Resumo:
A series of waveguides was inscribed in a borosilicate glass (BK7) by an 11 MHz repetition rate femtosecond laser operating with pulse energies from 16 to 30 nJ and focused at various depths within the bulk material. The index modification was measured using a quantitative phase microscopy technique that revealed central index changes ranging from 5×10-3 to 10-2, leading to waveguides that exhibited propagation losses of 0.2 dB/cm at a wavelength of 633 nm and 0.6 dB/cm at a wavelength of 1550 nm with efficient mode matching, less than 0.2 dB, to standard optical fibers. Analysis of the experimental data shows that, for a given inscription energy, the index modification has a strong dependence on inscription scanning velocity. At higher energies, the index modification increases with increasing inscription scanning velocity with other fabrication parameters constant.
Resumo:
Ultrashort-pulse lasers with spectral tuning capability have widespread applications in fields such as spectroscopy, biomedical research and telecommunications1–3. Mode-locked fibre lasers are convenient and powerful sources of ultrashort pulses4, and the inclusion of a broadband saturable absorber as a passive optical switch inside the laser cavity may offer tuneability over a range of wavelengths5. Semiconductor saturable absorber mirrors are widely used in fibre lasers4–6, but their operating range is typically limited to a few tens of nanometres7,8, and their fabrication can be challenging in the 1.3–1.5 mm wavelength region used for optical communications9,10. Single-walled carbon nanotubes are excellent saturable absorbers because of their subpicosecond recovery time, low saturation intensity, polarization insensitivity, and mechanical and environmental robustness11–16. Here, we engineer a nanotube–polycarbonate film with a wide bandwidth (>300 nm) around 1.55 mm, and then use it to demonstrate a 2.4 ps Er31-doped fibre laser that is tuneable from 1,518 to 1,558 nm. In principle, different diameters and chiralities of nanotubes could be combined to enable compact, mode-locked fibre lasers that are tuneable over a much broader range of wavelengths than other systems.
Resumo:
We introduce two techniques to measure the efficiency of inter mode FWM with respect to intra mode FWM. The first technique allows an estimation of the additional FWM penalty for any given system; the second isolates the contribution of each mode. Measurements are compared to an analytical model showing the FWM signal increases by ∼2dB with inter mode phase matching.
Resumo:
The growth of highly functionalised poly allyl alcohol films by pulsed plasma polymerisation of CH2 double bond; length as m-dashCHCH2OH on biomedical grade polyurethane has been followed by X-ray photoelectron spectroscopy (XPS) and contact angle measurements. Film thickness is observed to increase approximately linearly with plasma modification time, suggesting a layer-by-layer growth mode of poly allyl alcohol. Water contact angle measurements reveal the change in the surface free energy of wetting decreases linearly with plasma modification up to the monolayer point after which a constant limiting value of −24 mJ m−2 was attained. Films prepared at 20 W plasma power with a duty cycle of 10 μs:500 μs exhibit a high degree of hydroxyl (single bondOH) retention with minimal fragmentation of the monomer observed. Increasing the plasma power up to 125 W is found to improve single bondOH retention at the expense of ether formation generating films close to the monomer stoichiometry. Duty cycle plays an important role in controlling both film composition and thickness, with longer off times increasing single bondOH retention, while longer on times enhance allyl alcohol film growth.
Resumo:
We present the first demonstration of a tunable FBG device in POF utilizing thin-film resistive heater deposited on the fiber. A wavelength shift of 2nm, wavelength/power coefficient of -13.4pm/mW and T = 1.7s-1 are achieved.
Resumo:
We present what is to our knowledge the first demonstration of a tunable fiber Bragg grating device in polymer optical fiber that utilizes a thin-film resistive heater deposited on the surface of the fiber. The polymer fiber was coated via photochemical deposition of a Pd/Cu metallic layer with a procedure induced by vacuum-ultraviolet radiation at room temperature. The resulting device, when wavelength tuned via joule heating, underwent a wavelength shift of 2 nm for a moderate input power of 160 mW, a wavelength to input power coefficient of-13.4 pm/mW, and a time constant of 1.7 s-1. © 2007 Optical Society of America.
Resumo:
The femtosecond laser modification of refractive index in amorphous Al2O3:Nd thin film prepared by rf magnetron sputtering is investigated. Modifications of the refractive index in a sample with a single Al2O3:Nd layer and in a sample composed of the Al2O3:Nd layer and SiO2 layer on the top were compared. Advantages arising from addition of the SiO2 layer are shown. The film was patterned in order to form an active waveguide. Waveguide loss and mode composition were investigated experimentally and theoretically. Spectrum and kinetics of luminescence in the region of 1.06 μm were measured.
Resumo:
We have proposed and demonstrated passive harmonic mode locking of an erbium doped fiber laser with soliton pulse shaping using carbon nanotubes polyvinyl alcohol film. Two types of samples prepared by using filtration and centrifugation were studied. The demonstrated fiber laser can support 10th harmonic order corresponding to 245 MHz repetition rate with an output power of ~12 mW. More importantly, all stable harmonic orders show timing jitter below 10 ps. The output pulses energies are between 25 to 56 pJ. Both samples result in the same central wavelength of output optical spectrum with similar pulse duration of ~1 ps for all harmonic orders. By using the same laser configuration, centrifugated sample exhibits slightly lower pulse chirp. © 2012 Optical Society of America.