Resumo:
The ionic nitriding process presents some limitations related with the control of the thickness of the layer and its uniformity. Those limitations that happen during the process, are produced due to edge effects, damage caused by arcing arc and hollow cathode, mainly in pieces with complex geometry and under pressures in excess of 1 mbar. A new technique, denominated ASPN (active screen shapes nitriding) it has been used as alternative, for offering many advantages with respect to dc plasma conventional. The developed system presents a configuration in that the samples treated are surrounded by a large metal screen at high voltage cathodic potencials, (varying between 0 and 1200V) and currents up to 1 A. The sample is placed in floting potential or polarized at relatively lower bias voltages by an auxiliary source. As the plasma is not formed directly in the sample surface but in the metal screen, the mentioned effects are eliminated. This mechanism allows investigate ion of the transfer of nitrogen to the substrate. Optical and electronic microscopy are used to exam morphology and structure at the layer. X-ray difration for phase identification and microhardness to evaluate the efficiency of this process with respect to dc conventional nitriding
Resumo:
The ionic nitriding process presents some limitations related with the control of the thickness of the layer and its uniformity. Those limitations that happen during the process, are produced due to edge effects, damage caused by arcing arc and hollow cathode, mainly in pieces with complex geometry and under pressures in excess of 1 mbar. A new technique, denominated ASPN (active screen shapes nitriding) it has been used as alternative, for offering many advantages with respect to dc plasma conventional. The developed system presents a configuration in that the samples treated are surrounded by a large metal screen at high voltage cathodic potencials, (varying between 0 and 1200V) and currents up to 1 A. The sample is placed in floting potential or polarized at relatively lower bias voltages by an auxiliary source. As the plasma is not formed directly in the sample surface but in the metal screen, the mentioned effects are eliminated. This mechanism allows investigate ion of the transfer of nitrogen to the substrate. Optical and electronic microscopy are used to exam morphology and structure at the layer. X-ray difration for phase identification and microhardness to evaluate the efficiency of this process with respect to dc conventional nitriding
Resumo:
Carbide reinforced metallic alloys potentially improve some important mechanical properties required for the overall use of important engineering materials such as steel and nickel. Nevertheless, improved performance is achieved not only by composition enhancement but also by adequate processing techniques, such as novel sintering methods in the case of powder metallurgy. The method minimizes energy losses in addition to providing uniform heating during sintering. Thus, the general objective of this study was to evaluate the density, hardness, flexural strength, dilatometric behavior and to analyze the microstructure of metal matrix composites based nickel with addition of carbides of tantalum and / or niobium when sintered in a conventional furnace and Plasma assisted debinding and sintering (PADS). Initially, were defineds best parameters of granulation, screening and mixing procedure. After, mixtures of carbonyl Ni and 5%, 10% and 15 wt.% NbC and TaC were prepared in a Y-type mixer under wet conditions during 60 minutes. The mixtures were then dried and granulated using 1.5 wt. % paraffin diluted in hexane. Granulates were cold pressed under 600 MPa. Paraffin was then removed from the pressed pellets during a pre-sintering process carried out in a tubular furnace at 500 °C during 30 min. The heating rate was 3 ºC/min. The pellets were then sintered using either a plasma assisted reactor or a conventional resistive tubular furnace. For both methods, the heating rate was set to 8 ºC/min up to 1150 °C. The holding time was 60 minutes. The microstructure of the sintered samples was evaluated by SEM. Brinell hardness tests were also carried out. The results revealed that higher density and higher hardness values were observed in the plasma-assisted sintered samples. Hardness increased with the concentration of carbides in the Ni-matrix. The flexural strength also increased by adding the carbides. The decline was larger for the sample with addition of 5% 5% TaC and NbC. In general, compositions containing added carbide 10% showed less porous and more uniform distribution of carbides in the nickel matrix microstructural appearance. Thus, both added carbide and plasma sintering improved density, hardness, flexural strength and microstructural appearance of the composites
Resumo:
