2 resultados para Vidros fosfo-boratos com titânio
em Repositório da Produção Científica e Intelectual da Unicamp
Resumo:
Glass-ceramics are prepared by controlled separation of crystal phases in glasses, leading to uniform and dense grain structures. On the other hand, chemical leaching of soluble crystal phases yields porous glass-ceramics with important applications. Here, glass/ceramic interfaces of niobo-, vanado- and titano-phosphate glasses were studied by micro-Raman spectroscopy, whose spatial resolution revealed the multiphase structures. Phase-separation mechanisms were also determined by this technique, revealing that interface composition remained unchanged as the crystallization front advanced for niobo- and vanadophosphate glasses (interface-controlled crystallization). For titanophosphate glasses, phase composition changed continuously with time up to the equilibrium composition, indicating a spinodal-type phase separation.
Resumo:
The copolymer poly (L-co-D,L lactic acid), PLDLA, has gained prominence in the field of temporary prostheses due to the fact that their time of degradation is quite compatible with the requirement in the case of osseous fracture. In this work the in vivo degradation of devices from copolymer, as a system of plates and screws, used in fixation of the tibia of rabbits was studied. The devices were implanted in 15 adult rabbits, albinos, New Zealand race, and they were used as control devices of alloys of titanium (Ti-6Al-4V/ V grade). The use of copolymers, synthesized in the laboratory, was tested in the repair of fracture in rabbits'tibias, being assessed in the following times: 2 weeks, 2 months and 3 months. Morphological analysis of tissue surrounding the plate and screw system, for 2 weeks of implantation, showed the presence of osteoblasts, indicating a pre bone formation. After 2 months there was new bone formation in the region in contact with the polymer. This bone growth occurred simultaneously with the process of PLDLA degradation, invading the region where there was polymer and after 3 months there was an intense degradation of the copolymer and hence greater tissue invasion compared to 2 months which characterized bone formation in a region where the polymer degraded. The in vivo degradation study of the devices for PLDLA by means of histological evaluations during the period of consolidation of the fracture showed the efficiency of plate and screw system, and it was possible to check formation of bone tissue at the implantation site, without the presence of inflammatory reaction