51 resultados para AMORPHOUS V2O5
Resumo:
Large areas of Plinthosols with ferruginous materials such as plinthite and/or petroplinthite are fairly common in the Brazilian Amazon basin. This work was carried out to investigate the chemical behavior, mineralogical composition and weathering stage of four representative soil profiles with plinthite and petroplinthite, in Iranduba, AM (Central Amazon). Three well-drained soil profiles at high elevations were studied (P1, Plinthic Vetic Ferralsol; P2 and P3, Vetic Endopetric Plinthosol) and a contrasting poorly drained soil (P4 Haplic Plinthosol), located at low elevation. After profile descriptions, soil samples were collected from each horizon, air-dried, sieved (2 mm), and analyzed for particle-size distribution, pH, exchangeable cations (Al3+, Ca2+, Mg2+, K+, and Na+), as well as available P and total organic carbon (TOC) content. The minerals present in the clay and sand fractions, as well as in the ferruginous materials were identified by X-ray Diffraction (XRD). The weathering stage of these soils was assessed by means of Ki and Kr indexes, and the amounts of free and amorphous Fe and Al oxides by using dithionite citrate bicarbonate (DBC) and ammonium oxalate dissolution procedures, respectively. The results showed that all soils were extremely unfertile, with pH levels ranging between strong and moderate acidity, very low sum of bases and organic matter content, and of available P. The mineralogy of the soil profiles was very similar, mainly of the well-drained soils, with predominance of kaolinite and quartz in the clay and sand fractions, respectively. In the poorly-drained P4, 2:1 clay particles were also observed. These profiles can be considered highly developed according to the Ki index, however, the Ki value of P4 was higher, indicating that this soil was less developed than the others. In summary, these profiles with plinthite and petroplinthite can be characterized as highly developed and infertile soils and are, with exception of P4, well-drained.
Resumo:
Boron adsorption was studied in five representative soils (Rhodic Hapludox, Arenic Paleudalf and three Typic Hapludox) from the State of São Paulo, Brazil. Adsorption was higher in the clayey Oxisols, followed by the Alfisol and the coarser Oxisols. Calcium carbonate promoted an increase in the amount of adsorbed boron in all soils, with the most pronounced effect in the coarser-textured Oxisols. High correlation coefficients were found between adsorbed boron and clay and amorphous aluminum oxide contents and specific surface area (r = 0.79, 0.76 and 0.73, respectively, p < 0.01). Clay content, free aluminum oxide, and hot CaCl2 (0.01 mol L-1)-extracted boron explained 93% of the variation of adsorbed boron. Langmuir and Freundlich isotherms fitted well to the adsorbed data, and highest values for maximum boron adsorption were found in clayey soils, which were significantly correlated with contents of total, free and amorphous iron and aluminum oxides, as well with the physical attributes. Ninety four percent of the variation in the maximum adsorption could be related to the free iron content.
Resumo:
The catalytic decomposition of soybean oil was studied in a fix bed reactor at 673 and 773 K and using amorphous silica-alumina and the zeolites USY, H-Mordenite and H-ZSM-5 as catalysts. Both the selectivity and the catalytic activity were determined by studying the product composition resulting from the chemical reactions. Physicochemical characteristics of the catalysts were obtained by X-ray fluorescence, Fourier Transform infrared spectroscopy, 29Si and 27Al Nuclear Magnetic Ressonance and textural analysis. The zeolites USY and H-ZSM-5, showing higher Brönsted acidity, yielded products with higher concentration in aromatic hydrocarbons, whereas with both H-Mordenite and amorphous silica-alumina the main products were paraffins.
Resumo:
Independent of the sample form (powder or film), XRD analysis of Ir0,3Ti(0,7-x)Ce xO2, (nominal) mixtures, for x=0, shows the formation of a solid solution phase between IrO2 and TiO2, as well as the rutile phases of IrO2 and TiO2. The presence of the anatase phase of TiO2 is also confirmed. The introduction of 30 mol% CeO2 in the mixture reveals the presence of the CeO2 and Ce2O3 phases, besides the already mentioned ones, in the powder. In the film form, however, an amorphous phase is identified. When all of the TiO2 is substituded by CeO2, for both sample forms, the only phases found are IrO2, CeO2 and Ce2O3. This result suggests cerium oxides are not capable of forming solid solutions with either IrO2 or (Ir,Ti)O2 acting solely as a dispersant matrix for these phases. These results are consistent with the much higher electrochemically active surface area when CeO2 is introduced in the binary Ti/Ir0,3Ti0,7O2 mixture. It was possible to establish a relationship between the electrochemical stability of the supported films and their crystalline structure. The unexpected presence of TiO2 and Ti2O3 in the Ti/Ir0,3Ce0,7O2 (film sample) is attributed to oxidation of the Ti support during the calcination step.
