997 resultados para Rockwell Hardness test
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Purpose: To investigate the cumulative effects of brushing (B) or immersion (I), using different cleansing agents, on the surface roughness, hardness and color stability of a heat-polymerized denture resin, Lucitone 550 (L), and a hard chairside reline resin, Tokuyama Rebase Fast II (T). Methods: A total of 316 specimens (10 x 2 mm) were fabricated. The specimens (n= 9) were divided into brushing or immersion groups according to the following agents: dentifrice/distilled water (D), 1% sodium hypochlorite (Na0C1), Corega Tabs (Pb), 1% chlorhexidine gluconate (Chx), and 0.2% peracetic acid (Ac). Brushing and immersion were tested independently. Assays were performed after 1, 3, 21, 45 and 90 blushing cycles or immersion of 10 seconds each. Data were evaluated statistically by repeated measures ANOVA. Tukey's honestly significant difference (HSD) post-hoc test was used to determine differences between means (a= 0.05). Results: For L there was no statistically significant difference in roughness, except a significant decrease in roughness by brushing with D. T showed a significant effect on the roughness after 90 immersions with Ac. Hardness values decreased for L when specimens were immersed or brushed in Na0C1 and Pb. The hardness of T decreased with increases in the repetitions (immersion or brushing), regardless of the cleaning method. Values of color stability for L resin showed significant color change after brushing with and immersion in Ac and Pb. Brushing with D exhibited a higher incidence of color change. For T there were no significant differences between cleaning agents and repetitions in immersion. A color change was noted after three brushings with the Ac, Chx, and D. Brushing with dentifrice decreased roughness of L. Immersion in or brushing with Na0C1 and Pb decreased the hardness of L. For T, hardness decreased with increases in immersions or brushing. Color changes after the immersion in or brushing with cleaning agents were clinically acceptable according to National Bureau of Standards parameters for both resins.
Resumo:
Introduction: Indirect dental composites may have adequate clinical performance. However, the literature is scarce regarding indirect composite resins and these solutions should be considered to maintain their properties. The aim of the study was to evaluate the influence of beverages, mouthwashes and bleaching agents on the hardness of indirect composite resins. Methods: Five different brands of indirect composite resins were evaluated: Adoro, Resilab, Cristobal, Sinfony and Epricord. Ten specimens of each brand were immersed in eleven different solutions: four mouthwashes (Listerine, Oral-B, Plax, Periogard), four beverages (coke soft drink, red wine, coffee, orange juice), three dental bleaching agents (16% peroxide of carbamide, 7.5% and 38% peroxide of hydrogen) and artificial saliva (control group). The Knoop hardness was measured before (baseline) and after 12, 24, 36 and 60 hours of immersion in mouthwashes; after 7, 14 and 21 days of immersion in beverages and after 7 and 14 days of immersion in dental bleaching agents. The results were analyzed using 3-way repeated measures ANOVA and Tukey’s test (p<0.05). Results: All resins presented significant decrease on hardness values after immersion process whereas this reduction was higher for Resilab and Sinfony. The latter exhibited the lowest initial values of hardness while Cristobol resin presented the highest hardness values. The mouthwashes promoted a significant decrease in the hardness of specimens.
Resumo:
Clinical performance of composite resins depends largely on their mechanical properties,and those are influenced by several factors,such as the light-curing mode. The purpose of this study was to evaluate the influence of different light sources on degree of conversion(DC), Knoop hardness(KHN) and plasticization(P) of a composite resin. Disc-shaped specimens (5 x 2 mm) of Esthet-X(Dentsply) methacrylate-based microhybrid composite were light-cured using quartz-tungsten-halogen (QTH) Optilight Plus(Gnatus) or light-emitting diode(LED) Ultraled(Dabi Atlante) curing units at 400 and 340 mW/cm2 of irradiance, respectively. After 24 h, absorption spectra of composite were obtained using Nexus 670(Nicolet)FT-IR spectrometer in order to calculate the DC.The KHN was measured in the HMV-2000(Shimadzu) microhardness tester under 50 g loads for 15 s, and P was evaluated by percentage reductio of hardness after 24 h of alcohol storage. Data were subjected to t-Student test(alpha=0.05).QTH device showed lower P and higher KHN$ than LED (p<0.05), and no difference between the light-curing units was found for DC (p>0.05). The halogen-curing unit with higher irradiance promoted higher KHN and lower softening in alcohol than LED.
