996 resultados para Dentin bonding agents
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Objective: The aim of this study was to compare the correspondence between gap formation and apical microleakage in root canals filled with epoxy resin-based (AH Plus) combined or not with resinous primer or with a dimethacrylate-based root canal sealer (Epiphany). Material and Methods: Thirty-nine lower single-rooted human premolars were filled by the lateral condensation technique (LC) and immersed in a 50-wt% aqueous silver nitrate solution at 37 degrees C (24 h). After longitudinal sectioning, epoxy resin replicas were made from the tooth specimens. Both the replicas and the specimens were prepared for scanning electron microscopy (SEM). The gaps were observed in the replicas. Apical microleakage was detected in the specimens by SEM/energy dispersive spectroscopy (SEM/EDS). The data were analyzed statistically using an Ordinal Logistic Regression model and Analysis of Correspondence (alpha=0.05). Results: Epiphany presented more regions containing gaps between dentin and sealer (p<0.05). There was correspondence between the presence of gaps and microleakage (p<0.05). Microleakage was similar among the root-filling materials (p>0.05). Conclusions: The resinous primer did not improve the sealing ability of AH Plus sealer and the presence of gaps had an effect on apical microleakage for all materials.
Resumo:
Aim: To assess the immediate influence of dentine bonding systems (DBS) associated with 2% chlorhexidine digluconate (CHX) on glass-fibre post-bond strength to root dentine, in terms of coronal, middle and apical thirds. Methodology: Sixty bovine roots were root filled and randomly assigned to 1 of 6 groups (n = 10): SBMP (3-step etch-and-rinse system, Scotchbond Multi-Purpose), SB (2-step etch-and-rinse system, Single Bond 2), SE (2-step self-etching system, Clearfil SE Bond) and SBMP-CHX, SB-CHX and SE-CHX, respectively, associated with CHX. For all groups, a glassfibre post was luted with a dual-cure resin cement, RelyX ARC. After 7-day storage, specimens were subjected to the push-out test. Failure modes were analysed under optical microscopy (40x). Bond strength values were statistically analysed by two-way ANOVA and Bonferroni tests (P < 0.05). Results: The effect of DBS was significant (P < 0.05), and SE reached higher bond strength in comparison with the other DBS tested. CHX association did not show improvement with any DBS (P > 0.05); rather, it negatively affected SE, which was detected for all thirds. There was no difference between thirds (P > 0.05), except for the SE-CHX, which presented lower values for the apical third (P < 0.05). Adhesive cement/dentine adhesive failure was predominant for all groups. CHX did not influence the failure mode for any DBS (P > 0.05). Conclusions: The performance of the dentine bonding systems was material dependent. CHX did not improve immediate bond strength; however, CHX negatively affected the bond strength of the self-etching system, especially in the third apical
Resumo:
A utilização de espigões em dentes tratados endodonticamente é um dos temas mais estudados em Medicina Dentária. As opiniões são divergentes em relação aos procedimentos clínicos e materiais a serem utilizados para a colocação e remoção de espigões. O objetivo deste trabalho foi realizar uma revisão bibliográfica de forma a organizar conceitos e princípios clínicos para melhor esclarecer os fatores que determinam a necessidade de colocação, utilização e escolha do tipo de espigão, sua cimentação e técnicas para a remoção. Foram analisadas as características e propriedades dos cimentos de fosfato de zinco, ionômero de vidro, cimentos resinosos de polimerização química, polimerização dupla, foto-polimerizável e os sistemas adesivos etch and rinse, self etch e autoadesivos, bem como as técnicas para a remoção de espigões cimentados com diferentes cimentos e sistemas adesivos para depois acessar o remanescente de guta percha para o retratamento endodôntico. Foi feita uma pesquisa bibliográfica na base de dados electrónica PubMed, Google Scholar e RCAAP com as seguintes palavras chave: “Espigões”; “Retratamento Endodôntico”; “Ionómero de Vidro”; “Fosfato de Zinco”; “Cimentos Resinosos”; “Posts”; “Endodontic Retreatment”; “Glass Ionomer”; Zinc-phosphate”; “Resin Cements"; “Push Out Test”; “Posts AND Removal”. Concluiu-se que a cimentação de espigões pré-fabricados de fibra de vidro com cimentos resinosos de dupla polimerização associados aos sistemas adesivos self etch estão gradualmente substituindo os outros tipos de espigões e demais cimentos e possibilitam restaurar o dente de forma adequada e duradoura. E o uso de ultrassons apresenta maior eficácia e segurança na remoção dos espigões.
