13 resultados para barium bismuth tantalate
em Aston University Research Archive
Resumo:
The design and construction of a sputtering system for the deposition of barium titanate thin films is described. The growth and structure of barium titanate films deposited on a variety of substrates including amorphous carbon fi1ms, potassium bromide single crystals, and polycrystalline gold films has been studied. Films deposited on all substrates at room temperature were amorphous. Polycrystalline titanate films were formed on polycrystalline and amorphous substrates at temperatures above 450°C while films with a pronounced texture could be expitaxially deposited on single crystal potassium bromide above a temperature of only 200°C. Results of dielectric measurements made on the films are reported. Amorphous films were highly insulating (resistivities ~1014 ohm.cm with dielectric constants of between 10 and 20.
Resumo:
Lead bismuth eutectic (LBE) is a possible coolant for fast reactors and targets in spallation neutron sources. Its low melting point, high evaporation point, good thermal conductivity, low reactivity, and good neutron yield make it a safe and high performance coolant in radiation environments. The disadvantage is that it is a corrosive medium for most steels and container materials. This study was performed to evaluate the corrosion behavior of the austenitic stainless steel D9 in oxygen controlled LBE. In order to predict the corrosion behavior of steel in this environment detailed analyses have to be performed on the oxide layers formed on these materials and various other relevant materials upon exposure to LBE. In this study the corrosion/oxidation of D9 stainless steel in LBE was investigated in great detail. The oxide layers formed were characterized using atomic force microscopy, magnetic force microscopy, nanoindentation, and scanning electron microscopy with wavelength-dispersive spectroscopy (WDS) to understand the corrosion and oxidation mechanisms of D9 stainless steel in contact with the LBE. What was previously believed to be a simple double oxide layer was identified here to consist of at least 4 different oxide layers. It was found that the inner most oxide layer takes over the grain structure of what used to be the bulk steel material while the outer oxide layer consists of freshly grown oxides with a columnar structure. These results lead to a descriptive model of how these oxide layers grow on this steel under the harsh environments encountered in these applications.
Resumo:
This work revealed that the solid solution compounds of Sr 2-xBaxNb2O7 are promising lead-free materials for high-temperature piezoelectric sensor application. These compounds were confirmed as ferroelectric materials with high Curie points (> 900°C) by their piezoelectric activity after poling, ferroelectric domain switching in their P-E hysteresis loops and thermal depoling behavior. The effect of Ba substitution on the structure and properties of Sr 2-xBaxNb2O7 (x < 1.0) was investigated. The solid solution limit of Sr2-xBaxNb 2O7 was determined by XRD as x < 0.6. The a-, b-, c- axes, and cell volume increase with Ba addition. The textured ceramics of Sr2-xBaxNb2O7 were prepared for the first time. The highest d33 was measured as 3.6 ± 0.1 pC/N for Sr1.8Ba0.2Nb2O7. © 2012 The American Ceramic Society.
Resumo:
DUE TO COPYRIGHT RESTRICTIONS ONLY AVAILABLE FOR CONSULTATION AT ASTON UNIVERSITY LIBRARY AND INFORMATION SERVICES WITH PRIOR ARRANGEMENT
Resumo:
In this letter, we demonstrate an optically pumped semiconductor disk laser frequency doubled with a periodically poled lithium tantalate crystal. Crystals with various lengths were tested for intracavity frequency conversion. The semiconductor disk laser exploited GaInNAs-based active region with GaAsAlAs distributed Bragg mirror to produce emission at 1.2- μm wavelength. The frequency doubled power up to 760 mW at the wavelength of 610 nm was achieved with a 2-mm-long crystal. © 2010 IEEE.
Resumo:
In this paper, we investigate SHG efficiency dependency on crystal length. Four periodically-poled MgSLT crystals (PPMgSLT) of 2, 4, 11 and 25 mm in length were used, for intracavity frequency doubling of an optically-pumped GalnNAs semiconductor disk laser.
Resumo:
Intracavity frequency doubling of an optically pumped GaInNAs semiconductor disk laser by a periodically poled near-stoichiometric lithium tantalate crystal has been investigated. Stable second-harmonic generation at 610nm has been achieved with an output power of 730mW, limited only by the spectral acceptance range and Fresnel losses of the crystal. Spectral tuning of 8nm was realised with a Fabry-Pérot etalon. © The Institution of Engineering and Technology.
Resumo:
Grain size effects on the physical properties of polycrystalline ferroelectrics have been extensively studied for decades; however there are still major controversies regarding the dependence of the piezoelectric and ferroelectric properties on the grain size. Dense BaTiO3 ceramics with different grain sizes were fabricated by either conventional sintering or spark plasma sintering using micro- and nano-sized powders. The results show that the grain size effect on the dielectric permittivity is nearly independent of the sintering method and starting powder used. A peak in the permittivity is observed in all the ceramics with a grain size near 1μm and can be attributed to a maximum domain wall density and mobility. The piezoelectric coefficient d33 and remnant polarization Pr show diverse grain size effects depending on the particle size of the starting powder and sintering temperature. This suggests that besides domain wall density, other factors such as back fields and point defects, which influence the domain wall mobility, could be responsible for the different grain size dependence observed in the dielectric and piezoelectric/ferroelectric properties. In cases where point defects are not the dominant contributor, the piezoelectric constant d33 and the remnant polarization Pr increase with increasing grain size.