Multiferroic nanoparticles (NPs) of pristine and Ca, Ba co-doped BiFeO3 were synthesized by a facile sal gel route. Co-doping was done by fixing the total dopant concentration at 5 mol% and then the relative concentrations of Ca and Ba was varied. Structural, optical and magnetic properties of the NPs were investigated using different techniques. UV-Vis absorption spectra of BiFeO3 NPs showed a substantial blue shift of similar to 100 nm (530 nm -> 430 nm) on Ca. Ba co-doping which corresponds to increase in band gap by 0.5 eV. Fe-57 Mossbauer spectroscopy confirmed that iron is present only in 3(+) valence state in all co-doped samples. The coercive field increased by 18 times for Bi0.95Ca0.01Ba0.04FeO3 samples, which is the maximum enhancement, observed amongst all the 5 mol% doped samples. At the equimolar (2.5 mol % each) concentration of co-dopants, the coercive field shows a significant enhancement of about 9 times (220 Oe -> 2014 Oe) with concomitant increase in saturation magnetization by 7 times. Thus, equimolar co-doping causes simultaneous enhancement of the twin aspects of magnetic properties thereby making them better suited for device applications. (C) 2012 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Tin (Sn) doped zinc oxide (ZnO) thin films were synthesized by sol-gel spin coating method using zinc acetate di-hydrate and tin chloride di-hydrate as the precursor materials. The films were deposited on glass and silicon substrates and annealed at different temperatures in air ambient. The agglomeration of grains was observed by the addition of Sn in ZnO film with an average grain size of 60 nm. The optical properties of the films were studied using UV-VIS-NIR spectrophotometer. The optical band gap energies were estimated at different concentrations of Sn. The MOS capacitors were fabricated using Sn doped ZnO films. The capacitance-voltage (C-V), dissipation vs. voltage (D-V) and current-voltage (I-V) characteristics were studied and the electrical resistivity and dielectric constant were estimated. The porosity and surface area of the films were increased with the doping of Sn which makes these films suitable for opto-electronic applications. (C) 2012 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The role of defects on laser-excited photoluminescence of various ZnO nanostructures has been investigated. The study shows that defects present in ZnO nanostructures, specially Zn-related defects play a crucial role in determining the laser-excited photoluminescence intensity (LEI). ZnO nanoparticles as well as nanorods (NR) annealed in oxygen atmosphere exhibit remarkable enhancement in LEI. A similar enhancement is also shown by Al-doped ZnO NR. © 2012 Springer Science+Business Media, LLC.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The role of defects on laser-excited photoluminescence of various ZnO nanostructures has been investigated. The study shows that defects present in ZnO nanostructures, specially Zn-related defects play a crucial role in determining the laser-excited photoluminescence intensity (LEI). ZnO nanoparticles as well as nanorods (NR) annealed in oxygen atmosphere exhibit remarkable enhancement in LEI. A similar enhancement is also shown by Al-doped ZnO NR.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Pure and tin doped zinc oxide (Sn:ZnO) thin films were prepared for the first time by NSP technique using aqueous solutions of zinc acetate dehydrate, tin (IV) chloride fendahydrate and methanol. X-ray diffraction patterns confirm that the films are polycrystalline in nature exhibiting hexagonal wurtzite type, with (0 0 2) as preferred orientation. The structural parameters such as lattice constant ('a' and `c'), crystallite size, dislocation density, micro strain, stress and texture coefficient were calculated from X-ray diffraction studies. Surface morphology was found to be modified with increasing Sn doping concentration. The ZnO films have high transmittance 85% in the visible region, and the transmittance is found to be decreased with the increase of Sn doping concentration. The corresponding optical band gap decreases from 3.25 to 3.08 eV. Room temperature photoluminescence reveals the sharp emission of strong UV peak at 400 nm (3.10 eV) and a strong sharp green luminescence at 528 nm (2.34 eV) in the Sn doped ZnO films. The electrical resistivity is found to be 10(6) Omega-cm at higher temperature and 10(5) Omega-cm at lower temperature. (C) 2012 Elsevier Ltd. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Free-standing ZnO nanocrystals simultaneously doped with Fe and Cu with varying Fe/Cu compositions have been synthesized using colloidal methods with a mean size of similar to 7.7 nm. Interestingly, while the Cu-doped ZnO nanocrystal remains diamagnetic and Fe-doped samples show antiferromagnetic interactions between Fe sites without any magnetic ordering down to the lowest temperature investigated, samples doped simultaneously with Fe and Cu show a qualitative departure in exhibiting ferromagnetic interactions, with suggestions of ferromagnetic order at low temperature. XAS measurements establish the presence of Fe2+ and Fe3+ ions, with the concentration of the trivalent species increasing in the presence of Cu doping, providing direct evidence of the Fe2+ + Cu2+ sic Fe3+ + Cu+ redox couple being correlated with the ferromagnetic property. Using DFT, the unexpected ferromagnetic nature of these systems is explained in terms of a double exchange between Fe atoms, mediated by the Cu atom, in agreement with experimental observations.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Zinc Oxide (ZnO) and indium doped ZnO (IZO) thin films with different indium compositions were grown on p-type boron doped Si substrates by pulsed laser deposition (PLD). The effect of indium concentration on the structural, optical and electrical properties of the film was studied. XRD, XPS and Raman studies confirm the single phase formation and successful doping of In in to ZnO. We observed various photoluminescence emissions, ranging from UV to visible, with the incorporation of In into ZnO. Room temperature Current-Voltage (I-V) characteristics showed good p-n junction properties for n-type-undoped and In doped ZnO with p-type substrates. The turn on voltage was observed to be decreasing with increase in In composition.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

