687 resultados para STAINLESS-STEELS
Resumo:
The effect of test temperature, which controls the stability of austenite, on the impact toughness of a low carbon Fe-Ni-Mn-C austenitic steel and 304 stainless steel, has been investigated. Under impact conditions, stress-induced martensitic transformation occurred, in a region near the fracture surface, at test temperatures below 80degreesC for the Fe-Ni-Mn-C steel and below -25degreesC for 304 stainless steel. The former shows significant transformation toughening and the highest impact toughness was obtained at 10degreesC, which corresponds to the maximum amount of martensite formed by stress-induced transformation above the Ms temperature. The stress-induced martensitic transformation contributes negatively to the impact toughness in the 304 stainless steel. Increasing the amount of stress-induced transformation to martensite, lowered the impact toughness. The experimental results can be well explained by the Antolovich theory through the analysis of metallography and fractography. The different effect of stress-induced transformation on the impact toughness in Fe-Ni-Mn-C steel and 304 stainless steel has been further understood by applying the crystallographic model for stress-induced martensitic transformation to these two steels. (C) 2002 Kluwer Academic Publishers.
Resumo:
Stainless steel coatings obtained by High Velocity Oxygen Fuel (HVOF) were characterized using optical (OM) and scanning electron microscopy (SEM), electron probe micro-analysis, X-ray diffraction (XRD), open-circuit potential (E-OC) measurements, electrochemical impedance spectroscopy (EIS) and polarisation tests. Differences among coated steels were mainly related with the gun-substrate distance parameter (310 nm for samples A and B and 260 min for C and D). The open-circuit potential values measured for all the samples after 18 h of immersion in aerated and unstirred 3.4% NaCl solution were: - 0.334, - 0.360, - 0.379 and - 0.412 V vs. Ag/AgCl,KClsat. for samples A to D, respectively. For EIS measurements, Nyquist plots showed higher capacitive semi-circle for samples sprayed at longer distance, indicating higher corrosion resistance in NaCl solution. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Four types of stainless steel coatings prepared by a high velocity oxy-fuel spraying system (HVOF) were studied. Differences among coated steels were related to the spraying parameters, which influenced the behavior of the samples against the corrosion. The electrochemical behavior of the stainless steel coatings was strongly influenced by porosity, the presence of micro- and macro-cracks, and also of un-melted particles. Once the electrolyte reached the steel substrate via these defects, the galvanic pair formed between the coating and substrate-accelerated corrosion, leading to the depletion of the coating. (C) 2004 Elsevier Ltd. All rights reserved.
Resumo:
Corrosion research in steels is one of the areas in which Mossbauer spectroscopy has become a required analytical technique, since it is a powerful tool for both identifying and quantifying distinctive phases (which contain Fe) with accuracy. In this manuscript, this technique was used to the study of corrosion resistance of plasma nitrided AISI 316L samples in the presence of chloride anions. Plasma nitriding has been carried out using dc glow-discharge, nitriding treatments, in medium of 80 vol.% H-2 and 20 vol.% N-2, at 673 K, and at different time intervals: 2, 4, and 7 h. Treated samples were characterized by means of phase composition and morphological analysis, and electrochemical tests in NaCl aerated solution in order to investigate the influence of treatment time on the microstructure and the corrosion resistance, proved by conversion electron Mossbauer spectroscopy (CEMS), glancing angle X-ray diffraction (GAXRD), scanning electron microscopy (SEM) and potentiodynamic polarization. A modified layer of about 8 gin was observed for all the nitrided samples, independently of the nitriding time. A metastable phase, S phase or gamma(N), was produced. It seems to be correlated with gamma`-Fe-4 N phase. If the gamma(N) fraction decreases, the gamma` fraction increases. The gamma(N) magnetic nature was analyzed. When the nitriding time increases, the results indicate that there is a significant reduction in the relative fraction of the magnetic gamma(N) (in) phase. In contrast, the paramagnetic gamma(N) (p) phase increases. The GAXRD analysis confirms the Mossbauer results, and it also indicates CrN traces for the sample nitrided for 7 h. Corrosion results demonstrate that time in the plasma nitriding treatment plays an important role for the corrosion resistance. The sample treated for 4 h showed the best result of corrosion resistance. It seems that the epsilon/gamma` fraction ratio plays an important role in thin corrosion resistance since this sample shows the maximum value for this ratio. (c) 2008 Published by Elsevier B.V.
Resumo:
In recent years, considerable thought and study have been given to the use of chromized articles in place of chromium stainless steel articles. The present extensive application of chromizing, indeed, helps greatly to conserve this valuable metal.