The nickel alloys are widely used in the production of various materials, especially those that require mechanical strength characteristics associated with resistance to corrosion, for example, the stainless steel. Another use is the production of nickel alloy sintered from powder of metallic nickel. A promising alternative for the production of sintered components of nickel with an important reduction in costs of starting material is the use of mixtures of powders of Ni-NiO. This work aimed to study in situ reduction of NiO during sintering mixtures of Ni / NiO produced by powder metallurgy. The nickel mixtures have been processed by the technique of powder metallurgy and were pre-sintered in an oven under plasma reducing atmosphere of hydrogen. Mixtures Ni +15%NiO, Ni +25%NiO and Ni +35%NiO were studied and compared with samples consisting only of metallic Ni. Dilatometric tests were performed to study the sintering conditions of the mixtures. The consolidated material was analyzed for their microstructure and microhardness. Dilatometry graphs showed that the addition of nickel oxide in all compositions the active sintering the mixtures studied. In tests of microhardness indentations were made at different points of the sample surface. All compositions showed microhardness values close to the consolidated material from metallic nickel. However, sample containing Ni+35% NiO, showed a large dispersion of the values of microhardness tests performed at different points of the sample surface. Microstructural analysis of the material showed a higher concentration of voids and the presence of oxides in the waste composition of the mixtures Ni 35% NiO. The samples containing Ni+15%NiO showed microstructural characteristics and mechanical properties similar to metallic nickel consolidated under the same conditions of the compositions studied in this work and therefore had great potential for production of sintered nickel alloys
Resumo:
The Nb-Cu pseudoalloys present themselves as potential substitutes for the alloys from a well known system and already commercially applied, as the W-Cu alloys, used in applications such as heat sinks, electrical contacts and coils for the generation of high magnetic fields. Because it is an immiscible system, where there is mutual insolubility and low wettability of the liquid Cu on the Nb surface, the processing route used in this work was the Powder Metallurgy. Two Nb alloys were used, with additions of 10% and 20% in weight of Cu, and times of 20, 30 and 40 hours for the high energy milling of the starting powders. The milling evolution of the powders is presented through the characterization techniques, such as the LASER diffraction for particle size, XRD, SEM, EDS, DSC, dilatometry, TEM and chemical analysis. After the milling, portions of the loads were submitted to the annealing heat treatment. The process used for the samples consolidation was the hot pressing, which has been applied both on some milled powders samples, as on the annealed powders. Subsequent heat treatments were performed in the samples at temperatures of 1000ºC (solid phase) and 1100ºC (in the Cu liquid phase). All sets of consolidated samples, and also the two sets of the heat treated, were analyzed by XRD, SEM, EDS, density and Vickers microhardness. Moreover, other Nb powder samples with 10% and 20% in weight of Cu obtained by simple mechanical mixing, were consolidated, thermally treated and characterized with the same techniques applied to the others, and the results were compared among themselves. Despite the difficulty of consolidation and densification of the two pseudoalloys of the Nb-Cu system of this study, on the route that passes through the HEM, samples were obtained with densities around 90% of the theoretical density. And, on the processing route of which were only mixed, the values reached up to 97%. Therefore, in this work are also emphasized the processes that made possible these results.
Resumo:
Ceramic materials alumina basis have been widely used in structural components, mainly because owning properties such as high hardness, chemical inertness and good wear resistance, however, the low toughness is a factor that compromises its use in many other applications, featuring the addition of nickel as a possible solution to this problem, in this context, this work aims to study the addition of nickel alumina using the route of powder metallurgy processing of the material. The percentage of nickel were added 2, 4 and 6 wt%; and each composition to high energy milling in a planetary mill was performed for 2, 4, 9 and 16h. Subsequently, the samples were compacted at 300 MPa and sintered in a vacuum oven at 1400⁰C for 2h. The samples were characterized as the physical and mechanical properties, observing, in general, an improvement in sinterability of the material with increasing grinding time and nickel content, and mixing with a decrease of porosity and increase of hardness, density values above 80% of theoretical were obtained. The milling time of 4 hours and addition of 2% nickel, particularly if achieved higher hardness (HV 1068.7 +/- 32.6) and density of about 99% theoretical density.
Resumo:
Ceramic materials alumina basis have been widely used in structural components, mainly because owning properties such as high hardness, chemical inertness and good wear resistance, however, the low toughness is a factor that compromises its use in many other applications, featuring the addition of nickel as a possible solution to this problem, in this context, this work aims to study the addition of nickel alumina using the route of powder metallurgy processing of the material. The percentage of nickel were added 2, 4 and 6 wt%; and each composition to high energy milling in a planetary mill was performed for 2, 4, 9 and 16h. Subsequently, the samples were compacted at 300 MPa and sintered in a vacuum oven at 1400⁰C for 2h. The samples were characterized as the physical and mechanical properties, observing, in general, an improvement in sinterability of the material with increasing grinding time and nickel content, and mixing with a decrease of porosity and increase of hardness, density values above 80% of theoretical were obtained. The milling time of 4 hours and addition of 2% nickel, particularly if achieved higher hardness (HV 1068.7 +/- 32.6) and density of about 99% theoretical density.
