995 resultados para Niobium oxide


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Nanorod forms of metal oxides is recognised as one of the most remarkable morphologies. Their structure and functionality have driven important advancements in a vast range of electronic devices and applications. In this work, we postulate a novel concept to explain how numerous localised surface states can be engineered into the bandgap of niobium oxide nanorods using tungsten. We discuss their contributions as local state surface charges for the modulation of a Schottky barrier height, relative dielectric constant and their respective conduction mechanisms. Their effect on the hydrogen gas molecule interactions mechanisms are also examined herein. We synthesised niobium tungsten oxide (Nb17W2O25) nanorods via a hydrothermal growth method and evaluated the Schottky barrier height, ideality factor, dielectric constant and trap energy level from the measured I-V vs temperature characteristics in the presence of air and hydrogen to show the validity of our postulations.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Bismuth zinc niobium oxide (BZN) was successfully synthesized by a diol-based sol-gel reaction utilizing metal acetate and alkoxide precursors. Thermal analysis of a liquid suspension of precursors suggests that the majority of organic precursors decompose at temperatures up to 150°C, and organic free powders form above 350°C. The experimental results indicate that a homogeneous gel is obtained at about 200°C and then converts to a mixture of intermediate oxides at 350–400°C. Finally, single-phased BZN powders are obtained between 500 and 900°C. The degree of chemical homogeneity as determined by X-ray diffraction and EDS mapping is consistent throughout the samples. Elemental analysis indicates that the atomic ratio of metals closely matches a Bi1.5ZnNb1.5O7 composition. Crystallite sizes of the BZN powders calculated from the Scherrer equation are about 33–98 nm for the samples prepared at 500–700°C, respectively. The particle and crystallite sizes increase with increased sintering temperature. The estimated band gap of the BZN nanopowders from optical analysis is about 2.60–2.75 eV at 500-600°C. The observed phase formations and measured results in this study were compared with those of previous reports.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The formation of heterojunctions between two crystals with different band gap structures, acting as a tunnel for the unidirectional transfer of photo-generated charges, is an efficient strategy to enhance photocatalytic performance in semiconductor photocatalysts. The heterojunctions may also promote the photoactivity in the visible-light-response of any surface complex catalysts by influencing the transfer of photo-generated electrons. Herein, Nb2O5 microfibers, with a high surface area of interfaces between an amorphous phase and crystalline phase, were designed and synthesised by the calcination of hydrogen-form niobate while controlling the crystallization The photoactivity of these microfibers towards selective aerobic oxidation reactions was investigated. As predicted, the Nb2O5 microfibres containing heterojunctions exhibited the highest photoactivity. This could be due to the band gap difference between the amorphous phase and the crystalline phase, which shortened the charge mobile distance and improved the efficiency.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A series of vanadium-niobium oxide catalysts in which the vanadia content varies between 0.3 and 18mol%was prepared by coprecipitation. These catalysts were characterized by X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), low-energy ion scattering (LEIS), and by catalytic testing in the oxidative dehydrogenation reaction of propane. The results of the surface analysis by XPS and LEIS are compared. It is concluded that the active site on the catalyst surface contains 2.0 ± 0.3 vanadium atoms on average. This can be understood byassuming the existenceof two or three different sites:isolated vanadium atoms, pairs of vanadium atoms, or ensembles of three vanadium atoms. At higher vanadium concentration more vanadium clusters with a higher activity are at the surface.LEIS revealed that as the vanadium concentration in the catalyst increases, vanadium replaces niobium at the surface. At vanadium concentrations above 8 mol%, new phases such as P-(Nb, V)20S which are less active because vanadium is present in isolated sites are formed, while the vanadium surface concentration shows a slight decrease

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A composite of cellulose extracted from bagasse with Nb2O5 center dot nH(2)O in three different proportions (16.67, 37.5 and 50.0 wt%) was prepared using the co-precipitation method. The materials were characterized by X-ray diffractometry (XRD), Fourier transform infra-red spectroscopy (FTIR), thermogravimetric analysis (TG/DTG), differential scanning calorimetry (DSC) and scanning electron microscopy (SEM). TG data obtained show that the presence of inorganic material influenced slightly the stability of the hybrid material. The precipitation of 16.67 wt.% of oxide was sufficient to inhibit the combustion peaks present in the DSC curve of cellulose. This work will help find new applications for these materials. Published by Elsevier Ltd.