918 resultados para Unconfined compressive strength
Resumo:
In recent years, various types of organic and inorganic materials have been investigated for use as soil stabilizing agents in the construction of highways and airports. Since the properties and environmental conditions of soils vary so greatly from place to place, a stabilizing agent that is suitable for one type of soil may not be satisfactory for another. As a result, it is often desirable to evaluate several stabilizing agents under varying treatment conditions before deciding on a specific one to be used with a given soil. In addition many research programs have been initiated which investigate the effects of these stabilizing agents upon soils.
Resumo:
The results of a combined experimental program and numerical modeling program to evaluate the behavior of ungrouted hollow concrete blocks prisms under uniaxial compression are addressed. In the numerical program, three distinct approaches have been considered using a continuum model with a smeared approach, namely plane-stress, plane-strain and three-dimensional conditions. The response of the numerical simulations is compared with experimental data of masonry prisms using concrete blocks specifically designed for this purpose. The elastic and inelastic parameters were acquired from laboratory tests on concrete and mortar samples that constitute the blocks and the bed joint of the prisms. The results from the numerical simulations are discussed with respect to the ability to reproduce the global response of the experimental tests, and with respect to the failure behavior obtained. Good agreement between experimental and numerical results was found for the peak load and for the failure mode using the three-dimensional model, on four different sets of block/mortar types. Less good agreement was found for plain stress and plain strain models.
Resumo:
The central issue for pillar design in underground coal mining is the in situ uniaxial compressive strength (sigma (cm)). The paper proposes a new method for estimating in situ uniaxial compressive strength in coal seams based on laboratory strength and P wave propagation velocity. It describes the collection of samples in the Bonito coal seam, Fontanella Mine, southern Brazil, the techniques used for the structural mapping of the coal seam and determination of seismic wave propagation velocity as well as the laboratory procedures used to determine the strength and ultrasonic wave velocity. The results obtained using the new methodology are compared with those from seven other techniques for estimating in situ rock mass uniaxial compressive strength.
Resumo:
The reuse of structural concrete elements to produce new concrete aggregates is accepted as an alternative to dumping them and is favourable to the sustainability of natural reserves. Even though the construction sector is familiar with the use of coarse recycled concrete aggregates, the recycled concrete fines are classified as less noble resources. This research sets out to limit the disadvantages associated with the performance of concrete containing fine recycled concrete aggregates through the use of superplasticisers. Two types of latest generation superplasticisers were used that differ in terms of water reduction capacity and robustness, and the workability, density and compressive strength of each of the compositions analysed were then compared: a reference concrete, with no plasticisers, and concrete mixes with the superplasticisers. For each concrete family mixes with 0%, 10%, 30%, 50% and 100% replacement ratios of fine natural aggregates (FNA) by fine recycled concrete aggregates (FRA) were analysed. Concrete with incorporation of recycled aggregates was found to have poorer relative performance. The mechanical performance of concrete with recycled aggregates and superplasticisers was generally superior to that of the reference concrete with no admixtures and of conventional concrete with lower performance superplasticisers.
Resumo:
The compressive strength of concrete is an important factor in the design of concrete structures and pavements. To assure the quality of the concrete placed at the project, concrete compressive cylinders are made at the jobsite. These cylinders undergo a destructive test to determine their compressive strength. However, the determination of concrete compressive strength of the concrete actually in the structure or pavement is frequently desirable. For this reason, a nondestructive test of the concrete is required. A nondestructive test of concrete compressive strength should be economical, easily performed by field personnel, and capable of producing accurate, reproducible results. The nondestructive test should be capable of detecting the extent of poor concrete in a pavement or structure due to improper handling, placement, or variations in mixing or materials.
Resumo:
The current study investigated the effect of fly ash class, source and amount on the compressive strength and freeze-thaw durability of fly ash concrete. Concrete aggregates of varying quality were also included as test variables. The current results and those obtained from previous laboratory and field work indicate that compressive strength can·be affected by fly ash class, source and amount while aggregate quality is shown to have no effect on strength. Freeze-thaw durability of fly ash concrete is strongly affected by aggregate quality and to a lesser degree by fly ash class, amount and source.
Resumo:
The interrelation of curing time, curing temperature, strength, and reactions in lime-bentonite-water mixtures was examined. Samples were molded at constant density and moisture content and then cured for periods of from 1 to 56 days at constant temperatures that ranged from 5C to 60C. After the appropriate curing time the samples were tested for unconfined compressive strength. The broken samples were then analyzed by x-ray diffractometer and spectrophotometer to determine the identity of the reaction products present after each curing period. It was found that the strength gain of lime-clay mixtures cured at different temperatures is due to different phases of the complex reaction, lime & clay to CSH(gel) to CSH(II) to CSH(I) to tobermorite. The farther the reaction proceeds, the higher the strength. There was also evidence of lattice substitutions in the structure of the calcium silicate hydrates at curing temperatures of 50C and higher. No consistent relationship between time, temperature, strength, and the S/A ration of reaction products existed, but in order to achieve high strengths the apparent C/S ration had to be less than two. The curing temperature had an effect on the strength developed by a given amount of reacted silica in the cured lime-clay mixture, but at a given curing temperature the cured sample that had the largest amount of reacted silica gave the highest strength. Evidence was found to indicate that during the clay reaction some calcium is indeed adsorbed onto the clay structure rather than entering into a pozzolanic reaction. Finally, it was determined that it is possible to determine the amount of silica and alumina in lime-clay reaction products by spectrophotometric analysis with sufficient accuracy for comparison purposes. The spectrophotometric analysis techniques used during the investigation were simple and were not time consuming.
