It has been observed in various practical applications that data do not conform to the normal distribution, which is symmetric with no skewness. The skew normal distribution proposed by Azzalini(1985) is appropriate for the analysis of data which is unimodal but exhibits some skewness. The skew normal distribution includes the normal distribution as a special case where the skewness parameter is zero. In this thesis, we study the structural properties of the skew normal distribution, with an emphasis on the reliability properties of the model. More specifically, we obtain the failure rate, the mean residual life function, and the reliability function of a skew normal random variable. We also compare it with the normal distribution with respect to certain stochastic orderings. Appropriate machinery is developed to obtain the reliability of a component when the strength and stress follow the skew normal distribution. Finally, IQ score data from Roberts (1988) is analyzed to illustrate the procedure.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The deformation behavior of atomically clean, nanometer sized tungsten / gold contacts was studied at room temperature in ultra-high vacuum. An instrument that combines atomic force microscopy (AFM), scanning tunneling microscopy (STM), and field ion microscopy (FIM) into a single experimental apparatus was designed, constructed, and calibrated. A cross-hair force sensor having a spring constant of - 442 N/m was developed and its motion was monitored during indentation experiments with a differential interferometer. Tungsten tips of controlled size (12.8 nm < tip radius < 2 1.6 nm) were first shaped and characterized using FIM and then indented into a Au (1 10) single crystal to depths ranging from 1.5 nrn to 18 nm using the force sensor. Continuum mechanics models were found to be valid in predicting elastic deformation during initial contact and plastic zone depths despite our small size regime. Multiple discrete yielding events lasting < 1.5 ms were observed during the plastic deformation regime; at the yield points a maximum value for the principal shear stress was measured to be 5 + 1 GPa. During tip withdrawal, "pop-out" events relating to material relaxation within the contact were observed. Adhesion between the tip and sample led to experimental signatures that suggest neck formation prior to the break of contact. STM images of indentation holes revealed various shapes that can be attributed to the (1 1 1 ) (1 10) crystallographic slip system in gold. FIM images of the tip after indentation showed no evidence of tip damage