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Aim: To evaluate the physicochemical and mechanical properties of Portland cement-based experimental sealers (ES) with different radiopacifying agents (zirconium oxide and niobium oxide micro- and nanoparticles) in comparison with the following conventional sealers: AH Plus, MTA Fillapex and Sealapex. Methodology: The materials were tested for setting time, compressive strength, flow, film thickness, radiopacity, solubility, dimensional stability and formaldehyde release. Data were subjected to anova and Tukey tests (P < 0.05). Results: MTA Fillapex had the shortest setting time and lowest compressive strength values (P < 0.05) compared with the other materials. The ES had flow values similar to the conventional materials, but higher film thickness (P < 0.05) and lower radiopacity (P < 0.05). Similarly to AH Plus, the ES were associated with dimensional expansion (P > 0.05) and lower solubility when compared with MTA Fillapex and Sealapex (P < 0.05). None of the endodontic sealers evaluated released formaldehyde after mixing. Conclusion: With the exception of radiopacity, the Portland cement-based experimental endodontic sealers presented physicochemical properties according to the specifications no 57 ANSI/ADA (ADA Professional Product Review, 2008) and ISO 6876 (Dentistry - Root Canal Sealing Materials, 2012, British Standards Institution, London, UK). The sealers had setting times and flow ability that was adequate for clinical use, satisfactory compressive strength and low solubility. Additional studies should be carried out with the purpose of decreasing the film thickness and to determine the ideal ratio of radiopacifying agents in Portland cement-based root canal sealers. © 2013 International Endodontic Journal.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Context: Calcium oxide (CaO) may be added to mineral trioxide aggregate (MTA) or Portland cement (PC) to improve physicochemical and biological properties. Aims: To evaluate the physicochemical properties of PC associated with radiopacifiers and CaO. Materials and Methods: MTA Angelus, PC + 30% zirconium oxide (Zr), or 30% niobium oxide (Nb) associated with 10 or 20% of CaO were evaluated. Gilmore needles were used to evaluate initial and final setting time. Compressive strength was evaluated after the periods of 24 hours and 21 days. pH was analyzed after 3, 12, 24 hours, 7, 14, 21 days. Solubility and flow tests were performed based on the ISO 6876. The data obtained were submitted to analysis of variance and Tukey tests (P ≤ 0.05). Results: The associations with 10% CaO showed greater strength that the associations with 20% CaO. The shortest initial setting time was observed for the association PC + Zr + 20% CaO and MTA. All the cements presented alkaline pH. The flow of all cements was similar. The highest solubility was found in the associations with 20% CaO. Conclusion: The addition of CaO to PC favored the alkaline property and the PC + Zr + 20% CaO presented setting time similar to MTA.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Global niobium production is presently dominated by three operations, Araxá and Catalão (Brazil), and Niobec (Canada). Although Brazil accounts for over 90% of the world’s niobium production, a number of high grade niobium deposits exist worldwide. The advancement of these deposits depends largely on the development of operable beneficiation flowsheets. Pyrochlore, as the primary niobium mineral, is typically upgraded by flotation with amine collectors at acidic pH following a complicated flowsheet with significant losses of niobium. This research compares the typical two stage flotation flowsheet to a direct flotation process (i.e. elimination of gangue pre-flotation) with the objective of circuit simplification. In addition, the use of a chelating reagent (benzohydroxamic acid, BHA) was studied as an alternative collector for fine grained, highly disseminated pyrochlore. For the amine based reagent system, results showed that while comparable at the laboratory scale, when scaled up to the pilot level the direct flotation process suffered from circuit instability because of high quantities of dissolved calcium in the process water due to stream recirculation and fine calcite dissolution, which ultimately depressed pyrochlore. This scale up issue was not observed in pilot plant operation of the two stage flotation process as a portion of the highly reactive carbonate minerals was removed prior to acid addition. A statistical model was developed for batch flotation using BHA on carbonatite ore (0.25% Nb2O5) that could not be effectively upgraded using the conventional amine reagent scheme. Results showed that it was possible to produce a concentrate containing 1.54% Nb2O5 with 93% Nb recovery in ~15% of the original mass. Fundamental studies undertaken included FT-IR and XPS, which showed the adsorption of both the protonized amine and the neutral amine onto the surface of the pyrochlore (possibly at niobium sites as indicated by detected shifts in the Nb3d binding energy). The results suggest that the preferential flotation of pyrochlore over quartz with amines at low pH levels can be attributed to a difference in critical hemimicelle concentration (CHC) values for the two minerals. BHA was found to be absorbed on pyrochlore surfaces by a similar mechanism to alkyl hydroxamic acid. It is hoped that this work will assist in improving operability of existing pyrochlore flotation circuits and help promote the development of niobium deposits globally. Future studies should focus on investigation into specific gangue mineral depressants and inadvertent activation phenomenon related to BHA flotation of gangue minerals.