant application in energy retrofitting of historic and cultural heritage buildings, in which implies that the insulating material should be installed as an internal layer, rather than as an external insulating system. This type of solution involves a reduced internal useful area, especially in climatic zones where the demand for thermal insulation is higher, and so the insulating layer thickness, being idealistic to use materials with very high insulating properties, in order to reach same insulating level (or higher), but in lower thickness than the provided by traditional insulating materials. This research is developed in three main stages: bibliographic, experimental and simulation. The first stage starts by studying the existing references regarding thermally insulating materials, including existing insulating mortars and insulating panels. The second stage, mainly experimental, is centered in the study of the the influence of the microstructure and macrostructure in the physical and mechanical properties, and also in the thermal conductivity of the new mineral-based material. The thirds stage, through energy simulation, consists in theoretically quantifying the energy savings potential that can provide this type of insulating material, in a particular energy retrofitting case study. The experimental research is mainly focused in the study of the factors that influence the mechanical properties and the thermal conductivity of the thermal insulating mineral composites developed in this thesis. For this, the characterization of the studied materials has been performed, as well as the development of several experimental samples, in order to study the hydration of the mineral binder within the composites, but also the final microstructure and macrostructure, fundamental aspects for the understanding of the composite’s mechanical and insulating properties. Thus, is was possible to determine and quantify the factors that influence the studied material properties, providing a knowledge base and understanding of mineral composites that comprises mesoporous hydrophobic silica aerogel particles, being the first study up to date regarding the specific approach of the present study, regarding not just multiphase calcium sulfate plaster, but also other mineral binders. Particularly, the influence of the incorporation of hydrophobic silica aerogel particles, in high volume ratios into a mineral compound, based on different phases of calcium sulfate has been determined. However, to perform mixing, it is necessary to use a surfactant in order to compatibilize these particles with the water-based mineral binder. The use of such additives has an influence, not only in the aerogel, but the overall properties of the compound, so two different surfactant concentration has been studied: the first, the minimum amount of surfactant (used in this thesis) in order to develop the slurries (0.1% concentration of the mixing water), and the second, as the upper limit, the concentration usually used industrially to stabilize air bubbles in foamed concrete (5%). One of the side effects of using such additive, was the modification of the aerogel particles, by changing their behavior in respect to water, generating a partial invasion of the aerogel’s porous structure, by the mixing water. This behavior produces a very important increase in water/binder ratios, affecting the crystal habit and negatively influencing the mechanical properties of the gypsum matrix. This effect further increased when a higher concentration of surfactant (5%) is used. Regarding final materials properties, it was possible to achieve an ultra-lightweight mineral composite (200 kg/m3), with around 60% by volume of aerogel, presenting a very high insulating capacity (0.028 W/m•K), a noticeable lower thermal conductivity compared to the insulating mortars and traditional thermal insulating panels on the market, such as mineral wool or EPS; however, the limiting factor for future’s material application in buildings, is related to the very low mechanical properties achieved. Among the main factors related to the mechanical properties, it has been found an exponential correlation to the volume of gypsum in the composite. However, second-order factors such as the degree of hydration, or a better distribution of the binder between the aerogel particles, due to the increased surface area of the mineral powder, can increase the mechanical properties between two to three times, depending aerogel volume involved. In addition, it was found that the aerogel, together with the surfactant, is able to entrain a large amount of air volume (around 0.70 m3 per m3 of aerogel), which together with the evaporated water (not consumed by the binder during hydration), can reach generally around 40% of entrained air within the gypsum matrix, regardless of the amount of aerogel in the mixture. Thus, the entrained air into the matrix displaces the volume proportions of the aerogel and gypsum, reducing both mechanical and insulating properties of the mineral composite. On the other hand, it has been observed a direct contribution of three main phases into the thermal conductivity of the composite: gypsum, aerogel and entrained air. Thus, it was possible to develop a mathematical model (adapted from an existing one), capable of calculating quite accurate the thermal conductivity of such mineral composites, from the ratio these three components and for the range of volumes and materials used in this thesis. Finally, the energy simulation performed to a typical Spanish dwelling, from the years 1900 to 1959 (mainly constructed with massive clay bricks), within three climatic zones of Spain (A, D and E), showed the energy savings potential that can provide this type of insulating material, depending on the thickness of the applied layer. Particularly, for the climatic A zone, it has been found an optimal layer thickness of 1 cm, while for zone D and E, 3.5 and 3.9 cm respectively. In this manner, the new studied materials is capable of decreasing the thickness of the insulating layer by 35% and 80%, compared with rock wool panels or mineral mortars with the highest insulating performance of the Spanish market respectively.
Resumo:
In this research, strain-sensing and damage-sensing functional properties of cement composites have been studied on a conventional reinforced concrete (RC) beam. Carbon nanofiber (CNFCC) and fiber (CFCC) cement composites were used as sensors on a 4 m long RC beam. Different casting conditions (in situ or attached), service location (under tension or compression) and electrical contacts (embedded or superficial) were compared. Both CNFCC and CFCC were suitable as strain sensors in reversible (elastic) sensing condition testing. CNFCC showed higher sensitivities (gage factor up to 191.8), while CFCC only reached gage factors values of 178.9 (tension) or 49.5 (compression). Furthermore, damage-sensing tests were run, increasing the applied load progressively up to the RC beam failure. In these conditions, CNFCC sensors were also strain sensitive, but no damage sensing mechanism was detected for the strain levels achieved during the tests. Hence, these cement composites could act as strain sensors, even for severe damaged structures near to their collapse.
