895 resultados para PTFE facial membranes


Relevância:

80.00% 80.00%

Publicador:

Resumo:

This study was aimed at investigating the in vitro biocompatibility of a novel membrane of the composite poly(vinylidene-trifluoroethylene)/barium titanate (P(VDF-TrFE)/BT). Osteoblastic cells were obtained from human alveolar bone fragments and cultured under standard osteogenic condition until subconfluence. First passaged cells were cultured on P(VDF-TrFE)/BT and expanded polytetrafluoroethylene (e-PTFE - control) membranes in 24-well plates. Cell adhesion and spreading were evaluated at 30 min, and 4 and 24 h. For proliferation assay, cells were cultured for 1, 7, and 10 days. Cell viability was detected by trypan blue at 7 and 10 days. Total protein content and alkaline phosphatase (ALP) activity were measured at 7, 14, and 21 days. Cultures were stained with Alizarin red at 21 days, for detection of mineralized matrix. Data were compared by ANOVA and Student t test. Cell attachment (p = 0.001), cell number (p = 0.001), and ALP activity (p = 0.0001) were greater on P(VDF-TrFE)/BT. Additionally, doubling time was greater on P(VDF-TrFE)/BT (p = 0.03), indicating a decreased proliferation rate. Bone-like nodule formation took place only on P(VDF-TrFE)/BT. The present results showed that both membranes are biocompatible. However, P(VDF-TrFE)/BT presented a better in vitro biocompatibility and allowed bone-like nodule formation. Therefore, P(VDF-TrFE)/BT could be an alternative membrane to be used in guided tissue regeneration. (c) 2006 Wiley Periodicals, Inc.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Objective: The purpose of this study was to research a membrane material for use in guided bone regeneration. Study design: In this study, 25 male Wistar rats were used to analyze the biocompatibility and degradation process of biomembranes. The morphological changes in subcutaneous implantations were assessed after 7, 14, 21, 28 and 70 days. The materials were made of polyurethane polymer (AUG) obtained from vegetal oil (Ricinus communis) and polytetrafluoroethylene membrane (PTFE). The surface characteristics of the physical barriers in scanning electronic microscopic (SEM) were also evaluated. Results: In both groups, the initial histological analysis showed moderate inflammatory infiltrate, which was predominantly polymorphonuclear. There was also a presence of edema, which was gradually replaced by granulation tissue, culminating in a fibrous capsule. In the AUG group, some multinucleated giant cells were present in the contact interface, with the space previously occupied by the material. However, membrane degradation was not observed during the period studied. According to the present SEM findings, porosity was not detected in the AUG or PTFE membranes. Conclusion: The researched material is biocompatible and the degradation process is extremely slow or may not even occur at all.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Objective. The aim of this study was to perform quantitative and qualitative analyses of the initial repair pattern of an autogenous bone block graft when covered or not with e-PTFE membranes. Study design. Sixty male Wistar rats received a bone graft plus an e-PTFE membrane (MB) or just the graft (B). A block graft was harvested from the animal's calvarium and was laid and stabilized on the external cortical area near the angle of the mandible. Descriptive histology and histomorphometric analyses were carried out and the data were analyzed statistically by ANOVA and the Tukey test, with the level of significance set at 5%. Results. The results for group B showed that there was bone loss during the healing period (B0 = 1.38, B45 = 1.05, F = 7.91 > F C = 3.02), that is, the initial volume of the graft decreased in time. Bone tissue loss was about 24%. In contrast, the MB group showed bone tissue gain along the observation period (MB0 = 1.54, MB45 = 2.40, F = 7.91 > FC = 3.02), meaning that the total volume of newly formed bone was greater than the original graft area. Bone tissue gain was approximately 55%. MB showed significantly greater bone gain when compared to B (B45 = 1.05, MB45 = 2.40, F = 39.86 > FC = 1.90). These significant differences between B and MB could already be observed after 21 days. Conclusions. The bone block graft underwent resorption at an early healing stage, while additional new bone formation was observed when the bone graft was covered with an e-PTFE membrane. © 2005 Mosby, Inc. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This work assessed the performance of membranes made of natural latex extracted from Hevea brasiliensis prepared with three different methods: polymerized immediately after collection without the use of ammonia (L1); polymerized after preservation in ammonia solution (L2); and polymerized after storage in ammonia, followed by Soxhlet technique for the extraction of substances (L3). Polytetrafluoroethylene (PTFE) membrane was used as control. Two 10-mm diameter bone defects were surgically made in the calvaria of thirty adult male New Zealand rabbits. Defects (total n = 60) were treated with guided bone regeneration (GBR) using L1, L2, L3 or PTFE membranes (n = 15 for each membrane). Ten animals were euthanized after 7, 20 and 60 days postoperatively so that five samples (n = 5) of each treatment were collected at each time, and bone regeneration was assessed microscopically. The microscopic analysis revealed defects filled with blood clot and new bone formation at the margins of the defect in all 7-day samples, while 20-day defects were mainly filled with fibrous connective tissue. After 60 days defects covered with L1 membranes showed a significantly larger bone formation area in comparison to the other groups (P < 0.05, ANOVA, Tukey). Additionally, bone tissue hypersensitization for L1 and PTFE membranes was also investigated in six additional rabbits. The animals were subjected to the same surgical procedure for the confection of one 10-mm diameter bone defect that was treated with L1 (n = 3) or PTFE (n = 3). Fifty-three days later, a second surgery was performed to make a second defect, which was treated with the same type of membrane used in the first surgery. Seven days later, the animals were euthanized and samples analyzed. No differences among L1 and PTFE samples collected from sensitized and non-sensitized animals were found (P > 0.05, Kruskal-Wallis). Therefore, the results demonstrated that latex membranes presented performance comparable to PTFE membranes, and that L1 membranes induced higher bone formation. L1 and PTFE membranes produced no hypersensitization in the bone tissue.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Purpose: The aim of this study was to quantitatively evaluate and qualitatively describe autogenous bone graft healing with or without an expanded polytetrafluoroethylene (e-PTFE) membrane in ovariectornized rats. Materials and Methods: Eighty Wistar rats, weighing approximately 300 g each, were used. A graft was obtained from the parietal bone and fixed to the sidewall of each animal`s left mandibular ramus. The animals were randomly divided into four experimental groups (n = 20 in each group): group 1, sham operated and autogenous bone graft only- group 2, sham operated and autogenous bone graft covered by e-PTFE membrane; group 3, ovariectornized (OVX) and autogenous bone graft only- group 4, OVX and autogenous bone graft covered by e-PTFE membrane. The animals were sacrificed at five different time points: immediately after grafting or at 7, 21, 45, or 60 days after grafting. Histologic examination and morphometric measurement of the sections were performed, and values were submitted to statistical analyses. Results: Both groups (sham and OVX) experienced loss of the original graft volume when it was not covered by the membrane, whereas use of the membrane resulted in additional bone formation beyond the edges of the graft and under the membrane. Histologic analysis showed integration of the grafts in all animals, although a larger number of marrow spaces was found in OVX groups. Conclusions: Association of bone graft with an e-PTFE membrane resulted in maintenance of its original volume as well as formation of new bone that filled the space under the membrane. Osteopenia did not influence bone graft repair, regardless of whether or not it was associated with e-PTFE membrane, but descriptive histologic analysis showed larger numbers of marrow spaces in the bone graft and receptor bed and formation of new bone in the OVX animals. INT J ORAL MAXILLOFAC IMPLANTS 2009;24:1074-1082

