80 resultados para SRS-CU


Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper presents the electrolyte influence on deposition and dissolution processes of Cu nanoparticles on boron doped diamond electrodes (BDD). Morphological, structural and electrochemical analysis showed BDD films with good reproducibility, quality and reversible in a specific redox system. Electrodeposition of Cu nanoparticles on DDB electrodes in three different solutions was influenced by pH and ionic strength of the electrolytic medium. Analyzing the process as function of the scan rate, it was verified a better efficiency in 0,5 mol L-1 Na2SO4 solution. Under the influence of the pH and ionic strength, Cu nanoparticles on DDB may be obtained with different morphologies and it was important for defining the desired properties.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work applied a 2² factorial design to the optimization of the extraction of seven elements (calcium, magnesium, potassium, iron, zinc, copper and manganese) in brachiaria leaves, determined by flame atomic absorption spectrometry. The factors sample mass and digestion type were evaluated at two levels: 200/500 mg, and dry/wet, respectively. Principal component analysis allowed simultaneous discrimination of all the significant effects in one biplot. Wet digestion and mass of 200 mg were considered the best conditions. The decrease of 60% in sample mass allowed to save costs and reagents. The method was validated through the estimation of figures of merit.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work studies the effect of NTMP (nitrilotris(methylenephosphonic acid)) on the adsorption of Cu(II), Zn(II), and Cd(II) onto boehmite in the pH range 5-9.5. The data were analyzed using the 2-pK constant capacitance model (CCM) assuming ternary surface complex formation. Under stoichiometric conditions, NTMP is more effective for removing Cu(II) than Zn(II) from solution and the contribution of ternary surface complexes are important to model the adsorption of both metals. Under nonstoichiometric conditions and high surface loading with a Me(II)/NTMP ratio of 1:5, Cu(II) and Zn(II) adsorption is significantly suppressed. In the case of Cd(II) the free metal adsorption is the most dominant species.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An Nb2O|Cu corrosion-resistant coating was developed and applied onto AISI 1020 steel substrate by Powder Flame Spray. A galvanostatic electrochemical technique was employed, with and without ohmic drop, in four different soils (two corrosively aggressive and two less aggressive). Behavior of coatings in different soils was compared using a cathodic hydrogen reduction reaction (equilibrium potential, overvoltage and exchange current density) focusing on the effect of ohmic drop. Results allow recommendation of Nb2O5|Cu composite for use in buried structure protection.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A sequential extraction procedure was applied to wheat and soybean seed samples. The total protein content (determined by two distinct methods: Bradford and bicinchoninic acid-BCA) and distribution of Cu, Fe, Mn and Zn in each fraction was determined. The sequential extraction employed four different solutions: water, 0.5 mol L-1 NaCl, ethanol/water (70:30 v v-1) and 0.5 mol L-1 NaOH. For both samples, the highest concentration of metals was observed in those extracts associated with globulin-type proteins using NaCl solution. Regarding protein content, higher levels were obtained using the BCA method.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A simultaneous solid phase extraction procedure for enrichment of Cu(II), Cd(II) and Mn(II) has been developed. The method is based on adsorption of Cu(II), Cd(II) and Mn(II) ions on polyethylene glycol-silica gel pre-conditioned with acetate buffer (pH 5.5). The adsorbed metal ions are eluted with nitric acid (1 mol L -1) and determined by flame atomic absorption spectrometry. The calibration graph was linear in the range of 2-140 ng mL-1 for Cu(II), 1-40 ng mL-1 for Cd(II) and 4-100 ng mL-1 for Mn(II). The limits of detection were 0.66, 0.33 and 1.20 ng mL-1 for Cu(II), Cd(II) and Mn(II), respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The metal distribution in the surface sediment fractions of the Cachoeira River was evaluated based on the fractionation method using a five-step sequential extraction. The determination of metals was made by flame atomic absorption spectrophotometry (F AAS). Zn, Pb and Cu exhibit higher concentrations in the residual fraction of the sediment from sites that receive discharges from urban and industrial zones. High levels of Ni (60 ± 1 to 447 ± 9 µg L-1) were found in the river water, which may be detrimental to the "health" of rural communities that utilize the river water for domestic purposes without treatment.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper describes the evaluation of a new method of sample preparation using a cold finger system with continuous water flow for rice analysis by flame atomic absorption spectrometry. The limits of detection for Cu, Fe, Mn and Zn for the proposed method were 0.36, 1.84, 2.12 and 0.16 mg kg-1, respectively. The RSDs were lower than 6.0% for all elements and the CRM analyzed showed values with 95% agreement. The proposed method is simple and safe for the proposed objective and does not require the use of mixtures of acid or special equipment for sample preparation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Synthesis, spectral identification, and magnetic properties of three complexes of Ni(II), Cu(II), and Zn(II) are described. All three compounds have the general formula [M(L)2(H2O)2], where L = deprotonated phenol in the Schiff base 2-((z)-(3-methylpyridin-2-yleimino)methyl)phenol. The three complexes were synthesized in a one-step synthesis and characterized by elemental analysis, Fourier transform infrared spectroscopy, electronic spectra, X-ray diffraction (XRD), and room temperature magnetic moments. The Cu(II) and Ni(II) complexes exhibited room temperature magnetic moments of 1.85 B.M. per copper atom and 2.96 B.M. per nickel atom. The X-band electron spin resonance spectra of a Cu(II) sample in dimethylformamide frozen at 77 K (liquid nitrogen temperature) showed a typical ΔMS = ± 1 transition. The complexes ([M(L)2(H2O)2]) were investigated by the cyclic voltammetry technique, which provided information regarding the electrochemical mechanism of redox behavior of the compounds. Thermal decomposition of the complexes at 750 ºC resulted in the formation of metal oxide nanoparticles. XRD analyses indicated that the nanoparticles had a high degree of crystallinity. The average sizes of the nanoparticles were found to be approximately 54.3, 30.1, and 44.4 nm for NiO, CuO, and ZnO, respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Optimization of the main parameters of SWASV using boron-doped diamond electrode was described for the simultaneous determination of Zn, Cd, Pb and Cu free in coconut water. The values of electroanalytical parameters studied were optimized with the factorial design and center composite design. The optimized parameters for the preconcentration of metals were -1.50 V for potential, and 240 s for deposition time. For SWV, the optimized value was 11.56 mV for step potential. In addition, frequency and pulse height were defined at 100 Hz and 55 mV, respectively. Furthermore, the concentration of the supporting electrolyte (acetate buffer, pH 4.7) was optimized in 0.206 mol L-1. The optimized procedure was applied in two samples of coconut water: natural and processed. The limits of detection (LOD) obtained for Zn, Cd, Pb and Cu were 7.2; 4.4; 3.3 and 1.5 µg L-1, respectively. The concentrations of Cd and Pb were not detected. On the other hand, the values found for the concentrations of Zn and Cu were: < LOD (29 µg L-1) and (6.8 ± 0.9) µg L-1 for the natural sample; and (85.8 ± 4.2) µg L-1 and (7.7 ± 0.6) µg L-1 for the processed sample, respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A influência de adições de 2%, 4%, 6%, 8% e 10% de prata, em massa, na cinética de formação e precipitação de precipitados ricos em prata, na liga Cu-5% Al foi estudada através de medidas de variação da microdureza com a temperatura e o tempo. Os resultados obtidos indicaram que a presença da prata aumenta consideravelmente a dureza da liga e também interfere na cinética de precipitação, com uma mudança mecanística no processo que está relacionada com o teor de prata das ligas.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

