Three-point bending experiments were performed on as-cast and annealed samples of Zr52.5Cu17.9Ni14.6Al10Ti5 (Vit105) bulk metallic glasses over a wide range of temperatures varying from room temperature (293 K) to liquid nitrogen temperature (77 K). The results demonstrated that the free volume decrease due to annealing and/or cryogenic temperature can reduce the propensity for the formation of multiple shear bands and hence deteriorate plastic deformation ability. We clearly observed a sharp ductile-to-brittle transition (DBT), across which microscopic fracture feature transfers from micro-scale vein patterns to nano-scale periodic corrugations. Macroscopically, the corresponding fracture mode changes from ductile shear fracture to brittle tensile fracture. The shear transformation zone volume, taking into account free volume, temperature and strain rate, is proposed to quantitatively characterize the DBT behavior in fracture of metallic glasses.
Resumo:
The size of the shear transformation zone (STZ) that initiates the elastic to plastic transition in a Zr-based bulk metallic glass was estimated by conducting a statistical analysis of the first pop-in event during spherical nanoindentation. A series of experiments led us to a successful description of the distribution of shear strength for the transition and its dependence on the loading rate. From the activation volume determined by statistical analysis the STZ size was estimated based on a cooperative shearing model. (C) 2012 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
The existence of an indentation size effect (ISE) in the onset of yield in a Zr-based bulk metallic glass (BMG) is investigated by employing spherical-tip nanoindentation experiments. Statistically significant data on the load at which the first pop-in in the displacement occurs were obtained for three different tip radii and in two different structural states (as-cast and structurally relaxed) of the BMG. Hertzian contact mechanics were employed to convert the pop-in loads to the maximum shear stress underneath the indenter. Results establish the existence of an ISE in the BMG of both structural states, with shear yield stress increasing with decreasing tip radius. Structural relaxation was found to increase the yield stress and decrease the variability in the data, indicating ``structural homogenization'' with annealing. Statistical analysis of the data was employed to estimate the shear transformation zone (STZ) size. Results of this analysis indicate an STZ size of similar to 25 atoms, which increases to similar to 34 atoms upon annealing. These observations are discussed in terms of internal structure changes that occur during structural relaxation and their interaction with the stressed volumes in spherical indentation of a metallic glass. (C) 2012 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
The effect of hydrogen (H) charging on the shear yield strength (tau(max)) and shear transformation zone volume (Omega) of Ni-Nb-Zr metallic glass ribbons, with varying Zr content, were studied through the first pop-in loads during nanoindentation. Weight gain measurements after H charging and desorption studies were utilized to identify how the total H absorbed during charging is partitioned into mobile and immobile (or trapped) parts. These, in turn, indicate the significant role of H mobility in the amorphous structure on the yielding behavior. In high-Zr alloys, tau(max) increases significantly whereas Omega decreases. In low-Zr alloys, a slight decrease in tau(max) and increase in Omega were noted. These experimental observations are rationalized in terms of the mobility of the absorbed H in the amorphous structure and the possible role of it in the shear transformation zone dynamics during deformation of the metallic glass. (C) 2014 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
The dependence of shear yield strain, the activation energy and volume of shear transformation zone on the glass transition temperature was investigated through the analysis of statistical distributions of the first pop-in events during spherical indentation of four different thin film metallic glasses. Only the Cu-Zr metallic glass exhibits a bimodal distribution of the first pop-in loads, whereas W-Ru-B, Zr-Cu-Ni-Al and La-Co-Al metallic glasses show an unimodal distribution. Results show that shear yield strain and activation energy of shear transformation zone decrease whereas the volume of shear transformation zone increases with increasing homologous temperature, indicating that it is the activation energy rather than the volume of shear transformation zone that controls shear yield strain. (C) 2015 Elsevier B.V. All rights reserved.
Resumo:
Driven nonequilibrium structural phase transformation has been probed using time-varying resistance fluctuations or noise. We demonstrate that the non-Gaussian component (NGC) of noise obtained by evaluating the higher-order statistics of fluctuations, serves as a simple kinetic detector of these phase transitions. Using the Martensite transformation in free-standing wires of nickel-titanium binary alloys as a prototype, we observe clear deviations from the Gaussian background in the transformation zone, indicative of the long-range correlations in the system as the phase transforms. The viability of non-Gaussian statistics as a robust probe to structural phase transition was also confirmed by comparing the results from differential scanning calorimetry measurements. We further studied the response of the NGC to the modifications in the microstructure on repeated thermal cycling, as well as the variations in the temperature-drive rate, and explained the results using established simplistic models based on the different competing time scales. Our experiments (i) suggest an alternative method to estimate the transformation temperature scales with high accuracy and (ii) establish a connection between the material-specific evolution of microstructure to the statistics of its linear response. Since the method depends on an in-built long-range correlation during transformation, it could be portable to other structural transitions, as well as to materials of different physical origin and size.
