951 resultados para Extended Xray absorption fine structure (EXAFS) spectroscopies


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Tungsten oxide/titania (WO3/TiO2) nanopowders were synthesized by the polymeric precursor method which varied the WO3 content between 0 and 10 mol%. The powders were thermally treated in a conventional furnace and their structural, microstructural and electric properties were evaluated by X-ray diffraction (XRD), Raman spectrometry, N 2 physisorption, NH3 chemisorption, temperature-programmed reduction (TPR), X-ray absorption near-edge spectroscopy (XANES) in situ XANES and extended X-ray absorption fine structure spectroscopy (EXAFS) and transmission electron microscopy (TEM). XRD and Raman spectrometry confirmed the homogeneous distribution of an amorphous WO3 phase in the TiO 2 matrix which stabilized the anatase phase through the generation of [TiO5·V0] or [TiO5·V 0] complex sites. Conventional TPR-H2 (temperature programmed reduction) along with XANES TPR-H2 and XANES TPR-EtOH showed that WO3/TiO2 sample reduction occurs through the formation of these complex clusters. Moreover, the addition of WO3 promoted an increase in the surface acidity of doped samples as revealed by NH3 chemisorption. The WO3/TiO2 bulk-ceramic samples were further used to estimate their potential application in a humidity sensor in the range of 15-85% relative humidity. Probable reasons that lead to the different humidity sensor responses of samples were given based on the structural and surface characterizations. Correlation between the sensing performance of the sensor and its structural features are also discussed. Although all samples responded as a humidity sensor, the W2T sample (2 mol% added WO3) excelled for sensitivity due to the increase in acid sites, optimum mean pore size and pore size distribution. © 2013 Elsevier B.V.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The crystal structure and the local atomic order of a series of nanocrystalline ZrO(2)-CaO solid solutions with varying CaO content were studied by synchrotron radiation X-ray powder diffraction and extended X-ray absorption fine structure (EXAFS) spectroscopy. These samples were synthesized by a pH-controlled nitrate-glycine gel-combustion process. For CaO contents up to 8 mol%, the t' form of the tetragonal phase (c/a > 1) was identified, whereas for 10 and 12 mol% CaO, the t '' form (c/a=1; oxygen anions displaced from their ideal positions in the cubic phase) was detected. Finally, the cubic phase was observed for solid solutions with CaO content of 14 mol% CaO or higher. The t'/t '' and t ''/cubic compositional boundaries were determined to be at 9 (1) and 13 (1) mol% CaO, respectively. The EXAFS study demonstrated that this transition is related to a tetragonal-to-cubic symmetry change of the first oxygen coordination shell around the Zr atoms.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Experimental Extended X-ray Absorption Fine Structure (EXAFS) spectra carry information about the chemical structure of metal protein complexes. However, pre- dicting the structure of such complexes from EXAFS spectra is not a simple task. Currently methods such as Monte Carlo optimization or simulated annealing are used in structure refinement of EXAFS. These methods have proven somewhat successful in structure refinement but have not been successful in finding the global minima. Multiple population based algorithms, including a genetic algorithm, a restarting ge- netic algorithm, differential evolution, and particle swarm optimization, are studied for their effectiveness in structure refinement of EXAFS. The oxygen-evolving com- plex in S1 is used as a benchmark for comparing the algorithms. These algorithms were successful in finding new atomic structures that produced improved calculated EXAFS spectra over atomic structures previously found.