Resumo:
The aim was to compare eight types of luting agents when used to bond six indirect, laboratory restorative materials to dentin. Cylinders of the six restorative materials (Esteticor Avenir [gold alloy], Tritan [titanium], NobelRondo [feldspathic porcelain], Finesse All-Ceramic [leucite-glass ceramic], Lava [zirconia], and Sinfony [resin composite]) were ground and air-abraded. Cylinders of feldspathic porcelain and glass ceramic were additionally etched with hydrofluoric acid and were silane-treated. The cylinders were luted to ground human dentin with eight luting agents (DeTrey Zinc [zinc phosphate cement], Fuji I [conventional glass ionomer cement], Fuji Plus [resin-modified glass ionomer cement], Variolink II [conventional etch-and-rinse resin cement], Panavia F2.0 and Multilink [self-etch resin cements], and RelyX Unicem Aplicap and Maxcem [self-adhesive resin cements]). After water storage at 37°C for one week, the shear bond strength of the specimens (n=8/group) was measured, and the fracture mode was stereomicroscopically examined. Bond strength data were analyzed with two-factorial analysis of variance (ANOVA) followed by Newman-Keuls' Multiple Range Test (?=0.05). Both the restorative material and the luting agent had a significant effect on bond strength, and significant interaction was noted between the two variables. Zinc phosphate cement and glass ionomer cements produced the lowest bond strengths, whereas the highest bond strengths were found with the two self-etch and one of the self-adhesive resin cements. Generally, the fracture mode varied markedly with the restorative material. The luting agents had a bigger influence on bond strength between restorative materials and dentin than was seen with the restorative material.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Objectives. To evaluate the response of the pulpo-dentin complex following application of a resin-modified glass-ionomer cement or an adhesive system in deep cavities performed in human teeth.Methods. Deep class V cavities were prepared on the buccal surface of 26 premolars. In Group I the cavity walls (dentin) and enamel were conditioned with 32% phosphoric acid and the dentin adhesive system One Step (Bisco, Inc., Itasca, IL, USA) was applied. In Groups 2 and 3, before total etching and application of bonding agent, the cavity floor was lined with the resin-modified glass-ionomer cement-Vitrebond (3M ESPE Dental Products Division, St. Paul, MN, USA) or the calcium hydroxide cement-Dycal (control group, Dentsply, Mildford, DE, USA), respectively. The cavities were restored using light-cured Z-100 composite resin (3M ESPE). The teeth were extracted between 5 and 30 days and prepared for microscopic assessment. Serial sections were stained with H/E, Masson's trichrome, and Brown and Brenn techniques.Results. In Group 1, the inflammatory response was more evident than in Groups 2 and 3. Diffusion of dental material components across dentinal tubules was observed only in Group 1, in which the intensity of the pulp response increased as the remaining dentin thickness decreased. Bacteria were evidenced in the lateral walls of two samples (Group 2) which exhibited no inflammatory response or tissue disorganization.Conclusions. Based on the experimental conditions, it was concluded total acid etching followed by application of One Step bonding agent cannot be recommended as adequate procedures. In this clinical condition the cavity walls should be lined with a biocompatible dental material, such as Vitrebond or Dycal. 2003 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
Purpose: To evaluate the effect of cyclical mechanical loading on the bond strength of a fiber and a zirconia post bonded to root dentin.Materials and Methods: Forty single-rooted human teeth (maxillary incisors and canines) were sectioned, and the root canals were prepared at 12 mm. Twenty randomly seleced specimens received a quartz fiber post (FRC) (D.T. Light-Post) and 20 others received a zirconia post (ZR) (Cosmopost). The posts were resin luted (All Bond 2 + resin cement Duo-link) and each specimen was embedded in epoxy resin inside a PVC cylinder. Ten specimens with FRC post and 10 specimens with ZR post were submitted to fatigue testing (2,000,000 cycles; load: 50 N; angle of 45 degrees; frequency: 8 Hz), while the other 20 specimens were not fatigued. Thus, 4 groups were formed: G1: FRC+O cycles; G2: FRC+2,000,000 cycles; G3: ZR+O cycles; G4: ZR+2,000,000 cycles. Later, the specimens were cut perpendicular to their long axis to form 2-mm-thick disk-shaped samples (4 sections/specimen), which were submitted to the push-out test (1 mm/min). The mean bond strength values (MPa) were calculated for each tooth (n = 10) and data were submitted to statistical analysis (alpha = 0.05).Results: Two-way ANOVA revealed that the bond strength was significantly affected by mechanical cycling (p = 0.0014) and root post (p = 0.0325). The interaction was also statistically significant (p = 0.0010). Tukey's test showed that the mechanical cycling did not affect the bonding of FRC to root dentin, while fatigue impaired the bonding of zirconium to root dentin.Conclusion: (1) the bond strength of the FRC post to root dentin was not reduced after fatigue testing, whereas the bonding of the zirconia post was significantly affected by the fatigue. (2) Cyclical mechanical loading appears to damage the bond strength of the rigid post only.