Resumo:
The hydrothermal wave was investigated numerically for large-Prandtl-number fluid (Pr = 105.6) in a shallow cavity with different heated sidewalls. The traveling wave appears and propagates in the direction opposite to the surface flow (upstream) in the case of zero gravity when the applied temperature difference grows and over the critical value. The phase relationships of the disturbed velocity, temperature and pressure demonstrate that the traveling wave is driven by the disturbed temperature, which is named hydrothermal wave. The hydrothermal wave is so weak that the oscillatory flow field and temperature distribution can hardly be observed in the liquid layer. The exciting mechanism of hydrothermal wave is analyzed and discussed in the present paper.
Resumo:
Compression, tension and high-velocity plate impact experiments were performed on a typical tough Zr41.2Ti13.8Cu10Ni12.5Be22.5 (Vit 1) bulk metallic glass (BMG) over a wide range of strain rates from similar to 10(-4) to 10(6) s(-1). Surprisingly, fine dimples and periodic corrugations on a nanoscale were also observed on dynamic mode I fracture surfaces of this tough Vit 1. Taking a broad overview of the fracture patterning of specimens, we proposed a criterion to assess whether the fracture of BMGs is essentially brittle or plastic. If the curvature radius of the crack tip is greater than the critical wavelength of meniscus instability [F. Spaepen, Acta Metall. 23 615 (1975); A.S. Argon and M. Salama, Mater. Sci. Eng. 23 219 (1976)], microscale vein patterns and nanoscale dimples appear on crack surfaces. However, in the opposite case, the local quasi-cleavage/separation through local atomic clusters with local softening in the background ahead of the crack tip dominates, producing nanoscale periodic corrugations. At the atomic cluster level, energy dissipation in fracture of BMGs is, therefore, determined by two competing elementary processes, viz. conventional shear transformation zones (STZs) and envisioned tension transformation zones (TTZs) ahead of the crack tip. Finally, the mechanism for the formation of nanoscale periodic corrugation is quantitatively discussed by applying the present energy dissipation mechanism.
Resumo:
A systematic survey of the available data such as elastic constants, density, molar mass, and glass transition temperature of 45 metallic glasses is conducted. It is found that a critical strain controlling the onset of plastic deformation is material-independent. However, the correlation between elastic constants of solid glass and vitrification characteristics of its liquid does not follow a simple linear relation, and a characteristic volume, viz. molar volume, maybe relating to the characteristic size of a shear transformation zone (STZ), should be involved.
Resumo:
We derive an explicit expression for predicting the thicknesses of shear bands in metallic glasses. The model demonstrates that the shear-band thickness is mainly dominated by the activation size of the shear transformation zone (STZ) and its activation free volume concentration. The predicted thicknesses agree well with the results of measurements and simulations. The underlying physics is attributed to the local topological instability of the activated STZ. The result is of significance in understanding the origin of inhomogeneous flow in metallic glasses. (C) 2009 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
Taking shear-induced dilatation into consideration in shear transformation zone (STZ) operations, we derive a new yield criterion that reflects the pressure sensitivity in plastic flow in metallic glasses (MGs), which agrees well with experiments. Furthermore, an intrinsic theoretical correlation between the pressure sensitivity coefficient and the dilatation factor is revealed. It is found that the pressure sensitivity of plastic flow of MGs originates in the dilatation of microscale STZs.
Resumo:
We investigate the nanoscale periodic corrugation (NPC) structures on the dynamic fracture surface of a typical tough bulk metallic glass, submitted to high-velocity plate impact and scanned by atomic force microscopy (AFM). The detrended fluctuation analysis (DFA) of the recorded AFM profiles reveals that the valley landscapes of the NPC are nearly memoryless, characterized by Hurst parameter of 0.52 and exhibiting a self-similar fractal character with the dimension of about 1.48. Our findings confirm the existence of the “quasi-cleavage” fracture underpinned by tension transformation zones (TTZs) in metallic glasses.