Resumo:
Objectives: To determine the micro-hardness profile of two dual cure resin cements (RelyX - U100 (R), 3M-ESPE and Panavia F 2.0 (R), Kuraray) used for cementing fiber-reinforced resin posts (Fibrekor (R) - Jeneric Pentron) under three different curing protocols and two water storage times. Material and methods: Sixty 16mm long bovine incisor roots were endodontically treated and prepared for cementation of the Fibrekor posts. The cements were mixed as instructed, dispensed in the canal, the posts were seated and the curing performed as follows: a) no light activation; b) light-activation immediately after seating the post, and; c) light-activation delayed 5 minutes after seating the post. The teeth were stored in water and retrieved for analysis after 7 days and 3 months. The roots were longitudinally sectioned and the microhardness was determined at the cervical, middle and apical regions along the cement line. The data was analyzed by the three-way ANOVA test (curing mode, storage time and thirds) for each cement. The Tukey test was used for the post-hoc analysis. Results: Light-activation resulted in a significant increase in the microhardness. This was more evident for the cervical region and for the Panavia cement. Storage in water for 3 months caused a reduction of the micro-hardness for both cements. The U100 cement showed less variation in the micro-hardness regardless of the curing protocol and storage time. Conclusions: The micro-hardness of the cements was affected by the curing and storage variables and were material-dependent.
Resumo:
Objective: To evaluate the Vickers hardness of different acrylic resins for denture bases with and without the addition of glass fibres. Background: It has been suggested that different polymerisation methods, as well as the addition of glass fibre (FV) might improve the hardness of acrylic. Materials and methods: Five types of acrylic resin were tested: Vipi Wave (VW), microwave polymerisation; Vipi Flash (VF), auto-polymerisation; Lucitone (LT), QC20 (QC) and Vipi Cril (VC), conventional heat-polymerisation, all with or without glass fibre reinforcement (GFR) and distributed into 10 groups (n = 12). Specimens were then submitted to Vickers hardness testing with a 25-g load for 30 s. All data were submitted to ANOVA and Tukey's HSD test. Results: A significant statistical difference was observed with regard to the polymerisation method and the GFR (p < 0.05). Without the GFR, the acrylic resin VC presented the highest hardness values, and VF and LT presented the lowest. In the presence of GFR, VC resin still presented the highest Vickers hardness values, and VF and QC presented the lowest. Conclusions: The acrylic resin VC and VW presented higher hardness values than VF and QC resins. Moreover, GFR increased the Vickers hardness of resins VW, VC and LT.
Resumo:
Background. The use of external sources of energy may accelerate the setting rate of glass ionomer cements (GICs) allowing better initial mechanical properties. Aim. To investigate the influence of ultrasound and halogen light on the microleakage and hardness of enamel adjacent to GIC restorations, after artificial caries challenge. Design. Cavities were prepared in 60 primary canines, restored with GIC, and randomly distributed into three groups: control group (CG), light group (LG) - irradiation with a halogen lightcuring unit for 60 s, and ultrasonic group (UG) application of ultrasonic scaler device for 15 s. All specimens were then submitted to a cariogenic challenge in a pH cycling model. Half of sample in each group were immersed in methylene blue for 4 h and sectioned for dye penetration analysis. The remaining specimens were submitted to Knoop cross-sectional microhardness assessments, and mineral changes were calculated for adjacent enamel. Results. Data were compared using Kruskal-Wallis test and two- way ANOVA with 5% significance. Higher dye penetration was observed for the UG (P < 0.01). No significant mineral changes were observed between groups (P = 0.844). Conclusion. The use of halogen light- curing unit does not seem to interfere with the properties of GICs, whereas the use of ultrasound can affect its marginal sealing.