Resumo:
Carbide reinforced metallic alloys potentially improve some important mechanical properties required for the overall use of important engineering materials such as steel and nickel. Nevertheless, improved performance is achieved not only by composition enhancement but also by adequate processing techniques, such as novel sintering methods in the case of powder metallurgy. The method minimizes energy losses in addition to providing uniform heating during sintering. Thus, the general objective of this study was to evaluate the density, hardness, flexural strength, dilatometric behavior and to analyze the microstructure of metal matrix composites based nickel with addition of carbides of tantalum and / or niobium when sintered in a conventional furnace and Plasma assisted debinding and sintering (PADS). Initially, were defineds best parameters of granulation, screening and mixing procedure. After, mixtures of carbonyl Ni and 5%, 10% and 15 wt.% NbC and TaC were prepared in a Y-type mixer under wet conditions during 60 minutes. The mixtures were then dried and granulated using 1.5 wt. % paraffin diluted in hexane. Granulates were cold pressed under 600 MPa. Paraffin was then removed from the pressed pellets during a pre-sintering process carried out in a tubular furnace at 500 °C during 30 min. The heating rate was 3 ºC/min. The pellets were then sintered using either a plasma assisted reactor or a conventional resistive tubular furnace. For both methods, the heating rate was set to 8 ºC/min up to 1150 °C. The holding time was 60 minutes. The microstructure of the sintered samples was evaluated by SEM. Brinell hardness tests were also carried out. The results revealed that higher density and higher hardness values were observed in the plasma-assisted sintered samples. Hardness increased with the concentration of carbides in the Ni-matrix. The flexural strength also increased by adding the carbides. The decline was larger for the sample with addition of 5% 5% TaC and NbC. In general, compositions containing added carbide 10% showed less porous and more uniform distribution of carbides in the nickel matrix microstructural appearance. Thus, both added carbide and plasma sintering improved density, hardness, flexural strength and microstructural appearance of the composites
Resumo:
It seeks to find an alternative to the current tantalum electrolytic capacitors in the market due to its high cost. Niobium is a potential substitute, since both belong to the same group of the periodic table and because of this have many similar physical and chemical properties. Niobium has several technologically important applications, and Brazil has the largest reserves, around 96%. There are including niobium in reserves of tantalite and columbite in Rio Grande do Norte. These electrolytic capacitors have high capacitance specifies, ie they can store high energy in small volumes compared to other types of capacitors. This is the main attraction of this type of capacitor because is growing demand in the production of capacitors with capacitance specifies increasingly high, this because of the miniaturization of various devices such as GPS devices, televisions, computers, phones and many others. The production route of the capacitor was made by powder metallurgy. The initial niobium powder supplied by EEL-USP was first characterized by XRD, SEM, XRF and laser particle size, to then be sieved into three particle size, 200, 400 e 635mesh. The powders were then compacted and sintered at 1350, 1450 and 1550°C using two sintering time 30 and 60min. Sintering is one of the most important parts of the process as it affects properties as porosity and surface cleaning of the samples, which greatly affected the quality of the capacitor. The sintered samples then underwent a process of anodic oxidation, which created a thin film of niobium pentóxido over the whole porous surface of the sample, this film is the dielectric capacitor. The oxidation process variables influence the performance of the film and therefore the capacitor. The samples were characterized by electrical measurements of capacitance, loss factor, ESR, relative density, porosity and surface area. After the characterizations was made an annealing in air ate 260ºC for 60min. After this treatment were made again the electrical measurements. The particle size of powders and sintering affected the porosity and in turn the specific area of the samples. The larger de area of the capacitor, greater is the capacitance. The powder showed the highest capacitance was with the smallest particle size. Higher temperatures and times of sintering caused samples with smaller surface area, but on the other hand the cleaning surface impurities was higher for this cases. So a balance must be made between the gain that is achieved with the cleaning of impurities and the loss with the decreased in specific area. The best results were obtained for the temperature of 1450ºC/60min. The influence of annealing on the loss factor and ESR did not follow a well-defined pattern, because their values increased in some cases and decreased in others. The most interesting results due to heat treatment were with respect to capacitance, which showed an increase for all samples after treatment
Resumo:
