6 resultados para DIELECTRIC-RELAXATION
em Aston University Research Archive
Resumo:
The conformational characteristics of poly(dimethylsilmethylene), poly(dimethylsilethene), poly(dimethylsilethane) and a related material, poly(2,2,5,5-tetramethyl-1-oxa-2,5-disilapentane), have been investigated using the method of molecular mechanics. In this method, a quantitative analysis of the factors affecting the nature and magnitude of the bond rotation potentials governing their conformational behaviour has been undertaken. Along with their structural data, the results obtained were employed to calculate a variety of conformationally-dependent properties for these polymers, including the characteristic ratio, the dipole moment ratio and the mean-square radius of gyration. In addition, the dielectric relaxation behaviour of two samples of poly(2,2,5,5-tetramethyl-1-oxa-2,5-disilapentane) with molar masses Mw = 28000 and Mw = 46000 respectively, have been studied as a function of temperature (179K-205K) and frequency (100-105Hz). Activation energies for the α-relaxation process and Davidson-Cole empirical distribution factors have been calculated.
Resumo:
The dielectric relaxation behaviour of a series of cyclic and linear poly(dimethylsiloxanes) with overline nn in the range 28 to 99 has been studied, as a function of temperature (142.0K-157.5K) and frequency (12-105Hz). Activation energies for the -relaxation process, Davidson-Cole empirical distribution factors, , and mean-square dipole moments per repeat unit, < 2> , have been calculated. Differences in values of H_act reflected restricted dipolar rotation for the cyclic structures, compared to the linear structures, over the range of molecular weights studied. The dielectric relaxation behaviour of a series of linear oligomers of methyl phenyl siloxane, with n in the range 4 to 10, a series of linear fractions of poly(methyl phenyl siloxane), with overline n_n in the range 31 to 1370, and a cyclic oligomer of mehyl phenyl siloxane, with n = 10, has been studied as a function of temperature (155.5K-264.0K) and frequency (12-105Hz). Activation energies for the -relaxation process, Davidson-Cole and Cole-Cole empirical distribution factors, and , respectively, and mean-square dipole moments per repeat unit have been calculated. The reduced flexibility of short methyl phenyl siloxane chains, compared to dimethyl siloxane chains, was apparent from a comparison of dipole moment ratios. The dilectric relaxation behaviour of poly(methyl hydrogen siloxane) and poly(n-hexyl methyl siloxane) has been studied as a function of temperature and frequency. A polysiloxane liquid crystal has been synthesised and its dielectric relaxation behaviour has been studied, as a function of temperature and frequency, in the liquid crystalline phase and below T_g. Poly(p-phenylene vinylene) and related oligomers have been synthesised and characterised by a variety of experimental techniques. The Kerr effect of two oligomeric fractions, in solution in PPG 2025, has been measured. The electrical conductivities of the undoped and I_2-doped polymer and oligomers have been measured.
Resumo:
Charge transport and dielectric measurements were carried out on compacted powder and single-crystal samples of bistable RbxMn[Fe(CN)6]y·zH2O in the two valence-tautomeric forms (MnIIFeIII and MnIIIFeII) as a function of temperature (120-350 K) and frequency (10-2-106 Hz). The complex conductivity data reveal universal conductivity behavior and obey the Barton-Nakajima-Namikawa relationship. The charge transport is accompanied by dielectric relaxation that displays the same thermal activation energy as the conductivity. Surprisingly, the activation energy of the conductivity was found very similar in the two valence-tautomeric forms (0.55 eV), and the conductivity change between the two phases is governed mainly by the variation of the preexponential factor in each sample. The phase transition is accompanied by a large thermal hysteresis of the conductivity and the dielectric constant. In the hysteresis region, however, a crossover occurs in the charge transport mechanism at T < 220 K from an Arrhenius-type to a varying activation energy behavior, conferring an unusual “double-loop” shape to the hysteresis.
Resumo:
The dielectric properties of pure low to medium molecular weight poly(ethylene glycol) and poly(propylene glycol) and a variety of their salt complexes have been studied through the measurement of the dielectric permittivity and dielectric loss over a range of frequency and temperature. The major proportion of this study has been concerned with the examination of the nature of the interaction between mercuric chloride and poly(propylene glycol) (PPG). Other salt-poly-ether combinations have also been considered such as cobalt chloride-PPG cadmium chloride-PPG zinc chloride-PPG and ferric chloride-PEG (polyethylene glycol). Some of this work was also supported by chemical shift and spin-lattice Nuclear Magnetic Resonance (N.M.R.) spectroscopy. The dielectric permittivity data were analysed using the Onsager relation to calculate the mean dipole moment per dipolar unit. This approach was employed in the discussion of various models proposed for the structure of salt-polyether complexes. The effect of mercuric chloride on the statistical conformations of poly(propylene-glycol) was studied in a quantitative manner using the relationships of marchal-Benoit. The dielectric relaxation activation energy and mean energy difference between gauche and trans conformations of poly(propylene glycol) in the presence of mercuric chloride, both showed a distinct minimum when the concentration of mercuric chloride was close to 5 mole %. Opposite behaviour was observed for the Cole-Cole parameter. It was concluded that the majority of the dielectric data could be rationalised in terms of a 5-membered cyclic complex formed between mercuric chloride and PPG in which the complexed segment of the polyether-(OMeCH2CH2O)- adopted either gauche or cis conformations.