A series of Dy3+ (0.5-9 mol%) and Li+ (0.5-3 mol%) co-doped strontium cerate (Sr2CeO4) nanopowders are synthesized by low temperature solution combustion synthesis. The effects of Li+ doping on the crystal structure, chemical composition, surface morphology and photoluminescence properties are investigated. The X-ray diffraction results confirm that all the samples calcined at 900 degrees C show the pure orthorhombic (Pbam) phase. Scanning electron microscopy analysis reveals that the particles adopt irregular morphology and the porous nature of the product. Room temperature photoluminescence results indicate that the phosphor can be effectively excited by near UV radiation (290 to 390 nm) which results in the blue (484 nm) and yellow (575 nm) emission. Furthermore, PL emission intensity and wavelength are highly dependent on the concentration of Li+ doping. The emission intensity is enhanced by similar to 3 fold with Li+ doping. White light is achieved by merely varying dopant concentration. The colour purity of the phosphor is confirmed by CIE co-ordinates (x = 0.298, y = 0.360). The study demonstrates a simple and efficient method for the synthesis of novel nanophosphors with enhanced white emission.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Zn1-xMgxO ( <= x <= 0.1) ceramics were fabricated by conventional solid-state reaction of co-precipitated zinc oxide and magnesium hydroxide nanoparticles. Structural and morphological properties of the fabricated ceramics were studied using X-ray diffraction and scanning electron microscopic analysis. The dielectric measurements of the ceramics were carried out as a function of frequency and temperature respectively. Interestingly, Mg doped ZnO (MZO) samples exhibited colossal dielectric response (similar to 1 x 10(4) at 1 kHz) with Debye like relaxation. The detailed dielectric studies and thermal analyses showed that the unusual dielectric response of the samples were originated from the defected grain and grain boundary (GB) conductivity relaxations due to the absorbed atmospheric water vapor (moisture). Impedance spectroscopy was employed to determine the defected grain and GB resistances, capacitances and which supported Maxwell-Wagner type relaxation phenomena. (C) 2015 Elsevier Ltd. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

We report the synthesis of vanadium and nitrogen co-doped TiO2 for photocatalysis mainly emphasizing the state of nitrogen doping into TiO2 in the presence of vanadium ions. Considering the increase in antibiotic resistance developed by microbes due to the excess of pharmaceutical waste in the ecosystem, the photocatalytic activity was measured by degrading an antibiotic, chloramphenicol. A novel experiment was conducted by degrading the antibiotic and bacteria in each other's vicinity to focus on their synergistic photo-degradation by V-N co-doped TiO2. The catalysts were characterized using XRD, DRS, PL, TEM, BET and XPS analysis. Both interstitial and substitutional nitrogen doping were achieved with V-TiO2, showing high efficiency under visible light for antibiotic and bacterial degradation. In addition, the effect of doping concentration of nitrogen and vanadium in TiO2 and catalyst loading was studied thoroughly. Reusability experiments show that the prepared V-N co-doped TiO2 was stable for many cycles.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Cobalt-doped ZnO (Zn1-xCoxO) thin films were fabricated by reactive magnetron cosputtering. The processing conditions were carefully designed to avoid the occurrence of Co precipitations. The films are c-axis oriented, and the solubility limit of Co in ZnO is less than 17%, determined by x-ray diffraction. X-ray photoemission spectroscopy measurements show Co ions have a chemical valance of 2+. In this paper, hysteresis loops were clearly observed for Zn1-xCoxO films at room temperature. The coercive field, as well as saturation magnetization per Co atom, decreases with increasing Co content, within the range of 0.07