Resumo:
Aluminium is added to decrease matrix chromium losses on 430 stainless steel sintered on nitrogen atmosphere. Three different ways were used to add a 3% (in weight) aluminium: as elemental powder, as prealloyed powder, and as intermetallic Fe-AI compound. After die pressing at densities between 6.1-6.5 g/cm3, samples were sintered on vacuum and on N2-5%H2 atmosphere in a dilatometric furnace. Therefore, dimensional change was recorded during sintering. Weight gain was obtained after nitrogen sintering on all materials due to nitrides formation. Sample expansion was obtained on all nitrogen sintered steels with Al additions. Microstructure showed a dispersion of aluminium nitrides when pre-alloyed powders are used. On the contrary, aluminium nitride areas can be found when aluminium is added as elemental powders or as Fe-AI intermetallics. Also nitrogen atmosphere leads to austenite formation and hence, on cooling, dilatometric results showed a dimensional change at austenitic-ferritic phase transformation temperature.
Resumo:
The paper presents some preliminary results of an ongoing research intended to qualify a highly resistant duplex stainless steel wire as prestressing steel and, gets on insight on (he wires' fracture micromechanism and residual stresses field. SEM fractographic analysis of the stainless steel wires indicates an anisotropic fracture behavior in tension, in presence of surface flaws, attributed to the residual stresses generated through the fabrication process. The residual stresses magnitude influences the damage tolerance, its knowledge being a key issue in designating/qualifying the wires as prestressing steels.
Resumo:
The paper presents some preliminary results of an ongoing research intended to qualify a highly resistant duplex stainless steel wire as prestressing steel and, gets on insight on (he wires' fracture micromechanism and residual stresses field. SEM fractographic analysis of the stainless steel wires indicates an anisotropic fracture behavior in tension, in presence of surface flaws, attributed to the residual stresses generated through the fabrication process. The residual stresses magnitude influences the damage tolerance, its knowledge being a key issue in designating/qualifying the wires as prestressing steels.
Resumo:
Ion implantation modifies the surface composition and properties of materials by bombardment with high energy ions. The low temperature of the process ensures the avoidance of distortion and degradation of the surface or bulk mechanical properties of components. In the present work nitrogen ion implantation at 90 keV and doses above 1017 ions/cm2 has been carried out on AISI M2, D2 and 420 steels and engineering coatings such as hard chromium, electroless Ni-P and a brush plated Co-W alloy. Evaluation of wear and frictional properties of these materials was performed with a lubricated Falex wear test at high loads up to 900 N and a dry pin-on-disc apparatus at loads up to 40 N. It was found that nitrogen implantation reduced the wear of AISI 420 stainless steel by a factor of 2.5 under high load lubricated conditions and by a factor of 5.5 in low load dry testing. Lower but significant reductions in wear were achieved for AISI M2 and D2 steels. Wear resistance of coating materials was improved by up to 4 times in lubricated wear of hard Cr coatings implanted at the optimum dose but lower improvements were obtained for the Co-W alloy coating. However, hardened electroless Ni-P coatings showed no enhancement in wear properties. The benefits obtained in wear behaviour for the above materials were generally accompanied by a significant decrease in the running-in friction. Nitrogen implantation hardened the surface of steels and Cr and Co-W coatings. An ultra-microhardness technique showed that the true hardness of implanted layers was greater than the values obtained by conventional micro-hardness methods, which often result in penetration below the implanted depth. Scanning electron microscopy revealed that implantation reduced the ploughing effect during wear and a change in wear mechanism from an abrasive-adhesive type to a mild oxidative mode was evident. Retention of nitrogen after implantation was studied by Nuclear Reaction Analysis and Auger Electron Spectroscopy. It was shown that maximum nitrogen retention occurs in hard Cr coatings and AISI 420 stainless steel, which explains the improvements obtained in wear resistance and hardness. X-ray photoelectron spectroscopy on these materials revealed that nitrogen is almost entirely bound to Cr, forming chromium nitrides. It was concluded that nitrogen implantation at 90 keV and doses above 3x1017 ions/cm2 produced the most significant improvements in mechanical properties in materials containing nitride formers by precipitation strengthening, improving the load bearing capacity of the surface and changing the wear mechanism from adhesive-abrasive to oxidative.
Resumo:
The bearings in the air motors of modern jet aircraft engines must operate dry in hostile conditions at temperatures up to 500° C, where the thrust races in the actuators operate at temperatures up to 300° C. One of the few metallurgical combinations which can function efficiently under these conditions is martensitic stainless steel on tungsten carbide. The work described was initiated to isolate the wear mechanisms of two such steels in contact with tungsten carbide at temperatures up to 500° C. Experiments were carried out on angular contact bearings similar to these used in service, where both rolling and sliding is present and also for pure sliding conditions using a pin-on-disc apparatus. Wear measurements of the bearings were obtained with wear rates, friction and surface temperatures from the pin-on-disc machine for a series of loads and speeds. Extensive X-ray diffraction analysis was carried out on the wear debris, with also S.E.M. analysis and hardness tests on the worn surfaces along with profilometry measurements of the disc. The oxidational parameters of the steel were obtained from measurements of oxide growth rates by ellipsometry. Three distinct mechanisms of wear were established and the latter two were found to be present in both configurations. These involve an oxidational-abrasive mechanism at loads below 40 N with pin surface temperatures up to about 300 °C, with the mechanism changing to severe wear for higher loads. As the temperature increases a third wear mechanism appears due to transfer of relatively soft oxide films to the steel surface reducing the wear rate. Theoretical K factors were derived and compared with experimental values which were found to be in good agreement for the severe wear mechanism. The pin-on-disc experiments may be useful as a screening test for material selection, without the considerable cost of producing the angular contact bearings.