Resumo:
The characterization of rice husk ash, a deriving by-product of the burning of the rice husk during the rice processing is the object of this study. This by-product, for being rich in silica, can be an important raw material for the production of siliceous ceramics, such as thermal insulators and refractory. A combination of surface analysis, thermal analysis and microscopy analysis techniques was used for the characterization. The characterized by-product presented as main component the silica, under amorphous form, with a maximum content of alkalis around 1%, features that become it potentially interesting for the production of ceramic materials.
Resumo:
Copper, aluminum and iron concentrations were determined in four geochemical fractions of three different basaltic soils from the northwest region of the Parana State, Brazil. The fractions examined were the reducible manganese dioxide and amorphous iron oxide, crystaline iron oxide, organic and residual. Metal concentrations were determined in the extracts by flame atomic absorption spectrophotometry. High Fe concentrations were extracted from the crystalline iron oxide (>20%), as well as the amorphous iron oxide (>12%). Copper was extracted from the amorphous and crystalline iron oxides in the range 5 to 12%, but low concentrations were bound to organic matter. Low concentrations of aluminum were extracted (<8%) from the amorphous and crystaline iron oxides, and organic matter. High concentrations of aluminum were found in the residual fraction.
Resumo:
Nickel nanoparticles supported on amorphous silica ceramic matrix were synthesized by the polymeric precursor method. The nanostructure was characterized by NMR, BET, XRD, SEM, TEM, and flame atomic absorption spectrometry techniques. It was observed a dependence of the crystallite size on the thermal annealing, under a N2 atmosphere. The materials presented a high catalytic activity and selectivity upon the beta-pinene hydrogenation reaction. The magnetic hystereses were also correlated with the morphology of the processed material.
Resumo:
Titania powders were synthesized by a sol-gel process using titanium tetrabutoxide as precursor. The syntheses were performed in water or in solutions of dimethylformamide (dmf) or dimethylsulfoxide (dmso). It is demonstrated, by X-ray diffraction patterns of the synthesized powders, that the samples obtained in dmf or dmso solutions are crystalline (anatase phase) with some minor amount of brookite phase, whereas the sample synthesized in water is amorphous. The anatase phase can be obtained independently of any previous or further treatment of the synthesized powder, such as hydrothermal or heat treatment, providing a new, simple, quick and inexpensive route to synthesize anatase powders. From the peak broadening of the anatase (101) diffraction, the crystallite sizes were calculated as 6 nm.
Resumo:
A layered matrix, alpha-VOPO4.2H2O was used as host species to produce a VOPO4.dimethylacetamide intercalation compound. The oxovanadium matrix and the synthesized hybrid were characterized by elemental analysis, infrared spectroscopy, thermogravimetry, X-ray diffractometry and SEM microscopy. The X-ray diffraction patterns show that the VOPO4.dimethylacetamide compound is amorphous, but can be turned lamellar after a solubilization-crystallization process. The SEM micrographs obtained for the VOPO4-dimethylacetamide hybrid matrix show that the microstructure of VOPO4.2H2O is changed after reaction, with a delamination of the oxovanadium matrix.
