929 resultados para grinding wheel
Resumo:
The relative significance of corrosive and abrasive wear in ore grinding is discussed. Laboratory marked ball wear tests were carried out with magnetic taconite and quartzite under different conditions, namely dry, wet and in the presence of an organic liquid. The effect of different modes of aeration and of pyrrhotite addition on the ball wear using mild steel, high carbon low alloy steel and austenitic stainless steel balls was evaluated. Results indicate that abrasive wear plays a significant role in ore grinding in the absence of sulfides, and rheological properties of the ore slurry influenced such wear. The effect of oxygen on corrosive wear becomes increasingly felt in the presence of a sulfide mineral such as pyrrhotite. Wear characteristics of the three types of ball materials under different grinding conditions are illustrated.
Resumo:
Cyclic plastic deformation of subgrade and other engineered layers is generally not taken into account in the design of railway bridge transition zones, although the plastic deformation is the governing factor of frequent track deterioration. Actual stress behavior of fine grained subgrade/embankment layers under train traffic is, however, difficult to replicate using the conventional laboratory test apparatus and techniques. A new type of torsional simple shear apparatus, known as multi-ring shear apparatus, was therefore developed to evaluate the actual stress state and the corresponding cyclic plastic deformation characteristics of subgrade materials under moving wheel load conditions. Multi-ring shear test results has been validated using a theoretical model test results; the capability of the multi-ring shear apparatus for replicating the cyclic plastic deformation characteristics of subgrade under moving train wheel load conditions is thus established. This paper describes the effects of principal stress rotation (PSR) of the subgrade materials to the cyclic plastic deformation in a railroad and impacts of testing methods in evaluating the influence of principal stress rotation to the track deterioration of rail track.
Resumo:
Food-borne pathogens are present in normal healthy pigs and thus are also present in pig wastes and by-products. The presence of these pathogens can be viewed negatively (i.e. 'a spoke in the wheel') or as simply another issue that requires the adoption of appropriate guidelines and management procedures. A key component in the development of appropriate, effective guidelines and management practices is a solid basis of knowledge on which pathogens are present as well as the levels of these pathogens. This paper reviews Australian Pork Limited (APL) funded projects carried out in our laboratories that have provided a solid base of Australian data for the pig industry. These data will ensure that pathogens are not 'a spoke in the wheel' but rather an issue - like many others that confront the industry - that can be managed to ensure that there is no unacceptable risk to either public health or the environment.
Resumo:
Railway wheel vibrations are caused by a number of mechanisms. Two of these are considered: (a) gravitational load reaction acting on different points of the wheel rim, as the wheel rolls on, and (b) random fluctuating forces generated at the contact patch by roughness on the mating surfaces of the wheel and rail. The wheel is idealized as a thin ring, and the analysis is limited to a single wheel rolling on a rail. It is shown that the first mechanism results in a stationary pattern of vibration, which would not radiate any sound. The acceleration caused by roughness-excited forces is much higher at higher frequencies, but is of the same order as that caused by load reaction at lower frequencies. The computed acceleration level (and hence the radiated SPL) caused by roughness is comparable with the observed values, and is seen to increase by about 10 dB for a doubling of the wagon speed. The driving point impedance of the periodic rail-sleeper system at the contact patch, which is used in the analysis, is derived in a companion paper.
Resumo:
An engineering analysis of the design of two-wheel bullock carts has been carried out with the aid of a mathematical model. Non-dimensional expressions for the pull and the neck load have been developed. In the first instance, the cart is assumed to be cruising at constant velocity on a terrain with the effective coefficient of rolling friction varying over a wide range (0.001 to 0.5) and the gradient varying between +0.2 to −0.2. Subsequently, the effect of inertia force due to an acceleration parallel to the ground is studied. In the light of this analysis, two modifications to the design of the cart have been proposed and the relative merits of the current designs and the proposed designs are discussed.
Resumo:
Copper(I) complexes with {Cu(μ2-S)N}4 and {Cu(μ3-S)N}12 core portions of butterfly-shaped or double wheel architectures have been isolated in the reaction of Cu(I) with the Schiff base ligand C6H4(CHNC6H4S)2, aiso-abtâ, under different conditions. View the MathML source containing the tetranuclear electroneutral complex View the MathML source is formed by the reaction of CuI in acetonitrilic solution and recrystallization from DMF, whereas View the MathML source containing dodecanuclear View the MathML source wheels is accessible starting from CuBF4. Complexes 2 and 4 represent the first examples of cyclic complexes with the same overall stoichiometry but different ring sizes. The ligand induces two different coordination environments around copper(I) by switching between μ2- and μ3-sulfur bridging modes.
Resumo:
Surface topography has been known to play an important role in the friction and transfer layer formation during sliding. In the present investigation, EN8 steel flats were ground to attain different surface roughness with unidirectional grinding marks. Pure Mg pins were scratched on these surfaces using an Inclined Scratch Tester to study the influence of directionality of surface grinding marks on coefficient of friction and transfer layer formation. Grinding angle (i.e., the angle between direction of scratch and grinding marks) was varied between 0 degrees and 90 degrees during the tests. Experiments were conducted under both dry and lubricated conditions. Scanning electron micrographs of the contact surfaces of pins and flats were used to reveal the surface features that included the morphology of the transfer layer. It was observed that the average coefficient of friction and transfer layer formation depend primarily on the directionality of the grinding marks but were independent of surface roughness on the harder mating surface. In addition, a stick-slip phenomenon was observed, the amplitude of which depended both on the directionality of grinding marks and the surface roughness of the harder mating surface. The grinding angle effect on the coefficient of friction, which consists of adhesion and plowing components, was attributed to the variation of plowing component of friction. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Laboratory results of marked-ball wear tests are used to discuss the relative significance of corrosive and abrasive wear in wet grinding. The electrochemical mechanism was investigated by correlating the corrosive wear with the corrosion current obtained from polarization curves under abrasion. Slurry rheology governs the manner in which ground slurries coat grinding balls, thereby influencing not only the grinding efficiency but also abrasive wear. The effects of percent solids and a grinding aid are illustrated.