Resumo:
This study evaluated the effect of artificially accelerated aging (AAA) on the surface hardness of eight composite resins: Filtek Z250, Filtek Supreme, 4 Seasons, Herculite, P60, Tetric Ceram, Charisma, and Filtek Z100. Sixteen specimens were made from the test piece of each material, using an 8.0 × 2.0 mm teflon matrix. After 24 hours, eight specimens from each material were submitted to three surface hardness readings using a Shimadzu Microhardness Tester for 5 seconds at a load of 50 gf. The other eight specimens remained in the artificially accelerated aging machine for 382 hours and were submitted to the same surface hardness analysis. The means of each test specimen were submitted to the Kolmogorov-Smirnov test (p > 0.05), ANOVA and Tukey test (p < 0.05). With regard to hardness (F = 86.74, p < 0.0001) the analysis showed significant differences among the resin composite brands. But aging did not influence the hardness of any of the resin composites (F = 0.39, p = 0.53). In this study, there was interaction between the resin composite brand and the aging factors (F = 4.51, p < 0.0002). It was concluded that notwithstanding the type of resin, AAA did not influence surface hardness. However, with regard to hardness there was a significant difference among the resin brands.
Resumo:
Objective: The aim of this study was to evaluate the degree of conversion and hardness of different composite resins, photo-activated for 40 s with two different light guide tips, fiber optic and polymer. Methods: Five specimens were made for each group evaluated. The percentage of unreacted carbon double bonds (% C=C) was determined from the ratio of absorbance intensities of aliphatic C=C (peak at 1637 cm-1) against internal standard before and after curing of the specimen: aromatic C-C (peak at 1610 cm-1). The Vickers hardness measurements were performed in a universal testing machine. A 50 gf load was used and the indenter with a dwell time of 30 seconds. The degree of conversion and hardness mean values were analyzed separately by ANOVA and Tukey's test, with a significance level set at 5%. Results: The mean values of degree of conversion for the polymer and fiber optic light guide tip were statistically different (P<.001). The hardness mean values were statistically different among the light guide tips (P<.001), but also there was difference between top and bottom surfaces (P<.001). Conclusions: The results showed that the resins photo-activated with the fiber optic light guide tip promoted higher values for degree of conversion and hardness.
Resumo:
Microhardness maps of cross-sections of high-pressure diecast test bars of AZ91 have been determined. Specimens with rectangular cross-sections, 1, 2 and 3 mm thick, or with a circular cross-section 6.4 mm in diameter, have been studied. The hardness is generally higher near the edges in all specimens, and more so near the corners of the rectangular specimens. The hardness at the center of the castings is generally lower, due to a coarser solidification microstructure and the concentration of porosity. The evidence confirms that the surface of the castings is harder than the core, but it does not support the concept of a skin with a sharp. and definable boundary. This harder layer is irregular in hardness and depth and is not equally hard on opposite sides of the casting. The mean hardness obtained by integrating the microhardness maps over the entire cross-section increased with decreasing thickness of the bars, and was found to be in good correlation with each bar's yield strength. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Objective: The aim of this study was to evaluate the degree of conversion and hardness of different composite resins, photo-activated for 40 s with two different light guide tips, fiber optic and polymer. Methods: Five specimens were made for each group evaluated. The percentage of unreacted carbon double bonds (% C═C) was determined from the ratio of absorbance intensities of aliphatic C═C (peak at 1637 cm−1) against internal standard before and after curing of the specimen: aromatic C-C (peak at 1610 cm−1). The Vickers hardness measurements were performed in a universal testing machine. A 50 gf load was used and the indenter with a dwell time of 30 seconds. The degree of conversion and hardness mean values were analyzed separately by ANOVA and Tukey’s test, with a significance level set at 5%. Results: The mean values of degree of conversion for the polymer and fiber optic light guide tip were statistically different (P<.001). The hardness mean values were statistically different among the light guide tips (P<.001), but also there was difference between top and bottom surfaces (P<.001). Conclusions: The results showed that the resins photo-activated with the fiber optic light guide tip promoted higher values for degree of conversion and hardness.