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Nanopartículas de dióxido de titânio vêm sendo extensamente empregadas como fotocatalisa-dores, já que são eficientes na degradação de diversos poluentes. Visando a obtenção de titâ-nias com diferentes propriedades, realizaram-se sínteses através do método sol-gel, a partir da hidrólise do tetraisopropóxido de titânio (IV) TIPP e seguindo-se os princípios da Química Verde, dispensando-se temperaturas e pressões elevadas. Foi estudada a influência de dife-rentes parâmetros, como: pH, solvente, razão molar álcool/TIPP e ordem de adição dos rea-gentes. Foram obtidas titânias na forma cristalina anatásio, nanométricas, com elevadas áreas superficiais específicas e predominantemente mesoporosas. Visando-se obter titânias com melhores propriedades óticas, isto é, capazes de sofrer a fotoativação pela luz visível, foram sintetizadas titânias dopadas e co-dopadas com os metais ferro e rutênio (Fe3+ e Ru3+) e o a-metal N (N3). A síntese desses materiais também foi realizada através do método sol-gel, sendo a dopagem realizada durante o processo de hidrólise. As amostras foram caracterizadas na forma de pó por difração de raios-X, adsorção-dessorção de nitrogênio, microscopia ele-trônica de varredura e espectroscopia de refletância difusa no UV-Visível. A titânia pura a-presentou como única fase cristalina o anatásio, quando calcinada até 400 C, com a presença de traços de brookita. A partir de 600 C, observou-se o aparecimento da fase rutilo, que em 900C foi a única fase encontrada na titânia. A dopagem com Ru3+dificultou a transformação de fase anatásio para rutilo, ao contrário da dopagem com Fe3+. O processo de co-dopagem acelerou a formação de rutilo, que se apresentou como única fase nas amostras calcinadas a 600 C. As titânias dopadas apresentaram uma leve diminuição na energia de bandgap, sendo os dopantes capazes de deslocar a absorção para o vermelho. Foram realizados testes fotoca-talíticos visando à degradação do azocorante Reactive Yellow 145 com lâmpada de vapor de mercúrio de 125 W a fim de se comparar as atividades fotocatalíticas das titânias puras, dopa-das e co-dopadas, calcinadas a 300C. De todas as titânias sintetizadas, a titânia pura foi a que melhor degradou o corante, tendo um desempenho semelhante ao do TiO2 P25, da Evo-nik

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Siloxane Polymer exhibits low loss in the 800-1500 nm range which varies between 0.01 and 0.66 dB cm1. It is for such low loss the material is one of the most promising candidates in the application of engineering passive and active optical devices [1, 2]. However, current polymer fabrication techniques do not provide a methodology which allows high structurally solubility of Er3+ ions in siloxane matrix. To address this problem, Yang et al.[3] demonstrated a channel waveguide amplifier with Nd 3+-complex doped polymer, whilst Wong and co-workers[4] employed Yb3+ and Er3+ co-doped polymer hosts for increasing the gain. In some recent research we demonstrated pulsed laser deposition of Er-doped tellurite glass thin films on siloxane polymer coated silica substrates[5]. Here an alternative methodology for multilayer polymer-glass composite thin films using Er3+ - Yb3+ co-doped phosphate modified tellurite (PT) glass and siloxane polymer is proposed by adopting combinatorial pulsed laser deposition (PLD). © 2011 IEEE.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Using first-principles methods, we systematically study the mechanism of defect formation and electronic structures for 3d transition-metal impurities (V, Cr, Mn, Fe, and Co) doped in silicon nanowires. We find that the formation energies of 3d transition-metal impurities with electrons or holes at the defect levels always increase as the diameters of silicon nanowires decrease, which suggests that self-purification, i.e., the difficulty of doping in silicon nanowires, should be an intrinsic effect. The calculated results show that the defect formation energies of Mn and Fe impurities are lower than those of V, Cr, and Co impurities in silicon nanowires. It indicates that Mn and Fe can easily occupy substitutional site in the interior of silicon nanowires. Moreover, they have larger localized moments, which means that they are good candidates for Si-based dilute magnetic semiconductor nanowires. The doping of Mn and Fe atom in silicon nanowires introduces a pair of energy levels with t(2) symmetry. One of which is dominated by 3d electrons of Mn or Fe, and the other by neighboring dangling bonds of Si vacancies. In addition, a set of nonbonding states localized on the transition-metal atom with e symmetry is also introduced. (C) 2008 American Institute of Physics. [DOI: 10.1063/1.3000445]

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Si-doped ZnO can be synthesized on the surface of the early grown Zn2SiO4 nanostructures and form core/ shell coaxial heterostructure nanobelts with an epitaxial orientation relationship. A parallel interface with a periodicity array of edge dislocations and an inclined interface without dislocations can be formed. The visible green emission is predominant in PL spectra due to carrier localization by high density of deep traps from complexes of impurities and defects. Due to band tail localization induced by composition and defect fluctuation, and high density of free-carriers donated by doping, especially the further dissociation of excitons into free-carriers at high excitation intensity, the near-band-edge emission is dominated by the transition of free-electrons to free-holes, and furthermore, exhibits a significant excitation power-dependent red-shift characteristic. Due to the structure relaxation and the thermalization effects, carrier delocalization takes place in deep traps with increasing excitation density. As a result, the green emission passes through a maximum at 0.25I(0) excitation intensity, and the ratio of the violet to green emission increases monotonously as the excitation laser power density increases. The violet and green emission of ZnO nanostructures can be well tuned by a moderate doping and a variation in the excitation density.