Resumo:
The electrical properties of the grain boundary region of electroceramic sensor temperature based on inverse spinel Zn7Sb2O12 were investigated at high temperature. The zinc antimoniate was synthesized by a chemical route based on the modified Pechini method. The electric properties of Zn7Sb2O12 were investigated by impedance spectroscopy in the frequency range from 5 Hz to 13 MHz and from 250 up to 600 degreesC. The grain boundary conductivity follows the Arrhenius law, with two linear branches of different slopes. These branches exhibit activation energies with very similar values; the low-temperature (less than or equal to350 degreesC) and high-temperature (greater than or equal to400 degreesC) regions are equal to 1.15 and 1.16 eV, respectively. Dissimilar behavior is observed on the relaxation time (tau) curve as a function of temperature, where a single slope is identified. The negative temperature coefficient parameters and nature of the polarization phenomenon of the grain boundary are discussed. (C) 2003 American Institute of Physics.
Resumo:
This paper reports a study of influence of Cr concentration on the electrical properties and microstructure of SnO2-based powders doped with Mn and Nb, prepared by an organic route (Pechini method). All the samples were compacted into discs and sintered at 1300 degrees C for 3h, resulting in ceramics with relative density varying between 78% and 98%. The powders were characterized by X-ray diffraction analysis. Impedance spectroscopy characterization indicated that the conductivity decreases as Cr concentration increases, probably due to Cr segregation at grain boundaries, which reduces grain size, increasing the number of resistive boundaries.
Resumo:
This study consisted of an investigation of the influence of powder preparation on the phase and chemical compositions and microstructure of 9.5/65/35 PLZT materials sintered in an oxygen atmosphere. The powders with the formula Pb0.905La0.095(Zr0.65Ti0.35)(0.976)O-3+3.5 wt.% PbO were prepared by the polymeric organometallic precursor method (the Pechini method and the partial oxalate procedure). Phase composition was determined by X-ray diffraction of powder and EDS analysis, while grain size was determined based on the micrograph obtained from SEM. (C) 2001 Elsevier B.V. B.V. All rights reserved.
Resumo:
In this work, indium tin oxide (ITO) films were prepared using a wet chemical route, the Pechini method. This consists of a polyesterification reaction between an alpha-hydroxicarboxylate complex (indium citrate and tin citrate) with a polyalcohol (ethylene glycol) followed by a post annealing at 500 degrees C. A 10 at.% of doping of Sn4+ ions into an In2O3 matrix was successfully achieved through this method. In order to characterize the structure, the morphology as well as the optical and electrical properties of the produced ITO films, they were analyzed using different experimental techniques. The obtained films are highly transparent, exhibiting transmittance of about 85% at 550 nm. They are crystalline with a preferred orientation of [222]. Microscopy discloses that the films are composed of grains of 30 nm average size and 0.63 nm RMS roughness. The films' measured resistivity, mobility and charge carrier concentration were 5.8 x 10(-3) Omega cm, 2.9 cm(2)/V s and -3.5 x 10(20)/cm(3), respectively. While the low mobility value can be related to the small grain size, the charge carrier concentration value can be explained in terms of the high oxygen concentration level resulting from the thermal treatment process performed in air. The experimental conditions are being refined to improve the electrical characteristics of the films while good optical, chemical, structural and morphological qualities already achieved are maintained. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
In this work, the polymeric precursor method Was used to obtain disordered Zn2TiO4 powders, either Undoped or doped with Sn4+, Cr3+ and V5+, to be applied its photoluininescent material. The characterization was undertaken by means of thermal analysis (TG and DTA), X-ray diffraction (XRD), infrared spectroscopy (IR) and photoluminescence (PL). Previous works stated that titanate octahedra containing a short Ti-O distance show efficient luminescence at roorn temperature if these octahedra are isolated from each other. In the present work, the phenomenon was observed in condensed octahedra, sharing edges. The room temperature PL noticed in undoped Zn2TiO4 had its intensity increased by the dopant addition-the increase was of about 300% for V5+ doping 400% for Cr3+ and 800% for Sn4+. