A systematic survey of the possible methods of chemical extraction of iron by chloride formation has been presented and supported by a comparable study of :feedstocks, products and markets. The generation and evaluation of alternative processes was carried out by the technique of morphological analysis vihich was exploited by way of a computer program. The final choice was related to technical feasibility and economic viability, particularly capital cost requirements and developments were made in an estimating procedure for hydrometallurgjcal processes which have general applications. The systematic exploration included the compilation of relevant data, and this indicated a need.to investigate precipitative hydrolysis or aqueous ferric chloride. Arising from this study, two novel hydrometallurgical processes for manufacturing iron powder are proposed and experimental work was undertaken in the following .areas to demonstrate feasibility and obtain basic data for design purposes: (1) Precipitative hydrolysis of aqueous ferric chloride. (2) Gaseous chloridation of metallic iron, and oxidation of resultant ferrous chloride. (3) Reduction of gaseous ferric chloride with hydrogen. (4) Aqueous acid leaching of low grade iron ore. (5) Aqueous acid leaching of metallic iron. The experimentation was supported by theoretical analyses dealing with: (1) Thermodynamics of hydrolysis. (2) Kinetics of ore leaching. (3) Kinetics of metallic iron leaching. (4) Crystallisation of ferrous chloride. (5) Oxidation of anhydrous ferrous chloride. (6) Reduction of ferric chloride. Conceptual designs are suggested fbr both the processes mentioned. These draw attention to areas where further work is necessary, which are listed. Economic analyses have been performed which isolate significant cost areas, und indicate total production costs. Comparisons are mode with previous and analogous proposals for the production of iron powder.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Modern electron optical techniques together with X-ray and mineralogical examination have been used to study the occurrence and form of phosphorus bearing minerals in iron ores. Three ores have been studied - Bahariya and Aswan from Egypt and Frodingham ironstone from U.K. The iron in the Bahariya iron ore is mainly as hematite and goethite. The gangue minerals are halite, gypsum, barytes, quartz and calcite. Iron content is between 49.8 to 63.2% and phosphorus 0.14 to 0.34%. The phosphorus occurs as very fine particles of apatite which are distributed throughout the ore. Removal of the phosphorus would require very fine grinding followed by acid leaching. Aswan iron ore is an oolitic iron ore; the iron content between 41-57% and phosphorus content 0.1 to 2.9%. It is mainly hematitic with variable quantities of quartz, apatite and small amount of clay minerals. In the oolitic iron ore beds, apatite occurs in the hematite matrix; filling in the pores of the oolithic surfaces, or as matrix cementing the ooliths with the hematite grains. In sandstone claybeds the distribution of the apatite is mainly in the matrix. It is suggested that the liberation size for the apatite would be -80 m and flotation concentration could be applied for the removal of apatite from Aswan ore. Frodingham ironstone occurs in the lower Jurassic bed of the South Humberside area. The average iron content is 25% and the phosphorus is 0.32%. Seven mineral phases were identified by X-ray; calcite, quartz, chamosite, hematite, siderite, apatite, and chlorite. Apatite occurs as very fine grains in the hematite and chamosite ooliths; as matrix of fine grains intergrown with chamosite and calcite grains; and as anhedral and sub rounded grains in the ooliths (8-28 m). It is suggested that two processes are possible for the dephosphorisation; the Flox process or a reduction roast followed by fine grinding, magnetic separation, and acid leaching.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A novel route to prepare highly active and stable N2O decomposition catalysts is presented, based on Fe-exchanged beta zeolite. The procedure consists of liquid phase Fe(III) exchange at low pH. By varying the pH systematically from 3.5 to 0, using nitric acid during each Fe(III)-exchange procedure, the degree of dealumination was controlled, verified by ICP and NMR. Dealumination changes the presence of neighbouring octahedral Al sites of the Fe sites, improving the performance for this reaction. The so-obtained catalysts exhibit a remarkable enhancement in activity, for an optimal pH of 1. Further optimization by increasing the Fe content is possible. The optimal formulation showed good conversion levels, comparable to a benchmark Fe-ferrierite catalyst. The catalyst stability under tail gas conditions containing NO, O2 and H2O was excellent, without any appreciable activity decay during 70 h time on stream. Based on characterisation and data analysis from ICP, single pulse excitation NMR, MQ MAS NMR, N2 physisorption, TPR(H2) analysis and apparent activation energies, the improved catalytic performance is attributed to an increased concentration of active sites. Temperature programmed reduction experiments reveal significant changes in the Fe(III) reducibility pattern with the presence of two reduction peaks; tentatively attributed to the interaction of the Fe-oxo species with electron withdrawing extraframework AlO6 species, causing a delayed reduction. A low-temperature peak is attributed to Fe-species exchanged on zeolitic AlO4 sites, which are partially charged by the presence of the neighbouring extraframework AlO6 sites. Improved mass transport phenomena due to acid leaching is ruled out. The increased activity is rationalized by an active site model, whose concentration increases by selectively washing out the distorted extraframework AlO6 species under acidic (optimal) conditions, liberating active Fe species.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A series of zirconium phosphate supported WOx solid acid catalysts with W loadings from 1–25 wt% have been prepared on high surface area zirconium phosphate by a surface grafting method. Catalysts were characterized by N2 adsorption, FTIR, Raman, UV-Vis, 31P MAS NMR, pyridine TPD and X-ray methods. Spectroscopic measurements suggest a Keggin-type structure forms on the surface of zirconium phosphate as a ([triple bond, length as m-dash]ZrOH2+)(ZrPW11O405−) species. All catalysts show high activity in palmitic acid esterification with methanol. These materials can be readily separated from the reaction system for re-use, and are resistant to leaching of the active heteropolyacid, suggesting potential industrial applications in biodiesel synthesis. © The Royal Society of Chemistry 2006.