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The aim of the study was to evaluate the possibility to obtain guided bone regeneration with two types of physical barriers (calcium sulfate and PTFE nonporous barrier) in surgical defects created in rat parietal bones. In the right parietal bone the calcium sulfate barrier filled out the whole defect and in the left parietal bone the barrier of PTFE was positioned in the floor and externally to the surgical defect. After 7, 14, 30 and 45 days four animals were sacrificed in each period and the bone containing the defects were submitted to the microscopic analysis. The results of the study revealed that the PTFE barrier was more effective for bone regeneration in shallow transcortical defects compared to the calcium sulfate. However, additional experiments are necessary to determine if calcium sulfate would be successful in other bone defects types or the use of the material under another consistence could complement the results obtained in this work.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Purpose: The aim of this study was to quantitatively evaluate and qualitatively describe autogenous bone graft healing with or without an expanded polytetrafluoroethylene (e-PTFE) membrane in ovariectornized rats. Materials and Methods: Eighty Wistar rats, weighing approximately 300 g each, were used. A graft was obtained from the parietal bone and fixed to the sidewall of each animal's left mandibular ramus. The animals were randomly divided into four experimental groups (n = 20 in each group): group 1, sham operated and autogenous bone graft only- group 2, sham operated and autogenous bone graft covered by e-PTFE membrane; group 3, ovariectornized (OVX) and autogenous bone graft only- group 4, OVX and autogenous bone graft covered by e-PTFE membrane. The animals were sacrificed at five different time points: immediately after grafting or at 7, 21, 45, or 60 days after grafting. Histologic examination and morphometric measurement of the sections were performed, and values were submitted to statistical analyses. Results: Both groups (sham and OVX) experienced loss of the original graft volume when it was not covered by the membrane, whereas use of the membrane resulted in additional bone formation beyond the edges of the graft and under the membrane. Histologic analysis showed integration of the grafts in all animals, although a larger number of marrow spaces was found in OVX groups. Conclusions: Association of bone graft with an e-PTFE membrane resulted in maintenance of its original volume as well as formation of new bone that filled the space under the membrane. Osteopenia did not influence bone graft repair, regardless of whether or not it was associated with e-PTFE membrane, but descriptive histologic analysis showed larger numbers of marrow spaces in the bone graft and receptor bed and formation of new bone in the OVX animals. INT J ORAL MAXILLOFAC IMPLANTS 2009;24:1074-1082