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper, we report our initial research to obtain hexagonal rod-like elongated silver tungstate (alpha-Ag2WO4) microcrystals by different methods [sonochemistry (SC), coprecipitation (CP), and conventional hydrothermal (CH)] and to study their cluster coordination and optical properties. These microcrystals were structurally characterized by X-ray diffraction (XRD), Rietveld refinements, Fourier transform infrared (FT-IR), X-ray absorption near-edge structure (XANES), and extended X-ray absorption fine structure (EXAFS) spectroscopies. The shape and average size of these alpha-Ag2WO4 microcrystals were observed by field-emission scanning electron microscopy (FE-SEM). The optical properties of these microcrystals were investigated by ultraviolet-visible (UV-vis) spectroscopy and photoluminescence (PL) measurements. XRD patterns and Rietveld refinement data confirmed that alpha-Ag2WO4 microcrystals have an orthorhombic structure. FT-IR spectra exhibited four IR-active modes in a range from 250 to 1000 cm(-1). XANES spectra at the W L-3-edge showed distorted octahedral [WO6] clusters in the lattice, while EXAFS analyses confirmed that W atoms are coordinated by six O atoms. FE-SEM images suggest that the alpha-Ag2WO4 microcrystals grow by aggregation and the Ostwald ripening process. PL properties of alpha-Ag2WO4 microcrystals decrease with an increase in the optical band-gap values (3.19-3.23 eV). Finally, we observed that large hexagonal rod-like alpha-Ag2WO4 microcrystals prepared by the SC method exhibited a major PL emission intensity relative to alpha-Ag2WO4 microcrystals prepared by the CP and CH methods.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The x-ray absorption fine structure (XAFS) zinc K-edge steps for intact stages I,II and V,VI Xenopus laevis oocytes demonstrate that the zinc concentration is about 3 and 1 mM, respectively. However, the chi(k) function for the early stage oocytes differs markedly from that for the late one. Analysis of the XAFS data for stage I,II oocytes indicates that zinc is bound to 2.0 +/- 0.5 sulfur atoms at an average coordination distance of 2.29 +/- 0.02 angstroms and 2.0 +/- 0.5 nitrogen or oxygen (N/O) atoms at 2.02 +/- 0.02 angstroms. In marked contrast, in stage V,VI oocytes, zinc is bound to 4.1 +/- 0.4 N/O atoms at an average distance of 1.98 +/- 0.01 angstroms. Our previous studies demonstrated that 90% of the zinc in stage VI oocytes is sequestered within yolk platelets, associated with a single molecule, lipovitellin, the proteolytically processed product of vitellogenin. XAFS analysis of yolk platelets, lipovitellin, and vitellogenin demonstrates that zinc is bound to 4.0 +/- 0.5 N/O ligands at an average distance of 1.98 +/- 0.01 angstroms in each case, identical to that of stage V,VI oocytes. The higher shell contributions in the Fourier transforms indicate that two of the N/O zinc ligands are His in both stage V,VI and I,II oocytes. The results show that in stage I,II oocytes, there is a high concentration of a zinc protein whose zinc coordination site likely is composed of (His)2(Cys)2, such as, e.g., TFIIIA. As the oocytes develop, the predominant zinc species becomes one that exhibits the (His)2(N/0)2 zinc site found in lipovitellin. Hence, the ligands to the zinc atoms in intact oocytes and the changes that take place as a function of oogenesis and after their fertilization, during embryogenesis, now can be examined and explored.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The local and medium-range structures of siloxane-POE hybrids doped with Fe(III) ions and prepared by the sol-gel process were investigated by X-ray absorption near-edge structure (XANES)/extended X-ray absorption fine structure (EXAFS) and small-angle X-ray scattering (SAXS), respectively. The experimental results show that the structure of these composites depends on the doping level. EXAFS data reveal that, for low doping levels ([O]/[Fe] > 40, oxygens being of the ether-type of the POE chains), Fe(III) ions are surrounded essentially by a shell of chlorine atoms, suggesting the formation of FeCl4- anions. At high doping levels ([O]/[Fe] < 20), Fe(III) ions interacts mainly with oxygen atoms and form FeOx species. The relative proportion of FeOx species increases with iron concentration, this result being consistent with the results of SAXS measurements showing that increasing iron doping induces the formation of iron-rich nanodomains embedded in the polymer matrix.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The local atomic structures around the Zr atom of pure (undoped) ZrO(2) nanopowders with different average crystallite sizes, ranging from 7 to 40 nm, have been investigated. The nanopowders were synthesized by different wet-chemical routes, but all exhibit the high-temperature tetragonal phase stabilized at room temperature, as established by synchrotron radiation X-ray diffraction. The extended X-ray absorption fine structure (EXAFS) technique was applied to analyze the local structure around the Zr atoms. Several authors have studied this system using the EXAFS technique without obtaining a good agreement between crystallographic and EXAFS data. In this work, it is