Resumo:
Lead bismuth eutectic (LBE) is a possible coolant for fast reactors and targets in spallation neutron sources. Its low melting point, high evaporation point, good thermal conductivity, low reactivity, and good neutron yield make it a safe and high performance coolant in radiation environments. The disadvantage is that it is a corrosive medium for most steels and container materials. This study was performed to evaluate the corrosion behavior of the austenitic stainless steel D9 in oxygen controlled LBE. In order to predict the corrosion behavior of steel in this environment detailed analyses have to be performed on the oxide layers formed on these materials and various other relevant materials upon exposure to LBE. In this study the corrosion/oxidation of D9 stainless steel in LBE was investigated in great detail. The oxide layers formed were characterized using atomic force microscopy, magnetic force microscopy, nanoindentation, and scanning electron microscopy with wavelength-dispersive spectroscopy (WDS) to understand the corrosion and oxidation mechanisms of D9 stainless steel in contact with the LBE. What was previously believed to be a simple double oxide layer was identified here to consist of at least 4 different oxide layers. It was found that the inner most oxide layer takes over the grain structure of what used to be the bulk steel material while the outer oxide layer consists of freshly grown oxides with a columnar structure. These results lead to a descriptive model of how these oxide layers grow on this steel under the harsh environments encountered in these applications.
Resumo:
The effects of temperature on hydrogen assisted fatigue crack propagation are investigated in three steels in the low-to-medium strength range; a low alloy structural steel, a super duplex stainless steel, and a super ferritic stainless steel. Significant enhancement of crack growth rates is observed in hydrogen gas at atmospheric pressure in all three materials. Failure occurs via a mechanism of time independent, transgranular, cyclic cleavage over a frequency range of 0.1-5 Hz. Increasing the temperature in hydrogen up to 80°C markedly reduces the degree of embrittlement in the structural and super ferritic steels. No such effect is observed in the duplex stainless steel until the temperature exceeds 120°C. The temperature response may be understood by considering the interaction between absorbed hydrogen and micro-structural traps, which are generated in the zone of intense plastic deformation ahead of the fatigue crack tip. © 1992.
Resumo:
In this work, a low alloy steel and a fabrication process were developed to produce U-Bolts for commercial vehicles. Thus, initially five types of no-heat treated steel were developed with different additions of chrome, nickel, and silicon to produce strain hardening effect during cold-forming processing of the U-Bolts, assuring the required mechanical properties. The new materials exhibited a fine perlite and ferrite microstructure due to aluminum and vanadium additions, well known as grain size refiners. The mechanical properties were evaluated in a servo-hydraulic test machine system-MTS 810 according to ASTM A370-03; E739 and E08m-00 standards. The microstructure and fractography analyses of the cold-formed steels were performed by using optical and scanning electronic microscope techniques. To evaluate the performance of the steels and the production process, fatigue tests were carried out under load control (tensile-tensile), R = 0.1 and f = 30 Hz. The Weibull statistic methodology was used for the analysis of the fatigue results. At the end of this work the 0.21% chrome content steel, Alloy 2, presented the best fatigue performance.
Resumo:
With the aim of investigating a laser-welded dissimilar joint of TWIP and TRIP steel sheets, the microstructure was characterized by means of OM, SEM, and EBSD to differentiate the fusion zone, heat-affected zone, and the base material. OIM was used to differentiate between ferritic, bainitic, and martensitic structures. Compositions were measured by means of optical emission spectrometry and EDX to evaluate the effect of manganese segregation. Microhardness measurements and tensile tests were performed to evaluate the mechanical properties of the joint. Residual stresses and XRD phase quantification were used to characterize the weld. Grain coarsening and martensitic areas were found in the fusion zone, and they had significant effects on the mechanical properties of the weld. The heat-affected zone of the TRIP steel and the corresponding base material showed considerable differences in the microstructure and properties. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Polarization measurements were conducted to monitor the corrosion behavior of superduplex stainless steel ASTM A995M-Gr.SA/EN 10283-Mat#1.4469(GX2CrNiMo26-7-4) when exposed to a) an electrolyte containing 22,700 parts per million (ppm) of chloride ions at seven different temperatures and b) an electrolyte at 25 GC and different chloride ion concentrations (5800, 22,700, 58,000 and 80,000 ppm of Cl(-)). The polarization curves indicate that the passive films formed are only slightly affected by NaCl concentration, but the pitting potential decreases drastically increasing the temperature, in particular >60 degrees C. The image analysis of the microstructure after potentiodynamic polarization showed that the pitting number and size vary in function of the temperature of the tested medium. Nyquist diagrams were determined by electrochemical impedance spectroscopy to characterize the resistance of the passive layer. According to Nyquist plots, the arc polarization resistance decreases increasing the temperature due to a catalytic degradation of the oxide passive films. (C) 2009 Elsevier Inc. All rights reserved.