Resumo:
Owing to the complexity of the wear process, high stress grinding abrasion is quite different from two-body abrasive wear. Reported data on two-body abrasive wear reveal that the wear decreases with an increase in steel hardness. This relationship can be established without having to consider the microstructure of the steel grinding medium. However, it is known that hardness cannot be directly employed to predict the wear of steel balls under three-body grinding abrasion, as occurs during dry grinding of ores in ball mills. The present work suggests that the wear behaviour of grinding balls can be classified according to the microstructural family to which they belong. Thus, in this work on AISI 52100 steel, the separate groups of microstructures were spheroidite—pearlite, bainite, tempered martensite and martensite with retained austenite. It appears that wear behaviour of the first three groups follows the same trend as that observed for two-body wear. The data suggest that an optimum level of retained austenite could improve the wear resistance of microstructures containing martensite.
Resumo:
Marked-ball grinding tests were carried out under different grinding conditions and environments. Three types of balls were used, namely, cast hyper steel, high chrome cast iron and EN-31 (forged), which cover a wide range of chemical composition, microstructure and media hardness. The effect of pulp density on ball wear and grinding efficiency was also studied. Relative pulp viscosities at different percent solids for the ore slurry were also determined. As the Kudremukh ore contained about 0.2% pyrite, the effect of addition of pyrite on ball wear was studied separately. Results of marked-ball grinding tests indicated that ball wear increased with time and showed a sharp increase for wet grinding over dry grinding. Ball wear under wet grinding conditions was also influenced by the gaseous atmosphere in the mill. At 70% solids, the best results in terms of reduced ball wear coupled with satisfactory grinding efficiency were obtained. The influence of oxygen on the corrosive wear of grinding balls was increasingly felt only if sulphide minerals such as pyrite were also present in the ore. The various ball materials could be arranged in the following order with respect to their overall wear resistance: high chrome cast iron > EN-31 (forged) > cast hyper steel.Possible ball wear mechanisms involved in the grinding of Kudremukh ore are discussed.
Resumo:
Marked ball grinding tests were carried out in the laboratory with a lead-zinc sulphide ore under different experimental conditions using high carbon low alloy steel (cast and forged) and high chrome cast iron balls. Relative ball wear as a function of grinding period and milling conditions was evaluated for the different types of ball materials. The role of corrosion and abrasion-erosion in the wear of grinding media is brought out. Methods to minimise ball wear through control of mill atmosphere and addition of reagents are discussed.
Resumo:
Grinding media wear appears to be non-linear with the time of grinding in a laboratory-scale ball mill. The kinetics of wear can be expressed as a power law of the type w=atb, where the numerical constant a represents wear of a particular microstructure at time t = 1 min and b is the wear exponent which is independent of the particle size prevailing inside a ball mill at any instant of time of grinding. The wear exponent appears to be an indicator of the cutting wear mechanism in dry grinding: a plot of the inverse of the normalised wear exponent (Image ) versusHs (where Hs is the worn surface hardness of the media) yields a curve similar to that of a wear resistance plot obtained in the case of two-body sliding abrasive wear. This method of evaluating the cutting wear resistance of media is demonstrated by employing 15 different microstructures of AISI-SAE 52100 steel balls in dry grinding of quartz in a laboratory-scale ball mill.
Resumo:
The type of abrasion that the grinding medium experiences inside a ball mill is classified as high stress or grinding abrasion, because the stress levels at the surface of the medium exceed the yield stress of the metal when hard abrasives are crushed. During dry grinding of ores the medium undergoes not only abrasion but also erosion and impact. As all three mechanisms of wear occur simultaneously, it is difficult to follow the individual components of wear. However, it is possible to show that the overall kinetics of wear follows a simple power law of the type w = at(b), where w is the weight loss of the grinding medium for a specified grinding time t and a and b are constants. Experimental data, obtained from dry grinding of quartz for a wide range of times using AISI 52100 steel balls having various microstructures in a laboratory scale batch mill, are fitted to the proposed equation and the wear rate w is calculated from the first derivative of the equation. The mean particle sizes of the quartz charge DBAR corresponding to 50 and 80% retained size are determined by mechanical sieving of the ground product after a grinding time t and thus the relationship between wear rate and particle size of the abrasive is established. It is found that w increases rapidly with DBAR up to some critical size and then increases at a much lower rate.
Resumo:
Marked ball grinding tests were carried out in the laboratory using high carbon low alloy steel (cast and forged) and high chrome cast iron balls. Relative ball wear as a function of grinding period and milling conditions was evaluated for the different type of ball materials in the grinding of lead-zinc sulphide and phosphate ores. Results indicated that ball wear increased with time and showed a sharp increase for wet grinding over dry grinding. Ball wear under wet grinding conditions was also influenced by the gaseous atmosphere in the mill. The influence of oxygen on the corrosive wear of grinding balls was increasingly felt in case of sulphide ore grinding. The grinding ball materials could be arranged in the following order with respect to their overall wear resistance:
Resumo:
Wear of high carbon low alloy (HCLA) cast steel balls during the grinding of a chalcopyrite ore was evaluated under different experimental conditions. The role of oxygen in enhancing ball wear during wet finding is brought out. The influence of pH on ball wear was also examined from the view point of acid production during grinding and reactivity of sulphides. Contributions from corrosion and abrasion towards ball wear are quantified in terms of ball wear rates as a function of time, particle size and gaseous atmosphere in the mill.