Resumo:
A new bridge technique for the measurement of the dielectric absorption of liquids and solutions at microwave frequencies has been described and its accuracy assessed. 'l'he dielectric data of the systems studied is discussed in terms of the relaxation processes contributing to the dielectric absorption and the apparent dipole moments. Pyridine, thiophen and furan in solution have a distribution of relaxation times which may be attributed to the small size of the solute molecules relative to the solvent. Larger rigid molecules in solution were characterized by a single relaxation time as would be anticipated from theory. The dielectric data of toluene, ethyl-, isopropyl- and t-butylbenzene as pure liquids and in solution were described by two relaxation times, one identified with molecular re-orientation and a shorter relaxation time.· The subsequent work was investigation of the possible explanations of this short relaxation process. Comparable short relaxation times were obtained from the analysis of the dielectric data of solutions of p-chloro- and p-bromotoluene below 40°C, o- and m-xylene at 25°C and 1-methyl- and 2 methylnaphthalene at 50 C. Rigid molecules of similar shapes and sizes were characterized by a single relaxation time identified with molecular re-orientation. Contributions from a long relaxation process attributed to dipolar origins were reported for solutions of nitrobenzene, benzonitrile and p-nitrotoluene. A short relaxation process of possible dipolar origins contributed to the dielectric absorption of 4-methyl- and 4-t-butylpyridine in cyclohexane at 25°C. It was concluded that the most plausible explanation of the short relaxation process of the alkyl-aryl hydrocarbons studied appears to be intramolecular relaxation about the alkyl-aryl bond. Finally the mean relaxation times of some phenylsubstituted compounds were investigated to evaluate any shortening due to contributions from the process of relaxation about the phenyl-central atom bond. The relaxation times of triphenylsilane and phenyltrimethylsilane were significantly short.
Resumo:
A variety of methods have been reviewed for obtaining parallel or perpendicular alignment in liquid-crystal cells. Some of these methods have been selected and developed and were used in polarised spectroscopy, dielectric and electro-optic studies. Also, novel dielectric and electro-optic cells were constructed for use over a range of temperature. Dielectric response of thin layers of E7 and E8 (eutectic mixture liquid-crystals) have been measured in the frequency range (12 Hz-100 kHz) and over a range of temperature (183-337K). Dielectric spectra were also obtained for supercooled E7 and E8 in the Hz and kHz range. When the measuring electric field was parallel to the nematic director, one loss peak (low-frequency relaxation process) was observed for E7 and for E8, that exhibits a Debye-type behaviour in the supercooled systems. When the measuring electric field was perpendicular to the nematic director, two resolved dielectric processes have been observed. The phase transitions, effective molecular polarisabilities, anisotropy of polarisabilities and order parameters of three liquid crystal homologs (5CB, 6CB, and 7CB), 60CB and three eutectic nematic mixtures E7, E8, and E607 were calculated using optical and density data measured at several temperatures. The order parameters calculated using the different methods of Vuks, Neugebauer, Saupe-Maier, and Palffy-Muhoray are nearly the same for the liquid crystals considered in the present study. Also, the interrelationship between density and refractive index and the molecular structure of these liquid crystals were established. Accurate dielectric and dipole results of a range of liquid-crystal forming molecules at several temperatures have reported. The role of the cyano-end group, biphenyl core, and flexible tail in molecular association, were investigated using the dielectric method for some molecules which have a structural relationship to the nematogens. Analysis of the dielectric data for solution of the liquid-crystals indicated a high molecular association, comparable to that observed in the nematic or isotropic phases. Electro-optic Kerr effect were investigated for some alkyl cyanobiphenyls, their nematic mixtures and the eutectic mixture liquid-crystals E7 and E8 in the isotropic phase and solution. The Kerr constant of these liquid crystals found to be very high at the nematic-isotropic transition temperatures as the molecules are expected to be highly ordered close to phase transition temperatures. Dynamic Kerr effect behaviour and transient molecular reorientation were also observed in thin layers of some alkyl cyanobiphenyls. Dichroic ratio R and order parameters of solutions containing some azo and anthraquinone dyes in the nematic solvent (E7 and E8), were investigated by the measurement of the intensity of the absorption bands in the visible region of parallel aligned samples. The effective factors on the dichroic ratio of the dyes dissolved in the nematic solvents were determined and discussed.