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A regeneração periodontal e do rebordo ósseo utilizando barreiras físicas são procedimentos bem estabelecidos em cirurgias reconstrutivas. As características do biomaterial e o desenho da membrana empregados na regeneração tecidual guiada desempenham um papel importante na obtenção de bons resultados. O objetivo deste estudo experimental histológico foi comparar o uso de dois tipos de barreiras físicas na regeneração óssea guiada em defeitos criados na tíbia de ratos. Quinze animais foram divididos em três grupos: grupo I (barreira não-porosa de politetrafluoretileno), grupo II (blocos de hidroxiapatita de coral) e grupo III (controle que não recebeu nenhuma barreira). A análise histológica demonstrou várias quantidades de osso neoformado com ambos os tipos de barreiras. A barreira de politetrafluoretileno mostrou melhores resultados do que a hidroxiapatita. Os resultados deste estudo sugerem que a regeneração óssea pode ser conseguida com a técnica de submersão da barreira física.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A promising class of compounds for DNA transfection have been designed by conjugating various polyamines to bile-acid-based amphiphiles. Formulations containing these compounds were tested for their ability to facilitate the uptake of a beta-galactosidase reporter plasmid into COS-7 cells. Dioleoyl phosphatidyl ethanolamine (DOPE) formulations of some of the compounds were several times better than Lipofectin at promoting DNA uptake. The most active compounds contained the most hydrophilic bile acid components. The activity is clearly not related to affinity for DNA: the hydrophobic bile acid conjugates were found to form stable complexes with DNA at lower charge ratios than the hydrophilic conjugates. We suggest that the high activity of the best compounds is related to their facial amphiphilicity, which may confer an ability to destabilize membranes. The success of these unusual cationic transfection agents may inspire the design of even more effective gene delivery agents.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The bioactivity of three methacryloyloxyethyl phosphate (MOEP) grafted expanded polytetrafluoroethylene (ePTFE) membranes with varying surface coverage as well as unmodified ePTFE was investigated through a series of in vitro tests: calcium phosphate (CaP) growth in simulated body fluid (SBF), serum protein adsorption, and a morphology and attachment study of human osteoblast-like SaOS-2 cells. The graft copolymers were prepared by means of gamma irradiation induced grafting and displayed various surface morphologies and wettabilities depending on the grafting conditions used. Unmodified ePTFE did not induce nucleation of Cal? minerals, whereas all the grafted membranes revealed the growth of Cal? minerals after 7 days immersion in SBF. The sample with lowest surface grafting yield (24% coverage), a smooth graft morphology and relatively high hydrophobicity (theta(adv) = 120 degrees, theta(rec) = 80 degrees) showed carbonated hydroxyapatite growth covering the surface. On the other hand, the samples with high surface grafting yield (76% and 100%), a globular graft morphology and hydrophilic surfaces (theta(adv) = 60 degrees and 80 degrees, theta(rec) = 25 degrees and 15 degrees, respectively) exhibited irregular growth of non-apatitic Cap minerals. Irreversibly adsorbed protein measured after a 1 h immersion in serum solution was quantified by the amount of nitrogen on the surface using XPS, as well as by weight increase. All grafted membranes adsorbed 3-6 times more protein than the unmodified membrane. The sample with the highest surface coverage adsorbed the most protein. Osteoblast-like SaOS-2 cells cultured for 3 h revealed significantly higher levels of cell attachment on all grafted membranes compared to unmodified ePTFE. Although the morphology of the cells was heterogeneous, in general, the higher grafted surfaces showed a much better cell morphology than both the low surface-grafted and the control unmodified sample. The suite of in vitro tests confirms that a judicious choice of grafted monomer such as the phosphate-containing methacrylate monomer (MOEP) significantly improves the bioactivity of ePTFE in vitro. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Expanded polytetrafluoroethylene (ePTFE) membranes were modified by graft copolymerization with methacryloxyethyl phosphate (MOEP) in methanol and 2-butanone (methyl ethyl ketone (MEK)) at ambient temperature using gamma irradiation. The effect of dose rate (0.46 and 4.6 kGyh(-1)), monomer concentration (1-40 %) and solvent were studied and the modified membranes were characterized by weight increase, X-ray photoelectron spectroscopy (XPS), Fourier transform infrared spectroscopy (FTIR) and scanning electron microscopy (SEM). XPS was used to determine the % degree of surface coverage using the C-F (ePTFE membrane) and the C-C (MOEP graft copolymer) peaks. Grafting yield, as well as surface coverage, were found to increase with increasing monomer concentration and were significantly higher for samples grafted in MEK than in methanol solution. SEM images showed distinctly different surface morphologies for the membranes grafted in methanol (smooth) and MEK (globular), hence indicating phase separation of the homopolymer in MEK. We propose that in our system, the non-solvent properties of MEK for the homopolymer play a more important role than solvent chain transfer reactions in determining grafting outcomes. (c) 2005 Society of Chemical Industry.