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Tin oxide, SnO2. is a very used compound in industry and one of its uses is as varistor. For the current requirements of the technology is necessary a strict control of the chemical purity and the particle size of the raw material; for that reason the great interest that exists at the moment to develop synthesis methods that allow to get these requirements. In this work, ceramic powders of the Sn-Co-Nb-Ti-Al system using the controlled precipitation and polymeric precursor (Pechini) methods were synthesized. The raw material obtained was characterized using X-ray diffraction (XRD), thermal analysis (DTA/FG) and scanning electron microscopy (SEM). The sintering samples shown a good varistor behavior with non-linear coefficient (alpha) values similar to 22, and Er 2083 V/cm(2). (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
This paper aims to describe the synthesis of the semi-crystalline and crystalline powder of lanthanum doped with zirconium titanate (65/35), LZT through Pechini method. The analysis done by Raman demonstrated that semi-crystalline phase at 550 degrees C and crystalline phase after 600 degrees C were formed. The XRD pattern shows the ZrTiO4 phase formation demonstrating that La substitutions into the lattice take place. The calcined powder at different temperatures shows a semi-crystalline phase presenting photoluminescence effect when processed at low temperatures. From 300 to 400 degrees C a broadband is observed at 563 nm and 568 nm, respectively. Defects creation such as: Zr3+ center dot Vo(center dot center dot) and Ti3+ - V-O(center dot center dot), Zr and Ti replaced by La with vacancy formation, impurities and imperfections contributed to the photoluminescence effect. However, the main emission is due to a reverse Ti4+ -> O2- or/and Zr4+ -> O2- transition that occur within a regular titanate or zirconate eight-fold coordination [BO8-delta], B = Zr4+, Ti4+. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
PLZT(9/65/35) obtained by association between the Pechini method (ZT) and partial oxalate (PLZT) was prepared. The stoichiometric phase and monophasic (cubic) PLZT obtained by calcination did not occur after sintering. The sintering process, by using two stages, caused a liquid phase formation due to a PbO excess (5 and 10 wt%). Samples with high density (similar to 8 g/cm(3)) and optical transparency(similar to 12%) were obtained. However, an equilibrium between the excess of PbO of sample/atmosphere PbO leads to a segregated PbO phase on the boundaries of the microstructure. A diffusion of Zr, Ti and La ions from PLZT to PbO phase promoted a stoichiometric deviation of the matrix and modified the optical and dielectric characteristics. (C) 2000 Elsevier B.V. Ltd and Techna S.r.l. All rights reserved.
Resumo:
Zirconia-ceria powders with ceria concentration varying from 0 to 12 mol% were synthesized using a polymeric precursor route based on the Pechini process. Powder characteristics were evaluated with regard to the crystallite size, BET surface area, phase distribution, nitrogen adsorption/desorption behavior, and agglomeration state. Sintering was studied considering the shrinkage rate, densification, grain size, and phase evolution. It was demonstrated that the synthesis method is effective to prepare nanosized powders of tetragonal zirconia single-phase. Sinterability mainly depended on the agglomeration state of powders and the monoclinic phase content, fully tetragonal zirconia ceramic, with grain size of 2.4 mu m, was obtained after addition of at least 9 mol% ceria and sintering at 1500 degrees C for 4 h. (C) 2000 Elsevier B.V. Ltd. All rights reserved.
Resumo:
The polymeric precursor method was used to prepare multi-layered LiNbO3 films. The overall process consists of preparing a coating solution from the Pechini process and the deposited film is subsequently heat-treated. Two-layered films were prepared by this process, onto (0001) sapphire substrates. Two different routes were investigated for the heat-treatment. The amorphous route consisted of performing, after each deposition, a pre-treatment at low temperature to eliminate the organic material. In this case, the crystallization heat-treatment was performed only after the two layers had been deposited. on the other hand, a process layer-after-layer crystallization was used. Both routes led to (0001) LiNbO3 oriented films. However, only the film prepared by the layer-after-layer crystallization presented an epitaxial growth and a crack-free morphology. Moreover, the layer-after-layer crystallization process led to a film exhibiting the best optical properties. (C) 2001 Elsevier B.V. Ltd. All rights reserved.
