923 resultados para NB
Resumo:
We describe extensive studies on a family of perovskite oxides that are ferroelectric and ferromagnetic at ambient temperatures. The data include x-ray diffraction, Raman spectroscopy, measurements of ferroelectric and magnetic hysteresis, dielectric constants, Curie temperatures, electron microscopy
(both scanning electron microscope and transmission electron microscopy (TEM)) studies, and both longitudinal and transverse magnetoelectric constants a33 and a31. The study extends earlier work to lower Fe, Ta, and Nb concentrations at the B-site (from 15%–20% down to 5%). The magnetoelectric
constants increase supralinearly with Fe concentrations, supporting the earlier conclusions of a key role for Fe spin clustering. The room-temperature orthorhombic C2v point group symmetry inferred from earlier x-ray diffraction studies is confirmed via TEM, and the primitive unit cell size is found to be the basic perovskite Z¼1 structure of BaTiO3, also the sequence of phase transitions with increasing temperature from rhombohedral to orthorhombic to tetragonal to cubic mimics barium titanate.
Resumo:
Epitaxial (001)-oriented 0.7Pb(Mg0.33Nb0.67)O3-0.3PbTiO3 (PMN-PT) thin films were deposited by pulsed laser deposition on vicinal SrTiO3 (001) substrates using La0.7Sr0.3MnO3 as bottom electrode. Detailed microstructural investigations of these films were carried out using X-ray diffraction (XRD), atomic force microscopy (AFM) and transmission electron microscopy (TEM). Polarization-field hysteresis curves were measured at room temperature. Spontaneous polarization P s , remnant polarization P r and coercive voltage V c were found to be 25 μC/cm2, 15 μC/cm2 and 0.81 V, respectively. Field dependent dielectric constant measurements exhibited butterfly shaped curves, indicating the true ferroelectric nature of these films at room temperature. The dielectric constant and the dielectric loss at 100 kHz were found to be 238 and 0.14, respectively. The local piezoelectric properties of PMN-PT films were investigated by piezoelectric force microscopy and were found to exhibit a local piezoelectric coefficient of 7.8 pm/V.
Analysis of deformation behavior and workability of advanced 9Cr-Nb-V ferritic heat resistant steels
Resumo:
Hot compression tests were carried out on 9Cr–Nb–V heat resistant steels in the temperature range of 600–1200 °C and the strain rate range of 10−2–100 s−1 to study their deformation characteristics. The full recrystallization temperature and the carbon-free bainite phase transformation temperature were determined by the slope-change points in the curve of mean flow stress versus the inverse of temperature. The parameters of the constitutive equation for the experimental steels were calculated, including the stress exponent and the activation energy. The lower carbon content in steel would increase the fraction of precipitates by increasing the volume of dynamic strain-induced (DSIT) ferrite during deformation. The ln(εc) versus ln(Z) and the ln(σc) versus ln(Z) plots for both steels have similar trends. The efficiency of power dissipation maps with instability maps merged together show excellent workability from the strain of 0.05 to 0.6. The microstructure of the experimental steels was fully recrystallized upon deformation at low Z value owing to the dynamic recrystallization (DRX), and exhibited a necklace structure under the condition of 1050 °C/0.1 s−1 due to the suppression of the secondary flow of DRX. However, there were barely any DRX grains but elongated pancake grains under the condition of 1000 °C/1 s−1 because of the suppression of the metadynamic recrystallization (MDRX).
Resumo:
The formation of epitaxial BaTiO3/SrTiO3 multilayers; is studied in terms of the growth mechanism by investigating surface morphologies, crystalline orientations, microstructures, and structures of the interfaces, as well as by determining the dielectric properties. Under specific conditions, the epitaxial BaTiO3 films follow a layer-then-island (Stranski-Krastanov) mechanism on SrTiO3 (001)-oriented substrates. In view of actual efforts made to grow epitaxial superlattices involving very thin individual layers of BaTiO3 and/or SrTiO3, we have determined that the BaTiO3 films Of up to 6,nm thickness do not show any defects and have a sharp BaTiO3-on-SrTiO3 interface. On the contrary, SrTiO3-on-BaTiO3 interfaces within multilayers are rough, probably due to the different growth mechanisms of the two different materials, or due to a difference in the morphological stability of the growth surfaces caused by different surface energies of BaTiO3 and SrTiO3 and by different mobilities of the Ba and Sr atoms reaching the SrTi3 and BaTiO3 layers, respectively.
Resumo:
The growth mechanism of epitaxial BaTiO3 films on vicinal Nb-doped SrTiO3 (srTiO(3):Nb) (001) substrate surfaces was studied in terms of surface morphology, crystalline orientation, microstructure, and film/substrate interface. Well-oriented BaTiO3 thin films were grown on SrTiO3 substrates with well-defined terraces by pulsed laser deposition. The regularly terraced TiO2-terminated surfaces of vicinal SrTiO3:Nb (001) substrates were prepared by a definite chemical and thermal treatment. Under our conditions, BaTiO3 seems to grow with a layer-then-island (Stranski-Krastanov) growth mechanism. In order to investigate the orientation and crystallinity of the BaTiO3 films, x-ray diffraction and high-resolution transmission election microscopy were performed. Ferroelectricity of the BaTiO3 films was proved by electrical measurements performed on Pt/BaTiO3/SrTiO3:Nb heterostructures.
Resumo:
Energies and lifetimes are reported for the lowest 375 levels of five Br-like ions, namely SrIV, YV, ZrVI, NbVII, and MoVIII, mostly belonging to the 4s<sup>2</sup>4p<sup>5</sup>, 4s<sup>2</sup>4p<sup>4</sup>4ℓ, 4s4p<sup>6</sup>, 4s<sup>2</sup>4p<sup>4</sup>5ℓ, 4s<sup>2</sup>4p<sup>3</sup>4d<sup>2</sup>, 4s4p<sup>5</sup>4ℓ, and 4s4p<sup>5</sup>5ℓ configurations. Extensive configuration interaction has been included and the general-purpose relativistic atomic structure package (grasp) has been adopted for the calculations. Additionally, radiative rates are listed among these levels for all E1, E2, M1, and M2 transitions. From a comparison with the measurements, the majority of our energy levels are assessed to be accurate to better than 2%, although discrepancies between theory and experiment for a few are up to 6%. An accuracy assessment of the calculated radiative rates (and lifetimes) is more difficult, because no prior results exist for these ions.
Resumo:
Tesis (Maestría en Ciencias de la Ingeniería Mécanica con Especialidad en Materiales) UANL
Resumo:
Tesis (Maestría en Ciencias de la Ingeniería Mécanica con especialidad en Materiales) U.A.N.L.
Resumo:
Tesis (Maestro en Ciencias con Orientación en Química de los Materiales) UANL, 2012.