Hirota et al. [6] found that the magneto-Archimedes force could be used to levitate biological materials at different heights in pressurized oxygen, providing the possibility to separate them. However the magnetic levitation of mineral particles has not been widely explored. With this in mind some preliminary experiments were performed by levitating pure mineral materials in a paramagnetic solution manganese (II) chloride. Besides the report of levitation heights of various mineral particles in manganese (II) chloride solution, the lines obtained from the basic formula provided by previous researchers were compared with experimental data. The act of cryogenic paramagnetic fluid in the magneto-Archimedes levitation was also demonstrated. The obtained results are compared with the same particle levitation heights in manganese (II) chloride solution. © 2014 Elsevier B.V.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The surfaces of iron-containing sulphide minerals were oxidised by a range of inorganic oxidants, and the resultant surface alteration products studied using various spectroscopic techniques. The characterisation of surface oxidation is relevant to the alteration of ores in nature and their behaviour during flotation and leaching, of importance to the metallurgical industry. The sulphides investigated included pyrite (FeS2), hexagonal pyrrhotine (Fe9S10), monoclinic pyrrhotine (Fe7Se), violarite (FeNi2S4), pentlandite ((FeiNi)9Se), chalcopyrite (CuFeS2) and arsenopyrite (FeAsS). The surfaces were oxidised by various methods including acid (sulphuric), alkali (ammonium hydroxide), hydrogen peroxide, steam, electrochemical and air/oxygen (in a low-temperature (150ºC) furnace), The surfaces were examined using surface sensitive chemical spectroscopic methods including x-ray photoelectron spectroscopy (ms), Auger electron spectroscopy (LES) and conversion electron Mössbauer spectroscopy (CEKS). Physical characterisation of the surfaces was undertaken using scanning electron microscopy (SM), spectral reflectance measurements and optical microscopy. Bulk characterisation of the sulphide minerals was undertaken using x-ray diffraction and electron microprobe techniques. Observed phases suggested to form in most of the sulphide surfaces include Fe204, Fe1-x0, Fe202, Fe00H, Fe(OH)3, with iron II & III oxy-sulphates. The iron sulphides show variable extents of oxidation, indicating pyrite to be the most stable. Violarite shows stability to oxidation, suggested to result from both its stable spinel crystal structure, and from the rapid formation of sulphur at the surface protecting the sub-surface from further oxidation. The phenomenon of sub-surface enrichment (in metals), forming secondary sulphides, is exhibited by pentlandite and chalcopyrite, forming violarite and copper sulphides respectively. The consequences of this enrichment with regard to processing and leaching are discussed. Arsenopyrite, often a hindrance in ore processing, exhibits the formation of arsenic compounds at the surface, the dissolution of which is discussed in view of the possible environmental hazard caused by the local pollution of water systems. The results obtained allow a characterisation of the sulphides in terms of their relative stability to oxidation, and an order of stability of the sulphide surfaces is proposed. Models were constructed to explain the chemical compositions of the surfaces, and the inter-relationships between the phases determined at the surface and in the sub-surface. These were compared to the thermo-chemically predicted phases shown in Eh/pH and partial pressure diagrams! The results are discussed, both in terms of the mineralogy and geochemistry of natural ores, and the implications for extraction and processing of these ore minerals.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Modern electron optical techniques together with X-ray and mineralogical examination have been used to study the occurrence and form of phosphorus bearing minerals in iron ores. Three ores have been studied - Bahariya and Aswan from Egypt and Frodingham ironstone from U.K. The iron in the Bahariya iron ore is mainly as hematite and goethite. The gangue minerals are halite, gypsum, barytes, quartz and calcite. Iron content is between 49.8 to 63.2% and phosphorus 0.14 to 0.34%. The phosphorus occurs as very fine particles of apatite which are distributed throughout the ore. Removal of the phosphorus would require very fine grinding followed by acid leaching. Aswan iron ore is an oolitic iron ore; the iron content between 41-57% and phosphorus content 0.1 to 2.9%. It is mainly hematitic with variable quantities of quartz, apatite and small amount of clay minerals. In the oolitic iron ore beds, apatite occurs in the hematite matrix; filling in the pores of the oolithic surfaces, or as matrix cementing the ooliths with the hematite grains. In sandstone claybeds the distribution of the apatite is mainly in the matrix. It is suggested that the liberation size for the apatite would be -80 m and flotation concentration could be applied for the removal of apatite from Aswan ore. Frodingham ironstone occurs in the lower Jurassic bed of the South Humberside area. The average iron content is 25% and the phosphorus is 0.32%. Seven mineral phases were identified by X-ray; calcite, quartz, chamosite, hematite, siderite, apatite, and chlorite. Apatite occurs as very fine grains in the hematite and chamosite ooliths; as matrix of fine grains intergrown with chamosite and calcite grains; and as anhedral and sub rounded grains in the ooliths (8-28 m). It is suggested that two processes are possible for the dephosphorisation; the Flox process or a reduction roast followed by fine grinding, magnetic separation, and acid leaching.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The thesis examines the possibilities for the beneficiation of steel making slags by using mineral processing methods. Chemical and Mineralogical investigations have been carried out by SEM and EP}ffi to determine the most suitable separation methods in terms of crystal size, chemical composition and surface properties. Magnetic separation was applied in connection with size reductions for the extraction of the metallic iron prills and other iron containing phases and the results were related to the feed size and operating conditions. The behaviour of the slags in flotation tests was studied with respect to the recovery and grade. It was found that the free lime presence in the slags caused a high acid consumption of both weak and strong acids. It also reacted with acids and consequently produced a white precipitate, (CaS04 for H2 S04 ). The poor response of the phases to the flotation by different types of collector was found to be due to surface alteration caused by the free lime. The flocculation tests were carried out at the natural pH of the slags to prevent surface alterations. Settling tests were done to determine the suitable flocculants for the separation tests. The effect of the settling period, flocculant concentration, conditioning period and number of cleaning cycles were determined to optimize the separation tests. The discussion brings together this study with previous theoretically based work cited in the literature to elucidate the factor5governing the utilisation of steel making slags.