Resumo:
It is known that the dielectric properties of BaTiO3 (BT) are strongly dependent on its grain size. Coarse-grained ceramics of pure BT showed lower dielectric constant at room temperature then fine grained. Many authors considered that when the grain size is lower than 700 nm, the lattice of BT changes from tetragonal to pseudocubic, and the dielectric constant value is very low. In the doped BT this effect is more complex, because it is necessary to consider also the influence of dopants. The grain size effect on the structure and dielectric properties of niobium-doped barium titanate was investigated. Niobium-doped barium titanate was prepared from powders obtained by doping of commercial barium titanate and from organometallic complex using citrates as precursors (Pechini procedure). The crystal and microstructure of sintered niobium-doped barium titanate were determined. Dielectric constant and dissipation factor were measured. The observation confirmed that the structure and properties are strongly dependent on grain size. (C) 2003 Elsevier B.V. B.V. All rights reserved.
Resumo:
Pechini's method was used to prepare lead titanate zirconate with Zr/Ti ratio equal to 53/47. X-ray diffraction data revealed the presence of a rhombohedral phase, rich in zirconium, due to difference in carbonate stabilities, in PZT ceramics calcined at 600 degrees C. Infrared spectroscopy presented COO- bonds in the 1400 cm(-1) region, which disappeared after calcining at 700 degrees C. Seeds with rhombohedral (PZT 57/43) or tetragonal structure (PZT 45/55) were added to the precursor. The microstructure was differentially influenced by the nature of seed particles. Rhombohedral nuclei promoted preferential crystallization of lead zirconate. This heterogeneity directly reflected on values of k(p) and d(33). (C) 1999 Elsevier B.V. Limited and Techna S.r.l. All rights reserved.
Resumo:
Zinc oxide (ZnO) is an electroluminescent (EL) material that can emit light in different regions of electromagnetic spectrum when electrically excited. Since ZnO is chemically stable, inexpensive and environmentally friendly material, its EL property can be useful to construct solid-state lamps for illumination or as UV emitter. We present here two wet chemical methods to prepare ZnO thin-films: the Pechini method and the sol-gel method, with both methods resulting in crystalline and transparent films with transmittance > 85% at 550 nm. These films were used to make thin-film electroluminescent devices (TFELD) using two different insulator layers: lithium fluoride (LiF) or silica (SiO2). All the devices exhibit at least two wide emission bands in the visible range centered at 420 nm and at 380 nm attributed to the electronic defects in the ZnO optical band gap. Besides these two bands, the device using SiO2 and ZnO film obtained via sol-gel exhibits an additional band in the UV range centered at 350 nm which can be attributed to excitonic emission. These emission bands of ZnO can transfer their energy when a proper dopant is present. For the devices produced the voltage-current characteristics were measured in a specific range of applied voltage. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
The Pechini method as well as the simultaneous addition of seeds particles and dopant solutions of BaTiO3 (BT) and PbTiO3 (PT) were used to prepare the perovskite phase 0.88 PZN-0.07 BT-0.05 PT. To study the influence of seed particle frequency on the synthesis of the PZN ceramic, two ranges of seed particle size were used: the range from 30 to 100 nm, termed small seed particles (frequency of 10(15) particles/cm(3)); and the range from 100 to 900 nm, termed large seed particles (frequency of 10(13) particles/cm(3)). The crystalline nuclei size influenced the calcining process, the sintering process and the microstructure. Samples prepared with lower seed frequency displayed more amount of pyroclore phase, need higher temperatures for sintering and showed a more heterogeneous microstructure with poor dielectric properties. (C) 2000 Elsevier B.V. Ltd and Techna S.r.l. All rights reserved.
Resumo:
The 9.5/65/35 PLZT was prepared from the polymeric precursors (the Pechini and partial oxalate process) and by sintering in two stages in an oxygen atmosphere. After thermal treatment at 400 degreesC, the powders were calcinated and sintered at 1200 degreesC with slow heating and cooling rates. The second stage of sintering consisted of hot pressing at the same temperature in oxygen atmosphere. After calcination of PLZT powders obtained by both methods, as well as after sintering of PLZT obtained by Pechini process, the paraelectric cubic phase was formed. After sintering of PLZT obtained by partial oxalate procedure, small tetragonality of crystal structure was observed. After hot pressing PLZT was pseudocubic. SEM microstructural analyses were carried out of the sintering and hot pressed samples and indicated the small grain size less than 2 mum. (C) 2001 Elsevier B.V. B.V. All rights reserved.