Resumo:
Researches are always in quest for finding innovative methods for ground improvement using sustainable and environmental friendly solutions. Theproduction of large quantity of biowastes all over the world faces serious problems of handling and disposal. Coir pith is a biowaste from coir industry and sugarcane baggase is another biowaste obtained after extractingjuice from sugar cane. So the present study is an investigation into the effect of coir pith and sugarcane baggase on some geotechnical properties of red earth. The investigation includes study on variation of properties such as O.M.C, maximum dry density, C.B.R. values,unconfined compressive strength and permeability when these materials are included in soil. Several conclusions are arrived at, on the basis of the experiments conducted and it may be helpful for predicting the behavior of such soil matrix
Resumo:
The aim of this study was to evaluate the effect of ageing in distilled water on the hardness and compressive strength of a direct composite resin Z100, a feldspatic porcelain (Noritake) and three indirect composites (Artglass, Solidex and Targis). For the Vickers hardness tests, five disk-shaped specimens (2 x 4 mm) of each material were prepared according to the manufacturers' instructions. The hardness tests were conducted using a Vickers diamond indentor. Compressive strength measurements were recorded on cylindrical specimens with a diameter of 6 mm and a length of 12 mm. The compression tests were carried out with a constant cross-head speed of 0.5 mm min(-1) on a mechanical test machine. For each material, 10 specimens were tested after 7 days of dry storage at 37 +/- 1 degreesC and 10 specimens were tested after water storage at 37 +/- 1 degreesC for 180 days. Noritake porcelain specimens showed higher hardness values than the composites. Among the composite materials, Z100 promoted the highest VHN values, regardless of the ageing periods. The results showed that Solidex and Z100 had the highest compressive strength values. Ageing in water reduced the hardness for all composites, but had no long-term effect on the compressive strength.
Resumo:
The aim of this study was to evaluate the compressive strength of microhybrid (Filtek™ Z250) and nanofilled (Filtek™ Supreme XT) composite resins photo-activated with two different light guide tips, fiber optic and polymer, coupled with one LED. The power density was 653 mW cm -2 when using the fiber optic light tip and 596 mW cm-2 with the polymer. After storage in distilled water at 37 ± 2 °C for seven days, the samples were subjected to mechanical testing of compressive strength in an EMIC universal mechanical testing machine with a load cell of 5 kN and speed of 0.5 mm min-1. The statistical analysis was performed using ANOVA with a confidence interval of 95% and Tamhane's test. The results showed that the mean values of compressive strength were not influenced by the different light tips (p > 0.05). However, a statistical difference was observed (p < 0.001) between the microhybrid composite resin photo-activated with the fiber optic light tip and the nanofilled composite resin. Based on these results, it can be concluded that microhybrid composite resin photo-activated with the fiber optic light tip showed better results than nanofilled, regardless of the tip used, and the type of the light tip did not influence the compressive strength of either composite. Thus, the presented results suggest that both the fiber optic and polymer light guide tips provide adequate compressive strength to be used to make restorations. However, the fiber optic light tip associated with microhybrid composite resin may be an interesting option for restorations mainly in posterior teeth. © 2013 Astro Ltd.
Resumo:
Este estudo comparou a resistência à compressão de uma resina composta e de um compômero, fotoativados com luz halógena convencional de quarto-tungstênio (QTH) (XL 300, 3M/SPE) e LED azul (SmartLite PS; Dentsply/De Trey). Foram confeccionados 40 espécimes em forma de disco usando uma matriz bipartida de politetrafluoretileno (4,0 mm de diâmetro x 8,0 mm de altura) em que o material foi inserido incrementalmente. O tempo de polimerização de cada incremento foi de 40 s para a luz halógena convencional e de 10 s para o LED. Os espécimes foram aleatoriamente alocados em 4 grupos (n=10), de acordo com a fonte de luz e com o material restaurador. Depois de armazenadas em água destilada a 37°C ± 2°C por 24 h, a resistência à compressão dos espécimes foi testada em uma máquina universal de ensaios com célula de carga de 500 kgf a uma velocidade de carregamento de 0,5 mm/min. Os dados (em MPa) foram analisados estatisticamente por ANOVA e teste de Student-Newman-Keuls (p<0,05). Para a resina composta, a fotopolimerização com luz halógena não produziu diferença estatisticamente significante (p>0,05) em sua resistência à compressão quando comparada à fotopolimerização com LED. Contudo, a fotopolimerização do compômero com a luz halógena resultou em uma resistência à compressão significativamente maior que a feita o LED (p>0,05). A resina composta apresentou resistência à compressão significativamente maior que a do compômero, independente da fonte de luz. Concluiu-se que a resistência à compressão dos materiais fotopolimerizados com luz halógena e LED foi influenciada pela densidade de energia empregada e pela composição química dos materiais restauradores estéticos.
Resumo:
The present study aims to compare three types of internal fixation for fractures of the mandibular angle. Mechanical testing was performed on replicas of polyurethane hemimandibles sectioned at the angle region to simulate a fracture and fixed with three different hardwares. Fixation devices enrolled on this survey included the grid plates with and without an intermediate bar and the method described by Champy and colleagues in 1978 and the sample consisted of 10 hemimandibles for each group. Vertical loadings were applied on each hemimandible and recorded after a vertical displacement of 3 and 5 mm. Statistical analysis was made by means of the variance analysis (ANOVA) and the Duncan test with a significance level of 5%. The Champy technique showed a statistically significant increased resistance when compared to the grid plates after vertical displacements of 3 and 5 mm. The results of this survey suggest that the Champy technique, when compared to the grid plate positioned at the middle of the mandibular bone (placement site selected for this study), is more resistant than the grid plate and that the inclusion or not of an intermediate bar to the grid plates does not improve its resistance after linear vertical loadings.