Resumo:
The faulted slope zone of Biyang depression, a multiple hydrocarbon accumulation zone lying in a rich oil depression of Nanxiang basin, is a structural-sedimentary compounded slope, which is developed in Yanshanian period and has an area of 500 km2. From the ‘bottom up’, the developed strata may be divided into Yuhuangding formation in Neogene, Dacang Fang, Hetao-yuan plus Liaozhuang formations and Fenghuangzheng plus Pingyuan formation in Neogene, while Hetao-yuan formation is the main hydrocarbon-bearing target. Because of transtensional stress fields formed by persistent action of large-scale faulting in the south of the depression, sedimentary differential compaction in different stages, and tectonic inversion in later developing stage of the depression, a series of nose structure zones cut by different strike faults are developed. Therefore, the reservoir migration and accumulation are controlled by the complex faulted-nose structural zone, reservoir types are dominated by faulted-noses, faulted-blocks and fault-lithology, while lithology and stratigraphic unconformable reservoirs are locally developed. In combination with demands of practical production, applying with a new research approach of systematology and a combination with dynamic and static modes, guided by modern petroleum geologic theory, and based on previous data and studies, new techniques, methods of geophysical exploration, various computer simulation and forecasting techniques are applied in the new research of this paper. Starting from the structural features and formation mechanism, the forming mechanism of faulted structure, conditions and controlling factors of hydrocarbon accumulation, as well as various space-time allocation relationships in the process of accumulation are analyzed in the research. Besides that, the hydrocarbon migration, accumulation mechanism and dynamic evolution process are also discussed in the paper. Through the research, the accumulation rule of the faulted slope zone in faulted lake basin, the distribution and enrichment regularity of different reservoir controlling factors are systematically summarized. The summarizations indicate that the faulted slope is a favorable orientational zone, hydrocarbon is accumulated in nose structures and enriched in the main body of nose structures, faulted transformation zone and the ascent direction of laddering faulted blocks, the faults are the controlling factors, hydrocarbon accumulation zones controlled by fault-lithology are distributed along the faulting direcion. In the end, hydrocarbon migration and accumulation models of complex faulted-nose blocks are established. 1) Down cut model—‘flank-sheet’: the hydrocarbon is migrated like ‘sheet’ along a series of faults with parallel distribution and accumulated in the flank of nose structures; 2)Cross cut --‘axis-string’ model: the hydrocarbon cutting across the faults is migrated like ‘string’ and accumulated in the axis of nose structures. In view of different distribution models, reservoir forming combination patterns are divided and hydrocarbon reservoir evaluation exploration is carried out, which achieves good results in application. Key words: faulted slope zone; migration and accumulation model; reservoir controlling mechanism; reservoir-forming combination
Resumo:
Objetivo: Avaliar a acurácia da colposcopia utilizando a Classificação Colposcópica Internacional de 2002. Métodos: 3040 pacientes de população geral foram rastreadas para patologia cervical através de exame citopatológico, captura híbrida para HPV de alto risco e inspeção cervical. As colposcopias que resultaram em biópsia (n=468) executadas no rastreamento e acompanhamento destas pacientes foram gravadas, revistas por dois colposcopistas cegados e incluídas para análise. Resultados: Os observadores apresentaram excelente concordância (Kappa=0.843) no relato dos achados pela nova nomenclatura. A colposcopia apresentou sensibilidade de 86% e especificidade de 30.3% em diferenciar colo normal de colo anormal (LSIL, HSIL ou carcinoma); quando a colposcopia objetivava diferenciar colo normal ou LSIL de HSIL ou carcinoma, apresentou sensibilidade de 61.1% e especificidade de 94.4%. Os achados colposcópicos classificados como “maiores” pela nova classificação apresentaram valores preditivos positivos elevados para HSIL. Presença do achado colposcópico na zona de transformação e tamanho da lesão estavam associados a HSIL. Bordas externas definidas, associação de múltiplos achados distintos e presença de zona iodo negativa não estavam relacionados à gravidade das lesões. Conclusão: A colposcopia utilizando a Classificação Internacional de 2002 mostra-se um bom método de rastreamento, mas como método diagnóstico apresenta falhas, não podendo substituir a avaliação histológica. A categorização em achados colposcópicos “maiores” e “menores” apresentada pela nova classificação é adequada. Na realização da colposcopia, é importante também que a lesão seja situada em relação à zona de transformação e que seu tamanho seja indicado, já que estes foram fatores associados a lesões de alto grau.