Limitations in the performance of coherent transmission systems employing digital back-propagation due to four-wave mixing impairments are reported for the first time. A significant performance constraint is identified, originating from four-wave mixing between signals and amplified spontaneous emission noise which induces a linear increase in the standard deviation of the received field with signal power, and linear dependence on transmission distance.
Resumo:
We report the performance of coherently-detected nine-channel WDM transmission over high dispersion fibers, using polarization multiplexed m-ary quadrature amplitude modulation (m = 4, 16, 64, 256) at 112 Gbit/s. Compensation of fiber nonlinearities via digital back-propagation enables up to 10 dB improvement in maximum transmittable power and similar to 8 dB Q(eff) improvement which translates to a nine-fold enhancement in transmission reach for PM-256QAM, where the largest improvements are associated with higher-order modulation formats. We further demonstrate that even under strong nonlinear distortion the transmission reach only reduces by a factor of similar to 2.5 for a 2 unit increase in capacity (log(2)m) when full band DBP is employed, in proportion to the required back-to-back OSNR.
Resumo:
We quantify the benefits of intra-channel nonlinear compensation in meshed optical networks, in view of network configuration, fibre design aspect, and dispersion management. We report that for a WDM optical transport network employing flexible 28Gbaud PM-mQAM transponders with no in-line dispersion compensation, intrachannel nonlinear compensation, for PM-16QAM through traffic, offers significant improvements of up to 4dB in nonlinear tolerance (Q-factor) irrespective of the co-propagating modulation format, and that this benefit is further enhanced (1.5dB) by increasing local link dispersion. For dispersion managed links, we further report that advantages of intra-channel nonlinear compensation increase with in-line dispersion compensation ratio, with 1.5dB improvements after 95% in-line dispersion compensation, compared to uncompensated transmission. © 2012 Optical Society of America.
Resumo:
Tensile strengths, impact energies, and fracture toughness data are presented for pure Fe-0.5 C, Astaloy A with 0.2 and 0.6%C, and for Distaloy AB-0.6%C at relative densities of about 0.9, achieved by conventional pressing and sintering, and at close to 1.0, achieved by powder forging. At low relative density, properties are controlled by sizes of sinter necks; it is postulated that toughness scales as (x/a)4, x/a being the ratio of neck diameter to particle diameter. At high relative density, microvoid coalescence and good toughness is observed for low strength microstructures whereas cleavage and poor toughness is a concomitant of high strength.
Resumo:
Mechanisms of fatigue crack growth have been studied for a range of PM steels at relative densities of 0.90 and 1.0, for which strength, fracture toughness, and microstructural information was also available. It is shown that the Paris exponents for steady state crack growth are between 8 and 18 when ρr is approximately 0.9 but when ρr is approximately 1.0 the exponents are between 2.6 and 4.0, i.e in the range typical of wrought steels (2-4). At both densities, threshold stress intensities are between 5.5 and 10.8 MPa m1/2 when R = 0.1. Combinations of these thresholds and yield strengths are comparable with those for wrought steels. When R = 0.8, reductions in threshold to between 2.7 and 5 MPa m1/2 are attributed to crack closure effects. At ρr = 0.90, Fe-0.5C fails by progressive rupture of sinter necks. Astaloy A, with 0.2%C and 0.6%C, and Distaloy AB-0.6C have smaller plastic zone sizes and the cracks follow more difficult paths through particles as well as necks. When ρr is approximately 1.0, fracture is partially by true fatigue modes and partly by cleavage, the bursts of cleavage being more noticeable when Kmax is high.
Resumo:
The ageing response of 2124 Al-SiC particulate metal-matrix composite (MMC) and unreinforced alloy has been examined using hardness measurements and Arrhenius analysis. The formation of phases during precipitation has been studied using differential scanning calorimetry (DSC). The MMC exhibits accelerated ageing compared to unreinforced alloy, due to enhanced S′ formation. The activation energy for diffusion is lower in the MMC than in the unreinforced alloy. DSC scans show Guinier-Preston B (GPB) zone nucleation to occur at a lower temperature in the MMC, whilst the total volume of GPB zones formed is smaller than in the unreinforced alloy. A model has been proposed to explain the GPB zone formation behaviour, in which ease of GPB zone nucleation varies within the MMC, as a function of ageing time and of position within the matrix. S′ formation is enhanced in the MMC because of improved diffusion and a large increase in density of heterogeneous nucleation sites compared to the unreinforced alloy. © 1994 Chapman & Hall.
Resumo:
We use the GN-model to assess Nyquist-WDM 100/200Gbit/s PM-QPSK/16QAM signal reach on low loss, large core area fibre using extended range, variable gain hybrid Raman-EDFAs. 5000/1500km transmission is possible over a wide range of amplifier spans. © OSA 2014.
Resumo:
We report all-fibre Lyot filters formed by concatenating fibre gratings with structure tilted at 45° UV-inscribed in PM fibre. Such polarisation filters exhibit distinct transmission property for potential application in fibre lasers and sensors. © 2012 OSA.
Resumo:
Permanent-magnet (PM) synchronous machines (PMSMs) can provide excellent performance in terms of torque density, energy efficiency, and controllability. However, PMs on the rotor are prone to centrifugal force, which may break their physical integrity, particularly at high-speed operation. Typically, PMs are bound with carbon fiber or retained by alloy sleeves on the rotor surface. This paper is concerned with the design of a rotor retaining sleeve for a 1.12-MW 18-kr/min PM machine; its electromagnetic performance is investigated by the 2-D finite-element method (FEM). Theoretical and numerical analyses of the rotor stress are carried out. For the carbon fiber protective measure, the stresses of three PM configurations and three pole filler materials are compared in terms of operating temperature, rotor speed, retaining sleeve thickness, and interference fit. Then, a new hybrid protective measure is proposed and analyzed by the 2-D FEM for operational speeds up to 22 kr/min (1.2 times the rated speed). The rotor losses and machine temperatures with the carbon fiber retaining sleeve and the hybrid retaining sleeve are compared, and the sleeve design is refined. Two rotors using both designs are prototyped and experimentally tested to validate the effectiveness of the developed techniques for PM machines. The developed retaining sleeve makes it possible to operate megawatt PM machines at high speeds of 22 kr/min. This opens doors for many high-power high-speed applications such as turbo-generator, aerospace, and submarine motor drives.