Resumo:
This work presents a study on the dissolution of some commercial monometallic and non-supported deactivated catalysts in HF + H2O2 mixtures (and, eventually, other media) under mild experimental conditions, after a previous oxidation step. The samples were neither crushed nor grinded. The best experimental conditions were dependent on the nature of the support and of the active phase. For example, the Pt/Al2O3 catalyst was dissolved in about 10 minutes, without agitation and heating; however, dissolution of the Pd/Al2O3, Ni/Al2O3, Ni/SiO2, Cu/Al2O3 and V2O5 samples required a temperature of 60 ºC and an agitation of 400 rpm. A careful addition of a NaOH solution allowed a quantitative precipitation of aluminium as criolite (Na3AlF6) or precipitation of Si as Na2SiF6; NaF was obtained as a by-product. As expected, processing of Pd/C, V2O5 and CuO.Cr2O3 samples was relatively simple. Metals recovery from catalysts reached a quantitative level in all samples studied; it is particularly interesting that platinum and palladium could be easily recovered in a single step process, thus separing them from aluminium.
Resumo:
Ca1-xLa xTiO3 powders were prepared by the polymeric precursor method. X-ray diffraction (XRD), FT-Raman spectroscopy, transmission electron microscopy (TEM), and N2 and CO2 adsorption were used for the microstructural and surface characterization of the powders. Room temperature photoluminescence (PL) was observed in Ca1-xLa xTiO3 amorphous particles. The PL intensity of these powders was found to be dependent on the lanthanum molar concentration.
Resumo:
Thermal decomposition of [Bu4N]2[Zn(imnt)2] and [M(NH3)2(imnt)] complexes with M = Zn and Cd, and imnt = (bis 1,1-dicyanoethylene-2,2 dithiolate) in inert atmosphere was investigated by thermogravimetric analysis (TG) and differential scanning calorimetry (DSC). Pyrolysis studies at different temperatures, 300, 400, 500, and 600 ºC, in N2 atmosphere were performed and the products were characterized by X-ray diffraction (XRD), infrared and Raman spectroscopy, and scanning electron microscopy (SEM). The products were identified as sulfide sub-micron particles, along with amorphous carbon. Particle sizes estimated by SEM were ca. 50 nm for the cationic complexes and 500 nm for the neutral complexes.
Resumo:
We have produced nanocomposite films of Ni:SiO2 by an alternative polymeric precursor route. Films, with thickness of ~ 1000 nm, were characterized by several techniques including X-ray diffraction, scanning electron microscopy, atomic force microscopy, flame absorption atomic spectrometry, and dc magnetization. Results from the microstructural characterizations indicated that metallic Ni-nanoparticles with average diameter of ~ 3 nm are homogeneously distributed in an amorphous SiO2 matrix. Magnetization measurements revealed a blocking temperature T B ~ 7 K for the most diluted sample and the absence of an exchange bias suggesting that Ni nanoparticles are free from an oxide layer.
Resumo:
A comparison between silica by acid leaching of rice husk (RH) and silica obtained from thermal treatment of rice husk ash (RHA) is presented. The best leaching results were obtained using 10% hydrochloric acid followed by washing with water. The alternative method, calcination of RHA at 700 ºC for 6 h followed by grinding for 80 min, was more effective. Silica obtained from RH was about 97% amorphous, had a 17.37 µm mean particle size, and a specific surface area of 296 m²/g. On the other hand, for silica obtained from RHA the values were about 95% amorphous material 0.68 µm, and 81 m²/g.
Resumo:
A study on optimization of bath parameters for electrodeposition of Fe-W-B alloys from plating baths containing ammonia and citrate is reported. A 2³ full factorial design was successfully employed for experimental design analysis of the results. The corrosion resistance and amorphous character were evaluated. The bath conditions obtained for depositing the alloy with good corrosion resistance were: 0.01 M iron sulfate, 0.10 M sodium tungstate and 0.60 M ammonium citrate. The alloy was deposited at 12% current efficiency. The alloy obtained had Ecorr -0.841 V and Rp 1.463 x 10(4) Ohm cm². The deposit obtained under these conditions had an amorphous character and no microcracks were observed on its surface. Besides this, the bath conditions obtained for depositing the alloy with the highest deposition efficiency were: 0.09 M iron sulfate, 0.30 M sodium tungstate and 0.50 M ammonium citrate. The alloy was deposited at 50% current efficiency, with an average composition of 34 wt% W, 66 wt% Fe and traces of boron. The alloy obtained had Ecorr -0.800 V and Rp 1.895 x 10³ Ohm cm². Electrochemical corrosion tests verified that the Fe-W-B alloy deposited under both conditions had better corrosion resistance than Fe-Mo-B.