As temperaturas onde ocorre a solubilização da fase rica em prata, em ligas de Cu-Al-Ag, foram determinadas através de medidas de variação da resistência elétrica com a temperatura. As derivadas das curvas obtidas experimentalmente permitiram determinar com precisão essas temperaturas e também que se traçasse um esboço da região onde ocorre a transição monofásica para bifásica.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Estudou-se a influência de adições de 2, 6 e 8% Ag, em peso, na resistividade elétrica da liga Cu-5%Al, utilizando-se o método dos quatro pontos e um sistema de registro contínuo de variação da resistividade elétrica com a temperatura. Os resultados obtidos indicaram que a resistividade elétrica da liga aumenta com o aumento da concentração de prata e que as inflexões observadas nas curvas de variação da resistividade com a temperatura de aquecimento podem ser atribuídas à solubilização da prata na matriz de Cu-Al. Observou-se também que a velocidade de aquecimento da amostra é um fator importante na intensidade e forma dos eventos observados.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A influência de adições de 2, 4, 6 e 8% de prata, em peso, na cinética de recristalização da liga Cu-5%Al com taxas de deformação de 40, 70 e 90%, foi estudada utilizando-se metalografia por microscopia óptica e medidas de variação do tamanho de grão com o tempo e a temperatura de envelhecimento. Os resultados obtidos indicaram uma diminuição na velocidade de crescimento dos grãos e na energia de ativação correspondente, com o aumento da concentração de prata.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

As energias de ativação para nucleação de precipitados ricos em prata e de difusão da prata no cobre, em ligas de Cu-2%Al contendo 2, 4, 6, 8, 10 e 12%Ag, em peso, foram determinadas utilizando-se medidas de variação da microdureza com a temperatura e o tempo de envelhecimento. Os resultados indicaram que, com o método utilizado, é possível obter valores para as energias de ativação para nucleação da fase rica em prata e de difusão da prata no cobre bastante próximos daqueles citados na literatura.