Resumo:
Both strain and damage sensing properties on carbon nanofiber cement composites (CNFCC) are reported in the present paper. Strain sensing tests were first made on the material’s elastic range. The applied loading levels have been previously calculated from mechanical strength tests. The effect of several variables on the strain-sensing function was studied, e.g. cement pastes curing age, current density, loading rate or maximum stress applied. All these parameters were discussed using the gage factor as reference. After this first set of elastic experiments, the same specimens were gradually loaded until material’s failure. At the same time both strain and resistivity were measured. The former was controlled using strain gages, and the latter using a multimeter on a four probe setup. The aim of these tests was to prove the sensitivity of these CNF composites to sense their own damage, i.e. check the possibility of fabricating structural damage sensors with CNFCC’s. All samples with different CNF dosages showed good strain-sensing capacities for curing periods of 28 days. Furthermore, a 2%CNF reinforced cement paste has been sensitive to its own structural damage.
Resumo:
This research studies the self-heating produced by the application of an electric current to conductive cement pastes with carbonaceous materials. The main parameters studied were: type and percentage of carbonaceous materials, effect of moisture, electrical resistance, power consumption, maximum temperature reached and its evolution and ice melting kinetics are the main parameters studied. A mathematical model is also proposed, which predicts that the degree of heating is adjustable with the applied voltage. Finally, the results have been applied to ensure that cementitious materials studied are feasible to control ice layers in transportation infrastructures.
Resumo:
In this study the effect of structure and amount of polyglactin fibre incorporation into a brushite forming calcium phosphate cement system and the effect of mechanical compaction on the fibre modified system were investigated. In comparison the effect of resorbable polycaprolactone surface coating of cement specimens was investigated. The results showed that, apart from the mechanical properties of the reinforcing material, the structure of the incorporated fibres, regular or random, is crucial for the resulting flexural strength and modulus of elasticity. Fibre reinforcement could also be combined with mechanical compaction of the cement/fibre composite paste leading to a possible 7-fold increase in flexural strength or an almost 5-fold increase in modulus of elasticity. Reinforcement of the tensile surface of cement grafts may ultimately improve strength where required, especially in conjunction with bone fixation devices. © 2005 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
Steam injection is an oil recovery method accomplished by introducing steam directly into the oil well to the reservoir. The steam causes dilation of the casing, which, after reduction in temperature, tends to return to the initial dimensions: causing the formation of cracks in the cement and loss of hydraulic isolation.. In this context, the type of the SBR latex is used to improve the flexibility of the cement matrix by reducing the amount of fatigue failure. To prevent these failures, the mechanical resistance parameters should be carefully adjusted to well conditions. This work aims to study the mechanical behavior of cement slurry systems additivated with SBR latex for cementing oil wells subject to steam injection. Through the central composite factorial design was studied the behavior of the compressive strength by varying the density of the paste between 1.75 g /cm³ (14.6 lb/ Gal) and 1.89 g/cm³ (15,8lb / Gal), curing time between 4 days and 28 days and concentration of SBR Latex between 0 L / m³ and 534.722 L / m³ (0 gpc and 4 gpc). The results showed that increasing the concentration of SBR latex, within the given ranges, there was a decreased compression resistance and elastic modulus by increasing the elastic deformability of the slurry. From the results it can determine best slurries formulation conditions in oil well cementing operations subject to steam injection.
Resumo:
Steam injection is an oil recovery method accomplished by introducing steam directly into the oil well to the reservoir. The steam causes dilation of the casing, which, after reduction in temperature, tends to return to the initial dimensions: causing the formation of cracks in the cement and loss of hydraulic isolation.. In this context, the type of the SBR latex is used to improve the flexibility of the cement matrix by reducing the amount of fatigue failure. To prevent these failures, the mechanical resistance parameters should be carefully adjusted to well conditions. This work aims to study the mechanical behavior of cement slurry systems additivated with SBR latex for cementing oil wells subject to steam injection. Through the central composite factorial design was studied the behavior of the compressive strength by varying the density of the paste between 1.75 g /cm³ (14.6 lb/ Gal) and 1.89 g/cm³ (15,8lb / Gal), curing time between 4 days and 28 days and concentration of SBR Latex between 0 L / m³ and 534.722 L / m³ (0 gpc and 4 gpc). The results showed that increasing the concentration of SBR latex, within the given ranges, there was a decreased compression resistance and elastic modulus by increasing the elastic deformability of the slurry. From the results it can determine best slurries formulation conditions in oil well cementing operations subject to steam injection.
Resumo:
Presented in this report is an investigation of the use of "sand-lightweight" concrete in prestressed concrete structures. The sand-lightweight concrete consists of 100% sand substitution for fines, along with Idealite coarse and medium lightweight aggregate and Type I Portland Cement.