Resumo:
Purpose: The aim of this study was to evaluate the influence of dentin abrasion on the microshear bond strength of two self-etching adhesive systems, using either an ultrasound diamond bur or a high-speed diamond bur.Materials and Methods: Twenty noncarious human third molars were sectioned mesiodistally into halves. The enamel was ground to expose a flat dentin surface on both sections. The dentinal surfaces were randomly assigned to two groups, depending on the method of smear layer preparation: ultrasound diamond bur (UB) or conventional diamond bur (CB). The prepared dentin surfaces received one of two self-etching systems: Clearfil SE Bond (CF) and One-Up Bond F (OB). A composite cylinder with a 0.95-mm diameter was bonded to each specimen and the microshear bond test was performed. The results were expressed in MPa and were subjected to two-way analysis of variance (ANOVA) and Tukey's test (alpha = 0.05).Results: There was no significant difference in dentin bond strength when comparing the conventional and ultrasonic abrasion methods. When the adhesive systems were compared, Clearfil SE Bond achieved higher bond strength means than did One-Up Bond F.Conclusion: The dentin surface preparation method did not influence the microshear bond strength and the Clearfil SE Bond adhesive system, independent of bur type used, Clearfil SE Bond showed higher bond strengths than did the One-Up Bond F adhesive system.
Resumo:
This study sought to use scanning electronic microscopy (SEM) to evaluate the dentinal tubule occlusion potential of different desensitizing agents. Ten slices of bovine dentin were divided into six fragments, cleaned (using ultrasound), and etched for 15 seconds with a 35% phosphoric acid solution. All but one of the groups received a different desensitizing agent; the sixth group served as a control and received no additional treatment. After the agents were applied, the dentin specimens were analyzed by SEM and scores were assigned based on the extent of tubular obliteration. Only three agents demonstrated tubular sealing that was significantly different from that of the control group.
Resumo:
Ceramics have been widely used for esthetic and functional improvements. The resin cement is the material of choice for bonding ceramics to dental substrate and it can also dictate the final esthetic appearance and strength of the restoration. The correct use of the wide spectrum of resin luting agents available depends on the dental tooth substrate. This article presents three-year clinical results of a 41 years old female patient B.H.C complaining about her unattractive smile. Two all-ceramic crowns and two laminates veneers were placed in the maxillary incisors and cemented with a self-adhesive resin luting cement and conventional resin luting cement, respectively. After a three-year follow-up, the restorations and cement/teeth interface were clinically perfect with no chipping, fractures or discoloration. Proper use of different resin luting cements shows clinical appropriate behavior after a three-year follow-up. Self-adhesive resin luting cement may be used for cementing all-ceramic crowns with high predictability of success, mainly if there is a large dentin surface available for bonding and no enamel at the finish line. Otherwise, conventional resin luting agent should be used for achieving an adequate bonding strength to enamel.
Resumo:
The purpose of this in vitro study was to evaluate the effect of neodymium:yttrium-aluminum-garnet (Nd:YAG) laser irradiation on intracanal dentin surface by SEM analysis and its interference in the apical seal of filled canals. After endodontic treatment procedures, 34 maxillary human incisors were randomly assigned to 2 groups. In the negative control group (n=17), no additional treatment was performed and teeth were filled with vertically condensed gutta-percha; in the laser-treated group (n=17), the root canals were irradiated with Nd:YAG laser (1.5 W, 100 mJ, 15 Hz) before filling as described for the control group. Two specimens of each group were prepared for SEM analysis to evaluate the presence and extent of morphological changes and removal of debris; the other specimens were immersed in 0.5% methylene blue dye (pH 7.2) for 24 h for evaluation of the linear dye leakage at the apical third. SEM analysis of the laser-treated group showed dentin fusion and resolidification without smear layer or debris. The Student's t-test showed that the laser-treated group had significantly less leakage in apical third than the control group. Within the limitations of this study, it may be concluded that the morphological changes on the apical intraradicular dentin surface caused by Nd:YAG laser resulted in less linear dye apical leakage.
Inactivation of Matrix-bound Matrix Metalloproteinases by Cross-linking Agents in Acid-etched Dentin
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)