The development and study of detectors sensitive to flammable combustible and toxic gases at low cost is a crucial technology challenge to enable marketable versions to the market in general. Solid state sensors are attractive for commercial purposes by the strength and lifetime, because it isn t consumed in the reaction with the gas. In parallel, the use of synthesis techniques more viable for the applicability on an industrial scale are more attractive to produce commercial products. In this context ceramics with spinel structure were obtained by microwave-assisted combustion for application to flammable fuel gas detectors. Additionally, alternatives organic-reducers were employed to study the influence of those in the synthesis process and the differences in performance and properties of the powders obtained. The organic- reducers were characterized by Thermogravimetry (TG) and Derivative Thermogravimetry (DTG). After synthesis, the samples were heat treated and characterized by Fourier Transform Infrared Spectroscopy (FTIR), X-ray Diffraction (XRD), analysis by specific area by BET Method and Scanning Electron Microscopy (SEM). Quantification of phases and structural parameters were carried through Rietveld method. The methodology was effective to obtain Ni-Mn mixed oxides. The fuels influenced in obtaining spinel phase and morphology of the samples, however samples calcined at 950 °C there is just the spinel phase in the material regardless of the organic-reducer. Therefore, differences in performance are expected in technological applications when sample equal in phase but with different morphologies are tested
Resumo:
The clay mineral attapulgite is a group of hormitas, which has its structures formed by microchannels, which give superior technological properties classified the industrial clays, clays of this group has a very versatile range of applications, ranging from the drilling fluid for wells oil has applications in the pharmaceutical industry. Such properties can be improved by activating acid and / or thermal activation. The attapulgite when activated can improve by up to 5-8 times some of its properties. The clay was characterized by X-ray diffraction, fluorescence, thermogravimetric analysis, differential thermal analysis, scanning electron microscopy and transmission electron microscopy before and after chemical activation. It can be seen through the results the efficiency of chemical treatment, which modified the clay without damaging its structure, as well as production of polymer matrix composites with particles dispersed atapugita
Resumo:
This research studies the sintering of ferritic steel chips from the machining process. Were sintered metal powder obtained from machining process chips for face milling of a ferritic steel. The chip was produced by machining and characterized by SEM and EDS, and underwent a process of high energy mill powder characterized also by SEM and EDS. Were constructed three types of matrixes for uniaxial compression (relation l / d greater than 2.5). The differences in the design of the matrixes were essentially in the direction of load application, which for cylindrical case axial direction, while for the rectangular arrays, the longer side. Two samples were compressed with different geometries, a cylindrical and rectangular with the same compaction pressure of 700 MPa. The samples were sintered in a vacuum resistive furnace, heating rate 20 °C / min., isotherm 1300 °C for 60 minutes, and cooling rate of 25 °C / min to room temperature. The starting material of the rectangular sample was further annealed up to temperature of 800 ° C for 30 min. Sintered samples were characterized by scanning electron microscopy, optical microscopy and EDS. The sample compressed in the cylindrical matrix did not show a regular density reflecting in the sintered microstructure revealed by the irregular geometry of the pores, characterizing that the sintering was not complete, reaching only the second phase. As for the specimen compacted in the rectangular array, the analysis performed by scanning electron microscopy, optical microscopy and EDS indicate a good densification, and homogeneous microstructure in their full extent. Additionally, the EDS analyzes indicate no significant changes in chemical composition in the process steps. Therefore, it is concluded that recycling of chips, from the processed ferritic steel is feasible by the powder metallurgy. It makes possible rationalize raw material and energy by manufacture of known properties components from chips generated by the machining process, being benefits to the environment
Resumo:
Nickel alloys are frequently used in applications that require resistance at high temperatures associated with resistance to corrosion. Alloys of Ni-Si-C can be obtained by means of powder metallurgy in which powder mixtures are made of metallic nickel powders with additions of various alloying carriers for such were used in this study SiC, Si3N4 or Si metal with graphite. Carbonyl Ni powder with mean particle size of 11 mM were mixed with 3 wt% of SiC powders with an average particle size of 15, 30 and 50 μm and further samples were obtained containing 4 to 5% by mass of SiC with average particle size of 15 μm. Samples were also obtained by varying the carrier alloy, these being Si3N4 powder with graphite, with average particle size of 1.5 and 5 μm, respectively. As a metallic Si graphite with average particle size of 12.5 and 5 μm, respectively. The reference material used was nickel carbonyl sintered without adding carriers. Microstructural characterization of the alloys was made by optical microscopy and scanning electron microscopy with semi-quantitative chemical analysis. We determined the densities of the samples and measurement of microhardness. We studied the dissociation of carriers alloy after sintering at 1200 ° C for 60 minutes. Was evaluated also in the same sintering conditions, the influence of the variation of average particle size of the SiC carrier to the proportion of 3% by mass. Finally, we studied the influence of variation of the temperatures of sintering at 950, 1080 and 1200 ° C without landing and also with heights of 30, 60, 120 and 240 minutes for sintering where the temperature was 950 °C. Dilatometry curves showed that the SiC sintered Ni favors more effectively than other carriers alloy analyzed. SiC with average particle size of 15 μm active sintering the alloy more effectively than other SiC used. However, with the chemical and morphological analyzes for all leagues, it was observed that there was dissociation of SiC and Si3N4, as well as diffusion of Si in Ni matrix and carbon cluster and dispersed in the matrix, which also occurred for the alloys with Si carriers and metallic graphite. So the league that was presented better results containing Si Ni with graphite metallic alloy as carriers, since this had dispersed graphite best in the league, reaching the microstructural model proposed, which is necessary for material characteristic of solid lubricant, so how we got the best results when the density and hardness of the alloy
Resumo:
The MCM-41 mesoporous synthesis was done using rice hulls ash and chrysotile as natural alternative silica sources. For the using of these sources, chemical and thermic treatments were done in both materials. After chemical and thermic treatments, these materials were employed on the MCM-41 mesoctructures synthesis. The natural materials treated and employed in the synthesis were characterized by several techniques such as X-ray diffraction, N2 adsorption and desorption, scanning electronic microscopy and thermogravimetric analysis. MCM-41 standart samples synthetized with aerosil 200 commercial sílica were used to evaluation. The formed material from rice hulls ash showed values from BET specific area about 468 m².g-1, N2 adsorption and desorption isotherms and loss mass similar to reference materials. The silica from chrysotile calcined and leached was employed to mesoporous materials synthesis. The BET specific area showed values about 700 m².g-1, N2 adsorption and desorption isotherms type IV and loss mass similar to mesoporous materials. The formed material from calcined and leached chrysotile, without calcination, applied to phenol remotion carried high performance liquid chromatography and evaluated with organophilic clays with different treatments. By the characterization techniques were proved that mesoporous materials with lesser order that reference samples. The material formed from rice hulls ash without the calcination step achieved better adsorption results than organophilic clays
Resumo:
The 15Kh2MFA steel is a kind of Cr-Mo-V family steels and can be used in turbines for energy generation, pressure vessels, nuclear reactors or applications where the range of temperature that the material works is between 250 to 450°C. To improve the properties of these steels increasing the service temperature and the thermal stability is add a second particle phase. These particles can be oxides, carbides, nitrites or even solid solution of some chemical elements. On this way, this work aim to study the effect of addition of 3wt% of niobium carbide in the metallic matrix of 15Kh2MFA steel. Powder metallurgy was the route employed to produce this metallic matrix composite. Two different milling conditions were performed. Condition 1: milling of pure 15Kh2MFA steel and condition 2: milling of 15Kh2MFA steel with addition of niobium carbide. A high energy milling was carried out during 5 hours. Then, these two powders were sintered in a vacuum furnace (10-4torr) at 1150 and 1250°C during 60 minutes. After sintering the samples were normalized at 950°C per 3 minutes followed by air cooling to obtain a desired microstructure. Results show that the addition of niobium carbide helps to mill faster the particles during the milling when compared with that steel without carbide. At the sintering, the niobium carbide helps to sinter increasing the density of the samples reaching a maximum density of 7.86g/cm³, better than the melted steel as received that was 7,81g/cm³. In spite this good densification, after normalizing, the niobium carbide don t contributed to increase the microhardness. The best microhardness obtained to the steel with niobium carbide was 156HV and to pure 15Kh2MFA steel was 212HV. It happened due when the niobium carbide is added to the steel a pearlitic structure was formed, and the steel without niobium carbide submitted to the same conditions reached a bainitic structure