Resumo:
The presence of sulfates potentialize damage on cementbased materials, leading to structural failures. Therefore, structures must be designed to compensate for this effect. The mechanical properties of cement–chitin mixtures are investigated with different percentages of chitin (0.5, 1.3, and 2.1 wt.%) and aging of composite in a joint nanoscopic- and macroscopic-scale by experimental study. The objective is to increase the durability of concrete elements at coastal aquifers where concrete structures are in constant exposure to sulfate ions, chloride ions among others. Tapping mode AFM was used to characterize the surface structure and roughness of the cement pastes. To verify the chitin addition and the formation of sulfate-based aggregates Raman and IR spectra were recorded and are presented in this work. Then, force spectroscopy was used to obtain the nanomechanical properties at three different exposure times (1 day, 6 months, and 1 year) into water or a SO4 2 environment. Macroscopic parameters (e.g., compression strength of cylindrical probes) were assessed for comparison following standard guidelines. The results show a decrease of its mechanical properties as a function of the polymer concentration but more importantly, they correlate the elasticity and adhesion at the nanoscale with the behavior of the bulk material.
Resumo:
This study investigated the effect of the incorporation of an iodonium salt in experimental composites, on the bond strength of metallic brackets bonded to bovine teeth. Two hundred and seventy bovine teeth were embedded in self-curing acrylic resin and divided into 18 groups (n=15), according to the experimental composite with an iodonium salt at molar concentrations 0 (control), 0.5, or 1%; the light-activation times (8, 20 and 40 s); and the storage times (10 min or 24 h). Metallic brackets were fixed on the tooth surface using experimental composites. Photoactivation was performed with a quartz-tungsten-halogen light-curing unit curing unit for 8, 20 and 40 s. The specimens were stored in distilled water at 37 °C for 10 min or 24 h and submitted to bond strength test at 0.5 mm/min. The data were subjected to three-way ANOVA and Tukey's test (α=0.05). The Adhesive Remnant Index (ARI) was used to classify the failure modes. The shear bond strengths (MPa) at 10 min for light-activation times of 8, 20 and 40 s were: G1 - 4.6, 6.9 and 7.1; G2 - 8.1, 9.2 and 9.9; G3 - 9.1, 10.4 and 10.7; and at 24 h were: G1 - 10.9, 11.1 and 11.7; G2 - 11.8, 12.7 and 14.2; G3 - 12.1, 14.4 and 15.8. There was a predominance of ARI score 3 for groups with 10 min storage time, and ARI score 2 for groups with 24 h storage time. In conclusion, the addition of iodonium salt (C05 and C1) to the experimental composite may increase the bond strength of brackets to bovine enamel using reduced light exposure times.
Resumo:
To evaluate the influence of light-activation of second, third and fourth increments on degree of conversion (DC) and microhardness (KHN) of the top (T) and bottom (B) surface of the first increment. Forty samples (n = 5) were prepared. In groups 1-4, after each increment light-activation (multiple irradiation), T and B of the first increment were measured in DC and KHN. In groups 5-8, only the first increment was made (single irradiation) and measurements of DC and KHN were taken at 15 min intervals. The light-activation modes were (XL) 500 mW/cm(2) × 38 s (G1/G5); (S) 1000 mW/cm(2) × 19 s (G2/G6), (HP) 1400 mW/cm(2) × 14 s (G3/G7); (PE) 3200 mW/cm(2) × 6 s (G4/G8). Data for DC and KHN were analyzed separately by using PROC MIXED for repeated measures and Tukey-Kramer test (α = 0.05). For KHN, B showed lower values than T. PE resulted in lower values of KHN in B surface. For single and multiple irradiations, T and B of first measurement showed the lowest KHN and the fourth measurement showed the highest, with significant difference between them. For single irradiation, first and second increments presented similar KHN, different from the third and fourth increment, which did not differ between them. For multiple irradiations, the second light-activation resulted in KHN similar to first, third and fourth increments. For DC, except QTH, T presented higher DC than B. The light-activation of successive increments was not able to influence the KHN and DC of the first increment.
Resumo:
The durability of the cellulose-cement composites is a decisive factor to introduce such material in the market. Polymers have been used in concrete and mortar production to increase its durability. The goal of this work was the physical and mechanical characterization of cellulose-cement composites modified by a polymer and the subsequent durability evaluation. The work also evaluated the dispersion of acrylic polymer in composites made of Pinus caribaea residues. The physical properties observed were water absorption by immersion and bulk density. Rupture modulus and toughness were determined by flexural test. The specimens were obtained from pads, produced by pressing and wet curing. Samples were subjected to accelerated aging tests by repeated wetting and drying cycles and hot-water bath and natural aging. The scanning electron microscopy (SEM) allowed verifying the fiber and composite characteristics along the time. For the composite range analyzed, it was observed the polymer improved the mechanical properties of composites besides a significant decreasing in water absorption. The use of polymer improved the performance of vegetable fiber-cement composites when compared to the conventional mortar, due to water absorption decreasing.