Resumo:
The aim of the study was to develop a culturally adapted translation of the 12-item smell identification test from Sniffin' Sticks (SS-12) for the Estonian population in order to help diagnose Parkinson's disease (PD). A standard translation of the SS-12 was created and 150 healthy Estonians were questioned about the smells used as response options in the test. Unfamiliar smells were replaced by culturally familiar options. The adapted SS-12 was applied to 70 controls in all age groups, and thereafter to 50 PD patients and 50 age- and sex-matched controls. 14 response options from 48 used in the SS-12 were replaced with familiar smells in an adapted version, in which the mean rate of correct response was 87% (range 73-99) compared to 83% with the literal translation (range 50-98). In PD patients, the average adapted SS-12 score (5.4/12) was significantly lower than in controls (average score 8.9/12), p < 0.0001. A multiple linear regression using the score in the SS-12 as the outcome measure showed that diagnosis and age independently influenced the result of the SS-12. A logistic regression using the SS-12 and age as covariates showed that the SS-12 (but not age) correctly classified 79.0% of subjects into the PD and control category, using a cut-off of <7 gave a sensitivity of 76% and specificity of 86% for the diagnosis of PD. The developed SS-12 cultural adaption is appropriate for testing olfaction in Estonia for the purpose of PD diagnosis.
Resumo:
to investigate the pulmonary response to exercise of non-morbidly obese adolescents, considering the gender. a prospective cross-sectional study was conducted with 92 adolescents (47 obese and 45 eutrophic), divided in four groups according to obesity and gender. Anthropometric parameters, pulmonary function (spirometry and oxygen saturation [SatO2]), heart rate (HR), blood pressure (BP), respiratory rate (RR), and respiratory muscle strength were measured. Pulmonary function parameters were measured before, during, and after the exercise test. BP and HR were higher in obese individuals during the exercise test (p = 0.0001). SatO2 values decreased during exercise in obese adolescents (p = 0.0001). Obese males had higher levels of maximum inspiratory and expiratory pressures (p = 0.0002) when compared to obese and eutrophic females. Obese males showed lower values of maximum voluntary ventilation, forced vital capacity, and forced expiratory volume in the first second when compared to eutrophic males, before and after exercise (p = 0.0005). Obese females had greater inspiratory capacity compared to eutrophic females (p = 0.0001). Expiratory reserve volume was lower in obese subjects when compared to controls (p ≤ 0,05). obese adolescents presented changes in pulmonary function at rest and these changes remained present during exercise. The spirometric and cardiorespiratory values were different in the four study groups. The present data demonstrated that, in spite of differences in lung growth, the model of fat distribution alters pulmonary function differently in obese female and male adolescents.
Resumo:
To evaluate the influence of a fluorescent dye (rhodamine B) on the physical and mechanical properties of three different luting cements: a conventional adhesive luting cement (RelyX ARC, 3M/ESPE), a self-adhesive luting cement (RelyX U-200, 3M/ESPE), and a self-etching and self-adhesive luting cement (SeT PP, SDI). The cements were mixed with 0.03 wt% rhodamine B, formed into bar-shaped specimens (n = 10), and light cured using an LED curing unit (Radii, SDI) with a radiant exposure of 32 J/cm(2) . The Knoop hardness (KHN), flexural strength (FS), and Young's modulus (YM) analyses were evaluated after storage for 24 h. Outcomes were subjected to two-way ANOVA and Tukey's test (P = 0.05) for multiple comparisons. No significant differences in FS or YM were observed among the tested groups (P ≥ 0.05); the addition of rhodamine B increased the hardness of the luting cements tested. The addition of a fluorescent agent at 0.03 wt% concentration does not negatively affect the physical-mechanical properties of the luting cement polymerization behavior.
Resumo:
To assess binocular detection grating acuity using the LEA GRATINGS test to establish age-related norms in healthy infants during their first 3 months of life. In this prospective, longitudinal study of healthy infants with clear red reflex at birth, responses to gratings were measured at 1, 2, and 3 months of age using LEA gratings at a distance of 28 cm. The results were recorded as detection grating acuity values, which were arranged in frequency tables and converted to a one-octave scale for statistical analysis. For the repeated measurements, analysis of variance (ANOVA) was used to compare the detection grating acuity results between ages. A total of 133 infants were included. The binocular responses to gratings showed development toward higher mean values and spatial frequencies, ranging from 0.55 ± 0.70 cycles per degree (cpd), or 1.74 ± 0.21 logMAR, in month 1 to 3.11 ± 0.54 cpd, or 0.98 ± 0.16 logMAR, in month 3. Repeated ANOVA indicated differences among grating acuity values in the three age groups. The LEA GRATINGS test allowed assessment of detection grating acuity and its development in a cohort of healthy infants during their first 3 months of life.