shown that the local structure of ZrO(2) nanopowders can be described by a model consisting of two oxygen subshells (4 + 4 atoms) with different Zr-O distances, in agreement with those independently determined by X-ray diffraction. However, the EXAFS study shows that the second oxygen subshell exhibits a Debye-Waller (DW) parameter much higher than that of the first oxygen subshell, a result that cannot be explained by the crystallographic model accepted for the tetragonal phase of zirconia-based materials. However, as proposed by other authors, the difference in the DW parameters between the two oxygen subshells around the Zr atoms can be explained by the existence of oxygen displacements perpendicular to the z direction; these mainly affect the second oxygen subshell because of the directional character of the EXAFS DW parameter, in contradiction to the crystallographic value. It is also established that this model is similar to another model having three oxygen subshells, with a 4 + 2 + 2 distribution of atoms, with only one DW parameter for all oxygen subshells. Both models are in good agreement with the crystal structure determined by X-ray diffraction experiments.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Copper zinc tin sulfide (CZTS) is a promising Earthabundant thin-film solar cell material; it has an appropriate band gap of ~1.45 eV and a high absorption coefficient. The most efficient CZTS cells tend to be slightly Zn-rich and Cu-poor. However, growing Zn-rich CZTS films can sometimes result in phase decomposition of CZTS into ZnS and Cu2SnS3, which is generally deleterious to solar cell performance. Cubic ZnS is difficult to detect by XRD, due to a similar diffraction pattern. We hypothesize that synchrotron-based extended X-ray absorption fine structure (EXAFS), which is sensitive to local chemical environment, may be able to determine the quantity of ZnS phase in CZTS films by detecting differences in the second-nearest neighbor shell of the Zn atoms. Films of varying stoichiometries, from Zn-rich to Cu-rich (Zn-poor) were examined using the EXAFS technique. Differences in the spectra as a function of Cu/Zn ratio are detected. Linear combination analysis suggests increasing ZnS signal as the CZTS films become more Zn-rich. We demonstrate that the sensitive technique of EXAFS could be used to quantify the amount of ZnS present and provide a guide to crystal growth of highly phase pure films.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Irreversible photoexpansion effect has been observed in amorphous Ga10Ge2S65 glasses when its surface was exposed to light with energy greater than the band gap, 3.52 eV. A volume change of about 5% was reached in bulk samples by controlling illumination time and the laser power density. To understand the atomic scale processes of the photoexpansion effect, extended X-ray absorption fine structure (EXAFS) spectroscopy has been used as a local probe of the germanium environment in the glass samples before and after illumination. Modifications are observed in the average coordination shell around Ge atoms in the illuminated sample compared to the non-illuminated one. For the non-illuminated sample, the Ge coordination shell is described by a distorted tetrahedron of sulfur atoms at around 2.20 Angstrom. After illumination, the EXAFS signal can be explained by introducing an additional contribution to this average environment. Based on an analysis of the EXAFS data we proposed a two-shell model of 0.5 oxygen atoms at 2.01 Angstrom and 3.6 sulfur atoms at a 2.20 Angstrom. The existence of Ge-O bonds in the glass after illumination was confirmed by infrared measurements. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

X-ray absorption spectroscopy was used to study the local environment of tungsten atoms in NaPO3-BaF2,-WO3 glasses and the results were compared with crystalline references Na2WO4 and WO3. XANES measurements at the W-L-1 edge allowed to determine a distorted octahedral environment of tungsten atoms in these glasses similar to the local order of tungsten in monoclinic WO3. Extended X-ray absorption fine structure (EXAFS) has been used as a local probe to monitor the effect of WO3 concentration on the tungsten environment. Based on an analysis of the EXAFS data, we proposed a three-shell model of oxygen atoms around tungsten as in monoclinic WO3. With increasing WO3 concentration, it was found that R-2 decreases from 1.96 to 1.92 angstrom whereas R-3 increases from 2.07 to 2.12 angstrom. