9 resultados para antiwear additives
em Aston University Research Archive
Resumo:
A homologous series of ultra-violet stabilisers containing 2-hydroxybenzophenone (HBP) moiety as a uv absorbing chromophore with varying alkyl chain lengths and sizes were prepared by known chemical synthesis. The strong absorbance of the HBP chromophore was utilized to evaluate the concentration of these stabilisers in low density polyethylene films and concentration of these stabilisers in low density polyethylene films and in relevant solvents by ultra-violet/visible spectroscopy. Intrinsic diffusion coefficients, equilibrium solubilities, volatilities from LDPE films and volatility of pure stabilisers were studied over a temperature range of 5-100oC. The effects of structure, molecular weight and temperature on the above parameters were investigated and the results were analysed on the basis of theoretical models published in the literature. It has been found that an increase in alkyl chain lengths does not change the diffusion coefficients to a significant level, while attachment of polar or branched alkyl groups change their value considerably. An Arrhenius type of relationship for the temperature dependence of diffusion coefficients seems to be valid only for a narrow temperature range, and therefore extrapolation of data from one temperature to another leads to a considerable error. The evidence showed that increase in additive solubility in the polymer is favoured by lower heat of fusions and melting points of additives. This implies the validity of simple regular solution theory to provide an adequate basis for understanding the solubility of additives in polymers The volubility of stabilisers from low density polyethylene films showed that of an additive from a polymer can be expressed in terms of a first-order kinetic equation. In addition the rate of loss of stabilisers was discussed in relation to its diffusion, solubility and volatility and found that all these factors may contribute to the additive loss, although one may be a rate determining factor. Stabiliser migration from LDPE into various solvents and food simulants was studied at temperatures 5, 23, 40 and 70oC; from the plots of rate of migration versus square root time, characteristic diffusion coefficients were obtained by using the solution of Fick's diffusion equations. It was shown that the rate of migration depends primarily on partition coefficients between solvent and the polymer of the additive and also on the swelling action of the contracting media. Characteristic diffusion coefficients were found to approach to intrinsic values in non swelling solvents, whereas in the case of highly swollen polymer samples, the former may be orders of magnitude greater than the latter.
Resumo:
A variety of iron compounds containing vinyl or thiol functional groups (used as photoactivators) have been synthesised and some of these were successfully bound to both polyethylene and polypropylene backbones during processing in the presence of peroxide and interlinking agent. Concentrates (masterbatches) of the photoactivators in PP and PE were prepared and the pro-oxidant effect of the diluted masterbatches in absence and presence of an antioxidant was evaluated. An antioxidant photoactivator (FeDNC ) was found to sensitise the photoactivity of pro-oxidants (Metone A / Metone M) whereas an antioxidant (ZnDNC) was found to stabilise the polymer (PP and PE) containing both of these combinations. It was observed that the lower concentration of FeDNC sensitises the stability of the polymer containing very small concentration of NiDNC whereas higher concentration of FeDNC stabilises the polymer (LDPE) containing same amount of NiDNC compared to FeDNC alone. The photostability of unstabilised PP containing FeAc could be varied by varying the concentration of ZnDEC. Both the induction period and the UV - life time of the polymer increased by increasing concentration of ZnDEC. It is suggested that ligand exchange reaction may take place between FeAc and ZnDNC. A polymer bound UV stabiliser (HAEB) and a thermal stabiliser (DBBA) were used with a non extractable photoactivator (FeAc) in PP. Small concentrations of the stabilisers (HAEB and DBBA) in combination with the photoactivator (FeAc) sensitise the polymer. The antioxidant present in commercial polymer (LDPE and PP) was found to be of a hindered phenol type, which was found to antagonise with ZnDNC when used in combination with the photoactivators.
Resumo:
The decomposition of drugs in the solid state has been studied using aspirin and salsalate as models. The feasibility of using suspension systems for predicting the stability of these drugs in the solid state has been investigated.. It has been found that such systems are inappropriate in defining the effect of excipients on 'the decomposition of the active drug due to chqnges in the degradation pathway. Using a high performance liquid chromatographic method, magnesium stearate was shown to induce the formation of potentlally immunogenic products in aspirin powders. These products which included salicylsalicylic acid .and acetylsalicyclsalicylic acid were not detected in aspirin suspensions which had undergone the same extent of decomposition. By studying the effect of pH and of added excipients on the rate of decomposition of aspirin in suspension systems, it has been shown that excipients such as magnesium stearate containing magnesium oxide, most probably enhance the decomposition of both aspirin and salsalate by alkalinising the aqueous phase. In the solid state, pH effects produced by excipients appear to be relatively unimportant. Evidence is presented to suggest that the critical parameter is a depression in melting point induced by: the added excipient. Microscopical examination in fact showed the formation of clear liquid layers in aspirin samples containing added magnesium stearate but not in control samples. Kinetic equations which take into account both the diffusive barrier presented by the liquid films and the. geometry of the aspirin crystals were developed. Fitting of the .experimental data to these equations showed good agreement. with the postulated theory. Monitorjng of weight issues during the decomposition of aspirin revealed that in the solid systems studied where the bulk of the decomposition product sublimes, it is possible to estimate the extent of degradation from the residual weight, provided the initial weight is known. The corollary is that in such open systems, monitoring of decomposition products is inadequate for assessing the extent of decomposition. In addition to the magnesium stearate-aspirin system, mapyramine maleate-aspirin mixtures were used to model interactive systems. Work carried out in an attempt to stabilise such systems included microencapsulation and film coating. The protection obtained was dependent on the interactive species used. Gelatin for example appeared to stabilise aspirin against the adverse effects of magnesium stearate but increased its decomposition in the presence of mapyramine maleate.