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Transparent, flexible, and luminescent EU3+-doped siloxane-poly(ethylene glycol) (PEG) nanocomposites have been obtained by the sol-gel process. The inorganic (siloxane) and organic PEG phases are usually linked by weak bonds (hydrogen bonds or van der Waals forces), and small-angle X-ray scattering (SAXS) measurements suggest that the structure of these materials consists of fractal siloxane aggregates embedded in the PEG matrix. For low Eu3+ contents, n = 300 and n = 80, the aggregates are small and isolated and their fractal dimensions are 2.1 and 1.7, respectively. These values are close to those expected for gelation mechanisms consisting of reaction-limited cluster-cluster aggregation (RLCCA) and diffusion-limited cluster-cluster aggregation (DLCCA). For high Eu3+ content, SAYS results are consistent with a two-level structure: a primary level of siloxane aggregates and a second level, much larger, formed by the coalescence of the primary ones. The observed increase in the glass transition temperature for increasing Eu3+ content is consistent with the structural model derived from SAXS measurements. Extended X-ray absorption fine structure (EXAFS) and luminescence spectroscopy measurements indicate that under the experimental conditions utilized here Eu3+ ions do not strongly interact with the polymeric phase.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In order to determine structural changes during drying of inorganic gels, the local and long-range order structure of SnO2-x(OH)2x xerogels resulting from drying hydrogels with different concentrations of electrolyte (Cl- and NH+ 4) have been measured by extended X-ray absorption fine structure (EXAFS), X-ray diffraction (XRD) and N2 adsorption techniques. EXAFS measurements performed at the Sn K edge on the hydrogels and xerogels show the existence of microcrystallites with the cassiterite structure. Two drying modes have been used: freeze drying and drying by evaporation at 45°C. It is shown that the microcrystallite size determined by XRD and EXAFS techniques on the drying mode and on the electrolyte concentrations. The microcrystallite size measured on the freeze dried xerogels is similar to that of their parent hydrogels, whatever the concentration of electrolyte; however, during drying by evaporation, a preferential growth of microcrystallites along the c-axis of the cassiterite structure is observed. The size of these crystallites is enhanced with a decrease of the electrolyte concentration. Specific surface areas calculated by the Brunauer-Emmett-Teller method indicate that this preferential growth is related to the improvement of the network connectivity. The comparison of both drying processes indicates that crystallization and polycondensation are independent phenomena. © 1995 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ba(Zr0.75Ti0.25)O3 (BZT-75/25) powders were synthesized by the polymeric precursor method. Samples were structurally characterized by X-ray diffraction (XRD), Rietveld refinement, X-ray absorption near-edge structure (XANES) and extended X-ray absorption fine structure (EXAFS) techniques. Their electronic structures were evaluated by first-principle quantum mechanical calculations based on density functional theory at the B3LYP level. Their optical properties were investigated by ultraviolet-visible (UV-Vis) spectroscopy and photoluminescence (PL) measurements at room temperature. XRD patterns and Rietveld refinement data indicate that the samples have a cubic structure. XANES spectra confirm the presence of pyramidal [TiO5] clusters and octahedral [TiO6] clusters in the disordered BZT-75/25 powders. EXAFS spectra indicate distortion of Ti-O and Ti-O-Ti bonds the first and second coordination shells, respectively. UV-Vis absorption spectra confirm the presence of different optical bandgap values and the band structure indicates an indirect bandgap for this material. The density of states demonstrates that intermediate energy levels occur between the valence band (VB) and the conduction band (CB). These electronic levels are due to the predominance of 4d orbitals of Zr atoms in relation to 3d orbitals of Ti atoms in the CB, while the VB is dominated by 2p orbitals related to O atoms. There was good correlation between the experimental and theoretical optical bandgap values. When excited at 482 nm at room temperature, BZT-75/25 powder treated at 500 C for 2 h exhibited broad and intense PL emission with a maximum at 578 nm in the yellow region. © 2013 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)